1 0.21 0.05 0.66 0.002 0.007 0.75 2.11 0.83 0.31 0 0.62 0 0 0 5 -0.00128 0 6 -0.001317 0.6738 6 -0.001317 1.348 6 -0.001317 2.021 6 -0.00133 2.695 6 -0.001305 3.369 7 -0.001305 4.043 7 -0.001305 4.717 7 -0.001305 5.391 7 -0.001293 6.064 7 -0.001305 6.738 7 -0.001293 7.412 7 -0.001317 8.086 7 -0.001317 8.76 7 -0.00133 9.434 7 -0.001342 10.11 7 -0.001317 10.78 7 -0.001317 11.46 7 -0.001305 12.13 8 -0.001293 12.8 7 -0.001293 13.48 8 -0.001305 14.15 7 -0.001317 14.82 8 -0.00128 15.5 9 -0.001293 16.17 9 -0.001293 16.85 11 -0.001256 17.52 13 -0.001219 18.19 15 -0.001231 18.87 16 -0.001219 19.54 17 -0.001194 20.21 18 -0.001169 20.89 19 -0.001144 21.56 19 -0.001144 22.24 20 -0.001132 22.91 20 -0.00112 23.58 20 -0.00112 24.26 21 -0.001157 24.93 22 -0.00112 25.61 22 -0.001095 26.28 23 -0.001082 26.95 23 -0.001082 27.63 24 -0.001082 28.3 26 -0.001095 28.97 27 -0.001095 29.65 27 -0.001082 30.32 27 -0.001045 31 28 -0.001058 31.67 29 -0.001033 32.34 29 -0.001021 33.02 30 -0.001021 33.69 30 -0.0009959 34.37 31 -0.001021 35.04 33 -0.0009959 35.71 33 -0.0009711 36.39 34 -0.0009711 37.06 34 -0.0009587 37.73 35 -0.000934 38.41 36 -0.0009216 39.08 36 -0.0008969 39.76 37 -0.0009093 40.43 38 -0.0008969 41.1 38 -0.0008969 41.78 39 -0.0008721 42.45 40 -0.0008721 43.13 41 -0.0008969 43.8 41 -0.0008721 44.47 42 -0.0008721 45.15 42 -0.0008474 45.82 43 -0.0008598 46.49 44 -0.000835 47.17 44 -0.0008227 47.84 45 -0.0008103 48.52 46 -0.0008227 49.19 46 -0.000835 49.86 47 -0.0008474 50.54 48 -0.0008227 51.21 48 -0.0008103 51.88 49 -0.0007979 52.56 49 -0.000835 53.23 50 -0.0007732 53.91 52 -0.0007732 54.58 52 -0.0007484 55.25 52 -0.0007237 55.93 53 -0.0007113 56.6 54 -0.0007237 57.28 55 -0.0007237 57.95 55 -0.0006742 58.62 55 -0.0006618 59.3 56 -0.0006866 59.97 58 -0.0006742 60.64 58 -0.0006618 61.32 59 -0.0006495 61.99 59 -0.0006495 62.67 60 -0.0006371 63.34 61 -0.0006247 64.01 61 -0.0006 64.69 63 -0.0005752 65.36 63 -0.0005629 66.04 63 -0.0005752 66.71 64 -0.0005752 67.38 65 -0.0005752 68.06 66 -0.0005629 68.73 66 -0.0005629 69.4 66 -0.0005258 70.08 67 -0.0005134 70.75 68 -0.0005258 71.43 69 -0.0005134 72.1 70 -0.0005134 72.77 70 -0.000501 73.45 71 -0.0004763 74.12 72 -0.000501 74.8 72 -0.0004763 75.47 73 -0.0004639 76.14 73 -0.0004763 76.82 74 -0.0004268 77.49 75 -0.0004392 78.16 76 -0.0004268 78.84 77 -0.0004268 79.51 77 -0.0004144 80.19 78 -0.0003897 80.86 79 -0.0003897 81.53 80 -0.0004021 82.21 81 -0.0004021 82.88 81 -0.0004268 83.55 81 -0.0003897 84.23 82 -0.0003649 84.9 83 -0.0003526 85.58 83 -0.0003278 86.25 84 -0.0003278 86.92 84 -0.0003155 87.6 85 -0.0003031 88.27 86 -0.0003031 88.95 87 -0.0002783 89.62 87 -0.0002536 90.29 88 -0.0002536 90.97 88 -0.000266 91.64 89 -0.000266 92.31 90 -0.0002536 92.99 91 -0.0002536 93.66 91 -0.0002289 94.34 92 -0.0002412 95.01 93 -0.0002289 95.68 94 -0.0002289 96.36 94 -0.0002289 97.03 95 -0.0002041 97.71 95 -0.000167 98.38 96 -0.0001794 99.05 97 -0.0001546 99.73 98 -0.0002907 100.4 98 -0.0002041 101.1 98 -0.0001917 101.7 100 -0.000167 102.4 101 -0.0001052 103.1 101 -0.0002041 103.8 102 -0.0002041 104.4 102 -0.0001546 105.1 103 -0.0001299 105.8 104 -0.0001299 106.5 104 -0.0001794 107.1 105 -0.0001423 107.8 106 -8.041e-05 108.5 106 -6.804e-05 109.2 107 -8.041e-05 109.8 108 -5.567e-05 110.5 109 -4.33e-05 111.2 109 -3.093e-05 111.9 110 -3.093e-05 112.5 110 -3.093e-05 113.2 111 6.185e-06 113.9 112 6.185e-06 114.6 112 6.185e-06 115.2 113 6.185e-06 115.9 113 6.185e-06 116.6 114 -1.856e-05 117.2 115 -1.856e-05 117.9 116 6.185e-06 118.6 116 6.185e-06 119.3 117 6.185e-06 119.9 117 6.185e-06 120.6 118 6.185e-06 121.3 119 6.185e-06 122 120 6.185e-06 122.6 120 6.185e-06 123.3 121 6.185e-06 124 121 6.185e-06 124.7 123 6.185e-06 125.3 123 6.185e-06 126 123 6.185e-06 126.7 124 6.185e-06 127.4 125 6.185e-06 128 126 6.185e-06 128.7 127 6.804e-05 129.4 127 0.0001052 130 127 9.278e-05 130.7 128 6.804e-05 131.4 129 6.804e-05 132.1 130 5.567e-05 132.7 131 3.093e-05 133.4 131 5.567e-05 134.1 131 9.278e-05 134.8 133 6.804e-05 135.4 134 8.041e-05 136.1 134 0.0001175 136.8 134 0.0001175 137.5 135 0.0001175 138.1 136 8.041e-05 138.8 136 0.0001052 139.5 138 0.0001423 140.2 138 0.0001423 140.8 138 0.0001175 141.5 139 0.0001423 142.2 140 0.0001917 142.9 141 0.000167 143.5 141 0.0002041 144.2 141 0.0001794 144.9 142 0.0002165 145.5 143 0.0001423 146.2 144 0.0002165 146.9 145 0.0002289 147.6 145 0.0002536 148.2 145 0.000266 148.9 146 0.0002412 149.6 147 0.0002289 150.3 149 0.0002536 150.9 149 0.0002907 151.6 150 0.0003155 152.3 150 0.000266 153 150 0.0002907 153.6 152 0.0002907 154.3 152 0.0002907 155 152 0.0003031 155.7 153 0.0003278 156.3 154 0.0003649 157 156 0.0003402 157.7 156 0.0003278 158.3 156 0.0003402 159 157 0.0003278 159.7 158 0.0003649 160.4 159 0.0003649 161 159 0.0003897 161.7 159 0.0003773 162.4 160 0.0003897 163.1 161 0.0004144 163.7 161 0.0004144 164.4 162 0.0004268 165.1 163 0.0004144 165.8 164 0.0004144 166.4 165 0.0004515 167.1 166 0.0004639 167.8 166 0.0004639 168.5 166 0.0005134 169.1 167 0.0004763 169.8 168 0.0004268 170.5 169 0.0004639 171.2 169 0.0004763 171.8 170 0.000501 172.5 170 0.0004021 173.2 171 0.0004021 173.8 172 0.0005134 174.5 174 0.0005505 175.2 174 0.0005752 175.9 174 0.0005876 176.5 174 0.0005629 177.2 176 0.0005876 177.9 176 0.0005876 178.6 177 0.0006247 179.2 177 0.0006 179.9 178 0.0006495 180.6 178 0.0006247 181.3 180 0.0006495 181.9 180 0.0006371 182.6 181 0.0006495 183.3 181 0.0006124 184 181 0.0006495 184.6 183 0.0006495 185.3 184 0.0006618 186 184 0.0006866 186.7 184 0.0007113 187.3 185 0.0007237 188 186 0.0006866 188.7 187 0.0007361 189.3 188 0.0007361 190 188 0.0007113 190.7 188 0.000699 191.4 190 0.0007237 192 190 0.0007237 192.7 191 0.0007608 193.4 191 0.0007608 194.1 192 0.000835 194.7 193 0.0007484 195.4 193 0.0007608 196.1 194 0.0007855 196.8 195 0.0007855 197.4 196 0.0008227 198.1 196 0.0008227 198.8 196 0.0008721 199.5 198 0.000835 200.1 199 0.0008474 200.8 199 0.0008598 201.5 199 0.000835 202.1 200 0.0008845 202.8 201 0.0008721 203.5 202 0.0008845 204.2 202 0.0009093 204.8 202 0.0009093 205.5 203 0.000934 206.2 204 0.000934 206.9 205 0.0009587 207.5 206 0.0009835 208.2 206 0.0009835 208.9 206 0.0009711 209.6 207 0.0009835 210.2 209 0.0009835 210.9 209 0.0009835 211.6 209 0.001021 212.3 210 0.001008 212.9 211 0.001033 213.6 211 0.0009959 214.3 212 0.001021 215 213 0.001058 215.6 213 0.001082 216.3 214 0.001082 217 215 0.001082 217.6 215 0.001082 218.3 217 0.001082 219 217 0.001095 219.7 217 0.00107 220.3 218 0.00112 221 219 0.001107 221.7 219 0.001107 222.4 220 0.001181 223 221 0.001132 223.7 221 0.001181 224.4 222 0.001219 225.1 223 0.001219 225.7 224 0.001219 226.4 224 0.001231 227.1 225 0.001256 227.8 226 0.001243 228.4 227 0.001256 229.1 227 0.001256 229.8 227 0.00128 230.4 229 0.00128 231.1 229 0.00128 231.8 230 0.001317 232.5 231 0.00133 233.1 231 0.001317 233.8 232 0.00133 234.5 232 0.001293 235.2 233 0.00133 235.8 234 0.001355 236.5 234 0.001355 237.2 235 0.001379 237.9 236 0.001379 238.5 236 0.001404 239.2 237 0.001392 239.9 238 0.001404 240.6 238 0.001454 241.2 239 0.001454 241.9 240 0.001441 242.6 240 0.001466 243.3 242 0.001454 243.9 242 0.001454 244.6 242 0.001416 245.3 243 0.001466 245.9 244 0.001478 246.6 245 0.001515 247.3 245 0.001503 248 246 0.001503 248.6 247 0.001528 249.3 248 0.00154 250 248 0.001553 250.7 249 0.00159 251.3 249 0.001627 252 250 0.001614 252.7 250 0.00159 253.4 252 0.001602 254 252 0.001614 254.7 252 0.001577 255.4 254 0.00159 256.1 254 0.001602 256.7 255 0.001614 257.4 256 0.001614 258.1 256 0.001676 258.8 256 0.001639 259.4 258 0.001676 260.1 258 0.001676 260.8 259 0.001701 261.4 260 0.001701 262.1 260 0.001713 262.8 261 0.001713 263.5 262 0.001726 264.1 263 0.001713 264.8 263 0.00175 265.5 264 0.001701 266.2 264 0.001701 266.8 265 0.001763 267.5 266 0.001788 268.2 267 0.0018 268.9 267 0.001862 269.5 268 0.001812 270.2 268 0.001837 270.9 269 0.001849 271.6 270 0.001849 272.2 270 0.001874 272.9 271 0.001874 273.6 272 0.001849 274.2 272 0.001899 274.9 274 0.001899 275.6 274 0.001911 276.3 274 0.001911 276.9 276 0.001899 277.6 276 0.001936 278.3 277 0.001924 279 277 0.001948 279.6 278 0.001948 280.3 279 0.001961 281 280 0.001936 281.7 280 0.001961 282.3 281 0.001936 283 281 0.002023 283.7 282 0.001986 284.4 283 0.001986 285 284 0.002047 285.7 284 0.002047 286.4 285 0.002035 287.1 285 0.002035 287.7 286 0.002035 288.4 287 0.002047 289.1 287 0.002072 289.7 288 0.002097 290.4 289 0.002109 291.1 289 0.002146 291.8 290 0.002122 292.4 291 0.002122 293.1 292 0.002159 293.8 292 0.002196 294.5 293 0.002171 295.1 293 0.002146 295.8 295 0.002196 296.5 295 0.002196 297.2 295 0.002183 297.8 296 0.002171 298.5 297 0.002196 299.2 298 0.002196 299.9 299 0.002233 300.5 299 0.002233 301.2 300 0.002208 301.9 301 0.002245 302.5 301 0.002245 303.2 302 0.00227 303.9 302 0.002258 304.6 303 0.002295 305.2 304 0.002307 305.9 304 0.002258 306.6 306 0.00227 307.3 306 0.002307 307.9 306 0.002332 308.6 306 0.002344 309.3 308 0.002307 310 309 0.002332 310.6 309 0.002381 311.3 310 0.002369 312 310 0.002307 312.7 311 0.002394 313.3 312 0.002406 314 312 0.002431 314.7 313 0.002406 315.4 314 0.002456 316 315 0.002456 316.7 315 0.002406 317.4 316 0.002456 318 317 0.002505 318.7 317 0.002406 319.4 317 0.002567 320.1 319 0.002555 320.7 319 0.002468 321.4 318 0.002505 322.1 319 0.002493 322.8 320 0.002493 323.4 321 0.00253 324.1 323 0.002555 324.8 324 0.002567 325.5 326 0.002616 326.1 326 0.002629 326.8 326 0.002641 327.5 328 0.002629 328.2 328 0.002629 328.8 328 0.002616 329.5 328 0.002641 330.2 329 0.002654 330.9 328 0.002666 331.5 328 0.002629 332.2 331 0.002616 332.9 331 0.002654 333.5 334 0.002703 334.2 334 0.002691 334.9 335 0.002654 335.6 335 0.00274 336.2 336 0.00274 336.9 336 0.002765 337.6 337 0.002753 338.3 337 0.002753 338.9 338 0.00274 339.6 338 0.002703 340.3 339 0.002703 341 339 0.00279 341.6 340 0.002802 342.3 342 0.002802 343 342 0.002814 343.7 342 0.002814 344.3 343 0.002851 345 344 0.002851 345.7 344 0.002814 346.3 345 0.002864 347 346 0.002864 347.7 346 0.002889 348.4 347 0.002938 349 348 0.002901 349.7 349 0.002901 350.4 349 0.002913 351.1 349 0.002913 351.7 350 0.002926 352.4 352 0.00295 353.1 352 0.002938 353.8 353 0.002938 354.4 353 0.002963 355.1 354 0.002975 355.8 356 0.003049 356.5 356 0.003025 357.1 356 0.002975 357.8 356 0.003025 358.5 357 0.002988 359.2 358 0.003037 359.8 359 0.003062 360.5 360 0.002963 361.2 360 0.003037 361.8 360 0.003099 362.5 361 0.003062 363.2 362 0.003062 363.9 363 0.003087 364.5 364 0.003124 365.2 364 0.003136 365.9 365 0.003136 366.6 365 0.003161 367.2 366 0.003161 367.9 367 0.003148 368.6 367 0.003136 369.3 368 0.003185 369.9 368 0.003235 370.6 369 0.00321 371.3 370 0.003198 372 370 0.003185 372.6 371 0.003223 373.3 372 0.003247 374 373 0.003235 374.6 374 0.003284 375.3 374 0.00326 376 374 0.003297 376.7 376 0.003297 377.3 377 0.003247 378 378 0.003297 378.7 378 0.003309 379.4 378 0.003309 380 379 0.003297 380.7 380 0.003371 381.4 381 0.003346 382.1 381 0.003383 382.7 381 0.003421 383.4 382 0.003421 384.1 383 0.003396 384.8 384 0.003421 385.4 385 0.003433 386.1 385 0.003396 386.8 386 0.003421 387.5 387 0.003458 388.1 388 0.003458 388.8 388 0.003433 389.5 388 0.003445 390.1 389 0.003482 390.8 390 0.003482 391.5 391 0.00347 392.2 392 0.003495 392.8 392 0.003495 393.5 392 0.003482 394.2 393 0.003495 394.9 394 0.003557 395.5 395 0.003544 396.2 396 0.003569 396.9 396 0.003569 397.6 397 0.003569 398.2 397 0.003569 398.9 399 0.003569 399.6 399 0.003581 400.3 399 0.003569 400.9 400 0.003618 401.6 401 0.003631 402.3 401 0.003643 402.9 401 0.00368 403.6 403 0.003693 404.3 403 0.00368 405 404 0.003668 405.6 404 0.003668 406.3 405 0.00373 407 406 0.003693 407.7 406 0.003656 408.3 406 0.003693 409 408 0.00373 409.7 408 0.003742 410.4 409 0.003767 411 410 0.003755 411.7 410 0.003755 412.4 411 0.003779 413.1 411 0.003779 413.7 412 0.003779 414.4 413 0.003804 415.1 413 0.003792 415.8 414 0.003742 416.4 415 0.003854 417.1 416 0.003854 417.8 417 0.003891 418.4 417 0.003829 419.1 417 0.003866 419.8 418 0.003878 420.5 419 0.003952 421.1 420 0.003952 421.8 421 0.003952 422.5 421 0.003928 423.2 421 0.00394 423.8 422 0.003952 424.5 423 0.003977 425.2 424 0.003977 425.9 424 0.003977 426.5 426 0.004027 427.2 426 0.004014 427.9 427 0.004027 428.6 428 0.004027 429.2 428 0.004039 429.9 428 0.004076 430.6 429 0.004076 431.3 430 0.004076 431.9 431 0.004113 432.6 431 0.004126 433.3 432 0.004126 433.9 433 0.004126 434.6 434 0.00415 435.3 434 0.00415 436 435 0.004126 436.6 435 0.004138 437.3 436 0.004126 438 436 0.004113 438.7 438 0.004126 439.3 438 0.004163 440 438 0.004249 440.7 439 0.0042 441.4 440 0.0042 442 441 0.004225 442.7 442 0.004249 443.4 442 0.004237 444.1 442 0.004262 444.7 444 0.004299 445.4 444 0.004286 446.1 444 0.004299 446.7 446 0.004324 447.4 446 0.004336 448.1 446 0.004348 448.8 447 0.004336 449.4 448 0.004361 450.1 449 0.004361 450.8 450 0.004398 451.5 450 0.00441 452.1 451 0.004398 452.8 452 0.004423 453.5 453 0.004435 454.2 453 0.00446 454.8 453 0.004447 455.5 455 0.00441 456.2 455 0.004472 456.9 456 0.004497 457.5 456 0.004522 458.2 457 0.00446 458.9 458 0.004522 459.6 459 0.004472 460.2 459 0.004472 460.9 460 0.004522 461.6 460 0.004534 462.2 461 0.004534 462.9 461 0.004534 463.6 462 0.004583 464.3 463 0.004534 464.9 464 0.004596 465.6 464 0.004596 466.3 465 0.004596 467 466 0.004633 467.6 467 0.004682 468.3 467 0.004682 469 467 0.00467 469.7 469 0.00467 470.3 469 0.004682 471 470 0.004682 471.7 471 0.00467 472.4 471 0.004719 473 472 0.004707 473.7 473 0.004719 474.4 474 0.004732 475 474 0.004757 475.7 474 0.004744 476.4 476 0.004794 477.1 476 0.004806 477.7 477 0.004794 478.4 478 0.004781 479.1 478 0.004794 479.8 479 0.004818 480.4 480 0.004856 481.1 480 0.004868 481.8 481 0.00488 482.5 481 0.004868 483.1 482 0.00488 483.8 483 0.00488 484.5 484 0.004917 485.2 484 0.004917 485.8 485 0.004905 486.5 485 0.00488 487.2 486 0.00493 487.9 488 0.004942 488.5 488 0.004942 489.2 489 0.004955 489.9 489 0.004967 490.5 490 0.004979 491.2 491 0.005016 491.9 492 0.005004 492.6 492 0.005029 493.2 492 0.004967 493.9 493 0.004992 494.6 493 0.005016 495.3 495 0.005041 495.9 496 0.005078 496.6 496 0.005103 497.3 496 0.005115 498 497 0.005103 498.6 497 0.005128 499.3 499 0.005091 500 499 0.005115 500.7 500 0.005152 501.3 501 0.005152 502 501 0.00514 502.7 502 0.005165 503.4 503 0.005103 504 503 0.005165 504.7 503 0.005202 505.4 504 0.005202 506 506 0.005227 506.7 506 0.005251 507.4 506 0.005251 508.1 507 0.005251 508.7 508 0.005264 509.4 509 0.005289 510.1 510 0.005313 510.8 510 0.005289 511.4 510 0.005338 512.1 512 0.005289 512.8 512 0.005326 513.5 513 0.00535 514.1 513 0.005313 514.8 514 0.005375 515.5 514 0.005387 516.2 515 0.0054 516.8 516 0.0054 517.5 517 0.005425 518.2 517 0.005412 518.8 518 0.005412 519.5 518 0.005425 520.2 519 0.005449 520.9 521 0.005437 521.5 521 0.005486 522.2 521 0.005486 522.9 521 0.005511 523.6 523 0.005524 524.2 524 0.005511 524.9 524 0.005536 525.6 525 0.005536 526.3 526 0.005548 526.9 527 0.005573 527.6 527 0.005573 528.3 528 0.005561 529 528 0.00561 529.6 529 0.005623 530.3 530 0.00561 531 530 0.005598 531.7 530 0.005623 532.3 531 0.00561 533 532 0.005623 533.7 534 0.00566 534.3 535 0.005684 535 535 0.005684 535.7 535 0.005684 536.4 536 0.005734 537 536 0.005759 537.7 537 0.005771 538.4 538 0.005722 539.1 539 0.005722 539.7 539 0.005746 540.4 539 0.005759 541.1 540 0.005759 541.8 542 0.005759 542.4 542 0.005783 543.1 542 0.005796 543.8 543 0.005845 544.5 544 0.005833 545.1 545 0.005833 545.8 545 0.005858 546.5 546 0.005845 547.1 546 0.005858 547.8 547 0.00587 548.5 548 0.00587 549.2 549 0.00587 549.8 549 0.005907 550.5 550 0.005919 551.2 550 0.005919 551.9 552 0.005919 552.5 552 0.005944 553.2 553 0.005932 553.9 553 0.006006 554.6 554 0.006006 555.2 555 0.005994 555.9 556 0.006006 556.6 556 0.006018 557.3 557 0.006018 557.9 557 0.006043 558.6 558 0.006068 559.3 559 0.006068 560 560 0.006056 560.6 560 0.006068 561.3 561 0.00608 562 562 0.006117 562.6 563 0.006117 563.3 563 0.006142 564 564 0.00613 564.7 564 0.006154 565.3 565 0.006167 566 565 0.006167 566.7 567 0.006167 567.4 567 0.006167 568 567 0.006167 568.7 568 0.006253 569.4 569 0.006204 570.1 570 0.006216 570.7 571 0.006229 571.4 571 0.006253 572.1 571 0.006266 572.8 572 0.006253 573.4 573 0.006278 574.1 574 0.006303 574.8 574 0.006303 575.4 574 0.006315 576.1 576 0.006315 576.8 577 0.006328 577.5 578 0.00634 578.1 578 0.00634 578.8 578 0.00634 579.5 579 0.006352 580.2 580 0.006365 580.8 581 0.006365 581.5 582 0.006402 582.2 582 0.006402 582.9 583 0.006427 583.5 584 0.006439 584.2 584 0.006427 584.9 585 0.006414 585.6 585 0.006451 586.2 586 0.006451 586.9 587 0.006464 587.6 588 0.006464 588.3 588 0.006464 588.9 589 0.006501 589.6 589 0.006489 590.3 590 0.006451 590.9 590 0.006501 591.6 592 0.006513 592.3 592 0.006513 593 593 0.00655 593.6 593 0.006563 594.3 594 0.006563 595 595 0.0066 595.7 596 0.006612 596.3 596 0.006612 597 596 0.006612 597.7 597 0.006612 598.4 599 0.006612 599 599 0.006612 599.7 600 0.006625 600.4 600 0.006662 601.1 601 0.006699 601.7 601 0.006761 602.4 602 0.006724 603.1 603 0.006699 603.8 603 0.006699 604.4 604 0.006748 605.1 604 0.006736 605.8 605 0.006785 606.4 606 0.006748 607.1 606 0.006761 607.8 607 0.006773 608.5 608 0.00681 609.1 609 0.006785 609.8 609 0.006823 610.5 610 0.006785 611.2 610 0.006823 611.8 611 0.006835 612.5 612 0.00686 613.2 613 0.00681 613.9 613 0.00686 614.5 614 0.00686 615.2 614 0.006872 615.9 615 0.006884 616.6 616 0.006897 617.2 617 0.006909 617.9 617 0.006921 618.6 618 0.006921 619.2 619 0.006946 619.9 619 0.006959 620.6 620 0.006971 621.3 621 0.006946 621.9 621 0.006996 622.6 622 0.006946 623.3 623 0.006959 624 624 0.007008 624.6 624 0.007008 625.3 625 0.00702 626 626 0.00702 626.7 626 0.00702 627.3 627 0.007045 628 628 0.00707 628.7 628 0.00707 629.4 628 0.007082 630 630 0.007107 630.7 630 0.007107 631.4 631 0.007119 632.1 632 0.007119 632.7 632 0.007144 633.4 633 0.007144 634.1 634 0.007169 634.7 634 0.007144 635.4 635 0.007169 636.1 636 0.007206 636.8 637 0.007206 637.4 637 0.007218 638.1 638 0.007231 638.8 639 0.007218 639.5 639 0.007243 640.1 639 0.007243 640.8 640 0.007268 641.5 640 0.007231 642.2 642 0.007268 642.8 643 0.007305 643.5 643 0.007305 644.2 644 0.007317 644.9 644 0.007317 645.5 645 0.00733 646.2 646 0.007367 646.9 646 0.007305 647.5 646 0.007305 648.2 648 0.007354 648.9 649 0.007354 649.6 650 0.007367 650.2 650 0.007379 650.9 650 0.007392 651.6 652 0.007392 652.3 652 0.007404 652.9 653 0.007441 653.6 653 0.007429 654.3 653 0.007392 655 654 0.007367 655.6 656 0.007466 656.3 656 0.007491 657 657 0.007478 657.7 657 0.007491 658.3 659 0.007515 659 659 0.007528 659.7 659 0.007528 660.4 660 0.007491 661 661 0.007515 661.7 661 0.007565 662.4 662 0.00754 663 663 0.007552 663.7 664 0.007565 664.4 664 0.00759 665.1 665 0.007577 665.7 665 0.007577 666.4 667 0.007614 667.1 668 0.007614 667.8 668 0.007614 668.4 668 0.007602 669.1 669 0.007651 669.8 671 0.007676 670.5 670 0.007627 671.1 671 0.007639 671.8 671 0.007688 672.5 672 0.007701 673.2 674 0.007713 673.8 674 0.007738 674.5 675 0.007787 675.2 676 0.007775 675.9 676 0.007787 676.5 677 0.007738 677.2 678 0.007787 677.9 678 0.007787 678.5 679 0.007787 679.2 679 0.007837 679.9 680 0.007825 680.6 681 0.0078 681.2 682 0.0078 681.9 682 0.007837 682.6 683 0.007837 683.3 683 0.007886 683.9 684 0.007886 684.6 685 0.007924 685.3 685 0.007948 686 686 0.007911 686.6 686 0.007886 687.3 687 0.007886 688 688 0.007924 688.7 689 0.007961 689.3 689 0.007948 690 690 0.007973 690.7 691 0.007985 691.3 691 0.00801 692 693 0.007998 692.7 693 0.007985 693.4 693 0.007998 694 694 0.007998 694.7 695 0.00801 695.4 696 0.008047 696.1 696 0.008035 696.7 697 0.008072 697.4 697 0.00801 698.1 699 0.008035 698.8 699 0.008047 699.4 700 0.008084 700.1 701 0.008097 700.8 701 0.008159 701.5 702 0.008109 702.1 703 0.008146 702.8 703 0.008159 703.5 703 0.008109 704.2 704 0.008171 704.8 705 0.008159 705.5 706 0.008171 706.2 706 0.008171 706.8 707 0.008183 707.5 707 0.008183 708.2 709 0.008146 708.9 709 0.008183 709.5 710 0.008196 710.2 711 0.008233 710.9 711 0.008245 711.6 712 0.008258 712.2 712 0.008233 712.9 713 0.008282 713.6 714 0.008282 714.3 714 0.008295 714.9 715 0.008282 715.6 716 0.008258 716.3 717 0.008282 717 718 0.008332 717.6 718 0.008344 718.3 718 0.008381 719 719 0.008356 719.6 720 0.008369 720.3 721 0.008394 721 721 0.008394 721.7 722 0.008418 722.3 723 0.008431 723 724 0.008468 723.7 724 0.008443 724.4 725 0.008443 725 726 0.008468 725.7 726 0.00848 726.4 726 0.008493 727.1 728 0.008505 727.7 728 0.00853 728.4 729 0.008505 729.1 729 0.00853 729.8 730 0.008554 730.4 731 0.008567 731.1 731 0.008604 731.8 732 0.008567 732.5 733 0.008641 733.1 734 0.008567 733.8 734 0.008505 734.5 735 0.008542 735.1 736 0.008579 735.8 736 0.008616 736.5 736 0.008641 737.2 737 0.008629 737.8 738 0.008678 738.5 739 0.008641 739.2 739 0.008616 739.9 740 0.008653 740.5 740 0.008641 741.2 742 0.008653 741.9 743 0.008691 742.6 743 0.008715 743.2 743 0.008728 743.9 744 0.00874 744.6 744 0.008765 745.3 746 0.008765 745.9 746 0.008802 746.6 746 0.008789 747.3 748 0.008814 748 748 0.008802 748.6 749 0.008827 749.3 749 0.008814 750 750 0.008876 750.6 750 0.008888 751.3 750 0.008901 752 751 0.008926 752.7 752 0.008938 753.3 753 0.008938 754 753 0.009025 754.7 753 0.008963 755.4 754 0.009 756 755 0.009 756.7 756 0.009025 757.4 757 0.009049 758.1 757 0.009062 758.7 759 0.009123 759.4 759 0.009148 760.1 760 0.009185 760.8 761 0.009173 761.4 761 0.009123 762.1 762 0.009161 762.8 763 0.009198 763.4 764 0.009235 764.1 764 0.009272 764.8 765 0.009284 765.5 766 0.009297 766.1 767 0.009297 766.8 767 0.009297 767.5 768 0.009297 768.2 768 0.009297 768.8 769 0.009334 769.5 769 0.009359 770.2 771 0.009359 770.9 771 0.009346 771.5 771 0.009346 772.2 772 0.009396 772.9 774 0.009383 773.6 774 0.009408 774.2 775 0.009396 774.9 775 0.009346 775.6 776 0.009346 776.3 777 0.009445 776.9 778 0.009433 777.6 779 0.00947 778.3 779 0.00947 778.9 780 0.009507 779.6 780 0.00947 780.3 781 0.00947 781 782 0.009519 781.6 782 0.009519 782.3 783 0.009519 783 784 0.009507 783.7 784 0.009556 784.3 786 0.009581 785 786 0.009544 785.7 786 0.009569 786.4 787 0.009556 787 788 0.009569 787.7 788 0.009569 788.4 789 0.009569 789.1 790 0.009569 789.7 791 0.009544 790.4 792 0.009532 791.1 792 0.009519 791.7 793 0.009519 792.4 793 0.009507 793.1 794 0.009532 793.8 795 0.009519 794.4 796 0.009519 795.1 796 0.00947 795.8 796 0.009482 796.5 797 0.009445 797.1 798 0.00942 797.8 799 0.009359 798.5 799 0.009321 799.2 800 0.009247 799.8 800 0.009272 800.5 801 0.009222 801.2 801 0.009247 801.9 801 0.009173 802.5 801 0.009111 803.2 801 0.009074 803.9 801 0.009025 804.6 802 0.009 805.2 803 0.008926 805.9 803 0.008876 806.6 803 0.008839 807.2 804 0.008777 807.9 805 0.00874 808.6 805 0.008666 809.3 807 0.008629 809.9 807 0.00853 810.6 807 0.008493 811.3 809 0.008443 812 809 0.008369 812.6 810 0.008344 813.3 811 0.00827 814 811 0.008196 814.7 812 0.008146 815.3 812 0.00806 816 813 0.008072 816.7 814 0.008035 817.4 814 0.007862 818 815 0.007886 818.7 815 0.007812 819.4 817 0.007787 820 817 0.007738 820.7 818 0.007676 821.4 818 0.007651 822.1 819 0.007602 822.7 820 0.007552 823.4 821 0.007515 824.1 821 0.007404 824.8 821 0.007429 825.4 822 0.007404 826.1 823 0.007379 826.8 824 0.007342 827.5 825 0.007305 828.1 825 0.007293 828.8 826 0.007231 829.5 827 0.007218 830.2 827 0.007206 830.8 828 0.007218 831.5 829 0.007194 832.2 829 0.007169 832.9 829 0.007169 833.5 831 0.007144 834.2 831 0.007157 834.9 832 0.007157 835.5 832 0.007132 836.2 833 0.007144 836.9 834 0.007169 837.6 835 0.007181 838.2 835 0.007144 838.9 836 0.007058 839.6 837 0.007132 840.3 837 0.007132 840.9 838 0.007169 841.6 839 0.007181 842.3 839 0.007194 843 840 0.007218 843.6 841 0.007194 844.3 841 0.007206 845 843 0.007218 845.7 843 0.007243 846.3 843 0.007268 847 844 0.007342 847.7 844 0.007317 848.4 846 0.007354 849 847 0.007342 849.7 847 0.007342 850.4 847 0.007317 851 848 0.007367 851.7 849 0.007392 852.4 850 0.007404 853.1 850 0.007392 853.7 850 0.007392 854.4 852 0.007429 855.1 853 0.007441 855.8 853 0.007491 856.4 854 0.007441 857.1 854 0.007466 857.8 856 0.007515 858.5 856 0.007528 859.1 856 0.00754 859.8 857 0.00759 860.5 858 0.00759 861.2 859 0.00759 861.8 859 0.007602 862.5 860 0.007639 863.2 860 0.007639 863.8 861 0.007664 864.5 862 0.007664 865.2 862 0.007639 865.9 863 0.007688 866.5 864 0.007688 867.2 864 0.007713 867.9 865 0.007726 868.6 865 0.007738 869.2 867 0.007787 869.9 868 0.007738 870.6 868 0.00775 871.3 868 0.007787 871.9 869 0.007837 872.6 870 0.007849 873.3 871 0.007812 874 872 0.007812 874.6 872 0.007849 875.3 873 0.007886 876 874 0.007911 876.7 874 0.007924 877.3 875 0.007948 878 876 0.007985 878.7 876 0.007985 879.3 877 0.007998 880 877 0.008022 880.7 878 0.008022 881.4 879 0.00801 882 880 0.008035 882.7 880 0.00806 883.4 881 0.008097 884.1 882 0.008084 884.7 882 0.008109 885.4 883 0.008097 886.1 884 0.008097 886.8 884 0.008171 887.4 884 0.008159 888.1 886 0.008183 888.8 886 0.008196 889.5 886 0.008183 890.1 887 0.00822 890.8 888 0.00822 891.5 888 0.008245 892.1 889 0.00827 892.8 890 0.008295 893.5 892 0.008356 894.2 893 0.008369 894.8 893 0.008369 895.5 893 0.008332 896.2 894 0.008406 896.9 894 0.008369 897.5 895 0.008394 898.2 896 0.008418 898.9 897 0.008418 899.6 897 0.008443 900.2 897 0.00848 900.9 899 0.008493 901.6 899 0.008505 902.3 900 0.008542 902.9 900 0.008517 903.6 902 0.008542 904.3 903 0.008554 905 903 0.008542 905.6 903 0.008592 906.3 904 0.008592 907 904 0.008616 907.6 905 0.008653 908.3 906 0.008691 909 907 0.008641 909.7 907 0.00874 910.3 908 0.00874 911 909 0.008703 911.7 909 0.008715 912.4 910 0.008777 913 911 0.00874 913.7 911 0.008765 914.4 912 0.008765 915.1 913 0.008765 915.7 913 0.008827 916.4 914 0.008827 917.1 915 0.008814 917.8 915 0.008851 918.4 916 0.008888 919.1 917 0.008888 919.8 918 0.008901 920.5 918 0.008926 921.1 918 0.008938 921.8 919 0.008938 922.5 920 0.00895 923.1 920 0.009012 923.8 922 0.009037 924.5 922 0.009037 925.2 923 0.009 925.8 924 0.008938 926.5 925 0.009 927.2 925 0.009074 927.9 926 0.009136 928.5 926 0.009148 929.2 926 0.009148 929.9 928 0.009136 930.6 928 0.009173 931.2 929 0.009198 931.9 930 0.009235 932.6 930 0.009247 933.3 932 0.009247 933.9 932 0.009297 934.6 932 0.009346 935.3 933 0.009284 935.9 934 0.009284 936.6 933 0.009297 937.3 934 0.009346 938 935 0.009383 938.6 936 0.009371 939.3 937 0.009445 940 938 0.009482 940.7 939 0.009334 941.3 940 0.009396 942 940 0.009482 942.7 940 0.009495 943.4 942 0.009532 944 942 0.009519 944.7 943 0.009569 945.4 943 0.009569 946.1 943 0.009532 946.7 944 0.009569 947.4 945 0.009618 948.1 946 0.009606 948.8 947 0.01083 949.4 947 0.00989 950.1 948 0.009717 950.8 949 0.009693 951.4 949 0.00968 952.1 950 0.009668 952.8 950 0.00968 953.5 950 0.009705 954.1 953 0.009779 954.8 953 0.00973 955.5 954 0.009767 956.2 954 0.009866 956.8 955 0.009742 957.5 956 0.009829 958.2 956 0.009841 958.9 956 0.009816 959.5 957 0.009866 960.2 959 0.009866 960.9 959 0.00989 961.6 959 0.00989 962.2 959 0.009878 962.9 961 0.01 963.6 963 0.009989 964.2 965 0.01 964.9 965 0.01003 965.6 965 0.01001 966.3 965 0.01004 966.9 965 0.01 967.6 965 0.01 968.3 966 0.01004 969 967 0.0101 969.6 968 0.01009 970.3 968 0.01011 971 969 0.01011 971.7 970 0.01011 972.3 971 0.01014 973 972 0.01011 973.7 972 0.01011 974.4 972 0.01016 975 974 0.01016 975.7 975 0.01014 976.4 975 0.01022 977.1 975 0.01029 977.7 977 0.01037 978.4 976 0.01035 979.1 978 0.01031 979.7 978 0.01036 980.4 979 0.0104 981.1 979 0.01037 981.8 980 0.01035 982.4 980 0.01036 983.1 981 0.01042 983.8 982 0.01043 984.5 983 0.01043 985.1 983 0.01046 985.8 984 0.0105 986.5 985 0.01051 987.2 986 0.01052 987.8 986 0.01057 988.5 987 0.01058 989.2 988 0.01056 989.9 989 0.01052 990.5 990 0.0106 991.2 990 0.0106 991.9 990 0.01063 992.6 991 0.01063 993.2 992 0.01068 993.9 993 0.01067 994.6 993 0.01068 995.2 993 0.01065 995.9 994 0.01074 996.6 995 0.01073 997.3 997 0.01077 997.9 997 0.01068 998.6 997 0.01079 999.3 998 0.01081 1000 998 0.01082 1001 1000 0.01086 1001 1000 0.01083 1002 1000 0.01086 1003 1001 0.01079 1003 1001 0.01088 1004 1002 0.0109 1005 1004 0.01086 1005 1004 0.01086 1006 1004 0.01095 1007 1005 0.011 1007 1006 0.011 1008 1006 0.01103 1009 1007 0.01105 1009 1008 0.01105 1010 1008 0.01102 1011 1009 0.011 1011 1009 0.01112 1012 1010 0.01112 1013 1011 0.01113 1013 1011 0.01115 1014 1012 0.01115 1015 1013 0.0112 1015 1014 0.0112 1016 1015 0.01123 1017 1015 0.01124 1017 1015 0.01129 1018 1016 0.01128 1019 1017 0.0113 1020 1018 0.01133 1020 1018 0.01129 1021 1018 0.0112 1022 1019 0.01129 1022 1020 0.01133 1023 1021 0.01136 1024 1022 0.01137 1024 1022 0.01145 1025 1022 0.01145 1026 1024 0.01145 1026 1024 0.01146 1027 1025 0.01151 1028 1026 0.0115 1028 1027 0.01155 1029 1027 0.01154 1030 1028 0.01156 1030 1029 0.0116 1031 1029 0.01162 1032 1029 0.01161 1032 1030 0.01163 1033 1031 0.01163 1034 1032 0.01165 1034 1033 0.01166 1035 1033 0.01165 1036 1034 0.0117 1036 1034 0.01171 1037 1034 0.01175 1038 1036 0.01175 1038 1036 0.01171 1039 1037 0.0117 1040 1037 0.01178 1040 1038 0.0118 1041 1039 0.01183 1042 1040 0.01181 1042 1040 0.01185 1043 1041 0.01182 1044 1042 0.01185 1044 1043 0.01185 1045 1043 0.01185 1046 1043 0.01181 1046 1044 0.01183 1047 1045 0.01181 1048 1046 0.01189 1048 1047 0.01196 1049 1047 0.01191 1050 1048 0.01198 1050 1049 0.01207 1051 1050 0.01209 1052 1051 0.01209 1053 1051 0.01209 1053 1051 0.0121 1054 1053 0.01213 1055 1053 0.01215 1055 1054 0.01217 1056 1055 0.01218 1057 1055 0.01215 1057 1056 0.0122 1058 1057 0.01223 1059 1057 0.01228 1059 1058 0.01224 1060 1058 0.01223 1061 1060 0.01225 1061 1060 0.01225 1062 1061 0.01225 1063 1061 0.01228 1063 1062 0.01229 1064 1062 0.01229 1065 1063 0.01234 1065 1064 0.01235 1066 1064 0.01234 1067 1065 0.01238 1067 1067 0.01238 1068 1067 0.01235 1069 1068 0.01239 1069 1068 0.01239 1070 1068 0.01239 1071 1068 0.01243 1071 1069 0.01244 1072 1070 0.01249 1073 1072 0.01253 1073 1072 0.0125 1074 1073 0.01254 1075 1073 0.01254 1075 1074 0.01256 1076 1075 0.01259 1077 1076 0.01262 1077 1076 0.0126 1078 1076 0.0126 1079 1077 0.01262 1079 1078 0.01264 1080 1079 0.01267 1081 1079 0.01267 1081 1080 0.01267 1082 1081 0.01267 1083 1082 0.0127 1084 1082 0.01267 1084 1083 0.01269 1085 1084 0.0127 1086 1084 0.0127 1086 1084 0.01267 1087 1086 0.01267 1088 1086 0.01274 1088 1087 0.01275 1089 1087 0.01279 1090 1088 0.0128 1090 1089 0.0128 1091 1090 0.01279 1092 1090 0.0128 1092 1091 0.01286 1093 1092 0.01285 1094 1093 0.01287 1094 1093 0.01287 1095 1094 0.01292 1096 1094 0.01291 1096 1094 0.01295 1097 1096 0.01296 1098 1097 0.01297 1098 1097 0.01303 1099 1097 0.013 1100 1099 0.01305 1100 1099 0.01308 1101 1100 0.01305 1102 1101 0.01309 1102 1101 0.01309 1103 1102 0.01309 1104 1103 0.01312 1104 1103 0.01312 1105 1104 0.01313 1106 1104 0.01312 1106 1105 0.01317 1107 1106 0.01323 1108 1106 0.01326 1108 1107 0.01326 1109 1108 0.01324 1110 1109 0.01326 1110 1109 0.01329 1111 1110 0.01321 1112 1111 0.01326 1112 1111 0.01333 1113 1112 0.01339 1114 1113 0.0134 1115 1113 0.01342 1115 1114 0.01342 1116 1115 0.01343 1117 1115 0.01345 1117 1116 0.01349 1118 1117 0.0135 1119 1118 0.01343 1119 1119 0.01348 1120 1119 0.01355 1121 1119 0.01356 1121 1120 0.01355 1122 1122 0.01355 1123 1122 0.01356 1123 1122 0.01363 1124 1122 0.01364 1125 1123 0.01363 1125 1124 0.01364 1126 1125 0.01369 1127 1126 0.01375 1127 1126 0.01371 1128 1126 0.01371 1129 1128 0.01375 1129 1129 0.01376 1130 1129 0.01379 1131 1130 0.01376 1131 1130 0.0138 1132 1131 0.01377 1133 1131 0.01384 1133 1132 0.01382 1134 1133 0.01387 1135 1134 0.01387 1135 1134 0.01387 1136 1135 0.01391 1137 1136 0.01395 1137 1136 0.01402 1138 1137 0.01405 1139 1138 0.01401 1139 1138 0.01406 1140 1139 0.01407 1141 1140 0.01399 1141 1140 0.01395 1142 1142 0.01403 1143 1142 0.01408 1143 1143 0.0141 1144 1144 0.01412 1145 1144 0.0141 1146 1144 0.01413 1146 1145 0.01418 1147 1146 0.01418 1148 1147 0.01417 1148 1147 0.0142 1149 1148 0.01423 1150 1148 0.0142 1150 1150 0.01426 1151 1150 0.01427 1152 1151 0.01432 1152 1151 0.01431 1153 1152 0.01434 1154 1153 0.01425 1154 1153 0.01436 1155 1154 0.01437 1156 1154 0.01438 1156 1156 0.01442 1157 1157 0.01442 1158 1157 0.01447 1158 1158 0.01448 1159 1158 0.01448 1160 1159 0.0145 1160 1159 0.01448 1161 1160 0.01452 1162 1162 0.01455 1162 1162 0.01458 1163 1162 0.01454 1164 1163 0.01458 1164 1164 0.01462 1165 1165 0.0146 1166 1165 0.01463 1166 1165 0.01467 1167 1167 0.01468 1168 1167 0.01468 1168 1168 0.01459 1169 1169 0.01462 1170 1169 0.01467 1170 1169 0.01473 1171 1171 0.01465 1172 1172 0.01474 1172 1172 0.01474 1173 1172 0.01475 1174 1172 0.01479 1174 1174 0.01478 1175 1175 0.0148 1176 1175 0.01483 1177 1176 0.01483 1177 1177 0.01488 1178 1177 0.01484 1179 1177 0.01481 1179 1178 0.01484 1180 1180 0.01494 1181 1180 0.01493 1181 1181 0.01501 1182 1181 0.01496 1183 1182 0.01499 1183 1182 0.01504 1184 1183 0.01506 1185 1186 0.01499 1185 1185 0.01504 1186 1185 0.01502 1187 1185 0.01504 1187 1187 0.01511 1188 1188 0.01519 1189 1188 0.01516 1189 1189 0.01521 1190 1190 0.01526 1191 1190 0.01522 1191 1191 0.01526 1192 1192 0.01526 1193 1193 0.0153 1193 1194 0.01526 1194 1194 0.01525 1195 1194 0.01527 1195 1194 0.0153 1196 1195 0.01527 1197 1197 0.01526 1197 1197 0.01532 1198 1197 0.01537 1199 1198 0.01536 1199 1197 0.01537 1200 1199 0.01536 1201 1198 0.01541 1201 1199 0.01544 1202 1198 0.01542 1203 1198 0.01546 1203 1198 0.01541 1204 1199 0.01544 1205 1199 0.0154 1205 1198 0.01541 1206 1197 0.01544 1207 1197 0.01547 1208 1199 0.01544 1208 1199 0.01552 1209 1199 0.01547 1210 1199 0.01548 1210 1199 0.01546 1211 1199 0.01542 1212 1199 0.01541 1212 1197 0.0154 1213 1198 0.01542 1214 1199 0.01546 1214 1199 0.01549 1215 1199 0.01546 1216 1199 0.01548 1216 1199 0.01541 1217 1198 0.01543 1218 1199 0.01544 1218 1198 0.01544 1219 1198 0.01544 1220 1198 0.01546 1220 1198 0.01544 1221 1198 0.01544 1222 1199 0.01547 1222 1199 0.01544 1223 1198 0.01551 1224 1199 0.01547 1224 1199 0.01549 1225 1198 0.01551 1226 1199 0.01551 1226 1198 0.01546 1227 1198 0.01547 1228 1199 0.01547 1228 1199 0.01542 1229 1199 0.01547 1230 1199 0.01546 1230 1199 0.01551 1231 1199 0.01551 1232 1198 0.01551 1232 1199 0.01542 1233 1198 0.01538 1234 1198 0.01537 1234 1198 0.01546 1235 1197 0.01541 1236 1197 0.01541 1236 1199 0.01546 1237 1199 0.01546 1238 1199 0.01542 1238 1199 0.01543 1239 1198 0.01544 1240 1199 0.01542 1241 1199 0.01544 1241 1198 0.01542 1242 1199 0.01544 1243 1198 0.01543 1243 1199 0.01541 1244 1198 0.01538 1245 1199 0.01533 1245 1199 0.01547 1246 1198 0.01548 1247 1198 0.01537 1247 1199 0.01544 1248 1199 0.01546 1249 1199 0.01542 1249 1199 0.01541 1250 1199 0.01543 1251 1199 0.01543 1251 1199 0.01543 1252 1199 0.01546 1253 1199 0.01551 1253 1199 0.01544 1254 1199 0.01552 1255 1199 0.01542 1255 1199 0.01544 1256 1199 0.01542 1257 1199 0.01543 1257 1198 0.01543 1258 1199 0.01547 1259 1198 0.01542 1259 1198 0.01542 1260 1199 0.01538 1261 1199 0.01536 1261 1199 0.01538 1262 1198 0.01541 1263 1199 0.01543 1263 1199 0.01544 1264 1198 0.01541 1265 1199 0.01537 1265 1198 0.01537 1266 1199 0.01538 1267 1198 0.01536 1267 1199 0.01544 1268 1198 0.01533 1269 1198 0.01537 1269 1199 0.01538 1270 1199 0.01536 1271 1198 0.01546 1272 1199 0.01546 1272 1198 0.01547 1273 1198 0.01542 1274 1198 0.01543 1274 1198 0.01543 1275 1198 0.01544 1276 1199 0.01542 1276 1198 0.0154 1277 1199 0.0154 1278 1199 0.01533 1278 1199 0.01541 1279 1199 0.01537 1280 1199 0.01535 1280 1198 0.01532 1281 1199 0.01535 1282 1198 0.01536 1282 1198 0.01533 1283 1198 0.01533 1284 1199 0.01535 1284 1199 0.01531 1285 1199 0.01536 1286 1199 0.01532 1286 1199 0.0153 1287 1199 0.01535 1288 1198 0.01536 1288 1198 0.01532 1289 1199 0.01532 1290 1198 0.01536 1290 1199 0.01541 1291 1199 0.01537 1292 1199 0.01546 1292 1199 0.01538 1293 1199 0.01531 1294 1199 0.01541 1294 1198 0.01547 1295 1199 0.01543 1296 1198 0.01544 1296 1197 0.01544 1297 1199 0.01544 1298 1198 0.01541 1298 1199 0.01548 1299 1197 0.01547 1300 1199 0.01547 1300 1199 0.01543 1301 1198 0.01543 1302 1199 0.01544 1303 1199 0.01549 1303 1198 0.01547 1304 1198 0.01546 1305 1199 0.01544 1305 1198 0.01549 1306 1199 0.01546 1307 1199 0.01544 1307 1198 0.01547 1308 1199 0.01542 1309 1198 0.01544 1309 1199 0.01548 1310 1198 0.01544 1311 1199 0.01546 1311 1199 0.01542 1312 1199 0.01547 1313 1199 0.0154 1313 1199 0.0154 1314 1199 0.01538 1315 1199 0.01542 1315 1198 0.01538 1316 1198 0.01541 1317 1198 0.01546 1317 1199 0.0154 1318 1198 0.01532 1319 1198 0.01536 1319 1198 0.01537 1320 1199 0.01537 1321 1199 0.01531 1321 1199 0.01532 1322 1197 0.01531 1323 1199 0.01536 1323 1198 0.01536 1324 1199 0.01536 1325 1198 0.01537 1325 1199 0.01542 1326 1198 0.01538 1327 1198 0.01546 1327 1198 0.01536 1328 1199 0.01541 1329 1199 0.0154 1329 1199 0.01525 1330 1198 0.01525 1331 1199 0.01531 1331 1198 0.01535 1332 1198 0.01538 1333 1199 0.01538 1334 1198 0.01536 1334 1198 0.01553 1335 1199 0.01542 1336 1199 0.01537 1336 1198 0.01536 1337 1198 0.01536 1338 1199 0.0154 1338 1199 0.01546 1339 1199 0.01533 1340 1199 0.01542 1340 1199 0.01541 1341 1199 0.01537 1342 1198 0.01538 1342 1198 0.01541 1343 1199 0.01541 1344 1199 0.01537 1344 1199 0.01533 1345 1198 0.01541 1346 1198 0.01537 1346 1199 0.0154 1347 1199 0.01544 1348 1199 0.01537 1348 1198 0.01537 1349 1199 0.01535 1350 1198 0.01535 1350 1199 0.01533 1351 1198 0.01542 1352 1199 0.01541 1352 1199 0.01537 1353 1198 0.01541 1354 1199 0.01537 1354 1198 0.01541 1355 1199 0.01538 1356 1198 0.01538 1356 1198 0.01548 1357 1198 0.01533 1358 1198 0.01537 1358 1199 0.01535 1359 1198 0.01532 1360 1199 0.01543 1360 1199 0.0154 1361 1199 0.01541 1362 1199 0.01538 1362 1199 0.01541 1363 1198 0.01548 1364 1198 0.0154 1365 1199 0.01548 1365 1199 0.01535 1366 1199 0.01536 1367 1199 0.01537 1367 1199 0.01531 1368 1198 0.01536 1369 1198 0.0154 1369 1199 0.01536 1370 1199 0.01538 1371 1199 0.01537 1371 1199 0.01542 1372 1199 0.01541 1373 1198 0.01541 1373 1199 0.01541 1374 1198 0.01537 1375 1199 0.01532 1375 1199 0.01541 1376 1197 0.0154 1377 1199 0.0154 1377 1198 0.01541 1378 1199 0.01537 1379 1198 0.01546 1379 1199 0.01541 1380 1199 0.01543 1381 1199 0.01538 1381 1199 0.01537 1382 1199 0.01536 1383 1199 0.01537 1383 1199 0.01548 1384 1198 0.01537 1385 1199 0.01547 1385 1199 0.01541 1386 1199 0.01544 1387 1198 0.01531 1387 1198 0.01531 1388 1199 0.01535 1389 1199 0.01533 1389 1199 0.01533 1390 1198 0.01537 1391 1198 0.01549 1391 1199 0.01544 1392 1199 0.01536 1393 1199 0.01549 1393 1199 0.01533 1394 1198 0.01541 1395 1199 0.01536 1395 1199 0.01542 1396 1198 0.01533 1397 1199 0.01548 1398 1198 0.01522 1398 1199 0.01515 1399 1199 0.01546 1400 1198 0.01533 1400 1198 0.0153 1401 1198 0.0153 1402 1198 0.01536 1402 1199 0.01562 1403 1199 0.01538 1404 1199 0.01522 1404 1198 0.01537 1405 1198 0.01551 1406 1199 0.01556 1406 1199 0.01553 1407 1199 0.01514 1408 1198 0.01558 1408 1198 0.01535 1409 1199 0.01549 1410 1198 0.01495 1410 1199 0.01556 1411 1198 0.01592 1412 1199 0.01544 1412 1199 0.01499 1413 1198 0.01501 1414 1198 0.01516 1414 1199 0.01526 1415 1198 0.01532 1416 1199 0.01504 1416 1198 0.01568 1417 1198 0.0152 1418 1199 0.01517 1418 1199 0.01588 1419 1197 0.0154 1420 1199 0.01556 1420 1199 0.01544 1421 1199 0.01546 1422 1199 0.01547 1422 1199 0.01553 1423 1199 0.01542 1424 1199 0.01547 1424 1198 0.0152 1425 1198 0.01521 1426 1198 0.01558 1426 1199 0.01533 1427 1199 0.01536 1428 1198 0.01558 1429 1197 0.0157 1429 1199 0.01549 1430 1199 0.01542 1431 1199 0.01553 1431 1199 0.01541 1432 1198 0.01537 1433 1199 0.01537 1433 1199 0.01543 1434 1199 0.01543 1435 1198 0.01551 1435 1199 0.01538 1436 1199 0.01536 1437 1198 0.01531 1437 1198 0.01542 1438 1198 0.01547 1439 1199 0.01535 1439 1199 0.01533 1440 1198 0.01541 1441 1198 0.01548 1441 1199 0.01544 1442 1199 0.01548 1443 1199 0.01537 1443 1198 0.01542 1444 1198 0.01553 1445 1199 0.01553 1445 1198 0.01535 1446 1197 0.01531 1447 1199 0.01533 1447 1199 0.01537 1448 1198 0.0154 1449 1198 0.01541 1449 1198 0.01546 1450 1199 0.01546 1451 1199 0.01546 1451 1199 0.01541 1452 1198 0.0154 1453 1199 0.01538 1453 1199 0.01541 1454 1198 0.01542 1455 1198 0.01542 1455 1199 0.01542 1456 1199 0.01541 1457 1198 0.0154 1457 1199 0.01544 1458 1198 0.01533 1459 1198 0.01547 1460 1199 0.01533 1460 1198 0.01537 1461 1198 0.01533 1462 1199 0.01542 1462 1199 0.0154 1463 1199 0.01543 1464 1199 0.01546 1464 1199 0.01543 1465 1199 0.01541 1466 1198 0.01541 1466 1199 0.01543 1467 1199 0.01546 1468 1199 0.01538 1468 1198 0.01537 1469 1198 0.01537 1470 1199 0.01532 1470 1198 0.01543 1471 1198 0.0154 1472 1198 0.01537 1472 1199 0.0154 1473 1198 0.0153 1474 1198 0.01531 1474 1199 0.0153 1475 1199 0.01536 1476 1198 0.01541 1476 1199 0.01541 1477 1198 0.01538 1478 1199 0.01541 1478 1199 0.01537 1479 1198 0.01527 1480 1198 0.01532 1480 1199 0.01541 1481 1199 0.01533 1482 1198 0.01542 1482 1199 0.01532 1483 1199 0.01546 1484 1199 0.01538 1484 1198 0.01537 1485 1198 0.01548 1486 1198 0.01536 1486 1198 0.0154 1487 1199 0.01532 1488 1198 0.01531 1488 1199 0.01533 1489 1199 0.01532 1490 1199 0.0153 1491 1199 0.01533 1491 1198 0.0154 1492 1199 0.01533 1493 1198 0.01541 1493 1199 0.01552 1494 1198 0.01552 1495 1199 0.01547 1495 1198 0.0154 1496 1198 0.01542 1497 1198 0.01538 1497 1198 0.01541 1498 1199 0.01547 1499 1198 0.01541 1499 1182 0.01564 1500 1184 0.01551 1501 1184 0.01544 1501 1187 0.01546 1502 1188 0.01556 1503 1190 0.01561 1503 1192 0.01567 1504 1193 0.01562 1505 1192 0.01556 1505 1192 0.01562 1506 1190 0.01556 1507 1190 0.01554 1507 1190 0.01556 1508 1188 0.01552 1509 1187 0.01553 1509 1187 0.01547 1510 1187 0.01543 1511 1186 0.01544 1511 1184 0.01547 1512 1184 0.01542 1513 1184 0.01541 1513 1183 0.01538 1514 1183 0.01537 1515 1181 0.01536 1515 1181 0.01532 1516 1180 0.01531 1517 1179 0.0153 1517 1179 0.01528 1518 1178 0.0153 1519 1178 0.01522 1519 1177 0.0153 1520 1176 0.01519 1521 1176 0.01514 1522 1175 0.01512 1522 1174 0.01517 1523 1173 0.01511 1524 1172 0.01504 1524 1172 0.0151 1525 1172 0.01504 1526 1171 0.01502 1526 1170 0.01504 1527 1169 0.01501 1528 1169 0.01504 1528 1168 0.01501 1529 1168 0.01501 1530 1167 0.01489 1530 1166 0.01491 1531 1165 0.01493 1532 1165 0.01494 1532 1164 0.01491 1533 1163 0.01489 1534 1162 0.01485 1534 1162 0.01485 1535 1162 0.01483 1536 1161 0.01479 1536 1160 0.01476 1537 1159 0.01469 1538 1158 0.01479 1538 1158 0.01481 1539 1157 0.01481 1540 1156 0.01475 1540 1156 0.0147 1541 1155 0.01472 1542 1154 0.01468 1542 1154 0.01468 1543 1153 0.01467 1544 1153 0.01464 1544 1151 0.01457 1545 1151 0.01463 1546 1151 0.01442 1546 1150 0.01447 1547 1149 0.01453 1548 1148 0.01454 1548 1147 0.01442 1549 1147 0.01447 1550 1147 0.0145 1550 1146 0.01448 1551 1145 0.01452 1552 1144 0.01442 1553 1143 0.01432 1553 1143 0.01428 1554 1142 0.01422 1555 1142 0.01434 1555 1140 0.01437 1556 1140 0.01438 1557 1139 0.01438 1557 1139 0.01433 1558 1138 0.01425 1559 1137 0.01422 1559 1136 0.01412 1560 1136 0.01415 1561 1135 0.01417 1561 1135 0.01421 1562 1134 0.01415 1563 1133 0.01412 1563 1133 0.01418 1564 1132 0.01416 1565 1131 0.01412 1565 1130 0.01411 1566 1130 0.01407 1567 1129 0.01406 1567 1129 0.01408 1568 1128 0.01406 1569 1128 0.01402 1569 1127 0.01403 1570 1126 0.01403 1571 1125 0.0139 1571 1125 0.0139 1572 1124 0.01384 1573 1123 0.01389 1573 1122 0.01397 1574 1122 0.01395 1575 1122 0.01386 1575 1120 0.01392 1576 1120 0.01389 1577 1119 0.0139 1577 1119 0.01377 1578 1118 0.01377 1579 1118 0.01381 1579 1117 0.0138 1580 1115 0.0138 1581 1115 0.01375 1581 1115 0.01365 1582 1114 0.01369 1583 1112 0.0137 1583 1112 0.01365 1584 1112 0.01365 1585 1111 0.01359 1586 1110 0.0136 1586 1109 0.0136 1587 1109 0.01355 1588 1108 0.01352 1588 1108 0.01353 1589 1107 0.01349 1590 1106 0.01349 1590 1105 0.01349 1591 1104 0.01344 1592 1104 0.01343 1592 1103 0.01343 1593 1103 0.01345 1594 1102 0.0134 1594 1101 0.01334 1595 1101 0.01338 1596 1100 0.01333 1596 1100 0.01332 1597 1099 0.01338 1598 1099 0.01333 1598 1097 0.01329 1599 1097 0.01323 1600 1097 0.01319 1600 1095 0.01321 1601 1095 0.01321 1602 1094 0.01319 1602 1094 0.01316 1603 1093 0.01307 1604 1092 0.01312 1604 1091 0.01311 1605 1090 0.01307 1606 1090 0.01305 1606 1090 0.01308 1607 1088 0.01311 1608 1088 0.01302 1608 1087 0.01303 1609 1086 0.01302 1610 1086 0.01298 1610 1085 0.01303 1611 1085 0.01293 1612 1084 0.0129 1612 1083 0.01288 1613 1083 0.01291 1614 1082 0.01292 1614 1081 0.01287 1615 1080 0.01288 1616 1080 0.01276 1617 1079 0.01279 1617 1079 0.01265 1618 1078 0.01267 1619 1077 0.01276 1619 1076 0.01279 1620 1076 0.01269 1621 1075 0.01274 1621 1075 0.01267 1622 1074 0.01275 1623 1072 0.01267 1623 1072 0.01266 1624 1072 0.01267 1625 1071 0.01267 1625 1070 0.01264 1626 1069 0.01261 1627 1068 0.01254 1627 1068 0.01259 1628 1068 0.01256 1629 1067 0.01254 1629 1066 0.0126 1630 1065 0.01253 1631 1065 0.01254 1631 1065 0.01256 1632 1064 0.01246 1633 1063 0.01249 1633 1062 0.01249 1634 1061 0.01234 1635 1061 0.0124 1635 1060 0.01244 1636 1059 0.01241 1637 1059 0.0124 1637 1058 0.01238 1638 1058 0.01234 1639 1057 0.01235 1639 1056 0.01234 1640 1055 0.01229 1641 1055 0.0123 1641 1054 0.01244 1642 1053 0.01227 1643 1053 0.01234 1643 1052 0.01223 1644 1051 0.01219 1645 1051 0.01207 1645 1050 0.01204 1646 1049 0.01207 1647 1049 0.01204 1648 1048 0.01207 1648 1047 0.01222 1649 1047 0.0122 1650 1046 0.01194 1650 1045 0.01194 1651 1044 0.01224 1652 1043 0.0118 1652 1043 0.01225 1653 1043 0.01166 1654 1042 0.01219 1654 1040 0.01209 1655 1040 0.01156 1656 1040 0.01167 1656 1040 0.01206 1657 1038 0.01213 1658 1038 0.01186 1658 1037 0.01152 1659 1036 0.01137 1660 1036 0.01177 1660 1035 0.01209 1661 1034 0.01149 1662 1034 0.01201 1662 1033 0.01154 1663 1032 0.01192 1664 1031 0.01155 1664 1031 0.01162 1665 1030 0.01178 1666 1029 0.0118 1666 1029 0.01173 1667 1028 0.01166 1668 1028 0.01167 1668 1027 0.01159 1669 1026 0.01156 1670 1026 0.0115 1670 1025 0.01163 1671 1025 0.01152 1672 1023 0.01146 1672 1022 0.01145 1673 1022 0.01145 1674 1022 0.01156 1674 1021 0.01155 1675 1020 0.01147 1676 1019 0.01141 1676 1018 0.01135 1677 1018 0.0114 1678 1018 0.01139 1679 1017 0.01141 1679 1016 0.01121 1680 1015 0.01128 1681 1015 0.0113 1681 1014 0.01118 1682 1013 0.0113 1683 1012 0.01118 1683 1012 0.01121 1684 1011 0.01123 1685 1011 0.0112 1685 1010 0.01119 1686 1009 0.01115 1687 1008 0.01113 1687 1008 0.01105 1688 1007 0.01103 1689 1007 0.01102 1689 1006 0.01105 1690 1005 0.01099 1691 1004 0.01102 1691 1004 0.01104 1692 1003 0.01098 1693 1002 0.01093 1693 1002 0.01095 1694 1001 0.01088 1695 1000 0.01087 1695 1000 0.01088 1696 999 0.01088 1697 999 0.01086 1697 999 0.01082 1698 997 0.01079 1699 997 0.01079 1699 997 0.01083 1700 996 0.01076 1701 994 0.01076 1701 994 0.01074 1702 993 0.01076 1703 993 0.01068 1703 993 0.01066 1704 991 0.01063 1705 990 0.01067 1705 990 0.01066 1706 990 0.01062 1707 990 0.01058 1707 988 0.01058 1708 987 0.01055 1709 986 0.01056 1710 986 0.01056 1710 985 0.01058 1711 985 0.01051 1712 984 0.01047 1712 983 0.01048 1713 983 0.01045 1714 982 0.01047 1714 981 0.01046 1715 980 0.01046 1716 979 0.01043 1716 979 0.0104 1717 979 0.01039 1718 978 0.01036 1718 978 0.01034 1719 976 0.01032 1720 976 0.0103 1720 975 0.01029 1721 975 0.01026 1722 974 0.01026 1722 973 0.01019 1723 972 0.01016 1724 972 0.01015 1724 972 0.0102 1725 970 0.01009 1726 969 0.01011 1726 969 0.0101 1727 968 0.01006 1728 968 0.01006 1728 968 0.01003 1729 966 0.01001 1730 965 0.01003 1730 965 0.01001 1731 964 0.009804 1732 964 0.009989 1732 963 0.009928 1733 963 0.00994 1734 961 0.009878 1734 961 0.009928 1735 960 0.009792 1736 959 0.009779 1736 959 0.009754 1737 958 0.009804 1738 957 0.009779 1738 957 0.009816 1739 956 0.009779 1740 955 0.009779 1741 954 0.009816 1741 954 0.009705 1742 954 0.009655 1743 953 0.009705 1743 952 0.009668 1744 950 0.00973 1745 950 0.009631 1745 950 0.009631 1746 949 0.009655 1747 949 0.00968 1747 947 0.009631 1748 947 0.009631 1749 947 0.009618 1749 947 0.009594 1750 945 0.009519 1751 944 0.009532 1751 943 0.009556 1752 943 0.009482 1753 943 0.009507 1753 942 0.00947 1754 942 0.009495 1755 940 0.00942 1755 940 0.009371 1756 939 0.00942 1757 938 0.009408 1757 938 0.009321 1758 937 0.009371 1759 936 0.009321 1759 936 0.009272 1760 935 0.009272 1761 934 0.009222 1761 934 0.009247 1762 933 0.009247 1763 932 0.009235 1763 932 0.00921 1764 930 0.009198 1765 930 0.009136 1765 929 0.009136 1766 929 0.009148 1767 928 0.009111 1767 928 0.009123 1768 926 0.009123 1769 926 0.009111 1769 926 0.009074 1770 925 0.009037 1771 925 0.009025 1771 924 0.008987 1772 922 0.009012 1773 922 0.009037 1774 922 0.008975 1774 921 0.008864 1775 920 0.008938 1776 919 0.008913 1776 918 0.008876 1777 918 0.008864 1778 918 0.008802 1778 917 0.008851 1779 916 0.008827 1780 915 0.008789 1780 915 0.008777 1781 914 0.008765 1782 912 0.008752 1782 913 0.008777 1783 912 0.008765 1784 911 0.008728 1784 911 0.008703 1785 910 0.008703 1786 909 0.008678 1786 909 0.008641 1787 907 0.008653 1788 907 0.008629 1788 906 0.008604 1789 906 0.00853 1790 905 0.00848 1790 904 0.00853 1791 904 0.008567 1792 903 0.008567 1792 903 0.00853 1793 902 0.00853 1794 901 0.008505 1794 900 0.00848 1795 900 0.008443 1796 899 0.008418 1796 898 0.008394 1797 897 0.008418 1798 897 0.008381 1798 897 0.008369 1799 896 0.008369 1800 895 0.008332 1800 894 0.008245 1801 893 0.008282 1802 893 0.008245 1802 893 0.008245 1803 892 0.008233 1804 891 0.008233 1805 890 0.008208 1805 889 0.008208 1806 889 0.008196 1807 888 0.008171 1807 888 0.008183 1808 887 0.008183 1809 886 0.008109 1809 886 0.008146 1810 885 0.008134 1811 884 0.00806 1811 884 0.008022 1812 882 0.007998 1813 882 0.007985 1813 881 0.007998 1814 881 0.007948 1815 880 0.007961 1815 879 0.007948 1816 879 0.007948 1817 878 0.007948 1817 878 0.007911 1818 877 0.007874 1819 876 0.007874 1819 875 0.007849 1820 875 0.007837 1821 874 0.007825 1821 873 0.007812 1822 872 0.007763 1823 872 0.00775 1823 872 0.007738 1824 871 0.007763 1825 869 0.00775 1825 868 0.007726 1826 868 0.007713 1827 868 0.007651 1827 868 0.007688 1828 866 0.007688 1829 865 0.007627 1829 865 0.007602 1830 864 0.007528 1831 864 0.007392 1831 863 0.007354 1832 862 0.007478 1833 862 0.007491 1833 861 0.007515 1834 860 0.007491 1835 860 0.007453 1836 859 0.007453 1836 858 0.007453 1837 857 0.007416 1838 857 0.007404 1838 856 0.007392 1839 855 0.007392 1840 855 0.007379 1840 854 0.007354 1841 854 0.007293 1842 853 0.007342 1842 852 0.007293 1843 852 0.007293 1844 850 0.007268 1844 850 0.00728 1845 850 0.007268 1846 849 0.007206 1846 848 0.007243 1847 847 0.007206 1848 847 0.007181 1848 847 0.007181 1849 846 0.007144 1850 845 0.007132 1850 844 0.00707 1851 843 0.007095 1852 843 0.007144 1852 843 0.007119 1853 842 0.007058 1854 840 0.006996 1854 840 0.006934 1855 839 0.006946 1856 839 0.006959 1856 838 0.006946 1857 837 0.006934 1858 836 0.006934 1858 836 0.006909 1859 835 0.006909 1860 834 0.00686 1860 834 0.00686 1861 833 0.00686 1862 832 0.00686 1862 832 0.006823 1863 831 0.006798 1864 830 0.006823 1864 830 0.006773 1865 829 0.006798 1866 829 0.006736 1867 828 0.006674 1867 827 0.006699 1868 826 0.006699 1869 826 0.006674 1869 825 0.006637 1870 825 0.006612 1871 824 0.006662 1871 823 0.006662 1872 822 0.0066 1873 821 0.006563 1873 821 0.006526 1874 821 0.006526 1875 819 0.006526 1875 818 0.006476 1876 818 0.006451 1877 818 0.006464 1877 817 0.006464 1878 816 0.006451 1879 815 0.006414 1879 815 0.006439 1880 814 0.006427 1881 813 0.006377 1881 813 0.006365 1882 812 0.00634 1883 811 0.006315 1883 811 0.006328 1884 810 0.006328 1885 810 0.006303 1885 809 0.006291 1886 808 0.006241 1887 807 0.006241 1887 807 0.006241 1888 806 0.006241 1889 805 0.006241 1889 804 0.006179 1890 804 0.006179 1891 803 0.006154 1891 803 0.006154 1892 802 0.00613 1893 801 0.00613 1893 801 0.00608 1894 801 0.00613 1895 801 0.006105 1895 801 0.006056 1896 801 0.005981 1897 801 0.006018 1898 800 0.006006 1898 800 0.005994 1899 799 0.005994 1900 799 0.005932 1900 798 0.005907 1901 797 0.005907 1902 796 0.005957 1902 796 0.005907 1903 795 0.005858 1904 794 0.005833 1904 794 0.005858 1905 793 0.005833 1906 793 0.005969 1906 793 0.005882 1907 791 0.005759 1908 790 0.005722 1908 790 0.005722 1909 789 0.005734 1910 788 0.005709 1910 788 0.005684 1911 787 0.005684 1912 786 0.005635 1912 785 0.005598 1913 785 0.005635 1914 784 0.005585 1914 783 0.00561 1915 783 0.005585 1916 782 0.005573 1916 782 0.005573 1917 782 0.005536 1918 780 0.005524 1918 779 0.005511 1919 779 0.005474 1920 779 0.005499 1920 778 0.005474 1921 777 0.005437 1922 776 0.005412 1922 776 0.005425 1923 775 0.005412 1924 775 0.005375 1924 773 0.005387 1925 772 0.005363 1926 772 0.005326 1926 771 0.005313 1927 771 0.005313 1928 771 0.005289 1928 769 0.005214 1929 768 0.005239 1930 768 0.005239 1931 768 0.005227 1931 767 0.005289 1932 766 0.005214 1933 765 0.005165 1933 764 0.005165 1934 764 0.00519 1935 763 0.005103 1935 762 0.005115 1936 762 0.005091 1937 761 0.005066 1937 761 0.005041 1938 759 0.005091 1939 759 0.005078 1939 759 0.005029 1940 757 0.004992 1941 757 0.004942 1941 757 0.004979 1942 756 0.004967 1943 755 0.004893 1943 754 0.004893 1944 753 0.004905 1945 753 0.004917 1945 753 0.004992 1946 752 0.004979 1947 750 0.004905 1947 750 0.004818 1948 750 0.004818 1949 749 0.004818 1949 749 0.004794 1950 748 0.004843 1951 746 0.004695 1951 746 0.004534 1952 746 0.004608 1953 745 0.004571 1953 744 0.004658 1954 743 0.004695 1955 743 0.004682 1955 743 0.004682 1956 742 0.004682 1957 741 0.004682 1957 740 0.004633 1958 739 0.004571 1959 739 0.004546 1959 738 0.004534 1960 737 0.004509 1961 736 0.004522 1962 736 0.004522 1962 736 0.004522 1963 735 0.004522 1964 734 0.004484 1964 733 0.00446 1965 732 0.004423 1966 732 0.004373 1966 732 0.004398 1967 731 0.004398 1968 730 0.004385 1968 729 0.004361 1969 728 0.004299 1970 728 0.004336 1970 727 0.004336 1971 727 0.004324 1972 726 0.004286 1972 726 0.004262 1973 725 0.004225 1974 724 0.004225 1974 723 0.004212 1975 722 0.0042 1976 721 0.004212 1976 721 0.004163 1977 721 0.00415 1978 719 0.00415 1978 719 0.004126 1979 718 0.004101 1980 718 0.004089 1980 717 0.004076 1981 717 0.004051 1982 715 0.004039 1982 715 0.004039 1983 714 0.004027 1984 713 0.004014 1984 713 0.004014 1985 712 0.004014 1986 712 0.003891 1986 711 0.003915 1987 710 0.003903 1988 709 0.003928 1988 709 0.003928 1989 709 0.003891 1990 707 0.003891 1990 707 0.003854 1991 706 0.003816 1992 705 0.003755 1993 704 0.003804 1993 704 0.003755 1994 703 0.003767 1995 703 0.003742 1995 702 0.003643 1996 701 0.00373 1997 701 0.003742 1997 700 0.003643 1998 700 0.003668 1999 699 0.003618 1999 699 0.003643 2000 697 0.003631 2001 696 0.003569 2001 696 0.003532 2002 696 0.003581 2003 695 0.003557 2003 694 0.003594 2004 693 0.003557 2005 693 0.003507 2005 692 0.003495 2006 691 0.003482 2007 690 0.003482 2007 690 0.00352 2008 689 0.003458 2009 689 0.003445 2009 687 0.003445 2010 687 0.00347 2011 686 0.003458 2011 686 0.003458 2012 685 0.003433 2013 685 0.003346 2013 684 0.003359 2014 683 0.003322 2015 682 0.003272 2015 682 0.003297 2016 681 0.003272 2017 681 0.003284 2017 680 0.003284 2018 680 0.003198 2019 678 0.003223 2019 678 0.00321 2020 677 0.003185 2021 677 0.003185 2021 676 0.003161 2022 675 0.003161 2023 674 0.003136 2024 673 0.003099 2024 673 0.003099 2025 672 0.003136 2026 671 0.003087 2026 671 0.003025 2027 671 0.003087 2028 669 0.003 2028 669 0.002926 2029 668 0.002938 2030 668 0.003037 2030 667 0.002988 2031 666 0.002975 2032 665 0.002938 2032 665 0.002901 2033 664 0.002963 2034 663 0.002938 2034 663 0.002938 2035 662 0.002988 2036 661 0.002926 2036 661 0.002926 2037 660 0.002802 2038 660 0.002827 2038 659 0.00279 2039 658 0.00279 2040 657 0.002777 2040 657 0.002703 2041 656 0.002728 2042 655 0.002703 2042 655 0.002654 2043 654 0.002703 2044 653 0.002654 2044 653 0.002691 2045 652 0.002678 2046 650 0.002691 2046 650 0.002604 2047 650 0.002592 2048 649 0.002592 2048 649 0.002567 2049 648 0.002542 2050 646 0.002542 2050 646 0.002443 2051 646 0.002443 2052 645 0.002468 2052 643 0.002493 2053 643 0.002493 2054 643 0.002468 2055 643 0.002443 2055 642 0.002431 2056 641 0.002406 2057 641 0.002406 2057 639 0.002369 2058 639 0.002295 2059 638 0.002381 2059 638 0.002344 2060 637 0.002295 2061 636 0.002307 2061 635 0.00232 2062 635 0.002307 2063 634 0.00227 2063 633 0.002344 2064 633 0.002233 2065 632 0.002146 2065 632 0.002122 2066 631 0.002208 2067 630 0.002183 2067 629 0.002146 2068 628 0.002171 2069 628 0.002146 2069 628 0.002134 2070 627 0.002122 2071 626 0.002109 2071 625 0.002122 2072 625 0.002035 2073 624 0.002072 2073 624 0.00206 2074 622 0.002023 2075 622 0.00201 2075 621 0.001986 2076 621 0.001961 2077 620 0.001911 2077 619 0.001862 2078 618 0.001862 2079 617 0.001874 2079 617 0.001812 2080 617 0.001899 2081 616 0.001837 2081 615 0.001849 2082 614 0.0018 2083 614 0.001825 2083 613 0.001812 2084 612 0.001763 2085 612 0.001689 2086 610 0.001713 2086 610 0.001713 2087 610 0.001713 2088 609 0.001664 2088 608 0.001652 2089 607 0.001664 2090 607 0.00159 2090 606 0.001614 2091 606 0.00159 2092 605 0.001577 2092 604 0.001614 2093 603 0.001565 2094 603 0.001565 2094 602 0.001528 2095 602 0.001528 2096 601 0.001503 2096 601 0.001503 2097 600 0.001478 2098 600 0.001441 2098 599 0.001466 2099 598 0.001478 2100 597 0.001305 2100 596 0.001355 2101 596 0.001355 2102 596 0.001355 2102 595 0.001355 2103 594 0.001305 2104 593 0.001256 2104 592 0.001293 2105 592 0.001268 2106 591 0.001243 2106 590 0.001256 2107 590 0.001293 2108 589 0.001268 2108 588 0.001231 2109 588 0.001256 2110 587 0.001206 2110 586 0.001243 2111 585 0.001157 2112 585 0.001169 2112 584 0.001157 2113 584 0.00112 2114 583 0.001157 2114 582 0.00112 2115 582 0.001058 2116 581 0.001008 2116 580 0.0009464 2117 580 0.001021 2118 579 0.001008 2119 578 0.0009711 2119 578 0.0009711 2120 577 0.0009216 2121 576 0.0008598 2121 576 0.0008721 2122 574 0.0008721 2123 574 0.0008598 2123 573 0.0008721 2124 573 0.0008845 2125 572 0.0008598 2125 571 0.000835 2126 571 0.0007361 2127 571 0.0007361 2127 569 0.0006742 2128 568 0.0007113 2129 568 0.0007237 2129 567 0.0006618 2130 567 0.0006742 2131 566 0.0006742 2131 565 0.000699 2132 565 0.0007608 2133 564 0.0006124 2133 564 0.0005629 2134 563 0.0005381 2135 562 0.0006124 2135 562 0.0005381 2136 560 0.0005629 2137 560 0.0005258 2137 559 0.0005381 2138 559 0.0005505 2139 559 0.0004392 2139 557 0.0004763 2140 557 0.0004268 2141 556 0.0004392 2141 555 0.0004515 2142 555 0.0004144 2143 553 0.0004021 2143 553 0.0004268 2144 553 0.0004021 2145 552 0.0003773 2145 550 0.0003278 2146 550 0.0003031 2147 549 0.0003897 2147 549 0.0002907 2148 549 0.0002041 2149 548 0.000266 2150 546 0.0002165 2150 547 0.000266 2151 546 0.0002289 2152 546 0.0002165 2152 544 0.0001423 2153 544 0.0001794 2154 542 0.0001546 2154 542 0.0001299 2155 542 8.041e-05 2156 541 6.804e-05 2156 540 8.041e-05 2157 540 8.041e-05 2158 539 3.093e-05 2158 538 6.185e-06 2159 537 6.185e-06 2160 537 6.185e-06 2160 536 6.185e-06 2161 536 6.185e-06 2162 535 6.185e-06 2162 534 6.185e-06 2163 533 6.185e-06 2164 533 6.185e-06 2164 532 6.185e-06 2165 532 6.185e-06 2166 532 6.185e-06 2166 532 -3.093e-05 2167 534 -5.567e-05 2168 536 -6.804e-05 2168 535 6.185e-06 2169 534 -1.856e-05 2170 531 -8.041e-05 2170 529 -0.0002289 2171 528 -0.0002289 2172 525 -0.0002289 2172 524 -0.0002783 2173 522 -0.0003402 2174 521 -0.0003278 2174 521 -0.0003278 2175 521 -0.0003402 2176 519 -0.0003897 2176 520 -0.0003773 2177 519 -0.0004268 2178 518 -0.0004144 2178 518 -0.0003649 2179 517 -0.0004144 2180 517 -0.0004268 2181 516 -0.0004144 2181 515 -0.0004515 2182 514 -0.0005134 2183 514 -0.000501 2183 514 -0.0005258 2184 513 -0.0005505 2185 512 -0.0005752 2185 511 -0.0005505 2186 510 -0.0006 2187 510 -0.0006247 2187 510 -0.0006371 2188 509 -0.0006495 2189 508 -0.0006247 2189 507 -0.0006495 2190 506 -0.0006742 2191 506 -0.0006742 2191 506 -0.0007361 2192 504 -0.0007979 2193 504 -0.0007855 2193 503 -0.0007484 2194 503 -0.0007608 2195 502 -0.0007855 2195 501 -0.0007608 2196 501 -0.0007732 2197 499 -0.0007608 2197 499 -0.0008598 2198 499 -0.0008969 2199 498 -0.0008845 2199 496 -0.0009093 2200 496 -0.0009093 2201 496 -0.001058 2201 496 -0.001021 2202 494 -0.0009711 2203 494 -0.0009587 2203 493 -0.000934 2204 492 -0.0009959 2205 492 -0.001008 2205 491 -0.0009711 2206 491 -0.0009464 2207 489 -0.0009959 2207 489 -0.0009959 2208 489 -0.001008 2209 488 -0.001095 2209 487 -0.001021 2210 486 -0.001045 2211 486 -0.001132 2212 485 -0.00107 2212 484 -0.001144 2213 484 -0.001058 2214 483 -0.001058 2214 482 -0.001095 2215 481 -0.001157 2216 481 -0.001132 2216 481 -0.001132 2217 480 -0.001132 2218 479 -0.001181 2218 478 -0.001144 2219 478 -0.001058 2220 477 -0.001082 2220 477 -0.001181 2221 476 -0.001144 2222 474 -0.0009711 2222 474 -0.001243 2223 474 -0.001021 2224 473 -0.001268 2224 472 -0.001219 2225 472 -0.001219 2226 471 -0.001206 2226 471 -0.0009835 2227 470 -0.001157 2228 469 -0.00112 2228 468 -0.001256 2229 467 -0.001256 2230 467 -0.001157 2230 467 -0.001095 2231 466 -0.001132 2232 465 -0.001231 2232 464 -0.001243 2233 464 -0.001243 2234 463 -0.001293 2234 462 -0.001256 2235 462 -0.001256 2236 460 -0.001293 2236 460 -0.001243 2237 460 -0.00128 2238 459 -0.001317 2238 458 -0.001305 2239 458 -0.001268 2240 456 -0.001317 2240 456 -0.001317 2241 456 -0.001219 2242 455 -0.001416 2243 454 -0.001305 2243 453 -0.001355 2244 453 -0.001392 2245 453 -0.001441 2245 452 -0.001379 2246 450 -0.001317 2247 450 -0.001416 2247 449 -0.001454 2248 449 -0.001491 2249 449 -0.001317 2249 447 -0.001355 2250 446 -0.001416 2251 446 -0.001392 2251 446 -0.001491 2252 445 -0.001367 2253 444 -0.001454 2253 443 -0.001392 2254 442 -0.001454 2255 442 -0.001466 2255 442 -0.001392 2256 441 -0.001454 2257 440 -0.001404 2257 439 -0.001404 2258 439 -0.001491 2259 438 -0.001491 2259 437 -0.00154 2260 436 -0.001565 2261 436 -0.001478 2261 435 -0.001515 2262 434 -0.001515 2263 434 -0.001515 2263 433 -0.001404 2264 433 -0.001528 2265 432 -0.001515 2265 431 -0.001565 2266 431 -0.001515 2267 430 -0.001515 2267 429 -0.001553 2268 429 -0.001553 2269 428 -0.001553 2269 427 -0.001553 2270 426 -0.001565 2271 426 -0.001553 2271 424 -0.001565 2272 424 -0.001577 2273 424 -0.001639 2273 423 -0.001627 2274 422 -0.001614 2275 421 -0.001553 2276 421 -0.001553 2276 421 -0.00159 2277 419 -0.001577 2278 418 -0.001528 2278 418 -0.001565 2279 417 -0.001565 2280 417 -0.00154 2280 416 -0.001602 2281 415 -0.00154 2282 415 -0.001515 2282 414 -0.001491 2283 413 -0.001515 2284 412 -0.001454 2284 412 -0.001466 2285 411 -0.001515 2286 410 -0.001503 2286 410 -0.001466 2287 409 -0.001478 2288 408 -0.001441 2288 408 -0.001317 2289 407 -0.001379 2290 406 -0.001305 2290 406 -0.001268 2291 405 -0.001268 2292 404 -0.001206 2292 404 -0.001132 2293 403 -0.001169 2294 403 -0.001082 2294 402 -0.001082 2295 401 -0.001033 2296 401 -0.001033 2296 401 -0.0009464 2297 399 -0.0008969 2298 399 -0.0008598 2298 399 -0.0008845 2299 398 -0.0008103 2300 397 -0.000699 2300 396 -0.0006124 2301 396 -0.0005258 2302 395 -0.0005134 2302 394 -0.0004886 2303 394 -0.0003897 2304 393 -0.0004021 2304 392 -0.0003649 2305 392 -0.000266 2306 390 -0.0002289 2307 390 -0.000167 2307 389 -0.0001423 2308 388 -5.567e-05 2309 388 6.185e-06 2309 387 6.185e-06 2310 387 6.185e-06 2311 386 1.856e-05 2311 385 0.0001423 2312 384 0.0001423 2313 384 0.0002165 2313 384 0.000266 2314 382 0.0002783 2315 381 0.0002907 2315 381 0.0004021 2316 380 0.0004268 2317 380 0.0004639 2317 379 0.0005134 2318 378 0.0005629 2319 378 0.0005629 2319 378 0.0006495 2320 376 0.0006371 2321 376 0.0007113 2321 375 0.000699 2322 374 0.0007113 2323 374 0.0007608 2323 373 0.0008103 2324 371 0.0008227 2325 371 0.0008474 2325 370 0.0008103 2326 370 0.0008598 2327 369 0.0009216 2327 368 0.0009711 2328 368 0.0009835 2329 367 0.0009587 2329 367 0.0009216 2330 365 0.001008 2331 365 0.0009464 2331 364 0.001008 2332 364 0.001021 2333 363 0.00107 2333 362 0.001082 2334 362 0.00107 2335 361 0.00112 2335 360 0.001157 2336 360 0.001181 2337 359 0.001132 2338 359 0.001132 2338 358 0.001157 2339 357 0.001132 2340 356 0.001194 2340 356 0.00112 2341 355 0.001169 2342 355 0.001169 2342 354 0.001144 2343 353 0.00112 2344 353 0.001157 2344 352 0.001206 2345 351 0.001157 2346 350 0.001194 2346 349 0.001157 2347 349 0.001157 2348 349 0.001132 2348 348 0.001144 2349 346 0.001206 2350 346 0.001082 2350 345 0.001157 2351 345 0.001169 2352 345 0.001082 2352 343 0.001206 2353 343 0.001181 2354 342 0.001157 2354 342 0.001157 2355 341 0.001095 2356 340 0.001107 2356 339 0.00112 2357 338 0.001082 2358 338 0.001132 2358 337 0.001157 2359 337 0.001157 2360 336 0.001169 2360 335 0.001194 2361 335 0.00112 2362 334 0.001194 2362 333 0.001144 2363 333 0.001132 2364 332 0.001144 2364 331 0.001132 2365 331 0.001107 2366 330 0.00112 2366 329 0.00112 2367 329 0.001095 2368 328 0.001107 2369 328 0.001095 2369 327 0.001157 2370 326 0.001144 2371 326 0.00112 2371 324 0.001095 2372 324 0.001058 2373 323 0.001082 2373 322 0.001095 2374 321 0.001045 2375 321 0.001045 2375 320 0.001021 2376 320 0.001008 2377 319 0.0009959 2377 318 0.001045 2378 317 0.001021 2379 317 0.001058 2379 317 0.001033 2380 316 0.001058 2381 315 0.001033 2381 314 0.0009835 2382 313 0.001008 2383 313 0.0009959 2383 312 0.0009216 2384 311 0.0009711 2385 310 0.001008 2385 310 0.0009835 2386 310 0.001008 2387 309 0.0009216 2387 308 0.0009216 2388 307 0.0008845 2389 306 0.0009093 2389 306 0.0009835 2390 306 0.000934 2391 305 0.0009587 2391 304 0.0009093 2392 304 0.0009093 2393 302 0.0008969 2393 302 0.000934 2394 302 0.0008969 2395 301 0.0008598 2395 300 0.0008103 2396 299 0.0008227 2397 299 0.0008474 2397 298 0.0009093 2398 297 0.0009216 2399 296 0.0008969 2400 296 0.0008969 2400 295 0.0008474 2401 295 0.0008474 2402 293 0.0008474 2402 293 0.000835 2403 292 0.0007979 2404 292 0.0008227 2404 292 0.0007979 2405 291 0.0008227 2406 290 0.0008474 2406 289 0.0008845 2407 288 0.0008103 2408 288 0.0007608 2408 287 0.0007361 2409 286 0.0007361 2410 286 0.0007484 2410 285 0.0007608 2411 284 0.0007608 2412 284 0.0008227 2412 283 0.0008103 2413 283 0.000699 2414 282 0.0007979 2414 281 0.0006618 2415 281 0.0006742 2416 280 0.000699 2416 279 0.0007608 2417 278 0.000699 2418 277 0.000699 2418 277 0.0006495 2419 276 0.0006866 2420 276 0.0006124 2420 274 0.000699 2421 274 0.0006618 2422 274 0.0006371 2422 273 0.0006371 2423 273 0.0006 2424 271 0.0006 2424 270 0.0005752 2425 270 0.0005876 2426 270 0.0006 2426 268 0.0006247 2427 268 0.0004886 2428 267 0.0005752 2428 267 0.0005752 2429 267 0.0005876 2430 265 0.0005505 2431 265 0.0005629 2431 264 0.0004639 2432 263 0.0004392 2433 263 0.0004392 2433 262 0.0004639 2434 261 0.000501 2435 261 0.0005258 2435 260 0.0004392 2436 260 0.0004021 2437 259 0.0004144 2437 258 0.0004515 2438 257 0.0004515 2439 256 0.0004515 2439 256 0.0004639 2440 255 0.0004021 2441 254 0.0004268 2441 254 0.0004515 2442 253 0.0004021 2443 252 0.0004021 2443 252 0.0004515 2444 251 0.0004268 2445 250 0.0003649 2445 250 0.0003526 2446 249 0.0003278 2447 249 0.0004021 2447 248 0.0003649 2448 247 0.0004021 2449 246 0.0002907 2449 245 0.0003278 2450 245 0.0003278 2451 244 0.0003031 2451 243 0.0003155 2452 243 0.0003278 2453 242 0.0003031 2453 242 0.000266 2454 241 0.0003031 2455 240 0.0002165 2455 239 0.0002783 2456 239 0.0002289 2457 238 0.0002536 2457 238 0.0002412 2458 237 0.0002907 2459 237 0.000167 2459 236 0.000167 2460 234 0.0002289 2461 234 0.0001917 2461 234 0.0001794 2462 233 0.0001917 2463 232 0.0001794 2464 231 0.0001794 2464 231 0.0001546 2465 230 0.000167 2466 230 0.0001299 2466 229 0.0001052 2467 227 9.278e-05 2468 227 8.041e-05 2468 227 0.0001299 2469 227 5.567e-05 2470 226 9.278e-05 2470 226 8.041e-05 2471 224 0.0001052 2472 224 6.804e-05 2472 222 6.804e-05 2473 221 1.856e-05 2474 221 6.185e-06 2474 220 5.567e-05 2475 220 0.0001052 2476 219 5.567e-05 2476 218 1.856e-05 2477 218 6.804e-05 2478 217 3.093e-05 2478 217 6.185e-06 2479 216 6.185e-06 2480 215 6.185e-06 2480 214 6.185e-06 2481 213 6.185e-06 2482 213 6.185e-06 2482 213 6.185e-06 2483 212 6.185e-06 2484 211 6.185e-06 2484 210 -1.856e-05 2485 209 -5.567e-05 2486 209 -4.33e-05 2486 209 6.185e-06 2487 208 6.185e-06 2488 207 -5.567e-05 2488 206 -0.0001175 2489 206 -9.278e-05 2490 205 -3.093e-05 2490 204 -5.567e-05 2491 204 -3.093e-05 2492 202 -9.278e-05 2492 202 -5.567e-05 2493 202 -6.804e-05 2494 201 -0.0001052 2495 201 -5.567e-05 2495 200 -0.000167 2496 199 -0.0001423 2497 199 -0.0001175 2497 199 -0.000167 2498 198 -0.000167 2499 197 -0.000167 2499 196 -0.0001052 2500 195 -0.0001794 2501 195 -0.0002289 2501 194 -0.0001794 2502 194 -0.0002041 2503 193 -0.0002165 2503 192 -0.0001794 2504 191 -0.0002289 2505 191 -0.0002536 2505 190 -0.0002783 2506 190 -0.0002289 2507 189 -0.0003278 2507 188 -0.0003155 2508 188 -0.0002783 2509 187 -0.000266 2509 186 -0.000266 2510 185 -0.0002783 2511 184 -0.0002907 2511 184 -0.0003155 2512 184 -0.0003155 2513 183 -0.0002783 2513 182 -0.0003526 2514 181 -0.0003278 2515 181 -0.0003649 2515 180 -0.0003526 2516 179 -0.0003155 2517 179 -0.0003649 2517 177 -0.0003649 2518 177 -0.0004515 2519 177 -0.0004144 2519 176 -0.0004021 2520 176 -0.0004021 2521 174 -0.0003897 2521 174 -0.0003897 2522 174 -0.0004021 2523 172 -0.0004144 2523 171 -0.0004268 2524 171 -0.000501 2525 171 -0.0005381 2526 170 -0.0004763 2526 169 -0.0005505 2527 168 -0.0005381 2528 168 -0.000501 2528 167 -0.0004886 2529 166 -0.000501 2530 166 -0.0005258 2530 165 -0.0004886 2531 164 -0.0004763 2532 164 -0.0005258 2532 163 -0.0006247 2533 162 -0.0005381 2534 162 -0.0006247 2534 161 -0.0005752 2535 160 -0.0005752 2536 159 -0.0005876 2536 159 -0.0005629 2537 159 -0.0005629 2538 157 -0.0006 2538 156 -0.0005629 2539 156 -0.0005629 2540 156 -0.0006618 2540 156 -0.0006495 2541 155 -0.0006618 2542 154 -0.0006618 2542 153 -0.0007113 2543 152 -0.000699 2544 152 -0.0006371 2544 151 -0.0006247 2545 150 -0.0007237 2546 150 -0.0007237 2546 149 -0.0007113 2547 149 -0.000699 2548 148 -0.0007237 2548 147 -0.0007361 2549 146 -0.0007113 2550 145 -0.0007608 2550 145 -0.0007484 2551 144 -0.0007732 2552 144 -0.0007732 2552 142 -0.0007237 2553 142 -0.0007361 2554 141 -0.0007979 2554 141 -0.0007732 2555 140 -0.0008103 2556 140 -0.0008227 2557 138 -0.0008103 2557 138 -0.0007855 2558 137 -0.0007855 2559 137 -0.000835 2559 136 -0.0008227 2560 135 -0.0008721 2561 134 -0.0008227 2561 134 -0.0009093 2562 134 -0.0008721 2563 132 -0.0008969 2563 132 -0.0009093 2564 131 -0.0008969 2565 131 -0.0008227 2565 130 -0.0008969 2566 129 -0.000934 2567 129 -0.0009093 2567 127 -0.0009216 2568 127 -0.0008845 2569 127 -0.0009216 2569 126 -0.0009216 2570 126 -0.0009959 2571 124 -0.0009216 2571 124 -0.001008 2572 123 -0.0009711 2573 123 -0.001021 2573 121 -0.0009959 2574 121 -0.0009959 2575 120 -0.001082 2575 120 -0.001045 2576 119 -0.0009959 2577 118 -0.001021 2577 117 -0.001045 2578 117 -0.001033 2579 116 -0.001021 2579 115 -0.001033 2580 115 -0.001045 2581 115 -0.001058 2581 113 -0.001157 2582 113 -0.001132 2583 112 -0.00112 2583 112 -0.001082 2584 111 -0.00112 2585 110 -0.001095 2585 109 -0.00107 2586 109 -0.00112 2587 108 -0.001045 2588 107 -0.001169 2588 106 -0.001169 2589 106 -0.001181 2590 106 -0.001144 2590 105 -0.001169 2591 104 -0.001157 2592 103 -0.001132 2592 102 -0.001144 2593 102 -0.001169 2594 102 -0.001132 2594 101 -0.001132 2595 100 -0.001157 2596 99 -0.001305 2596 98 -0.001243 2597 98 -0.001219 2598 97 -0.001219 2598 96 -0.001219 2599 96 -0.001181 2600 95 -0.001243 2600 95 -0.001256 2601 94 -0.001256 2602 93 -0.001392 2602 92 -0.001293 2603 92 -0.001243 2604 91 -0.001256 2604 90 -0.001293 2605 90 -0.001256 2606 89 -0.001317 2606 89 -0.001355 2607 88 -0.001416 2608 88 -0.00128 2608 86 -0.001355 2609 86 -0.001367 2610 84 -0.001342 2610 84 -0.001367 2611 84 -0.001379 2612 84 -0.001392 2612 83 -0.001379 2613 82 -0.001392 2614 81 -0.001404 2614 81 -0.001454 2615 80 -0.001454 2616 79 -0.001404 2616 78 -0.001441 2617 77 -0.001454 2618 77 -0.001503 2618 77 -0.001441 2619 76 -0.001441 2620 75 -0.001441 2621 75 -0.001454 2621 73 -0.001503 2622 73 -0.001491 2623 72 -0.001515 2623 71 -0.001491 2624 71 -0.001503 2625 70 -0.001491 2625 70 -0.001466 2626 69 -0.001491 2627 68 -0.001577 2627 67 -0.001577 2628 66 -0.00154 2629 66 -0.001553 2629 66 -0.001565 2630 65 -0.001565 2631 64 -0.001565 2631 64 -0.00159 2632 63 -0.001602 2633 63 -0.001627 2633 61 -0.001652 2634 60 -0.001639 2635 59 -0.001614 2635 59 -0.001639 2636 59 -0.001664 2637 58 -0.001763 2637 57 -0.001713 2638 57 -0.001639 2639 56 -0.001639 2639 55 -0.001689 2640 55 -0.001676 2641 54 -0.001689 2641 53 -0.001689 2642 52 -0.001713 2643 52 -0.001713 2643 52 -0.001763 2644 50 -0.00175 2645 50 -0.001676 2645 49 -0.001812 2646 48 -0.001763 2647 48 -0.001738 2647 47 -0.00175 2648 46 -0.001788 2649 46 -0.001788 2649 45 -0.0018 2650 44 -0.001788 2651 44 -0.001812 2652 43 -0.001849 2652 43 -0.001837 2653 42 -0.001837 2654 41 -0.001849 2654 40 -0.001812 2655 40 -0.001862 2656 40 -0.001911 2656 39 -0.001924 2657 38 -0.001887 2658 38 -0.001874 2658 38 -0.001825 2659 37 -0.001874 2660 37 -0.001899 2660 36 -0.001911 2661 36 -0.001899 2662 36 -0.001911 2662 35 -0.001936 2663 34 -0.001899 2664 34 -0.001924 2664 34 -0.001948 2665 34 -0.001899 2666 34 -0.001887 2666 33 -0.001887 2667 32 -0.001973 2668 30 -0.001986 2668 30 -0.001936 2669 28 -0.001948 2670 27 -0.001973 2670 27 -0.001973 2671 26 -0.002023 2672 26 -0.002035 2672 24 -0.00206 2673 23 -0.002047 2674 23 -0.002035 2674 22 -0.001998 2675 21 -0.001082 2676 21 -0.001874 2676 20 -0.002035 2677 20 -0.00206 2678 20 -0.002084 2678 19 -0.002084 2679 19 -0.002097 2680 18 -0.002097 2680 18 -0.002084 2681 18 -0.00112 2682 17 -0.001874 2683 17 -0.002047 2683 16 -0.002097 2684 16 -0.002233 2685 16 -0.002122 2685 16 -0.002159 2686 15 -0.002122 2687 15 -0.002146 2687 15 -0.002146 2688 14 -0.002109 2689 14 -0.002183 2689 14 -0.002208 2690 13 -0.002159 2691 13 -0.002122 2691 13 -0.002134 2692 13 -0.002146 2693 13 -0.002084 2693 13 -0.002109 2694 13 -0.002221 2695 13 -0.002196 2695 12 -0.002183 2696 12 -0.002245 2697 12 -0.002221 2697 12 -0.002183 2698 12 -0.002196 2699 12 -0.002159 2699 11 -0.002183 2700 11 -0.002171 2701 11 -0.002122 2701 11 -0.002146 2702 11 -0.002134 2703 11 -0.002221 2703 11 -0.002208 2704 11 -0.002208 2705 11 -0.002171 2705 11 -0.002171 2706 11 -0.002196 2707 11 -0.002159 2707 11 -0.002208 2708 11 -0.002183 2709 10 -0.002233 2709 10 -0.002208 2710 10 -0.002196 2711 10 -0.002183 2711 10 -0.002208 2712 10 -0.002221 2713 10 -0.002233 2714 10 -0.002208 2714 10 -0.002208 2715 10 -0.002196 2716 10 -0.002196 2716 10 -0.002196 2717 10 -0.002183 2718 11 -0.002196 2718 10 -0.002196 2719 10 -0.002196 2720 10 -0.002196 2720 9 -0.002183 2721 9 -0.002196 2722 10 -0.002183 2722 9 -0.002171 2723 9 -0.002196 2724 9 -0.002208 2724 9 -0.002196 2725 9 -0.002208 2726 11 -0.002208 2726 9 -0.002196 2727 9 -0.002183 2728 9 -0.002159 2728 9 -0.002183 2729 9 -0.002208 2730 9 -0.002208 2730 9 -0.002196 2731 9 -0.002196 2732 10 -0.002208 2732 9 -0.002196 2733 9 -0.002159 2734 9 -0.002183 2734 9 -0.002183 2735 9 -0.002159 2736 9 -0.002171 2736 9 -0.002221 2737 9 -0.002258 2738 10 -0.002159 2738 9 -0.002183 2739 9 -0.002221 2740 9 -0.002171 2740 9 -0.002159 2741 9 -0.002196 2742 9 -0.002208 2742 9 -0.002196 2743 9 -0.002183 2744 9 -0.002159 2745 9 -0.002171 2745 9 -0.002183 2746 9 -0.002183 2747 9 -0.002183 2747 9 -0.002183 2748 9 -0.002196 2749 9 -0.002196 2749 9 -0.002233 2750 9 -0.002171 2751 10 -0.002196 2751 9 -0.002196 2752 9 -0.002196 2753 9 -0.002183 2753 9 -0.002159 2754 9 -0.002146 2755 9 -0.002183 2755 9 -0.002171 2756 10 -0.002146 2757 9 -0.002134 2757 9 -0.002134 2758 2 0.21 0.05 0.66 0.002 0.007 0.75 2.11 0.83 0.31 0 0.62 0 0 0 4 -6.804e-05 0 5 -6.804e-05 0.3809 5 -5.567e-05 0.7617 5 -5.567e-05 1.143 5 -5.567e-05 1.523 5 -6.804e-05 1.904 5 -9.278e-05 2.285 5 -6.804e-05 2.666 5 -5.567e-05 3.047 6 -5.567e-05 3.428 5 -5.567e-05 3.809 5 -5.567e-05 4.189 5 -4.33e-05 4.57 5 -6.804e-05 4.951 6 -8.041e-05 5.332 6 -5.567e-05 5.713 6 -3.093e-05 6.094 6 -5.567e-05 6.475 6 -4.33e-05 6.855 6 -5.567e-05 7.236 6 -0.0001299 7.617 6 -0.0001299 7.998 8 -0.0001052 8.379 9 -6.804e-05 8.76 9 -3.093e-05 9.141 11 -3.093e-05 9.521 13 6.185e-06 9.902 14 6.185e-06 10.28 16 6.185e-06 10.66 17 3.093e-05 11.04 18 6.804e-05 11.43 20 6.804e-05 11.81 20 4.33e-05 12.19 21 3.093e-05 12.57 23 3.093e-05 12.95 23 1.856e-05 13.33 23 4.33e-05 13.71 24 5.567e-05 14.09 24 8.041e-05 14.47 26 3.093e-05 14.85 26 1.856e-05 15.23 27 6.804e-05 15.62 27 0.0001299 16 28 0.0001546 16.38 29 0.000167 16.76 30 0.000167 17.14 30 0.0001917 17.52 31 0.0001917 17.9 33 0.0001917 18.28 34 0.0002165 18.66 35 0.0002165 19.04 36 0.0002289 19.42 37 0.0002536 19.8 38 0.000266 20.19 38 0.0002783 20.57 38 0.000266 20.95 39 0.0002907 21.33 40 0.0003155 21.71 40 0.0002907 22.09 40 0.0003031 22.47 41 0.0003155 22.85 41 0.0003155 23.23 42 0.0003155 23.61 43 0.0003278 23.99 44 0.0003155 24.38 45 0.0003278 24.76 46 0.0003155 25.14 47 0.0003278 25.52 48 0.0003526 25.9 48 0.0003773 26.28 49 0.0004021 26.66 50 0.0004021 27.04 52 0.0004144 27.42 52 0.0004268 27.8 53 0.0004515 28.18 54 0.0004515 28.56 55 0.0004639 28.95 55 0.0004763 29.33 56 0.0004886 29.71 56 0.0005134 30.09 57 0.0005134 30.47 58 0.0005258 30.85 59 0.0005258 31.23 59 0.0005629 31.61 61 0.0005629 31.99 63 0.0005752 32.37 63 0.0006124 32.75 64 0.0005381 33.13 65 0.0005258 33.52 66 0.0005876 33.9 66 0.0006124 34.28 66 0.0006247 34.66 67 0.0006371 35.04 68 0.0006371 35.42 68 0.0006495 35.8 68 0.0006618 36.18 68 0.0006618 36.56 68 0.0006618 36.94 68 0.0006618 37.32 69 0.0006618 37.71 70 0.0006495 38.09 71 0.0006742 38.47 72 0.0006866 38.85 73 0.0007113 39.23 75 0.0007237 39.61 77 0.0007608 39.99 77 0.0007608 40.37 78 0.0007855 40.75 79 0.0007855 41.13 80 0.0007855 41.51 81 0.0007855 41.89 84 0.0008103 42.28 84 0.0008227 42.66 85 0.000835 43.04 86 0.0008598 43.42 86 0.0008598 43.8 87 0.0008721 44.18 87 0.0008721 44.56 88 0.0008721 44.94 88 0.0008598 45.32 88 0.0008721 45.7 88 0.0009093 46.08 88 0.0009216 46.46 88 0.0009216 46.85 88 0.0008969 47.23 89 0.0008845 47.61 91 0.0009093 47.99 92 0.000934 48.37 93 0.0009587 48.75 95 0.000934 49.13 97 0.000934 49.51 98 0.0009835 49.89 99 0.0009959 50.27 99 0.001008 50.65 100 0.001045 51.04 101 0.001045 51.42 101 0.001008 51.8 102 0.001008 52.18 102 0.001045 52.56 102 0.001045 52.94 103 0.001033 53.32 105 0.001058 53.7 105 0.001058 54.08 106 0.001033 54.46 106 0.001045 54.84 107 0.00107 55.22 109 0.001082 55.61 109 0.001082 55.99 109 0.001095 56.37 110 0.001132 56.75 111 0.001157 57.13 112 0.001144 57.51 113 0.001157 57.89 113 0.001194 58.27 113 0.001219 58.65 115 0.00112 59.03 116 0.001082 59.41 116 0.001144 59.8 117 0.001169 60.18 118 0.001194 60.56 119 0.001206 60.94 119 0.001206 61.32 120 0.001206 61.7 121 0.001231 62.08 122 0.001231 62.46 123 0.001243 62.84 123 0.001256 63.22 124 0.001268 63.6 125 0.00128 63.98 126 0.00128 64.37 127 0.001293 64.75 127 0.00128 65.13 129 0.001293 65.51 129 0.001317 65.89 130 0.001317 66.27 131 0.001317 66.65 131 0.00133 67.03 131 0.001342 67.41 131 0.001342 67.79 133 0.001355 68.17 134 0.001379 68.55 134 0.001379 68.94 136 0.001416 69.32 136 0.001429 69.7 138 0.001416 70.08 138 0.001392 70.46 139 0.001416 70.84 140 0.001441 71.22 140 0.001441 71.6 141 0.001441 71.98 142 0.001454 72.36 142 0.001454 72.74 143 0.001454 73.13 144 0.001478 73.51 145 0.001478 73.89 145 0.001503 74.27 146 0.001503 74.65 147 0.001491 75.03 148 0.001515 75.41 149 0.001528 75.79 149 0.001515 76.17 150 0.001515 76.55 151 0.001528 76.93 152 0.00154 77.31 152 0.001553 77.7 153 0.001553 78.08 155 0.001577 78.46 155 0.001565 78.84 156 0.001577 79.22 156 0.001577 79.6 157 0.001602 79.98 158 0.001627 80.36 159 0.001639 80.74 158 0.001639 81.12 159 0.001639 81.5 159 0.001652 81.88 159 0.001652 82.27 161 0.001664 82.65 162 0.001701 83.03 163 0.001689 83.41 163 0.001689 83.79 165 0.001701 84.17 166 0.00175 84.55 167 0.001775 84.93 168 0.001775 85.31 169 0.001775 85.69 169 0.001775 86.07 170 0.001788 86.46 171 0.001788 86.84 171 0.001825 87.22 171 0.001849 87.6 172 0.001874 87.98 174 0.001862 88.36 174 0.001874 88.74 176 0.001874 89.12 176 0.001899 89.5 177 0.001924 89.88 177 0.001936 90.26 177 0.001948 90.64 180 0.001986 91.03 181 0.002047 91.41 182 0.002097 91.79 183 0.002072 92.17 184 0.002072 92.55 184 0.002109 92.93 184 0.002134 93.31 186 0.002159 93.69 186 0.002171 94.07 187 0.002183 94.45 188 0.002196 94.83 188 0.002233 95.22 188 0.002245 95.6 189 0.002245 95.98 190 0.002258 96.36 191 0.002282 96.74 191 0.002282 97.12 192 0.002295 97.5 193 0.002295 97.88 194 0.00232 98.26 195 0.002332 98.64 196 0.002344 99.02 197 0.002357 99.4 198 0.002357 99.79 199 0.002369 100.2 199 0.002369 100.5 199 0.002406 100.9 200 0.002418 101.3 200 0.002394 101.7 202 0.002431 102.1 202 0.002468 102.5 203 0.00248 102.8 204 0.002468 103.2 205 0.002505 103.6 206 0.002468 104 206 0.002468 104.4 206 0.002493 104.7 207 0.00253 105.1 208 0.002517 105.5 209 0.002555 105.9 209 0.002567 106.3 211 0.002542 106.6 212 0.002542 107 213 0.002592 107.4 213 0.002567 107.8 214 0.002579 108.2 214 0.002567 108.5 214 0.002579 108.9 215 0.002579 109.3 217 0.002616 109.7 217 0.002641 110.1 218 0.002654 110.4 218 0.002654 110.8 219 0.002666 111.2 220 0.002691 111.6 222 0.002703 112 222 0.002703 112.4 224 0.002715 112.7 224 0.002728 113.1 224 0.002753 113.5 225 0.002765 113.9 226 0.002765 114.3 227 0.002765 114.6 227 0.002777 115 228 0.002802 115.4 228 0.00279 115.8 230 0.002802 116.2 230 0.002814 116.5 231 0.002814 116.9 231 0.002827 117.3 231 0.002839 117.7 233 0.002827 118.1 234 0.002851 118.4 234 0.002864 118.8 235 0.002889 119.2 236 0.002889 119.6 237 0.002913 120 238 0.002913 120.4 238 0.002913 120.7 240 0.002913 121.1 241 0.002963 121.5 241 0.002938 121.9 242 0.002963 122.3 242 0.002975 122.6 243 0.002975 123 244 0.002975 123.4 245 0.002988 123.8 246 0.003012 124.2 247 0.003049 124.5 248 0.003037 124.9 249 0.003062 125.3 250 0.003074 125.7 249 0.003074 126.1 250 0.003087 126.4 250 0.003087 126.8 252 0.003087 127.2 252 0.003087 127.6 252 0.003111 128 253 0.003111 128.3 255 0.003124 128.7 255 0.003136 129.1 256 0.003148 129.5 256 0.003148 129.9 257 0.003161 130.3 258 0.003185 130.6 259 0.003198 131 260 0.003198 131.4 261 0.00321 131.8 261 0.00321 132.2 263 0.003223 132.5 263 0.003223 132.9 264 0.00321 133.3 264 0.003235 133.7 266 0.003235 134.1 267 0.00326 134.4 267 0.003272 134.8 268 0.003297 135.2 269 0.003297 135.6 270 0.003309 136 270 0.003334 136.3 271 0.003359 136.7 272 0.003359 137.1 274 0.003371 137.5 274 0.003297 137.9 274 0.003297 138.3 274 0.003322 138.6 275 0.003322 139 277 0.003297 139.4 277 0.003346 139.8 277 0.003359 140.2 277 0.003396 140.5 279 0.003408 140.9 280 0.003383 141.3 281 0.003396 141.7 281 0.003445 142.1 282 0.00347 142.4 283 0.003507 142.8 284 0.003532 143.2 285 0.003532 143.6 286 0.003544 144 286 0.003532 144.3 288 0.003507 144.7 288 0.003507 145.1 289 0.003532 145.5 289 0.003557 145.9 291 0.003557 146.3 291 0.003581 146.6 292 0.003594 147 293 0.003631 147.4 294 0.003705 147.8 295 0.003755 148.2 295 0.003693 148.5 296 0.003606 148.9 297 0.003581 149.3 298 0.003631 149.7 299 0.003668 150.1 300 0.003693 150.4 300 0.003693 150.8 301 0.00368 151.2 300 0.003693 151.6 302 0.00373 152 302 0.00373 152.3 303 0.003755 152.7 305 0.003742 153.1 305 0.003767 153.5 306 0.003755 153.9 306 0.003779 154.2 306 0.003779 154.6 306 0.003755 155 307 0.003755 155.4 308 0.003779 155.8 309 0.003792 156.2 310 0.003816 156.5 311 0.003816 156.9 312 0.003829 157.3 312 0.003829 157.7 313 0.003854 158.1 315 0.003866 158.4 317 0.003891 158.8 317 0.003928 159.2 318 0.003928 159.6 319 0.003928 160 320 0.003928 160.3 320 0.003952 160.7 321 0.003952 161.1 321 0.003965 161.5 321 0.003977 161.9 323 0.003977 162.2 324 0.003977 162.6 324 0.003977 163 324 0.00399 163.4 325 0.004014 163.8 326 0.004014 164.2 327 0.004027 164.5 328 0.004027 164.9 328 0.004027 165.3 329 0.004039 165.7 329 0.004076 166.1 331 0.004076 166.4 331 0.004089 166.8 332 0.004101 167.2 334 0.004126 167.6 334 0.004126 168 335 0.004126 168.3 336 0.00415 168.7 336 0.004175 169.1 337 0.004188 169.5 338 0.004212 169.9 339 0.0042 170.2 339 0.004188 170.6 340 0.004212 171 341 0.004212 171.4 342 0.004188 171.8 342 0.004212 172.1 343 0.004225 172.5 344 0.004225 172.9 345 0.004225 173.3 345 0.004237 173.7 346 0.004274 174.1 346 0.004286 174.4 348 0.004324 174.8 349 0.004324 175.2 349 0.004336 175.6 350 0.004286 176 351 0.004324 176.3 352 0.004336 176.7 353 0.004361 177.1 353 0.004361 177.5 354 0.004373 177.9 355 0.004373 178.2 356 0.00441 178.6 356 0.00441 179 357 0.004423 179.4 359 0.004423 179.8 359 0.004435 180.1 360 0.004435 180.5 360 0.004435 180.9 361 0.004472 181.3 361 0.004484 181.7 362 0.004484 182.1 363 0.004484 182.4 363 0.004509 182.8 364 0.004522 183.2 365 0.004484 183.6 366 0.004484 184 367 0.004484 184.3 367 0.004423 184.7 368 0.004497 185.1 369 0.004571 185.5 370 0.004596 185.9 371 0.004621 186.2 371 0.004621 186.6 373 0.004633 187 373 0.004645 187.4 374 0.004645 187.8 374 0.004645 188.1 375 0.00467 188.5 377 0.004682 188.9 377 0.004719 189.3 378 0.004707 189.7 378 0.004707 190 379 0.004719 190.4 380 0.004732 190.8 381 0.004769 191.2 382 0.004744 191.6 384 0.004744 192 383 0.004769 192.3 384 0.004769 192.7 385 0.004769 193.1 385 0.004794 193.5 386 0.004818 193.9 386 0.004818 194.2 387 0.004831 194.6 388 0.004843 195 389 0.004868 195.4 390 0.004843 195.8 390 0.004856 196.1 392 0.004868 196.5 393 0.00488 196.9 393 0.004893 197.3 394 0.004917 197.7 396 0.00493 198 396 0.00493 198.4 396 0.00493 198.8 398 0.004955 199.2 399 0.004979 199.6 399 0.004967 200 399 0.004979 200.3 400 0.005016 200.7 401 0.005016 201.1 401 0.005029 201.5 402 0.005041 201.9 403 0.005041 202.2 403 0.005066 202.6 404 0.005066 203 405 0.005091 203.4 405 0.005066 203.8 406 0.005041 204.1 406 0.005066 204.5 407 0.005078 204.9 408 0.005091 205.3 410 0.005128 205.7 410 0.00514 206 410 0.005177 206.4 412 0.005177 206.8 412 0.005177 207.2 413 0.00519 207.6 413 0.005214 207.9 414 0.005239 208.3 415 0.005251 208.7 417 0.005264 209.1 417 0.005264 209.5 418 0.005251 209.9 419 0.005276 210.2 419 0.005289 210.6 421 0.005313 211 421 0.005338 211.4 422 0.005363 211.8 423 0.005387 212.1 424 0.005425 212.5 424 0.005412 212.9 425 0.0054 213.3 426 0.0054 213.7 426 0.0054 214 427 0.005412 214.4 428 0.005412 214.8 428 0.005437 215.2 429 0.005449 215.6 430 0.005474 215.9 430 0.005486 216.3 431 0.005499 216.7 431 0.005499 217.1 432 0.005511 217.5 433 0.005536 217.9 434 0.005548 218.2 435 0.005548 218.6 436 0.005561 219 437 0.005585 219.4 438 0.005561 219.8 438 0.005511 220.1 439 0.005573 220.5 440 0.005598 220.9 441 0.00561 221.3 442 0.005647 221.7 442 0.005647 222 442 0.00566 222.4 442 0.00566 222.8 444 0.00566 223.2 444 0.005684 223.6 445 0.005684 223.9 446 0.005697 224.3 446 0.005709 224.7 447 0.005709 225.1 449 0.005722 225.5 450 0.005746 225.8 450 0.005771 226.2 450 0.005709 226.6 452 0.005697 227 453 0.005709 227.4 453 0.005771 227.8 454 0.00582 228.1 455 0.005845 228.5 456 0.005833 228.9 457 0.005808 229.3 458 0.005858 229.7 460 0.005907 230 460 0.005907 230.4 461 0.005907 230.8 463 0.005944 231.2 463 0.005969 231.6 464 0.005957 231.9 464 0.006006 232.3 464 0.006018 232.7 464 0.005994 233.1 465 0.006031 233.5 465 0.006031 233.8 467 0.006006 234.2 467 0.006006 234.6 468 0.006006 235 469 0.006031 235.4 469 0.006031 235.8 471 0.006043 236.1 472 0.006056 236.5 472 0.00608 236.9 473 0.006105 237.3 474 0.006142 237.7 475 0.006154 238 476 0.006167 238.4 476 0.006179 238.8 477 0.006179 239.2 478 0.006192 239.6 478 0.006192 239.9 478 0.006204 240.3 480 0.006216 240.7 481 0.006241 241.1 481 0.006266 241.5 481 0.006278 241.8 483 0.006278 242.2 483 0.006278 242.6 485 0.006291 243 485 0.006303 243.4 486 0.006328 243.8 487 0.00634 244.1 487 0.00634 244.5 488 0.00634 244.9 489 0.006352 245.3 489 0.006365 245.7 490 0.006377 246 491 0.006377 246.4 492 0.00639 246.8 492 0.00639 247.2 493 0.006414 247.6 495 0.006427 247.9 496 0.006451 248.3 496 0.006476 248.7 498 0.006489 249.1 499 0.006501 249.5 499 0.006489 249.8 499 0.006513 250.2 501 0.00655 250.6 501 0.00655 251 502 0.006563 251.4 502 0.00655 251.7 503 0.006575 252.1 503 0.006587 252.5 504 0.006575 252.9 505 0.006587 253.3 506 0.006587 253.7 506 0.006587 254 507 0.006625 254.4 508 0.006649 254.8 509 0.006649 255.2 510 0.006662 255.6 510 0.006686 255.9 511 0.006699 256.3 512 0.006711 256.7 513 0.006736 257.1 514 0.006748 257.5 514 0.006748 257.8 515 0.006761 258.2 515 0.006761 258.6 516 0.006785 259 517 0.006785 259.4 518 0.006785 259.7 518 0.006798 260.1 519 0.00681 260.5 520 0.006835 260.9 521 0.006823 261.3 521 0.006847 261.7 522 0.00686 262 523 0.006872 262.4 524 0.006897 262.8 525 0.006884 263.2 526 0.006897 263.6 526 0.006897 263.9 528 0.006921 264.3 528 0.006959 264.7 528 0.006959 265.1 530 0.006996 265.5 530 0.007008 265.8 531 0.00702 266.2 532 0.007033 266.6 532 0.007058 267 534 0.00702 267.4 534 0.00702 267.7 535 0.007058 268.1 536 0.007058 268.5 536 0.007095 268.9 537 0.007119 269.3 538 0.007119 269.6 539 0.007144 270 540 0.007107 270.4 540 0.007058 270.8 542 0.007058 271.2 542 0.007095 271.6 542 0.007095 271.9 543 0.007119 272.3 544 0.007157 272.7 545 0.007169 273.1 546 0.007206 273.5 546 0.007169 273.8 547 0.007119 274.2 548 0.007194 274.6 549 0.007218 275 549 0.007218 275.4 549 0.007231 275.7 550 0.007255 276.1 552 0.007293 276.5 553 0.007293 276.9 553 0.007293 277.3 554 0.007317 277.6 555 0.007342 278 556 0.007367 278.4 557 0.00733 278.8 557 0.007354 279.2 558 0.007392 279.6 559 0.007392 279.9 559 0.007416 280.3 560 0.007429 280.7 561 0.007466 281.1 562 0.007466 281.5 563 0.007453 281.8 564 0.007491 282.2 564 0.007491 282.6 565 0.007515 283 566 0.00754 283.4 567 0.007528 283.7 567 0.007528 284.1 568 0.007552 284.5 568 0.007577 284.9 569 0.007602 285.3 571 0.00759 285.6 571 0.007565 286 571 0.007565 286.4 573 0.00759 286.8 573 0.007614 287.2 574 0.007627 287.5 574 0.007651 287.9 576 0.007651 288.3 576 0.007664 288.7 578 0.007688 289.1 578 0.007688 289.5 578 0.007726 289.8 580 0.007738 290.2 581 0.007738 290.6 581 0.007738 291 582 0.007738 291.4 582 0.007738 291.7 583 0.007738 292.1 584 0.007775 292.5 585 0.0078 292.9 585 0.007812 293.3 586 0.007837 293.6 587 0.007849 294 588 0.007812 294.4 589 0.007738 294.8 589 0.00775 295.2 591 0.00775 295.5 592 0.007787 295.9 592 0.007849 296.3 592 0.007924 296.7 593 0.007911 297.1 594 0.007911 297.5 594 0.007924 297.8 596 0.007924 298.2 596 0.007924 298.6 597 0.007998 299 599 0.007985 299.4 598 0.007973 299.7 599 0.007948 300.1 600 0.007961 300.5 601 0.007998 300.9 601 0.008035 301.3 602 0.00801 301.6 603 0.008047 302 603 0.008109 302.4 604 0.008134 302.8 605 0.008134 303.2 606 0.008134 303.5 607 0.008121 303.9 607 0.008134 304.3 608 0.008146 304.7 609 0.008171 305.1 609 0.008134 305.4 610 0.008121 305.8 611 0.008146 306.2 612 0.008196 306.6 613 0.008183 307 614 0.00822 307.4 614 0.008233 307.7 616 0.008245 308.1 617 0.008258 308.5 617 0.008245 308.9 618 0.008258 309.3 619 0.008282 309.6 620 0.00827 310 621 0.008282 310.4 621 0.008319 310.8 621 0.008319 311.2 622 0.008344 311.5 623 0.008369 311.9 624 0.008369 312.3 625 0.008394 312.7 625 0.008319 313.1 626 0.008307 313.4 627 0.008319 313.8 628 0.008356 314.2 628 0.008381 314.6 629 0.008418 315 630 0.008443 315.4 631 0.008455 315.7 632 0.008431 316.1 632 0.008418 316.5 633 0.008455 316.9 633 0.00848 317.3 634 0.008505 317.6 635 0.00853 318 635 0.008542 318.4 636 0.008542 318.8 636 0.008542 319.2 637 0.008554 319.5 638 0.008542 319.9 639 0.008554 320.3 640 0.008579 320.7 642 0.008592 321.1 642 0.008604 321.4 643 0.008604 321.8 643 0.008641 322.2 644 0.008653 322.6 646 0.008653 323 646 0.008678 323.4 646 0.008678 323.7 647 0.008691 324.1 648 0.008703 324.5 649 0.008678 324.9 650 0.008703 325.3 650 0.008703 325.6 650 0.008728 326 650 0.00874 326.4 652 0.00874 326.8 653 0.00874 327.2 653 0.008777 327.5 655 0.008777 327.9 656 0.008802 328.3 657 0.008802 328.7 658 0.008814 329.1 659 0.008839 329.4 660 0.008876 329.8 660 0.008901 330.2 661 0.008864 330.6 661 0.008827 331 662 0.008839 331.3 663 0.008901 331.7 664 0.008864 332.1 664 0.008876 332.5 665 0.008926 332.9 666 0.00895 333.3 667 0.008975 333.6 668 0.008987 334 668 0.008987 334.4 669 0.009 334.8 669 0.008975 335.2 670 0.009 335.5 671 0.009012 335.9 671 0.009 336.3 673 0.009 336.7 674 0.009025 337.1 675 0.009049 337.4 675 0.009074 337.8 676 0.009074 338.2 676 0.009086 338.6 677 0.009111 339 678 0.009123 339.3 678 0.009123 339.7 680 0.009136 340.1 681 0.009123 340.5 681 0.009148 340.9 682 0.009161 341.3 683 0.009173 341.6 683 0.009198 342 685 0.009247 342.4 685 0.009235 342.8 686 0.009222 343.2 686 0.009235 343.5 687 0.009235 343.9 688 0.009247 344.3 689 0.00926 344.7 690 0.00926 345.1 690 0.009272 345.4 691 0.009272 345.8 693 0.009297 346.2 693 0.009284 346.6 693 0.009297 347 694 0.009334 347.3 695 0.009359 347.7 696 0.009334 348.1 696 0.009321 348.5 697 0.009321 348.9 698 0.009371 349.2 699 0.009408 349.6 700 0.00942 350 701 0.009396 350.4 701 0.00942 350.8 702 0.00942 351.2 703 0.009445 351.5 703 0.009445 351.9 703 0.009445 352.3 705 0.00947 352.7 706 0.00947 353.1 707 0.009507 353.4 707 0.009495 353.8 708 0.009507 354.2 709 0.009532 354.6 709 0.009544 355 711 0.009544 355.3 711 0.009556 355.7 712 0.009556 356.1 713 0.009569 356.5 714 0.009594 356.9 714 0.009606 357.2 715 0.009594 357.6 715 0.009618 358 717 0.009618 358.4 717 0.009618 358.8 718 0.009618 359.2 718 0.009643 359.5 719 0.009655 359.9 720 0.009655 360.3 721 0.009668 360.7 721 0.009668 361.1 722 0.009693 361.4 723 0.009693 361.8 724 0.009717 362.2 725 0.009742 362.6 726 0.009754 363 727 0.009767 363.3 728 0.009767 363.7 728 0.009767 364.1 728 0.009767 364.5 729 0.009779 364.9 730 0.009779 365.2 731 0.009804 365.6 731 0.009816 366 732 0.009841 366.4 732 0.009866 366.8 733 0.009853 367.1 734 0.009841 367.5 734 0.009866 367.9 735 0.009866 368.3 736 0.009903 368.7 736 0.009915 369.1 737 0.009928 369.4 738 0.009965 369.8 739 0.009989 370.2 739 0.009965 370.6 740 0.009952 371 742 0.01001 371.3 743 0.01003 371.7 743 0.01005 372.1 743 0.01004 372.5 745 0.01006 372.9 746 0.0101 373.2 746 0.01009 373.6 746 0.01011 374 747 0.01015 374.4 749 0.01016 374.8 749 0.01018 375.1 750 0.01018 375.5 750 0.01018 375.9 751 0.01019 376.3 753 0.01021 376.7 753 0.01021 377.1 753 0.01024 377.4 754 0.01024 377.8 755 0.01026 378.2 756 0.01027 378.6 757 0.01029 379 757 0.01029 379.3 758 0.01032 379.7 758 0.01036 380.1 759 0.01039 380.5 760 0.0104 380.9 761 0.01042 381.2 761 0.01046 381.6 762 0.01046 382 763 0.01046 382.4 764 0.01047 382.8 764 0.01051 383.1 765 0.01055 383.5 766 0.01056 383.9 768 0.01056 384.3 768 0.01058 384.7 769 0.01062 385 770 0.01061 385.4 771 0.01062 385.8 771 0.01066 386.2 771 0.01068 386.6 773 0.01072 387 775 0.01073 387.3 775 0.01074 387.7 775 0.01076 388.1 777 0.01079 388.5 777 0.01083 388.9 778 0.01083 389.2 779 0.01084 389.6 779 0.01083 390 780 0.01082 390.4 781 0.01084 390.8 782 0.01084 391.1 783 0.01086 391.5 784 0.0109 391.9 784 0.01092 392.3 785 0.01092 392.7 786 0.01092 393 786 0.01092 393.4 787 0.01095 393.8 788 0.011 394.2 789 0.01103 394.6 789 0.01102 395 790 0.01102 395.3 792 0.011 395.7 793 0.01107 396.1 793 0.01105 396.5 793 0.01105 396.9 794 0.01105 397.2 796 0.01105 397.6 796 0.01105 398 797 0.01105 398.4 798 0.01103 398.8 799 0.01098 399.1 800 0.01095 399.5 800 0.01093 399.9 801 0.0109 400.3 801 0.01088 400.7 801 0.01086 401 801 0.01078 401.4 801 0.01074 401.8 802 0.01071 402.2 803 0.01066 402.6 803 0.01058 402.9 804 0.01053 403.3 805 0.01047 403.7 806 0.01042 404.1 807 0.01039 404.5 807 0.01031 404.9 808 0.01026 405.2 809 0.01016 405.6 810 0.01011 406 810 0.01005 406.4 811 0.009989 406.8 811 0.009928 407.1 813 0.009866 407.5 814 0.009829 407.9 814 0.009754 408.3 814 0.009705 408.7 815 0.009655 409 816 0.009618 409.4 817 0.009594 409.8 817 0.009569 410.2 818 0.009495 410.6 818 0.00947 410.9 819 0.00942 411.3 820 0.009346 411.7 821 0.009297 412.1 821 0.009272 412.5 822 0.009222 412.9 824 0.009198 413.2 824 0.009148 413.6 825 0.009111 414 826 0.009086 414.4 826 0.009074 414.8 827 0.009037 415.1 828 0.009 415.5 829 0.008987 415.9 829 0.008963 416.3 830 0.008901 416.7 830 0.008901 417 832 0.008876 417.4 832 0.008851 417.8 833 0.008839 418.2 834 0.008827 418.6 835 0.008814 418.9 835 0.008777 419.3 836 0.008765 419.7 837 0.008752 420.1 838 0.008752 420.5 838 0.008703 420.9 839 0.008715 421.2 840 0.008715 421.6 840 0.008728 422 842 0.008703 422.4 843 0.008678 422.8 843 0.008678 423.1 843 0.008678 423.5 844 0.008678 423.9 845 0.008691 424.3 846 0.008703 424.7 847 0.008715 425 847 0.008703 425.4 847 0.008728 425.8 849 0.008703 426.2 849 0.008728 426.6 850 0.00874 426.9 850 0.00874 427.3 851 0.008765 427.7 852 0.008789 428.1 853 0.008802 428.5 854 0.008814 428.8 854 0.008814 429.2 855 0.008839 429.6 856 0.008851 430 857 0.008851 430.4 858 0.008876 430.8 859 0.008901 431.1 859 0.008926 431.5 860 0.008926 431.9 861 0.00895 432.3 861 0.008987 432.7 862 0.008975 433 863 0.009 433.4 864 0.009037 433.8 864 0.009049 434.2 865 0.009074 434.6 866 0.009111 434.9 867 0.009111 435.3 868 0.009086 435.7 868 0.009086 436.1 868 0.009123 436.5 869 0.009099 436.8 871 0.009136 437.2 872 0.009136 437.6 872 0.009161 438 872 0.009161 438.4 874 0.009198 438.8 875 0.00921 439.1 875 0.009235 439.5 876 0.00921 439.9 877 0.00926 440.3 878 0.009284 440.7 879 0.009309 441 879 0.009321 441.4 880 0.009359 441.8 881 0.009359 442.2 882 0.009383 442.6 882 0.00942 442.9 883 0.009396 443.3 884 0.009383 443.7 885 0.009408 444.1 885 0.009445 444.5 886 0.009445 444.8 886 0.009482 445.2 887 0.009507 445.6 888 0.009507 446 889 0.009519 446.4 890 0.009532 446.7 890 0.009569 447.1 892 0.009569 447.5 892 0.009594 447.9 893 0.009618 448.3 893 0.009631 448.7 894 0.009618 449 896 0.009655 449.4 896 0.009693 449.8 897 0.009705 450.2 897 0.009717 450.6 899 0.009705 450.9 899 0.009705 451.3 900 0.009754 451.7 900 0.009754 452.1 901 0.009767 452.5 901 0.009792 452.8 903 0.009816 453.2 904 0.009841 453.6 904 0.009853 454 904 0.009866 454.4 905 0.009866 454.7 906 0.009915 455.1 907 0.00989 455.5 907 0.009915 455.9 908 0.00994 456.3 909 0.009989 456.7 910 0.009965 457 911 0.009977 457.4 911 0.01001 457.8 912 0.01004 458.2 912 0.01004 458.6 912 0.01006 458.9 914 0.01006 459.3 913 0.01004 459.7 913 0.01006 460.1 914 0.01009 460.5 915 0.01009 460.8 915 0.01018 461.2 916 0.01021 461.6 918 0.01024 462 919 0.01027 462.4 921 0.01031 462.7 922 0.01034 463.1 922 0.01036 463.5 924 0.01039 463.9 925 0.01039 464.3 926 0.01041 464.6 928 0.01043 465 928 0.01043 465.4 929 0.01046 465.8 930 0.01047 466.2 931 0.01052 466.6 931 0.01053 466.9 932 0.01055 467.3 932 0.01057 467.7 933 0.01058 468.1 934 0.0106 468.5 935 0.01058 468.8 936 0.01062 469.2 936 0.01063 469.6 937 0.01066 470 938 0.01067 470.4 939 0.01068 470.7 940 0.01071 471.1 940 0.01073 471.5 941 0.01076 471.9 942 0.01076 472.3 943 0.01077 472.6 943 0.01077 473 943 0.01081 473.4 944 0.01084 473.8 946 0.01088 474.2 947 0.01087 474.6 947 0.0109 474.9 948 0.0109 475.3 949 0.01093 475.7 950 0.01098 476.1 950 0.01099 476.5 950 0.011 476.8 952 0.01103 477.2 953 0.01105 477.6 954 0.01107 478 954 0.0111 478.4 955 0.01109 478.7 956 0.0111 479.1 957 0.01112 479.5 957 0.01114 479.9 958 0.01115 480.3 959 0.01119 480.6 960 0.01121 481 960 0.01121 481.4 961 0.01123 481.8 962 0.01125 482.2 963 0.01123 482.5 964 0.01123 482.9 964 0.01128 483.3 965 0.01131 483.7 965 0.01135 484.1 966 0.01137 484.5 967 0.0114 484.8 968 0.01142 485.2 968 0.01142 485.6 969 0.01145 486 971 0.01149 486.4 971 0.01149 486.7 972 0.01149 487.1 972 0.01151 487.5 974 0.01155 487.9 974 0.01156 488.3 975 0.01157 488.6 976 0.01162 489 976 0.01165 489.4 977 0.01166 489.8 978 0.01166 490.2 979 0.01166 490.5 979 0.0117 490.9 980 0.01173 491.3 981 0.01172 491.7 982 0.01175 492.1 983 0.01177 492.5 983 0.0118 492.8 984 0.01181 493.2 985 0.01182 493.6 986 0.01182 494 986 0.01185 494.4 987 0.01187 494.7 988 0.01188 495.1 989 0.01191 495.5 990 0.01194 495.9 990 0.01197 496.3 991 0.01202 496.6 992 0.01202 497 993 0.01194 497.4 993 0.01194 497.8 994 0.01201 498.2 994 0.01206 498.5 996 0.0121 498.9 997 0.01208 499.3 997 0.01206 499.7 998 0.01212 500.1 999 0.01215 500.5 1000 0.01217 500.8 1000 0.01217 501.2 1001 0.01222 501.6 1001 0.01222 502 1002 0.01224 502.4 1003 0.01224 502.7 1004 0.01228 503.1 1004 0.01234 503.5 1005 0.01236 503.9 1006 0.01238 504.3 1007 0.01239 504.6 1007 0.01239 505 1008 0.0124 505.4 1009 0.01244 505.8 1009 0.01246 506.2 1011 0.01248 506.5 1011 0.01249 506.9 1012 0.01254 507.3 1012 0.01254 507.7 1014 0.01256 508.1 1015 0.01256 508.4 1015 0.01256 508.8 1015 0.01261 509.2 1017 0.01264 509.6 1018 0.01265 510 1018 0.01267 510.4 1018 0.01267 510.7 1019 0.01267 511.1 1020 0.01269 511.5 1021 0.0127 511.9 1022 0.01267 512.3 1022 0.01267 512.6 1024 0.0127 513 1024 0.01272 513.4 1025 0.01274 513.8 1026 0.01279 514.2 1026 0.01281 514.5 1027 0.01281 514.9 1028 0.0128 515.3 1029 0.01282 515.7 1029 0.01287 516.1 1030 0.01291 516.4 1031 0.01295 516.8 1032 0.01297 517.2 1033 0.01296 517.6 1033 0.01296 518 1034 0.013 518.4 1034 0.01301 518.7 1036 0.01305 519.1 1036 0.01307 519.5 1037 0.01307 519.9 1037 0.01309 520.3 1039 0.01313 520.6 1040 0.01316 521 1040 0.01318 521.4 1041 0.01319 521.8 1042 0.01321 522.2 1043 0.01322 522.5 1043 0.01326 522.9 1044 0.01324 523.3 1045 0.01326 523.7 1045 0.01328 524.1 1047 0.01328 524.4 1047 0.01329 524.8 1048 0.01335 525.2 1049 0.01337 525.6 1049 0.01342 526 1051 0.01343 526.3 1051 0.01344 526.7 1052 0.01345 527.1 1053 0.0134 527.5 1053 0.01337 527.9 1054 0.01349 528.3 1055 0.01355 528.6 1056 0.01358 529 1056 0.01359 529.4 1058 0.01359 529.8 1058 0.01363 530.2 1058 0.01364 530.5 1060 0.01365 530.9 1060 0.01369 531.3 1061 0.0137 531.7 1061 0.0136 532.1 1062 0.01361 532.4 1063 0.01369 532.8 1065 0.01373 533.2 1065 0.01375 533.6 1065 0.01379 534 1066 0.01379 534.3 1068 0.01381 534.7 1068 0.01384 535.1 1068 0.01387 535.5 1069 0.01389 535.9 1070 0.01392 536.3 1071 0.01395 536.6 1072 0.01396 537 1072 0.01397 537.4 1073 0.014 537.8 1074 0.01402 538.2 1075 0.01403 538.5 1076 0.01407 538.9 1077 0.01407 539.3 1077 0.0141 539.7 1078 0.01411 540.1 1079 0.01415 540.4 1079 0.01415 540.8 1080 0.01415 541.2 1081 0.0142 541.6 1082 0.01422 542 1083 0.01425 542.3 1083 0.01426 542.7 1084 0.01427 543.1 1085 0.01427 543.5 1086 0.01432 543.9 1086 0.01433 544.2 1087 0.01433 544.6 1087 0.01433 545 1089 0.01437 545.4 1090 0.01439 545.8 1090 0.01441 546.2 1091 0.01443 546.5 1092 0.01443 546.9 1093 0.01446 547.3 1094 0.0145 547.7 1094 0.0145 548.1 1094 0.0145 548.4 1095 0.01453 548.8 1096 0.01454 549.2 1097 0.01454 549.6 1097 0.01455 550 1099 0.01458 550.3 1099 0.01459 550.7 1100 0.01462 551.1 1101 0.01465 551.5 1102 0.01469 551.9 1103 0.0147 552.2 1104 0.01472 552.6 1105 0.01474 553 1105 0.01475 553.4 1107 0.01478 553.8 1107 0.01481 554.2 1107 0.01483 554.5 1108 0.01481 554.9 1109 0.01483 555.3 1109 0.01484 555.7 1110 0.01486 556.1 1111 0.01486 556.4 1111 0.01484 556.8 1112 0.01488 557.2 1113 0.01489 557.6 1114 0.01494 558 1115 0.01494 558.3 1115 0.01493 558.7 1117 0.01496 559.1 1118 0.01493 559.5 1118 0.01488 559.9 1119 0.01494 560.2 1119 0.015 560.6 1119 0.01504 561 1121 0.01506 561.4 1122 0.01509 561.8 1122 0.01512 562.1 1123 0.01515 562.5 1124 0.01515 562.9 1125 0.01516 563.3 1126 0.01519 563.7 1126 0.01521 564.1 1127 0.01521 564.4 1128 0.01525 564.8 1129 0.01527 565.2 1129 0.01527 565.6 1130 0.0153 566 1131 0.01531 566.3 1132 0.01532 566.7 1132 0.01535 567.1 1133 0.01536 567.5 1134 0.01533 567.9 1134 0.01536 568.2 1136 0.01533 568.6 1136 0.01542 569 1137 0.01546 569.4 1138 0.01549 569.8 1139 0.01551 570.1 1140 0.01547 570.5 1140 0.01549 570.9 1140 0.01547 571.3 1142 0.01547 571.7 1143 0.01551 572.1 1143 0.01559 572.4 1144 0.01561 572.8 1144 0.01557 573.2 1146 0.01557 573.6 1147 0.01561 574 1147 0.01563 574.3 1147 0.01566 574.7 1149 0.01567 575.1 1149 0.01569 575.5 1151 0.01572 575.9 1151 0.01572 576.2 1152 0.01573 576.6 1153 0.01577 577 1153 0.01579 577.4 1154 0.01582 577.8 1155 0.01583 578.1 1156 0.01585 578.5 1156 0.01585 578.9 1157 0.01585 579.3 1158 0.01587 579.7 1159 0.01588 580 1159 0.01589 580.4 1160 0.01593 580.8 1161 0.01596 581.2 1162 0.01598 581.6 1162 0.01598 582 1163 0.01598 582.3 1164 0.01599 582.7 1165 0.01601 583.1 1165 0.01603 583.5 1167 0.01603 583.9 1167 0.01605 584.2 1168 0.01608 584.6 1169 0.01609 585 1169 0.01611 585.4 1169 0.01613 585.8 1172 0.01615 586.1 1172 0.01617 586.5 1172 0.01619 586.9 1173 0.01621 587.3 1174 0.01624 587.7 1175 0.01624 588 1176 0.01625 588.4 1176 0.01627 588.8 1177 0.01629 589.2 1178 0.01629 589.6 1178 0.01631 590 1179 0.01634 590.3 1180 0.01637 590.7 1181 0.01637 591.1 1182 0.01641 591.5 1183 0.01642 591.9 1184 0.01642 592.2 1184 0.01643 592.6 1185 0.01645 593 1186 0.01647 593.4 1187 0.01646 593.8 1187 0.01645 594.1 1188 0.01648 594.5 1189 0.01655 594.9 1190 0.01657 595.3 1190 0.01658 595.7 1190 0.01662 596 1192 0.01664 596.4 1193 0.01664 596.8 1194 0.01667 597.2 1194 0.01667 597.6 1194 0.01664 598 1196 0.01669 598.3 1197 0.01677 598.7 1197 0.01679 599.1 1197 0.01677 599.5 1199 0.01679 599.9 1199 0.01683 600.2 1199 0.01678 600.6 1199 0.01676 601 1199 0.01678 601.4 1199 0.01676 601.8 1199 0.01678 602.1 1199 0.01676 602.5 1199 0.01676 602.9 1199 0.01676 603.3 1199 0.01674 603.7 1199 0.01674 604 1198 0.01671 604.4 1198 0.01672 604.8 1198 0.01673 605.2 1198 0.01672 605.6 1198 0.01672 605.9 1198 0.01669 606.3 1198 0.01672 606.7 1198 0.01671 607.1 1198 0.01669 607.5 1198 0.01672 607.9 1199 0.01672 608.2 1199 0.01669 608.6 1198 0.01671 609 1198 0.01671 609.4 1199 0.01666 609.8 1199 0.0166 610.1 1198 0.01661 610.5 1199 0.01666 610.9 1199 0.01664 611.3 1199 0.01667 611.7 1199 0.01668 612 1198 0.01669 612.4 1199 0.01671 612.8 1198 0.01672 613.2 1199 0.01669 613.6 1198 0.01671 613.9 1199 0.01663 614.3 1199 0.01666 614.7 1198 0.01664 615.1 1198 0.01664 615.5 1199 0.01662 615.9 1199 0.01666 616.2 1199 0.01668 616.6 1198 0.01668 617 1199 0.01668 617.4 1198 0.01669 617.8 1199 0.01669 618.1 1199 0.01668 618.5 1199 0.01667 618.9 1198 0.01666 619.3 1198 0.01664 619.7 1199 0.01663 620 1198 0.01666 620.4 1198 0.01668 620.8 1199 0.01669 621.2 1199 0.01668 621.6 1198 0.01669 621.9 1198 0.01668 622.3 1199 0.01668 622.7 1199 0.01666 623.1 1198 0.01666 623.5 1199 0.01668 623.8 1199 0.01667 624.2 1199 0.01667 624.6 1198 0.01667 625 1199 0.01666 625.4 1199 0.01667 625.8 1199 0.01666 626.1 1198 0.01667 626.5 1199 0.01669 626.9 1199 0.01669 627.3 1199 0.01667 627.7 1198 0.01664 628 1199 0.01666 628.4 1198 0.01666 628.8 1199 0.01666 629.2 1199 0.01667 629.6 1199 0.01667 629.9 1199 0.01664 630.3 1199 0.01664 630.7 1199 0.01664 631.1 1199 0.01664 631.5 1199 0.01664 631.8 1198 0.01664 632.2 1199 0.01662 632.6 1198 0.01663 633 1198 0.01664 633.4 1198 0.01664 633.8 1199 0.01662 634.1 1199 0.01663 634.5 1198 0.01664 634.9 1198 0.01664 635.3 1199 0.01662 635.7 1199 0.01662 636 1198 0.01662 636.4 1199 0.01662 636.8 1199 0.01664 637.2 1198 0.01664 637.6 1199 0.01663 637.9 1199 0.01664 638.3 1199 0.01662 638.7 1199 0.01663 639.1 1199 0.01662 639.5 1198 0.01664 639.8 1199 0.01664 640.2 1198 0.01664 640.6 1198 0.01664 641 1198 0.01663 641.4 1198 0.01663 641.7 1198 0.01662 642.1 1199 0.01663 642.5 1198 0.01661 642.9 1198 0.01663 643.3 1199 0.01661 643.7 1199 0.0166 644 1199 0.0166 644.4 1198 0.01658 644.8 1198 0.01657 645.2 1198 0.01658 645.6 1198 0.0166 645.9 1198 0.0166 646.3 1199 0.0166 646.7 1199 0.01661 647.1 1198 0.0166 647.5 1198 0.01657 647.8 1198 0.0166 648.2 1199 0.0166 648.6 1198 0.0166 649 1198 0.01658 649.4 1198 0.0166 649.7 1199 0.0166 650.1 1199 0.0166 650.5 1199 0.0166 650.9 1198 0.0166 651.3 1199 0.0166 651.7 1199 0.0166 652 1199 0.01657 652.4 1199 0.01657 652.8 1199 0.01658 653.2 1199 0.01656 653.6 1199 0.01662 653.9 1198 0.0166 654.3 1198 0.0166 654.7 1199 0.0166 655.1 1198 0.0166 655.5 1198 0.01657 655.8 1199 0.0166 656.2 1198 0.01658 656.6 1198 0.01656 657 1198 0.0166 657.4 1199 0.0166 657.7 1199 0.01662 658.1 1199 0.0166 658.5 1198 0.0166 658.9 1198 0.01658 659.3 1199 0.0166 659.6 1198 0.0166 660 1199 0.0166 660.4 1198 0.0166 660.8 1199 0.0166 661.2 1199 0.01661 661.6 1199 0.01662 661.9 1198 0.01662 662.3 1199 0.0166 662.7 1199 0.01656 663.1 1199 0.01655 663.5 1199 0.01655 663.8 1199 0.01655 664.2 1199 0.01656 664.6 1199 0.01657 665 1199 0.0166 665.4 1198 0.01657 665.7 1198 0.01658 666.1 1199 0.01661 666.5 1199 0.01661 666.9 1199 0.0166 667.3 1199 0.01658 667.6 1198 0.01658 668 1199 0.01657 668.4 1199 0.0166 668.8 1199 0.0166 669.2 1198 0.0166 669.6 1198 0.0166 669.9 1199 0.01658 670.3 1199 0.01658 670.7 1199 0.01661 671.1 1199 0.0166 671.5 1199 0.0166 671.8 1199 0.0166 672.2 1198 0.01658 672.6 1199 0.0166 673 1199 0.01657 673.4 1199 0.0166 673.7 1199 0.0166 674.1 1199 0.0166 674.5 1199 0.0166 674.9 1199 0.0166 675.3 1199 0.01656 675.6 1199 0.01655 676 1199 0.01653 676.4 1198 0.01655 676.8 1198 0.01656 677.2 1199 0.0166 677.5 1198 0.01656 677.9 1198 0.01656 678.3 1199 0.01655 678.7 1199 0.01655 679.1 1198 0.01655 679.5 1199 0.01656 679.8 1199 0.01655 680.2 1199 0.01655 680.6 1199 0.0165 681 1199 0.0165 681.4 1199 0.01651 681.7 1199 0.01653 682.1 1199 0.01655 682.5 1199 0.01656 682.9 1199 0.01657 683.3 1199 0.01655 683.6 1199 0.01653 684 1199 0.01653 684.4 1199 0.01653 684.8 1198 0.01653 685.2 1199 0.01655 685.5 1199 0.01655 685.9 1199 0.01655 686.3 1199 0.01653 686.7 1199 0.01652 687.1 1199 0.01652 687.5 1198 0.01646 687.8 1199 0.01646 688.2 1198 0.0165 688.6 1199 0.01648 689 1199 0.01652 689.4 1199 0.01652 689.7 1199 0.01652 690.1 1199 0.0165 690.5 1199 0.01652 690.9 1199 0.01651 691.3 1199 0.0165 691.6 1199 0.01652 692 1199 0.01651 692.4 1199 0.0165 692.8 1199 0.0165 693.2 1199 0.01646 693.5 1199 0.01645 693.9 1199 0.01648 694.3 1199 0.0165 694.7 1199 0.01655 695.1 1199 0.01652 695.5 1199 0.0165 695.8 1199 0.01648 696.2 1199 0.01646 696.6 1198 0.01647 697 1199 0.01648 697.4 1199 0.01648 697.7 1198 0.0165 698.1 1199 0.0165 698.5 1199 0.0165 698.9 1199 0.0165 699.3 1199 0.0165 699.6 1199 0.01647 700 1198 0.01646 700.4 1199 0.0165 700.8 1199 0.0165 701.2 1199 0.01651 701.5 1199 0.0165 701.9 1198 0.01648 702.3 1198 0.0165 702.7 1198 0.0165 703.1 1199 0.0165 703.4 1199 0.01652 703.8 1199 0.01651 704.2 1198 0.01646 704.6 1199 0.01647 705 1199 0.01645 705.4 1199 0.01647 705.7 1199 0.01647 706.1 1199 0.0165 706.5 1199 0.0165 706.9 1199 0.0165 707.3 1199 0.0165 707.6 1199 0.01646 708 1198 0.01648 708.4 1199 0.0165 708.8 1199 0.0165 709.2 1199 0.0165 709.5 1198 0.01651 709.9 1199 0.0165 710.3 1199 0.0165 710.7 1199 0.0165 711.1 1199 0.0165 711.4 1199 0.01643 711.8 1199 0.01646 712.2 1198 0.01645 712.6 1199 0.0165 713 1199 0.01651 713.4 1198 0.0165 713.7 1198 0.0165 714.1 1199 0.0165 714.5 1199 0.01651 714.9 1199 0.01651 715.3 1199 0.01651 715.6 1199 0.0165 716 1199 0.0165 716.4 1199 0.01648 716.8 1198 0.0165 717.2 1199 0.0165 717.5 1198 0.01646 717.9 1199 0.01642 718.3 1199 0.01648 718.7 1199 0.0165 719.1 1199 0.01647 719.4 1199 0.01646 719.8 1199 0.01646 720.2 1199 0.01647 720.6 1199 0.01646 721 1198 0.01647 721.3 1199 0.01645 721.7 1199 0.01645 722.1 1199 0.01647 722.5 1198 0.01647 722.9 1199 0.01645 723.3 1199 0.01647 723.6 1199 0.01646 724 1199 0.0164 724.4 1199 0.01641 724.8 1199 0.01645 725.2 1198 0.01645 725.5 1199 0.01645 725.9 1199 0.01645 726.3 1199 0.01643 726.7 1199 0.01645 727.1 1199 0.01646 727.4 1199 0.01647 727.8 1199 0.01645 728.2 1199 0.01645 728.6 1198 0.01645 729 1199 0.01642 729.3 1199 0.01643 729.7 1198 0.0164 730.1 1199 0.0164 730.5 1198 0.0164 730.9 1199 0.0164 731.3 1199 0.0164 731.6 1199 0.01642 732 1199 0.01641 732.4 1199 0.01641 732.8 1199 0.01642 733.2 1198 0.01645 733.5 1198 0.01648 733.9 1199 0.01645 734.3 1199 0.01641 734.7 1198 0.01639 735.1 1199 0.01642 735.4 1199 0.01642 735.8 1199 0.01643 736.2 1198 0.01645 736.6 1198 0.01641 737 1199 0.01645 737.3 1199 0.01646 737.7 1199 0.01645 738.1 1199 0.01643 738.5 1198 0.01645 738.9 1199 0.01645 739.2 1199 0.01646 739.6 1199 0.01642 740 1199 0.01642 740.4 1199 0.01641 740.8 1199 0.01641 741.2 1199 0.01642 741.5 1199 0.01643 741.9 1199 0.01639 742.3 1199 0.0164 742.7 1199 0.01642 743.1 1199 0.01643 743.4 1199 0.01642 743.8 1199 0.01643 744.2 1199 0.01641 744.6 1199 0.01641 745 1199 0.01642 745.3 1199 0.01641 745.7 1198 0.01641 746.1 1198 0.01636 746.5 1199 0.01636 746.9 1199 0.01641 747.2 1199 0.0164 747.6 1198 0.01639 748 1198 0.0164 748.4 1199 0.01641 748.8 1199 0.01643 749.2 1198 0.01643 749.5 1199 0.01645 749.9 1199 0.01641 750.3 1198 0.0164 750.7 1199 0.0164 751.1 1198 0.0164 751.4 1199 0.01636 751.8 1199 0.01637 752.2 1199 0.01641 752.6 1199 0.01641 753 1198 0.0164 753.3 1199 0.01639 753.7 1199 0.01641 754.1 1199 0.0164 754.5 1199 0.01639 754.9 1198 0.0164 755.2 1199 0.01642 755.6 1198 0.01642 756 1198 0.01641 756.4 1198 0.01643 756.8 1198 0.01645 757.1 1199 0.01645 757.5 1199 0.01645 757.9 1199 0.01645 758.3 1199 0.01642 758.7 1199 0.01645 759.1 1199 0.01645 759.4 1199 0.01642 759.8 1199 0.01641 760.2 1199 0.01642 760.6 1199 0.01641 761 1199 0.01641 761.3 1198 0.0164 761.7 1199 0.0164 762.1 1199 0.01641 762.5 1198 0.0164 762.9 1199 0.01641 763.2 1199 0.01637 763.6 1198 0.01635 764 1199 0.01637 764.4 1199 0.01639 764.8 1199 0.01642 765.1 1199 0.01645 765.5 1198 0.01646 765.9 1199 0.01643 766.3 1199 0.01642 766.7 1198 0.01642 767.1 1198 0.01645 767.4 1199 0.01642 767.8 1199 0.01642 768.2 1199 0.01641 768.6 1199 0.01641 769 1199 0.01641 769.3 1199 0.01642 769.7 1199 0.0164 770.1 1198 0.0164 770.5 1199 0.0164 770.9 1199 0.0164 771.2 1199 0.0164 771.6 1199 0.01641 772 1198 0.01641 772.4 1198 0.0164 772.8 1199 0.01642 773.1 1198 0.01642 773.5 1199 0.0164 773.9 1198 0.0164 774.3 1199 0.01641 774.7 1199 0.0164 775.1 1198 0.01642 775.4 1199 0.01642 775.8 1198 0.01642 776.2 1199 0.01641 776.6 1199 0.01642 777 1199 0.01641 777.3 1199 0.0164 777.7 1199 0.01637 778.1 1199 0.01639 778.5 1199 0.01641 778.9 1199 0.01641 779.2 1199 0.01642 779.6 1199 0.01641 780 1199 0.01641 780.4 1199 0.01642 780.8 1199 0.01647 781.1 1199 0.01645 781.5 1199 0.01639 781.9 1199 0.01637 782.3 1199 0.0164 782.7 1199 0.0164 783 1198 0.0164 783.4 1199 0.01642 783.8 1199 0.0164 784.2 1199 0.0164 784.6 1199 0.01641 785 1199 0.01643 785.3 1198 0.01642 785.7 1199 0.0164 786.1 1199 0.0164 786.5 1199 0.01641 786.9 1199 0.0164 787.2 1199 0.01642 787.6 1199 0.01647 788 1199 0.01648 788.4 1198 0.01652 788.8 1198 0.01642 789.1 1199 0.01641 789.5 1199 0.01645 789.9 1199 0.01642 790.3 1199 0.01636 790.7 1199 0.01636 791 1198 0.01643 791.4 1199 0.01647 791.8 1198 0.01648 792.2 1199 0.01646 792.6 1198 0.0165 793 1199 0.01648 793.3 1198 0.01645 793.7 1199 0.0164 794.1 1199 0.01635 794.5 1199 0.01635 794.9 1198 0.01642 795.2 1199 0.01647 795.6 1198 0.0164 796 1199 0.01642 796.4 1199 0.01643 796.8 1198 0.01645 797.1 1198 0.01643 797.5 1199 0.01645 797.9 1199 0.01646 798.3 1199 0.01648 798.7 1198 0.01645 799 1199 0.01645 799.4 1199 0.01646 799.8 1199 0.01648 800.2 1198 0.01646 800.6 1199 0.01643 800.9 1199 0.01642 801.3 1198 0.01642 801.7 1199 0.01648 802.1 1199 0.0164 802.5 1199 0.01643 802.9 1198 0.01647 803.2 1199 0.01645 803.6 1199 0.01642 804 1199 0.01643 804.4 1198 0.01646 804.8 1199 0.01647 805.1 1198 0.01647 805.5 1199 0.01643 805.9 1198 0.01643 806.3 1199 0.01647 806.7 1198 0.01648 807 1199 0.01646 807.4 1199 0.01645 807.8 1199 0.01643 808.2 1199 0.01645 808.6 1199 0.01646 808.9 1199 0.01648 809.3 1199 0.01646 809.7 1199 0.01643 810.1 1198 0.01645 810.5 1199 0.01648 810.9 1199 0.0165 811.2 1198 0.01648 811.6 1198 0.01647 812 1199 0.01646 812.4 1199 0.0165 812.8 1199 0.01655 813.1 1198 0.01652 813.5 1199 0.01652 813.9 1199 0.01648 814.3 1199 0.0165 814.7 1199 0.0165 815 1199 0.0165 815.4 1199 0.01652 815.8 1199 0.01648 816.2 1199 0.01648 816.6 1199 0.0165 816.9 1199 0.0165 817.3 1199 0.01641 817.7 1198 0.01646 818.1 1199 0.01646 818.5 1198 0.01647 818.8 1199 0.01645 819.2 1198 0.01648 819.6 1198 0.01646 820 1198 0.01646 820.4 1199 0.01641 820.8 1199 0.01642 821.1 1198 0.01645 821.5 1199 0.01647 821.9 1199 0.0165 822.3 1199 0.0165 822.7 1198 0.01651 823 1198 0.01651 823.4 1199 0.0165 823.8 1199 0.01651 824.2 1199 0.01652 824.6 1199 0.01651 824.9 1199 0.01648 825.3 1198 0.01648 825.7 1198 0.01648 826.1 1199 0.0165 826.5 1199 0.0165 826.8 1199 0.0165 827.2 1199 0.0165 827.6 1199 0.0165 828 1199 0.0165 828.4 1199 0.01647 828.8 1199 0.01648 829.1 1198 0.01648 829.5 1199 0.01648 829.9 1199 0.01648 830.3 1199 0.0165 830.7 1199 0.0165 831 1199 0.0165 831.4 1199 0.0165 831.8 1199 0.0165 832.2 1199 0.01648 832.6 1199 0.01648 832.9 1198 0.01647 833.3 1198 0.01647 833.7 1198 0.01645 834.1 1199 0.01646 834.5 1198 0.01647 834.8 1199 0.0165 835.2 1199 0.01648 835.6 1199 0.01648 836 1199 0.01648 836.4 1199 0.01647 836.7 1198 0.01647 837.1 1198 0.01645 837.5 1199 0.01647 837.9 1198 0.01646 838.3 1199 0.01648 838.7 1199 0.01648 839 1199 0.01648 839.4 1199 0.0165 839.8 1199 0.01646 840.2 1199 0.01648 840.6 1198 0.01646 840.9 1198 0.01648 841.3 1199 0.0165 841.7 1199 0.0165 842.1 1198 0.01648 842.5 1198 0.01648 842.8 1199 0.01646 843.2 1198 0.01645 843.6 1199 0.01648 844 1199 0.01646 844.4 1199 0.01645 844.7 1199 0.01647 845.1 1199 0.01648 845.5 1198 0.01646 845.9 1199 0.01645 846.3 1198 0.01646 846.7 1198 0.01645 847 1198 0.01645 847.4 1199 0.01646 847.8 1199 0.01646 848.2 1199 0.01646 848.6 1199 0.01645 848.9 1198 0.0165 849.3 1199 0.0165 849.7 1199 0.01648 850.1 1199 0.01648 850.5 1198 0.01646 850.8 1198 0.01648 851.2 1199 0.01647 851.6 1199 0.01645 852 1198 0.01639 852.4 1199 0.01641 852.7 1199 0.01646 853.1 1199 0.01648 853.5 1199 0.01646 853.9 1199 0.01639 854.3 1199 0.0164 854.6 1198 0.01642 855 1199 0.01643 855.4 1198 0.01646 855.8 1198 0.01646 856.2 1198 0.01643 856.6 1198 0.01645 856.9 1199 0.01647 857.3 1199 0.01648 857.7 1198 0.01647 858.1 1199 0.01645 858.5 1199 0.01643 858.8 1199 0.01647 859.2 1199 0.01642 859.6 1199 0.01643 860 1199 0.01645 860.4 1198 0.01645 860.7 1199 0.01647 861.1 1199 0.01645 861.5 1199 0.01645 861.9 1199 0.01642 862.3 1199 0.01636 862.6 1199 0.0163 863 1199 0.01626 863.4 1199 0.01631 863.8 1199 0.01642 864.2 1199 0.01645 864.6 1199 0.01642 864.9 1199 0.01642 865.3 1199 0.01641 865.7 1198 0.01642 866.1 1198 0.01646 866.5 1198 0.01645 866.8 1199 0.01641 867.2 1199 0.0164 867.6 1199 0.0164 868 1199 0.01642 868.4 1198 0.01641 868.7 1198 0.01646 869.1 1199 0.01647 869.5 1199 0.01645 869.9 1199 0.01645 870.3 1198 0.01645 870.6 1199 0.01646 871 1199 0.01646 871.4 1198 0.01642 871.8 1198 0.01641 872.2 1199 0.01642 872.6 1199 0.01646 872.9 1199 0.01642 873.3 1198 0.01643 873.7 1199 0.0165 874.1 1199 0.01651 874.5 1199 0.0165 874.8 1199 0.0165 875.2 1199 0.01645 875.6 1199 0.01641 876 1199 0.0164 876.4 1199 0.01637 876.7 1199 0.01637 877.1 1199 0.01641 877.5 1198 0.01641 877.9 1198 0.01642 878.3 1199 0.01645 878.6 1199 0.01643 879 1199 0.01645 879.4 1198 0.01642 879.8 1198 0.01645 880.2 1199 0.01647 880.5 1199 0.01645 880.9 1198 0.01645 881.3 1198 0.01645 881.7 1199 0.01647 882.1 1199 0.01645 882.5 1199 0.0164 882.8 1198 0.0164 883.2 1199 0.0164 883.6 1199 0.01636 884 1199 0.01632 884.4 1198 0.01635 884.7 1198 0.01637 885.1 1199 0.01642 885.5 1198 0.01637 885.9 1199 0.0164 886.3 1199 0.01639 886.6 1199 0.01634 887 1199 0.01642 887.4 1199 0.01646 887.8 1199 0.01643 888.2 1198 0.01642 888.5 1198 0.01643 888.9 1199 0.0164 889.3 1199 0.01636 889.7 1199 0.01641 890.1 1198 0.0164 890.5 1199 0.0164 890.8 1199 0.01641 891.2 1199 0.0164 891.6 1199 0.01634 892 1198 0.0163 892.4 1199 0.01629 892.7 1199 0.01634 893.1 1199 0.01636 893.5 1199 0.01637 893.9 1198 0.01637 894.3 1198 0.01637 894.6 1199 0.01639 895 1199 0.01637 895.4 1199 0.01636 895.8 1199 0.01639 896.2 1199 0.01637 896.5 1198 0.01639 896.9 1198 0.01639 897.3 1199 0.01641 897.7 1199 0.0164 898.1 1199 0.0164 898.4 1199 0.0164 898.8 1199 0.0164 899.2 1199 0.01639 899.6 1198 0.0164 900 1192 0.01637 900.4 1192 0.01641 900.7 1193 0.01648 901.1 1193 0.0165 901.5 1193 0.0165 901.9 1193 0.01646 902.3 1193 0.01641 902.6 1192 0.0164 903 1190 0.01637 903.4 1190 0.01635 903.8 1190 0.0163 904.2 1188 0.01626 904.5 1188 0.01631 904.9 1187 0.01636 905.3 1187 0.0162 905.7 1186 0.01611 906.1 1184 0.01613 906.4 1183 0.01613 906.8 1183 0.01614 907.2 1182 0.01614 907.6 1181 0.01611 908 1180 0.0161 908.4 1180 0.01609 908.7 1179 0.01609 909.1 1178 0.0161 909.5 1177 0.01614 909.9 1176 0.01613 910.3 1176 0.01608 910.6 1175 0.01604 911 1174 0.01599 911.4 1173 0.01595 911.8 1172 0.01595 912.2 1172 0.01594 912.5 1172 0.01589 912.9 1170 0.01587 913.3 1169 0.01583 913.7 1169 0.01583 914.1 1168 0.0158 914.4 1167 0.01577 914.8 1167 0.0158 915.2 1166 0.01578 915.6 1165 0.01577 916 1165 0.01572 916.3 1164 0.01572 916.7 1163 0.0157 917.1 1162 0.01568 917.5 1162 0.01567 917.9 1161 0.01569 918.3 1159 0.01564 918.6 1159 0.01563 919 1158 0.01557 919.4 1158 0.01556 919.8 1156 0.01556 920.2 1156 0.01553 920.5 1155 0.01548 920.9 1154 0.01547 921.3 1153 0.01544 921.7 1153 0.01541 922.1 1152 0.01541 922.4 1151 0.01537 922.8 1151 0.01532 923.2 1150 0.0153 923.6 1149 0.01527 924 1148 0.0153 924.3 1147 0.01531 924.7 1147 0.01527 925.1 1147 0.0152 925.5 1144 0.01517 925.9 1144 0.01516 926.3 1144 0.01517 926.6 1143 0.01507 927 1142 0.01506 927.4 1141 0.0151 927.8 1140 0.0151 928.2 1140 0.01511 928.5 1139 0.01509 928.9 1138 0.01504 929.3 1137 0.01501 929.7 1136 0.015 930.1 1136 0.01499 930.4 1135 0.01501 930.8 1134 0.01499 931.2 1134 0.01493 931.6 1133 0.0149 932 1132 0.01491 932.3 1131 0.01488 932.7 1130 0.01485 933.1 1130 0.01484 933.5 1129 0.01483 933.9 1129 0.0148 934.2 1128 0.01478 934.6 1127 0.01476 935 1126 0.01476 935.4 1126 0.01476 935.8 1125 0.01468 936.2 1123 0.01463 936.5 1123 0.01462 936.9 1122 0.01464 937.3 1122 0.01463 937.7 1120 0.01459 938.1 1119 0.01458 938.4 1119 0.01453 938.8 1119 0.01453 939.2 1118 0.01452 939.6 1117 0.01452 940 1117 0.01452 940.3 1115 0.01447 940.7 1115 0.01444 941.1 1114 0.01442 941.5 1112 0.01441 941.9 1112 0.01438 942.2 1111 0.01434 942.6 1111 0.01432 943 1110 0.01431 943.4 1109 0.01429 943.8 1108 0.01427 944.2 1108 0.01426 944.5 1106 0.01422 944.9 1106 0.01417 945.3 1105 0.01417 945.7 1104 0.01415 946.1 1104 0.01412 946.4 1103 0.01408 946.8 1102 0.01408 947.2 1101 0.01407 947.6 1101 0.01407 948 1100 0.01412 948.3 1099 0.01405 948.7 1098 0.01401 949.1 1097 0.01402 949.5 1097 0.01399 949.9 1096 0.01396 950.2 1095 0.01392 950.6 1094 0.01392 951 1094 0.01392 951.4 1093 0.01394 951.8 1092 0.01394 952.1 1092 0.01387 952.5 1090 0.01377 952.9 1090 0.01375 953.3 1090 0.01373 953.7 1089 0.0137 954.1 1087 0.01371 954.4 1087 0.01373 954.8 1086 0.01368 955.2 1085 0.01365 955.6 1085 0.01366 956 1084 0.01358 956.3 1083 0.01358 956.7 1082 0.01358 957.1 1081 0.01353 957.5 1081 0.01348 957.9 1080 0.01349 958.2 1079 0.01347 958.6 1079 0.01345 959 1078 0.01343 959.4 1077 0.01338 959.8 1076 0.01339 960.1 1076 0.01338 960.5 1074 0.01334 960.9 1074 0.01335 961.3 1073 0.01333 961.7 1072 0.0133 962.1 1072 0.01332 962.4 1071 0.01328 962.8 1070 0.01326 963.2 1069 0.01327 963.6 1068 0.01329 964 1068 0.01328 964.3 1067 0.01323 964.7 1066 0.01323 965.1 1065 0.01317 965.5 1065 0.01313 965.9 1064 0.01308 966.2 1063 0.01305 966.6 1062 0.01303 967 1061 0.01305 967.4 1060 0.01307 967.8 1060 0.01303 968.1 1059 0.01301 968.5 1058 0.013 968.9 1058 0.01295 969.3 1057 0.01291 969.7 1056 0.01292 970.1 1055 0.0129 970.4 1054 0.01286 970.8 1054 0.01285 971.2 1053 0.01283 971.6 1053 0.01285 972 1051 0.01283 972.3 1051 0.01282 972.7 1050 0.0128 973.1 1049 0.0128 973.5 1049 0.01279 973.9 1047 0.01267 974.2 1047 0.01265 974.6 1046 0.01264 975 1045 0.01264 975.4 1044 0.01265 975.8 1043 0.01266 976.1 1043 0.01267 976.5 1043 0.01265 976.9 1041 0.01262 977.3 1040 0.01262 977.7 1040 0.01259 978 1040 0.01257 978.4 1038 0.01259 978.8 1037 0.01256 979.2 1037 0.01255 979.6 1036 0.01253 980 1035 0.01251 980.3 1034 0.0125 980.7 1034 0.01246 981.1 1033 0.01245 981.5 1032 0.01244 981.9 1032 0.0124 982.2 1030 0.0124 982.6 1029 0.01235 983 1029 0.01235 983.4 1029 0.01234 983.8 1028 0.01232 984.1 1027 0.0123 984.5 1026 0.01224 984.9 1026 0.01223 985.3 1025 0.01222 985.7 1024 0.01222 986 1023 0.01224 986.4 1022 0.0122 986.8 1022 0.01219 987.2 1021 0.01217 987.6 1019 0.01214 988 1018 0.01214 988.3 1018 0.01214 988.7 1018 0.0121 989.1 1017 0.01209 989.5 1016 0.01208 989.9 1015 0.01207 990.2 1015 0.01208 990.6 1014 0.01207 991 1013 0.01203 991.4 1012 0.01198 991.8 1011 0.01197 992.1 1010 0.01194 992.5 1010 0.01193 992.9 1009 0.01189 993.3 1008 0.01187 993.7 1008 0.01185 994 1007 0.01181 994.4 1006 0.0118 994.8 1005 0.01181 995.2 1005 0.01182 995.6 1004 0.0118 995.9 1003 0.01177 996.3 1002 0.01173 996.7 1002 0.01173 997.1 1001 0.01172 997.5 1000 0.0117 997.9 1000 0.01166 998.2 999 0.01165 998.6 998 0.01162 999 997 0.01161 999.4 997 0.01163 999.8 997 0.01166 1000 996 0.01166 1001 994 0.01161 1001 993 0.01157 1001 993 0.01155 1002 992 0.01151 1002 992 0.0115 1002 990 0.0115 1003 990 0.01146 1003 989 0.01145 1004 988 0.01142 1004 988 0.0114 1004 987 0.01141 1005 986 0.0114 1005 986 0.01139 1005 984 0.01139 1006 984 0.01135 1006 983 0.01133 1007 982 0.0113 1007 982 0.01128 1007 981 0.01126 1008 980 0.01123 1008 979 0.01123 1009 978 0.01125 1009 978 0.01121 1009 977 0.01119 1010 976 0.01118 1010 975 0.01118 1010 974 0.01115 1011 973 0.01115 1011 973 0.01112 1012 972 0.01112 1012 972 0.01109 1012 971 0.01107 1013 969 0.01108 1013 969 0.01104 1013 968 0.01105 1014 968 0.01102 1014 967 0.01098 1015 966 0.01095 1015 965 0.01094 1015 965 0.01087 1016 964 0.01086 1016 963 0.01087 1017 962 0.01086 1017 961 0.01084 1017 961 0.01082 1018 959 0.01083 1018 959 0.01082 1018 958 0.01078 1019 957 0.01076 1019 957 0.01076 1020 956 0.01076 1020 955 0.01073 1020 955 0.01072 1021 954 0.01071 1021 953 0.01067 1021 952 0.01065 1022 952 0.01065 1022 950 0.01062 1023 950 0.01061 1023 949 0.01061 1023 948 0.01061 1024 947 0.01057 1024 947 0.01051 1025 946 0.01046 1025 945 0.01051 1025 944 0.01051 1026 943 0.01047 1026 943 0.01043 1026 943 0.01042 1027 942 0.01041 1027 940 0.01041 1028 940 0.01039 1028 940 0.01036 1028 938 0.01034 1029 937 0.01032 1029 937 0.01034 1029 936 0.01031 1030 936 0.01027 1030 934 0.01026 1031 934 0.01024 1031 933 0.01022 1031 932 0.0102 1032 932 0.01021 1032 931 0.01016 1033 930 0.01015 1033 929 0.01013 1033 929 0.01011 1034 928 0.01008 1034 927 0.01006 1034 926 0.01006 1035 926 0.01006 1035 924 0.01004 1036 924 0.01003 1036 923 0.009952 1036 922 0.009928 1037 922 0.00994 1037 921 0.009952 1037 920 0.009915 1038 918 0.009928 1038 918 0.009915 1039 918 0.009903 1039 917 0.00989 1039 917 0.00989 1040 915 0.009816 1040 915 0.009754 1041 914 0.00968 1041 913 0.009668 1041 912 0.009693 1042 911 0.009717 1042 911 0.009693 1042 910 0.009705 1043 909 0.009643 1043 909 0.009594 1044 907 0.009618 1044 907 0.009618 1044 906 0.009606 1045 905 0.009581 1045 904 0.009594 1045 904 0.009581 1046 903 0.009581 1046 902 0.009556 1047 901 0.009519 1047 901 0.009482 1047 900 0.009445 1048 900 0.009544 1048 898 0.009519 1049 897 0.009519 1049 897 0.009544 1049 897 0.009458 1050 896 0.009408 1050 894 0.009433 1050 894 0.009408 1051 893 0.009359 1051 893 0.009284 1052 892 0.009272 1052 891 0.009309 1052 890 0.009297 1053 889 0.009247 1053 889 0.009198 1053 888 0.009161 1054 887 0.009111 1054 886 0.009123 1055 886 0.009136 1055 884 0.009123 1055 884 0.009074 1056 883 0.009049 1056 882 0.009049 1057 882 0.009012 1057 881 0.009037 1057 880 0.009049 1058 879 0.009086 1058 879 0.009037 1058 878 0.00895 1059 877 0.008901 1059 877 0.008926 1060 875 0.008938 1060 875 0.008876 1060 874 0.008901 1061 873 0.008876 1061 872 0.008839 1061 872 0.008851 1062 871 0.008814 1062 870 0.008802 1063 869 0.008789 1063 868 0.008789 1063 868 0.008802 1064 867 0.008802 1064 867 0.00874 1065 865 0.008715 1065 865 0.008691 1065 864 0.008666 1066 863 0.008678 1066 862 0.008629 1066 862 0.008604 1067 861 0.008641 1067 860 0.008604 1068 860 0.008592 1068 859 0.008567 1068 858 0.008542 1069 857 0.008542 1069 857 0.008505 1069 856 0.008493 1070 854 0.008468 1070 854 0.008443 1071 854 0.008443 1071 853 0.008431 1071 851 0.008344 1072 850 0.008258 1072 850 0.008381 1073 850 0.008356 1073 849 0.008295 1073 848 0.008282 1074 847 0.008245 1074 847 0.00822 1074 846 0.008233 1075 844 0.008208 1075 844 0.008171 1076 843 0.008183 1076 843 0.008171 1076 842 0.008171 1077 841 0.008171 1077 840 0.008159 1077 839 0.008097 1078 839 0.00806 1078 837 0.008072 1079 837 0.008047 1079 836 0.008047 1079 836 0.008022 1080 835 0.00801 1080 834 0.007961 1080 833 0.007911 1081 832 0.007886 1081 832 0.007911 1082 831 0.007924 1082 830 0.007837 1082 829 0.007812 1083 829 0.0078 1083 828 0.007812 1084 827 0.007787 1084 826 0.007775 1084 825 0.0078 1085 825 0.007787 1085 824 0.007787 1085 823 0.007738 1086 822 0.007713 1086 821 0.007688 1087 821 0.007688 1087 819 0.007664 1087 819 0.007651 1088 818 0.007627 1088 818 0.007614 1088 817 0.007602 1089 817 0.007602 1089 815 0.00759 1090 815 0.007565 1090 814 0.00754 1090 813 0.00754 1091 813 0.007528 1091 812 0.007478 1092 811 0.007429 1092 811 0.007416 1092 810 0.007404 1093 809 0.007392 1093 808 0.007367 1093 807 0.007354 1094 806 0.007317 1094 805 0.007317 1095 805 0.00733 1095 804 0.007293 1095 803 0.007305 1096 803 0.007268 1096 802 0.007206 1096 801 0.007218 1097 801 0.007206 1097 801 0.007206 1098 801 0.007144 1098 801 0.007095 1098 801 0.007095 1099 800 0.007107 1099 800 0.007082 1100 799 0.007033 1100 798 0.00702 1100 797 0.007008 1101 797 0.007008 1101 796 0.006996 1101 796 0.006971 1102 794 0.006946 1102 793 0.006946 1103 793 0.006909 1103 793 0.006921 1103 792 0.006897 1104 791 0.00686 1104 789 0.006847 1104 789 0.006847 1105 788 0.00681 1105 788 0.006785 1106 786 0.006761 1106 786 0.006724 1106 786 0.006724 1107 784 0.006699 1107 784 0.006699 1108 782 0.006662 1108 782 0.006649 1108 781 0.006649 1109 781 0.0066 1109 780 0.006587 1109 779 0.00655 1110 778 0.00655 1110 778 0.006563 1111 777 0.006538 1111 776 0.006526 1111 776 0.006513 1112 775 0.006501 1112 774 0.006476 1112 772 0.006451 1113 772 0.006427 1113 771 0.006464 1114 771 0.006451 1114 770 0.006402 1114 769 0.00639 1115 768 0.006365 1115 768 0.006352 1116 767 0.00634 1116 765 0.00634 1116 765 0.006315 1117 764 0.006278 1117 764 0.006253 1117 763 0.006229 1118 762 0.006216 1118 761 0.006179 1119 761 0.006204 1119 760 0.006204 1119 759 0.00613 1120 758 0.006117 1120 757 0.006105 1120 757 0.00608 1121 756 0.006117 1121 755 0.006105 1122 755 0.006056 1122 754 0.005981 1122 753 0.005957 1123 753 0.005969 1123 752 0.005981 1124 750 0.006006 1124 750 0.005969 1124 750 0.005944 1125 749 0.005919 1125 747 0.005907 1125 747 0.005907 1126 746 0.005895 1126 745 0.005858 1127 744 0.005833 1127 743 0.005808 1127 743 0.005771 1128 742 0.005771 1128 741 0.005771 1128 740 0.005734 1129 739 0.005734 1129 739 0.005709 1130 738 0.005709 1130 737 0.005684 1130 736 0.005672 1131 736 0.00566 1131 735 0.00561 1132 734 0.00561 1132 734 0.005598 1132 733 0.005573 1133 732 0.005536 1133 732 0.005548 1133 730 0.005524 1134 730 0.005486 1134 729 0.005449 1135 728 0.005363 1135 728 0.005338 1135 727 0.005363 1136 726 0.0054 1136 725 0.0054 1136 725 0.0054 1137 724 0.005363 1137 723 0.005363 1138 722 0.00535 1138 721 0.005289 1138 721 0.005276 1139 720 0.005276 1139 719 0.005264 1140 718 0.005239 1140 718 0.005214 1140 717 0.00519 1141 716 0.005165 1141 715 0.005177 1141 714 0.005177 1142 713 0.005152 1142 713 0.005152 1143 712 0.005115 1143 711 0.005078 1143 711 0.005066 1144 710 0.005041 1144 709 0.005029 1144 708 0.005041 1145 707 0.005016 1145 707 0.004992 1146 706 0.004979 1146 705 0.004942 1146 704 0.004917 1147 703 0.004917 1147 703 0.00488 1148 703 0.004831 1148 701 0.004818 1148 700 0.004843 1149 700 0.004831 1149 700 0.004843 1149 699 0.004818 1150 698 0.004831 1150 697 0.004831 1151 696 0.004818 1151 696 0.004769 1151 695 0.004719 1152 694 0.004719 1152 693 0.004682 1152 693 0.00467 1153 692 0.00467 1153 691 0.004633 1154 690 0.004621 1154 689 0.004596 1154 689 0.004596 1155 688 0.004608 1155 687 0.004571 1156 686 0.004534 1156 685 0.004484 1156 685 0.004472 1157 684 0.004484 1157 683 0.004472 1157 682 0.004447 1158 682 0.004447 1158 681 0.004435 1159 680 0.004423 1159 679 0.004385 1159 678 0.004373 1160 678 0.004336 1160 677 0.004324 1160 676 0.004311 1161 675 0.004299 1161 675 0.004311 1162 674 0.004274 1162 673 0.004249 1162 672 0.004212 1163 671 0.004225 1163 671 0.004188 1164 670 0.004188 1164 669 0.00415 1164 668 0.004126 1165 668 0.004076 1165 667 0.004089 1165 667 0.004089 1166 665 0.004089 1166 664 0.004089 1167 664 0.004076 1167 663 0.004027 1167 662 0.004027 1168 661 0.00399 1168 660 0.00394 1168 660 0.003952 1169 659 0.00394 1169 658 0.003928 1170 658 0.003928 1170 657 0.003878 1170 656 0.003841 1171 655 0.003816 1171 655 0.003792 1172 653 0.003792 1172 653 0.003792 1172 652 0.003779 1173 652 0.003755 1173 650 0.003693 1173 650 0.00368 1174 650 0.003656 1174 649 0.003643 1175 647 0.003631 1175 647 0.003631 1175 646 0.003631 1176 646 0.003544 1176 644 0.003544 1176 644 0.00352 1177 643 0.003569 1177 643 0.00352 1178 642 0.003495 1178 641 0.003495 1178 640 0.003482 1179 639 0.003482 1179 638 0.003445 1180 638 0.003421 1180 636 0.003396 1180 636 0.003359 1181 636 0.003383 1181 635 0.003346 1181 634 0.00326 1182 634 0.003284 1182 633 0.003272 1183 632 0.00326 1183 632 0.003272 1183 633 0.003297 1184 635 0.003284 1184 636 0.00326 1184 635 0.003235 1185 634 0.00326 1185 633 0.003223 1186 632 0.003161 1186 630 0.003136 1186 628 0.003111 1187 625 0.003087 1187 624 0.003025 1188 621 0.003025 1188 621 0.002988 1188 620 0.00295 1189 619 0.002913 1189 618 0.002889 1189 617 0.002851 1190 617 0.002864 1190 616 0.002839 1191 615 0.00279 1191 614 0.00279 1191 614 0.00279 1192 612 0.002777 1192 612 0.002728 1192 610 0.002715 1193 610 0.002691 1193 610 0.002703 1194 609 0.002691 1194 608 0.002691 1194 607 0.002641 1195 607 0.002579 1195 606 0.002592 1196 605 0.002629 1196 605 0.002641 1196 604 0.002604 1197 603 0.002542 1197 603 0.00248 1197 602 0.002493 1198 601 0.002443 1198 601 0.002456 1199 600 0.002443 1199 599 0.002431 1199 599 0.002406 1200 597 0.002406 1200 597 0.002332 1200 596 0.002307 1201 596 0.00227 1201 594 0.002245 1202 594 0.002208 1202 592 0.002233 1202 592 0.002282 1203 592 0.00227 1203 590 0.00227 1204 590 0.00227 1204 589 0.002245 1204 589 0.002159 1205 588 0.002159 1205 587 0.002134 1205 586 0.002109 1206 585 0.002109 1206 585 0.002109 1207 584 0.002084 1207 583 0.002072 1207 582 0.00206 1208 582 0.00201 1208 581 0.001961 1208 580 0.001948 1209 579 0.001986 1209 578 0.001948 1210 578 0.001936 1210 577 0.001961 1210 576 0.001874 1211 575 0.001887 1211 574 0.001899 1212 574 0.001862 1212 573 0.001812 1212 572 0.001788 1213 571 0.00175 1213 571 0.001763 1213 570 0.00175 1214 569 0.001713 1214 568 0.001713 1215 567 0.001738 1215 567 0.001713 1215 566 0.001664 1216 566 0.001652 1216 564 0.001627 1216 564 0.001577 1217 563 0.001577 1217 562 0.001565 1218 562 0.001528 1218 560 0.001515 1218 560 0.001503 1219 559 0.001478 1219 559 0.001454 1220 557 0.001441 1220 557 0.001441 1220 556 0.001429 1221 555 0.001429 1221 555 0.001379 1221 553 0.001379 1222 553 0.001379 1222 553 0.00133 1223 552 0.001342 1223 550 0.001317 1223 549 0.00133 1224 549 0.00133 1224 549 0.00128 1224 547 0.001256 1225 546 0.001243 1225 546 0.001206 1226 546 0.001206 1226 544 0.001206 1226 543 0.001169 1227 542 0.001144 1227 542 0.001144 1228 542 0.001107 1228 540 0.00112 1228 540 0.00112 1229 539 0.001095 1229 539 0.001045 1229 537 0.001058 1230 537 0.001033 1230 536 0.001021 1231 535 0.0009711 1231 534 0.0009587 1231 534 0.0009464 1232 533 0.000934 1232 532 0.0008969 1232 531 0.0008598 1233 531 0.0008598 1233 530 0.0008598 1234 529 0.0009093 1234 528 0.0008845 1234 528 0.0008598 1235 527 0.0008474 1235 526 0.0008227 1236 526 0.0008103 1236 524 0.0008103 1236 524 0.0008103 1237 523 0.0007855 1237 522 0.0007855 1237 521 0.0007855 1238 521 0.0007484 1238 521 0.0006742 1239 519 0.0006618 1239 518 0.0006495 1239 517 0.0006618 1240 517 0.0006247 1240 516 0.0006247 1240 515 0.0005876 1241 515 0.0005876 1241 514 0.0005876 1242 513 0.0005629 1242 512 0.0005505 1242 512 0.0005258 1243 511 0.000501 1243 510 0.0004886 1244 510 0.0004639 1244 509 0.0004639 1244 508 0.0004144 1245 507 0.0004268 1245 506 0.0003773 1245 506 0.0004021 1246 505 0.0004268 1246 504 0.0004268 1247 503 0.0004392 1247 503 0.0003897 1247 502 0.0003155 1248 502 0.0003155 1248 501 0.0003526 1248 500 0.0003278 1249 499 0.0002783 1249 499 0.0002907 1250 497 0.000266 1250 496 0.0002412 1250 496 0.0001917 1251 496 0.0002165 1251 494 0.0002165 1252 494 0.0001917 1252 493 0.0001794 1252 492 0.0002165 1253 492 0.0002289 1253 491 0.0001917 1253 490 0.000167 1254 489 0.0001175 1254 488 0.0001175 1255 488 0.0001052 1255 487 9.278e-05 1255 486 0.0001052 1256 485 9.278e-05 1256 485 9.278e-05 1256 484 1.856e-05 1257 483 6.185e-06 1257 482 6.185e-06 1258 481 6.185e-06 1258 481 6.185e-06 1258 480 6.185e-06 1259 479 6.185e-06 1259 478 6.185e-06 1260 478 6.185e-06 1260 478 6.185e-06 1260 476 -3.093e-05 1261 476 -3.093e-05 1261 475 -5.567e-05 1261 474 -9.278e-05 1262 474 -8.041e-05 1262 473 -0.0001052 1263 471 -0.0001052 1263 471 -0.0001423 1263 471 -0.000167 1264 470 -0.0001423 1264 468 -0.0001917 1264 468 -0.0002289 1265 467 -0.0002289 1265 467 -0.0002536 1266 465 -0.000266 1266 465 -0.0002907 1266 464 -0.0003031 1267 464 -0.0003031 1267 463 -0.0003278 1268 461 -0.0003649 1268 461 -0.0003402 1268 460 -0.0003155 1269 460 -0.0003526 1269 459 -0.0003773 1269 458 -0.0003526 1270 457 -0.0003402 1270 456 -0.0003402 1271 456 -0.0003402 1271 454 -0.0003773 1271 454 -0.0003773 1272 453 -0.0004021 1272 453 -0.0004515 1272 451 -0.0004639 1273 450 -0.0004515 1273 449 -0.0004639 1274 449 -0.000501 1274 449 -0.0005134 1274 448 -0.0004763 1275 446 -0.0005134 1275 446 -0.0005134 1276 446 -0.0005381 1276 445 -0.0005258 1276 444 -0.0005134 1277 442 -0.0005134 1277 442 -0.0005752 1277 442 -0.0006 1278 441 -0.0006371 1278 440 -0.0006371 1279 439 -0.0006247 1279 438 -0.0006124 1279 437 -0.0006 1280 437 -0.0006866 1280 436 -0.0006742 1280 435 -0.0006866 1281 435 -0.0006866 1281 434 -0.000699 1282 433 -0.000699 1282 432 -0.0007113 1282 431 -0.0007732 1283 431 -0.0007732 1283 430 -0.0007732 1283 429 -0.0007979 1284 428 -0.0008103 1284 428 -0.0008227 1285 428 -0.0008474 1285 427 -0.0008598 1285 426 -0.0008845 1286 424 -0.0008969 1286 424 -0.0008598 1287 423 -0.0008845 1287 422 -0.0009711 1287 421 -0.0009216 1288 421 -0.0009835 1288 419 -0.0009835 1288 419 -0.0009959 1289 418 -0.001021 1289 417 -0.0009959 1290 417 -0.001045 1290 416 -0.001107 1290 415 -0.00112 1291 415 -0.001095 1291 413 -0.001058 1291 413 -0.001095 1292 412 -0.001095 1292 411 -0.001157 1293 411 -0.001157 1293 410 -0.001157 1293 409 -0.001181 1294 408 -0.001181 1294 408 -0.001181 1295 407 -0.001194 1295 406 -0.001169 1295 405 -0.001219 1296 405 -0.001268 1296 404 -0.001243 1296 403 -0.001219 1297 403 -0.001206 1297 402 -0.001268 1298 401 -0.001305 1298 401 -0.001305 1298 400 -0.001305 1299 399 -0.001268 1299 399 -0.001256 1299 398 -0.001293 1300 397 -0.001305 1300 396 -0.001293 1301 396 -0.00128 1301 395 -0.001268 1301 394 -0.001243 1302 393 -0.001243 1302 392 -0.001231 1303 392 -0.001231 1303 391 -0.001206 1303 390 -0.001206 1304 389 -0.001157 1304 389 -0.001107 1304 388 -0.00107 1305 386 -0.001021 1305 386 -0.001082 1306 385 -0.001107 1306 385 -0.001021 1306 385 -0.001021 1307 384 -0.0009216 1307 383 -0.0008103 1307 381 -0.0007608 1308 381 -0.000699 1308 381 -0.0006371 1309 379 -0.0005752 1309 379 -0.0005134 1309 378 -0.0004639 1310 378 -0.0004268 1310 376 -0.0003649 1311 376 -0.0003278 1311 374 -0.0002536 1311 374 -0.0002041 1312 372 -0.0001423 1312 372 -0.0001175 1312 371 -4.33e-05 1313 371 6.185e-06 1313 370 6.185e-06 1314 369 4.33e-05 1314 368 8.041e-05 1314 367 0.0001546 1315 367 0.0002412 1315 367 0.0002783 1315 366 0.0002783 1316 365 0.0003278 1316 364 0.0003897 1317 363 0.0004639 1317 362 0.0004886 1317 362 0.0005629 1318 360 0.0005876 1318 360 0.0005876 1319 359 0.0006 1319 358 0.0006371 1319 358 0.0006742 1320 356 0.0007113 1320 356 0.0007113 1320 355 0.0006742 1321 355 0.000699 1321 354 0.0008721 1322 353 0.0009093 1322 353 0.0009093 1322 351 0.000934 1323 350 0.0009711 1323 349 0.0009959 1323 349 0.001033 1324 348 0.001058 1324 348 0.001095 1325 346 0.001082 1325 346 0.001082 1325 345 0.00107 1326 345 0.00112 1326 343 0.001082 1327 343 0.001082 1327 342 0.001082 1327 342 0.00112 1328 340 0.00112 1328 340 0.00112 1328 339 0.001132 1329 338 0.001132 1329 337 0.001132 1330 337 0.001132 1330 336 0.00112 1330 335 0.001157 1331 334 0.001157 1331 333 0.001132 1331 331 0.00112 1332 331 0.001095 1332 331 0.001107 1333 329 0.001157 1333 328 0.001132 1333 328 0.001157 1334 327 0.001169 1334 327 0.001169 1335 327 0.001157 1335 327 0.001181 1335 326 0.001219 1336 326 0.001219 1336 324 0.001095 1336 324 0.001082 1337 323 0.00112 1337 321 0.001157 1338 321 0.001181 1338 320 0.001194 1338 319 0.001194 1339 318 0.001256 1339 317 0.001256 1339 317 0.001219 1340 316 0.001157 1340 315 0.00112 1341 314 0.00112 1341 313 0.001132 1341 313 0.001157 1342 312 0.001169 1342 311 0.001107 1343 310 0.00112 1343 310 0.001107 1343 309 0.001144 1344 309 0.001132 1344 308 0.00112 1344 306 0.001107 1345 306 0.001107 1345 305 0.001095 1346 305 0.00112 1346 304 0.001107 1346 302 0.001082 1347 302 0.001082 1347 302 0.001107 1347 301 0.001107 1348 299 0.001107 1348 299 0.001107 1349 298 0.001107 1349 297 0.001095 1349 296 0.001082 1350 296 0.00112 1350 295 0.001082 1351 295 0.001107 1351 293 0.001107 1351 292 0.00107 1352 292 0.00107 1352 291 0.001045 1352 290 0.001008 1353 290 0.001008 1353 288 0.0009959 1354 288 0.0009835 1354 288 0.0009835 1354 287 0.000934 1355 286 0.0008598 1355 285 0.000835 1355 285 0.0009216 1356 284 0.001008 1356 284 0.0009711 1357 282 0.0009587 1357 281 0.0009711 1357 280 0.0009711 1358 279 0.0009216 1358 278 0.0009093 1359 277 0.0008721 1359 277 0.0008845 1359 277 0.0009216 1360 276 0.0009464 1360 276 0.0009587 1360 274 0.0009587 1361 274 0.0008969 1361 273 0.0008845 1362 272 0.0008845 1362 271 0.0008845 1362 270 0.0008845 1363 270 0.0008721 1363 269 0.0008845 1363 268 0.0008598 1364 267 0.0007979 1364 267 0.0008103 1365 266 0.0008227 1365 265 0.0007608 1365 264 0.0007732 1366 263 0.0007979 1366 263 0.000835 1367 262 0.0008227 1367 261 0.0008227 1367 261 0.000835 1368 260 0.0008103 1368 259 0.0007732 1368 259 0.0007608 1369 257 0.0007361 1369 256 0.0007361 1370 256 0.0007237 1370 255 0.0007237 1370 254 0.0006866 1371 254 0.0007113 1371 252 0.0007732 1371 252 0.0008103 1372 252 0.0008103 1372 250 0.0008103 1373 250 0.0007979 1373 249 0.0007855 1373 249 0.0007361 1374 248 0.0007237 1374 247 0.0007237 1375 246 0.000699 1375 245 0.0006618 1375 244 0.0006 1376 244 0.0005134 1376 242 0.0004886 1376 242 0.0006371 1377 242 0.0005876 1377 240 0.0005258 1378 240 0.0006124 1378 239 0.0006371 1378 238 0.0005752 1379 238 0.0005752 1379 237 0.0005876 1379 236 0.0006124 1380 236 0.0006247 1380 234 0.0005752 1381 234 0.0005876 1381 233 0.0005752 1381 232 0.0005629 1382 231 0.0005381 1382 231 0.0005258 1383 230 0.0005258 1383 229 0.0005134 1383 227 0.000501 1384 227 0.0004886 1384 227 0.0004763 1384 226 0.0004763 1385 226 0.0004763 1385 224 0.0004886 1386 224 0.0005134 1386 224 0.0004763 1386 222 0.0004268 1387 221 0.0004144 1387 220 0.0004515 1387 220 0.0004268 1388 219 0.0004144 1388 218 0.0004268 1389 217 0.0004268 1389 217 0.0004268 1389 216 0.0003773 1390 215 0.0003402 1390 215 0.0003278 1391 213 0.0003526 1391 213 0.0003155 1391 212 0.0003031 1392 211 0.0002783 1392 211 0.0002783 1392 210 0.0002783 1393 209 0.0002783 1393 209 0.000266 1394 208 0.000266 1394 206 0.000266 1394 206 0.000266 1395 206 0.0002412 1395 205 0.0002536 1395 204 0.0002412 1396 202 0.0001917 1396 202 0.0001794 1397 202 0.0001917 1397 201 0.0001794 1397 200 0.0001794 1398 199 0.0001794 1398 199 0.0001299 1399 198 6.804e-05 1399 197 0.0001175 1399 196 0.0001299 1400 196 0.0001052 1400 195 0.0001299 1400 194 6.804e-05 1401 193 0.0001052 1401 193 6.804e-05 1402 192 3.093e-05 1402 191 1.856e-05 1402 190 1.856e-05 1403 190 6.185e-06 1403 189 6.185e-06 1403 188 6.185e-06 1404 187 1.856e-05 1404 187 6.185e-06 1405 186 6.185e-06 1405 185 6.185e-06 1405 184 6.185e-06 1406 184 6.185e-06 1406 183 6.185e-06 1407 182 6.185e-06 1407 181 6.185e-06 1407 181 6.185e-06 1408 180 6.185e-06 1408 179 6.185e-06 1408 178 6.185e-06 1409 177 6.185e-06 1409 177 6.185e-06 1410 176 -1.856e-05 1410 176 -6.804e-05 1410 174 -5.567e-05 1411 174 -6.804e-05 1411 173 -6.804e-05 1411 172 -6.804e-05 1412 171 -4.33e-05 1412 171 -6.804e-05 1413 170 -6.804e-05 1413 169 -6.804e-05 1413 169 -0.0001052 1414 167 -0.0001052 1414 167 -0.0001299 1415 166 -0.0001175 1415 165 -0.0001299 1415 165 -0.0001299 1416 164 -0.0001299 1416 163 -0.000167 1416 163 -0.000167 1417 162 -0.0001794 1417 161 -0.0002041 1418 159 -0.0002041 1418 159 -0.0002289 1418 159 -0.0002289 1419 158 -0.0002041 1419 157 -0.0002289 1419 156 -0.0002412 1420 156 -0.0002289 1420 155 -0.0002536 1421 154 -0.0002536 1421 153 -0.0002783 1421 152 -0.0002907 1422 152 -0.0003031 1422 151 -0.0003278 1423 150 -0.0003402 1423 149 -0.0003278 1423 149 -0.0003278 1424 149 -0.0003278 1424 148 -0.0003773 1424 146 -0.0003649 1425 146 -0.0003649 1425 145 -0.0003897 1426 144 -0.0003897 1426 143 -0.0003897 1426 142 -0.0004021 1427 142 -0.0003897 1427 141 -0.0004021 1427 140 -0.0004268 1428 140 -0.0004268 1428 138 -0.0004144 1429 138 -0.0004392 1429 137 -0.0004515 1429 137 -0.0004886 1430 135 -0.0004763 1430 134 -0.0005381 1431 134 -0.0005752 1431 134 -0.0005381 1431 132 -0.0005258 1432 132 -0.0005381 1432 131 -0.0005505 1432 130 -0.0005629 1433 129 -0.0005752 1433 129 -0.0006247 1434 128 -0.0006247 1434 127 -0.0005876 1434 127 -0.0005752 1435 126 -0.0005876 1435 125 -0.0006124 1435 124 -0.0005876 1436 123 -0.0006 1436 123 -0.0006 1437 122 -0.0006 1437 121 -0.0006124 1437 120 -0.0006371 1438 120 -0.0006618 1438 118 -0.0006618 1439 118 -0.0006742 1439 116 -0.0006866 1439 116 -0.000699 1440 116 -0.0007113 1440 115 -0.0007113 1440 113 -0.0007361 1441 113 -0.0007237 1441 113 -0.0007237 1442 112 -0.0007237 1442 111 -0.0007484 1442 110 -0.0007484 1443 109 -0.0007608 1443 109 -0.0007608 1443 108 -0.0007608 1444 107 -0.0007855 1444 106 -0.0007979 1445 106 -0.0007979 1445 105 -0.0007732 1445 104 -0.0007732 1446 103 -0.0008227 1446 102 -0.0008227 1447 102 -0.000835 1447 101 -0.0008721 1447 100 -0.0008969 1448 100 -0.0009093 1448 99 -0.0009093 1448 98 -0.0008969 1449 97 -0.0009216 1449 96 -0.0009216 1450 96 -0.0009216 1450 95 -0.000934 1450 94 -0.000934 1451 94 -0.0009587 1451 93 -0.0009587 1451 92 -0.0009711 1452 91 -0.0009959 1452 91 -0.0009959 1453 90 -0.001021 1453 89 -0.001021 1453 88 -0.001021 1454 88 -0.001021 1454 87 -0.001045 1455 86 -0.001045 1455 85 -0.001058 1455 84 -0.00107 1456 84 -0.00107 1456 83 -0.00107 1456 82 -0.001095 1457 81 -0.001082 1457 81 -0.001107 1458 80 -0.00112 1458 80 -0.00112 1458 79 -0.001132 1459 78 -0.001144 1459 77 -0.001132 1459 77 -0.001132 1460 76 -0.00112 1460 76 -0.001095 1461 74 -0.00112 1461 73 -0.001157 1461 73 -0.001169 1462 73 -0.001169 1462 72 -0.001194 1463 71 -0.001219 1463 71 -0.001219 1463 70 -0.001256 1464 70 -0.001268 1464 69 -0.001293 1464 69 -0.001367 1465 68 -0.001429 1465 67 -0.001416 1466 67 -0.001367 1466 66 -0.001317 1466 66 -0.001317 1467 65 -0.001293 1467 63 -0.001342 1467 62 -0.001416 1468 61 -0.001404 1468 59 -0.001392 1469 58 -0.001355 1469 56 -0.001392 1469 55 -0.001379 1470 55 -0.001392 1470 55 -0.001392 1471 53 -0.001416 1471 52 -0.001454 1471 52 -0.001466 1472 52 -0.001478 1472 50 -0.001491 1472 50 -0.001491 1473 49 -0.001491 1473 48 -0.001491 1474 48 -0.001491 1474 47 -0.001515 1474 46 -0.001503 1475 46 -0.001515 1475 45 -0.001515 1475 45 -0.001515 1476 44 -0.001528 1476 43 -0.001553 1477 42 -0.001565 1477 42 -0.001553 1477 41 -0.001565 1478 41 -0.001565 1478 41 -0.001577 1478 39 -0.001577 1479 39 -0.00159 1479 38 -0.00159 1480 38 -0.001577 1480 37 -0.001602 1480 36 -0.001614 1481 35 -0.001614 1481 34 -0.001614 1482 34 -0.001614 1482 34 -0.001627 1482 33 -0.001639 1483 32 -0.001639 1483 31 -0.001689 1483 31 -0.00175 1484 30 -0.00175 1484 30 -0.00175 1485 30 -0.001738 1485 29 -0.001726 1485 29 -0.001713 1486 28 -0.001689 1486 28 -0.001689 1486 27 -0.001713 1487 27 -0.001713 1487 27 -0.001726 1488 26 -0.001738 1488 26 -0.001763 1488 26 -0.001763 1489 25 -0.00175 1489 24 -0.001763 1490 23 -0.00175 1490 24 -0.001738 1490 23 -0.00175 1491 23 -0.00175 1491 23 -0.001763 1491 23 -0.001738 1492 22 -0.00175 1492 21 -0.001763 1493 21 -0.001812 1493 21 -0.001812 1493 20 -0.001812 1494 20 -0.001825 1494 20 -0.0018 1494 20 -0.001788 1495 19 -0.001812 1495 19 -0.001825 1496 19 -0.001862 1496 18 -0.001874 1496 18 -0.001948 1497 17 -0.001961 1497 17 -0.001911 1498 17 -0.001862 1498 17 -0.001849 1498 16 -0.001837 1499 17 -0.001862 1499 16 -0.001862 1499 16 -0.001862 1500 16 -0.001887 1500 16 -0.001887 1501 16 -0.001862 1501 16 -0.001874 1501 15 -0.001911 1502 15 -0.001887 1502 15 -0.001887 1502 15 -0.001911 1503 15 -0.001924 1503 15 -0.001899 1504 14 -0.001887 1504 15 -0.001887 1504 14 -0.001887 1505 14 -0.001911 1505 14 -0.001887 1506 13 -0.001887 1506 14 -0.001887 1506 14 -0.001887 1507 13 -0.001887 1507 13 -0.001899 1507 13 -0.001887 1508 13 -0.001911 1508 13 -0.001911 1509 13 -0.001887 1509 13 -0.001887 1509 13 -0.001887 1510 13 -0.001862 1510 13 -0.001874 1510 13 -0.001887 1511 13 -0.001887 1511 13 -0.001887 1512 13 -0.001887 1512 12 -0.001862 1512 13 -0.001899 1513 13 -0.001924 1513 12 -0.001911 1514 12 -0.001924 1514 12 -0.001936 1514 12 -0.001936 1515 12 -0.001911 1515 12 -0.001911 1515 12 -0.001948 1516 12 -0.001961 1516 12 -0.001961 1517 12 -0.001948 1517 12 -0.001924 1517 12 -0.001911 1518 12 -0.001924 1518 12 -0.001936 1518 12 -0.001936 1519 12 -0.001911 1519 12 -0.001924 1520 11 -0.001936 1520 11 -0.001911 1520 12 -0.001911 1521 11 -0.001936 1521 11 -0.001911 1522 12 -0.001924 1522 11 -0.001911 1522 11 -0.001911 1523 11 -0.001911 1523 11 -0.001899 1523 11 -0.001899 1524 11 -0.001911 1524 11 -0.001924 1525 11 -0.001924 1525 11 -0.001936 1525 11 -0.001936 1526 11 -0.001936 1526 11 -0.001936 1526 11 -0.001936 1527 10 -0.001936 1527 11 -0.001936 1528 11 -0.001911 1528 11 -0.001911 1528 10 -0.001899 1529 11 -0.001911 1529 11 -0.001924 1530 11 -0.001936 1530 11 -0.001936 1530 10 -0.001936 1531 10 -0.001936 1531 10 -0.001936 1531 10 -0.001924 1532 11 -0.001924 1532 11 -0.001936 1533 10 -0.001936 1533 11 -0.001924 1533 10 -0.001936 1534 10 -0.001936 1534 10 -0.001924 1534 10 -0.001911 1535 10 -0.001911 1535 10 -0.001948 1536 10 -0.001936 1536 11 -0.001948 1536 10 -0.001936 1537 10 -0.001911 1537 10 -0.001948 1538 10 -0.001961 1538 10 -0.001924 1538 10 -0.001911 1539 10 -0.001887 1539 10 -0.001899 1539 10 -0.001899 1540 10 -0.001899 1540 10 -0.001887 1541 10 -0.001911 1541 9 -0.001936 1541 10 -0.001936 1542 9 -0.001948 1542 9 -0.001948 1542 9 -0.001924 1543 11 -0.001911 1543 9 -0.001911 1544 9 -0.001936 1544 9 -0.001924 1544 9 -0.001924 1545 9 -0.001936 1545 9 -0.001936 1546 10 -0.001936 1546 10 -0.001936 1546 9 -0.001936 1547 9 -0.001936 1547 9 -0.001998 1547 9 -0.002047 1548 9 -0.001973 1548 10 -0.001948 1549 9 -0.001911 1549 9 -0.001899 1549 9 -0.001911 1550 9 -0.001948 1550 9 -0.001948 1550 9 -0.001973 1551 9 -0.001973 1551 9 -0.001961 1552 9 -0.001961 1552 9 -0.001948 1552 9 -0.001948 1553 9 -0.001961 1553 9 -0.001948 1554 9 -0.001936 1554 9 -0.001936 1554 9 -0.001948 1555 9 -0.001961 1555 9 -0.001973 1555 9 -0.001948 1556 9 -0.001911 1556 9 -0.001899 1557 9 -0.001911 1557 9 -0.001924 1557 9 -0.001948 1558 9 -0.001948 1558 9 -0.001998 1558 9 -0.001973 1559 4 0.21 0.05 0.66 0.002 0.007 0.75 2.11 0.83 0.31 0 0.62 0 0 0 5 -0.0001428 0 6 -0.0001552 0.2344 6 -0.0001428 0.4688 6 -0.0001552 0.7031 6 -0.0001552 0.9375 6 -0.0001428 1.172 6 -0.0001552 1.406 6 -0.0001676 1.641 6 -0.00018 1.875 7 -0.0001676 2.109 7 -0.0001428 2.344 9 -0.0001428 2.578 10 -0.0001304 2.813 12 -0.0001179 3.047 13 -0.0001055 3.281 15 -8.07e-05 3.516 16 -6.828e-05 3.75 18 -4.345e-05 3.984 20 -3.104e-05 4.219 21 -6.207e-06 4.453 23 6.207e-06 4.688 23 6.207e-06 4.922 26 6.207e-06 5.156 27 6.207e-06 5.391 28 6.207e-06 5.625 29 1.862e-05 5.859 30 4.345e-05 6.094 32 5.587e-05 6.328 34 9.311e-05 6.563 34 0.0001179 6.797 35 0.0001179 7.031 36 0.0001304 7.266 37 0.0001428 7.5 38 0.0001552 7.734 39 0.0001552 7.969 40 0.0001676 8.203 41 0.00018 8.438 41 0.0001924 8.672 42 0.0002173 8.906 43 0.0002297 9.141 44 0.0002297 9.375 45 0.0002297 9.609 46 0.0002421 9.844 48 0.0002669 10.08 48 0.0002793 10.31 48 0.0002793 10.55 49 0.0002793 10.78 51 0.0002793 11.02 52 0.0003042 11.25 52 0.000329 11.48 53 0.000329 11.72 54 0.0003414 11.95 55 0.0003662 12.19 55 0.0003787 12.42 57 0.0003911 12.66 58 0.0004035 12.89 59 0.0004035 13.13 60 0.0004159 13.36 61 0.0004283 13.59 62 0.0004283 13.83 63 0.0004531 14.06 63 0.0004656 14.3 65 0.000478 14.53 65 0.0004904 14.77 66 0.0004904 15 67 0.0005028 15.23 68 0.0005028 15.47 69 0.0005276 15.7 70 0.0005276 15.94 71 0.00054 16.17 72 0.0005525 16.41 73 0.0005649 16.64 74 0.0005773 16.88 75 0.0005897 17.11 76 0.0005897 17.34 77 0.0005897 17.58 77 0.0006145 17.81 79 0.000627 18.05 80 0.0006518 18.28 81 0.0006518 18.52 81 0.0006642 18.75 82 0.0006766 18.98 84 0.0007139 19.22 84 0.0007139 19.45 85 0.0007263 19.69 86 0.0007387 19.92 87 0.0007387 20.16 88 0.0007635 20.39 88 0.0007759 20.63 90 0.0007883 20.86 91 0.0008008 21.09 91 0.0008008 21.33 92 0.0008008 21.56 93 0.0008256 21.8 95 0.000838 22.03 95 0.0008504 22.27 96 0.0008504 22.5 97 0.0008504 22.73 98 0.0008504 22.97 99 0.0008752 23.2 99 0.0008877 23.44 101 0.0009125 23.67 102 0.0009001 23.91 102 0.0009001 24.14 104 0.0009249 24.38 105 0.0009373 24.61 106 0.0009497 24.84 106 0.0009497 25.08 108 0.0009746 25.31 109 0.000987 25.55 109 0.0009994 25.78 110 0.0009994 26.02 112 0.001024 26.25 112 0.001024 26.48 113 0.001024 26.72 114 0.001049 26.95 115 0.001061 27.19 116 0.001074 27.42 116 0.001099 27.66 118 0.001111 27.89 119 0.001111 28.13 119 0.001124 28.36 121 0.001124 28.59 121 0.001148 28.83 123 0.001161 29.06 123 0.001161 29.3 124 0.001161 29.53 125 0.001161 29.77 127 0.001186 30 127 0.001198 30.23 128 0.001198 30.47 129 0.00121 30.7 131 0.00121 30.94 131 0.001235 31.17 132 0.001248 31.41 133 0.00126 31.64 134 0.00126 31.88 135 0.00126 32.11 136 0.001273 32.34 137 0.001297 32.58 138 0.001322 32.81 138 0.001347 33.05 140 0.001359 33.28 141 0.001359 33.52 141 0.001372 33.75 142 0.001372 33.98 143 0.001372 34.22 144 0.001372 34.45 145 0.001384 34.69 146 0.001409 34.92 146 0.001409 35.16 148 0.001434 35.39 149 0.001446 35.63 149 0.001459 35.86 150 0.001459 36.09 152 0.001471 36.33 152 0.001484 36.56 153 0.001496 36.8 154 0.001508 37.03 156 0.001521 37.27 156 0.001533 37.5 157 0.001546 37.73 159 0.001558 37.97 159 0.001558 38.2 160 0.00157 38.44 161 0.001595 38.67 162 0.00162 38.91 163 0.001633 39.14 164 0.001645 39.38 165 0.001657 39.61 166 0.00167 39.84 166 0.001682 40.08 168 0.001695 40.31 168 0.001719 40.55 169 0.001719 40.78 170 0.001744 41.02 171 0.001757 41.25 173 0.001757 41.48 174 0.001782 41.72 174 0.001794 41.95 174 0.001819 42.19 176 0.001844 42.42 177 0.001856 42.66 177 0.001868 42.89 179 0.001868 43.13 180 0.001881 43.36 181 0.001906 43.59 181 0.001918 43.83 182 0.001918 44.06 184 0.001931 44.3 184 0.001955 44.53 185 0.001968 44.77 186 0.001968 45 187 0.00198 45.23 188 0.002005 45.47 189 0.002017 45.7 190 0.00203 45.94 191 0.002055 46.17 191 0.002067 46.41 192 0.002067 46.64 194 0.002092 46.88 195 0.002117 47.11 195 0.002117 47.34 196 0.002117 47.58 198 0.002154 47.81 198 0.002166 48.05 199 0.002179 48.28 201 0.002179 48.52 201 0.002204 48.75 202 0.002216 48.98 202 0.002216 49.22 204 0.002241 49.45 204 0.002253 49.69 205 0.002253 49.92 206 0.002253 50.16 207 0.002278 50.39 209 0.002303 50.63 209 0.002315 50.86 210 0.002328 51.09 211 0.00234 51.33 212 0.002365 51.56 213 0.002377 51.8 214 0.002377 52.03 215 0.00239 52.27 216 0.00239 52.5 217 0.002415 52.73 217 0.002415 52.97 218 0.00244 53.2 220 0.002452 53.44 220 0.002464 53.67 221 0.002477 53.91 223 0.002477 54.14 224 0.002514 54.38 224 0.002526 54.61 225 0.002526 54.84 226 0.002551 55.08 227 0.002564 55.31 228 0.002576 55.55 229 0.002601 55.78 230 0.002613 56.02 231 0.002638 56.25 231 0.002638 56.48 233 0.002651 56.72 234 0.002663 56.95 234 0.002688 57.19 235 0.002713 57.42 237 0.002713 57.66 238 0.002725 57.89 238 0.002737 58.13 240 0.00275 58.36 240 0.002762 58.59 242 0.002762 58.83 242 0.002787 59.06 243 0.0028 59.3 244 0.0028 59.53 245 0.002812 59.77 245 0.002837 60 247 0.002849 60.23 248 0.002862 60.47 249 0.002886 60.7 249 0.002886 60.94 251 0.002899 61.17 252 0.002911 61.41 252 0.002924 61.64 254 0.002924 61.88 254 0.002949 62.11 256 0.002949 62.34 256 0.002961 62.58 257 0.002986 62.81 259 0.002998 63.05 259 0.002998 63.28 260 0.003011 63.52 261 0.003023 63.75 262 0.003035 63.98 263 0.003048 64.22 264 0.003073 64.45 264 0.003098 64.69 266 0.003098 64.92 267 0.00311 65.16 268 0.00311 65.39 268 0.003135 65.63 269 0.003147 65.86 270 0.003147 66.09 271 0.003147 66.33 272 0.003184 66.56 273 0.003184 66.8 274 0.003209 67.03 275 0.003234 67.27 276 0.003234 67.5 277 0.003246 67.73 277 0.003246 67.97 279 0.003259 68.2 280 0.003271 68.44 281 0.003309 68.67 281 0.003321 68.91 282 0.003333 69.14 284 0.003346 69.38 284 0.003346 69.61 285 0.003346 69.84 286 0.003358 70.08 288 0.003371 70.31 288 0.003383 70.55 289 0.003395 70.78 290 0.003433 71.02 291 0.003433 71.25 292 0.003445 71.48 293 0.00347 71.72 294 0.003495 71.95 295 0.003495 72.19 295 0.003507 72.42 296 0.003507 72.66 297 0.00352 72.89 298 0.003532 73.13 299 0.003544 73.36 300 0.003544 73.59 301 0.003569 73.83 302 0.003582 74.06 303 0.003607 74.3 304 0.003607 74.53 305 0.003619 74.77 306 0.003631 75 306 0.003644 75.23 308 0.003656 75.47 309 0.003656 75.7 310 0.003656 75.94 310 0.003693 76.17 312 0.003693 76.41 312 0.003706 76.64 313 0.003706 76.88 314 0.003743 77.11 315 0.003755 77.34 317 0.003755 77.58 317 0.00378 77.81 318 0.003805 78.05 319 0.003805 78.28 320 0.003805 78.52 321 0.003805 78.75 321 0.003842 78.98 323 0.003842 79.22 324 0.003855 79.45 324 0.003855 79.69 325 0.003867 79.92 327 0.00388 80.16 328 0.003904 80.39 328 0.003904 80.63 329 0.003929 80.86 331 0.003942 81.09 331 0.003954 81.33 332 0.003967 81.56 333 0.003967 81.8 334 0.003967 82.03 335 0.003979 82.27 335 0.003991 82.5 337 0.004004 82.73 337 0.004004 82.97 338 0.004029 83.2 339 0.004041 83.44 340 0.004053 83.67 342 0.004066 83.91 342 0.004066 84.14 343 0.004091 84.38 344 0.004103 84.61 345 0.004116 84.84 346 0.004116 85.08 347 0.00414 85.31 349 0.004153 85.55 349 0.004178 85.78 349 0.004202 86.02 351 0.004215 86.25 353 0.004215 86.48 353 0.004227 86.72 353 0.00424 86.95 355 0.004252 87.19 356 0.004277 87.42 356 0.004265 87.66 357 0.004289 87.89 359 0.004302 88.13 359 0.004314 88.36 360 0.004327 88.59 361 0.004327 88.83 362 0.004339 89.06 363 0.004351 89.3 364 0.004364 89.53 365 0.004376 89.77 366 0.004401 90 367 0.004413 90.23 367 0.004426 90.47 368 0.004438 90.7 370 0.004451 90.94 370 0.004463 91.17 371 0.004476 91.41 372 0.0045 91.64 374 0.004513 91.88 374 0.004513 92.11 375 0.004538 92.34 376 0.004538 92.58 378 0.004538 92.81 378 0.00455 93.05 379 0.004562 93.28 380 0.004587 93.52 381 0.0046 93.75 381 0.004625 93.98 383 0.004637 94.22 384 0.004649 94.45 385 0.004674 94.69 385 0.004687 94.92 387 0.004699 95.16 387 0.004699 95.39 388 0.004711 95.63 389 0.004724 95.86 390 0.004736 96.09 392 0.004749 96.33 392 0.004761 96.56 393 0.004786 96.8 394 0.004798 97.03 395 0.004811 97.27 396 0.004823 97.5 396 0.004848 97.73 398 0.00486 97.97 399 0.004873 98.2 399 0.004873 98.44 400 0.004873 98.67 401 0.004898 98.91 402 0.00491 99.14 403 0.004922 99.38 403 0.004935 99.61 404 0.00496 99.84 405 0.004972 100.1 406 0.004997 100.3 407 0.005022 100.5 409 0.005034 100.8 409 0.005034 101 410 0.005034 101.3 411 0.005071 101.5 412 0.005071 101.7 412 0.005096 102 414 0.005121 102.2 415 0.005134 102.4 415 0.005134 102.7 417 0.005146 102.9 417 0.005158 103.1 418 0.005171 103.4 419 0.005183 103.6 421 0.00522 103.8 421 0.00522 104.1 422 0.005233 104.3 423 0.005245 104.5 424 0.005245 104.8 424 0.00527 105 426 0.005283 105.2 428 0.005295 105.5 428 0.005307 105.7 429 0.005332 105.9 430 0.005345 106.2 431 0.005369 106.4 431 0.005394 106.6 433 0.005394 106.9 434 0.005432 107.1 435 0.005432 107.3 435 0.005444 107.6 436 0.005469 107.8 437 0.005481 108 438 0.005494 108.3 438 0.005494 108.5 440 0.005531 108.8 441 0.005543 109 442 0.005543 109.2 443 0.005556 109.5 443 0.005568 109.7 445 0.005593 109.9 446 0.005605 110.2 446 0.005593 110.4 447 0.005618 110.6 448 0.00563 110.9 449 0.005655 111.1 450 0.00568 111.3 451 0.005692 111.6 453 0.005692 111.8 453 0.005717 112 454 0.005729 112.3 455 0.005742 112.5 456 0.005767 112.7 456 0.005792 113 458 0.005792 113.2 459 0.005816 113.4 460 0.005829 113.7 461 0.005841 113.9 462 0.005854 114.1 462 0.005891 114.4 464 0.005891 114.6 465 0.005903 114.8 465 0.005941 115.1 467 0.005953 115.3 467 0.005953 115.5 468 0.005965 115.8 469 0.00599 116 470 0.00599 116.3 471 0.006027 116.5 471 0.00604 116.7 473 0.006052 117 474 0.006065 117.2 474 0.006065 117.4 475 0.006089 117.7 477 0.006102 117.9 478 0.006114 118.1 478 0.006127 118.4 480 0.006152 118.6 481 0.006152 118.8 481 0.006189 119.1 482 0.006201 119.3 483 0.006214 119.5 484 0.006226 119.8 485 0.006251 120 486 0.006263 120.2 487 0.006276 120.5 488 0.006288 120.7 489 0.006313 120.9 490 0.006313 121.2 491 0.006325 121.4 492 0.00635 121.6 492 0.006363 121.9 493 0.00635 122.1 494 0.00635 122.3 496 0.006375 122.6 496 0.0064 122.8 497 0.006425 123 498 0.006437 123.3 499 0.006437 123.5 500 0.006462 123.8 501 0.006474 124 502 0.006487 124.2 503 0.006499 124.5 503 0.006512 124.7 505 0.006524 124.9 506 0.006549 125.2 506 0.006561 125.4 507 0.006574 125.6 509 0.006586 125.9 510 0.006598 126.1 510 0.006623 126.3 511 0.006636 126.6 512 0.006648 126.8 512 0.006661 127 514 0.006661 127.3 515 0.006673 127.5 515 0.006685 127.7 517 0.00671 128 517 0.00671 128.2 518 0.006735 128.4 519 0.006747 128.7 521 0.006785 128.9 521 0.006797 129.1 522 0.00681 129.4 524 0.006822 129.6 524 0.006834 129.8 525 0.006859 130.1 526 0.006872 130.3 527 0.006896 130.5 528 0.006909 130.8 529 0.006921 131 530 0.006934 131.3 531 0.006959 131.5 531 0.006971 131.7 532 0.006971 132 534 0.006996 132.2 535 0.007008 132.4 535 0.007021 132.7 536 0.007021 132.9 537 0.007045 133.1 538 0.00707 133.4 539 0.00707 133.6 540 0.007095 133.8 542 0.00712 134.1 542 0.00712 134.3 543 0.007132 134.5 544 0.007157 134.8 544 0.007182 135 546 0.007182 135.2 546 0.007207 135.5 548 0.007219 135.7 549 0.007232 135.9 549 0.007256 136.2 549 0.007269 136.4 551 0.007281 136.6 553 0.007294 136.9 553 0.007306 137.1 554 0.007319 137.3 555 0.007331 137.6 556 0.007368 137.8 557 0.007368 138 558 0.007381 138.3 559 0.007405 138.5 560 0.007418 138.8 561 0.007418 139 562 0.00743 139.2 562 0.007468 139.5 564 0.00748 139.7 564 0.00748 139.9 565 0.007517 140.2 567 0.007517 140.4 567 0.00753 140.6 568 0.007554 140.9 569 0.007579 141.1 569 0.007579 141.3 571 0.007604 141.6 572 0.007629 141.8 573 0.007641 142 574 0.007679 142.3 574 0.007679 142.5 576 0.007691 142.7 577 0.007691 143 578 0.007703 143.2 579 0.007728 143.4 579 0.007741 143.7 581 0.007765 143.9 582 0.007778 144.1 582 0.007803 144.4 583 0.007815 144.6 584 0.00784 144.8 585 0.007865 145.1 585 0.00789 145.3 587 0.007902 145.5 589 0.007902 145.8 589 0.007902 146 590 0.007914 146.3 591 0.007927 146.5 592 0.007927 146.7 592 0.007939 147 593 0.007964 147.2 594 0.007977 147.4 596 0.007977 147.7 596 0.007989 147.9 598 0.008001 148.1 599 0.008026 148.4 600 0.008039 148.6 601 0.008051 148.8 601 0.008076 149.1 602 0.008088 149.3 603 0.008101 149.5 603 0.008126 149.8 604 0.008138 150 605 0.008138 150.2 606 0.008175 150.5 607 0.008175 150.7 608 0.0082 150.9 609 0.008225 151.2 610 0.008225 151.4 610 0.008237 151.6 612 0.00825 151.9 613 0.008275 152.1 614 0.008275 152.3 615 0.008287 152.6 615 0.008312 152.8 617 0.008312 153 617 0.008337 153.3 618 0.008349 153.5 619 0.008349 153.8 620 0.008349 154 621 0.008374 154.2 622 0.008386 154.5 623 0.008411 154.7 625 0.008411 154.9 625 0.008423 155.2 626 0.008436 155.4 628 0.008448 155.6 628 0.008448 155.9 630 0.008448 156.1 631 0.008473 156.3 631 0.008498 156.6 632 0.00851 156.8 633 0.00851 157 634 0.008535 157.3 635 0.008548 157.5 635 0.008548 157.7 636 0.008572 158 637 0.008597 158.2 637 0.008597 158.4 638 0.00861 158.7 639 0.008622 158.9 640 0.008647 159.1 641 0.008647 159.4 642 0.008672 159.6 643 0.008684 159.8 644 0.008697 160.1 646 0.008709 160.3 646 0.008721 160.5 647 0.008734 160.8 648 0.008746 161 650 0.008784 161.3 650 0.008796 161.5 651 0.008808 161.7 653 0.008833 162 653 0.008846 162.2 654 0.008858 162.4 655 0.00887 162.7 656 0.008883 162.9 657 0.008908 163.1 658 0.00892 163.4 659 0.008932 163.6 660 0.008957 163.8 660 0.008957 164.1 662 0.008995 164.3 663 0.009007 164.5 664 0.009007 164.8 664 0.009019 165 665 0.009032 165.2 667 0.009057 165.5 668 0.009069 165.7 668 0.009069 165.9 669 0.009081 166.2 671 0.009119 166.4 671 0.009119 166.6 671 0.009119 166.9 673 0.009131 167.1 674 0.009156 167.3 675 0.009168 167.6 675 0.009181 167.8 676 0.009206 168 678 0.009218 168.3 678 0.00923 168.5 679 0.00923 168.8 681 0.00923 169 681 0.009255 169.2 682 0.009293 169.5 683 0.009305 169.7 684 0.00933 169.9 685 0.00933 170.2 686 0.00933 170.4 687 0.009355 170.6 688 0.009367 170.9 689 0.009379 171.1 690 0.009404 171.3 690 0.009417 171.6 692 0.009429 171.8 693 0.009429 172 693 0.009454 172.3 694 0.009466 172.5 696 0.009491 172.7 696 0.009504 173 696 0.009516 173.2 698 0.009541 173.4 699 0.009541 173.7 701 0.009553 173.9 703 0.009566 174.1 705 0.009578 174.4 707 0.009578 174.6 708 0.00959 174.8 709 0.00959 175.1 709 0.00959 175.3 709 0.00959 175.5 709 0.00959 175.8 709 0.00959 176 709 0.00959 176.3 710 0.00959 176.5 709 0.00959 176.7 709 0.00959 177 710 0.00959 177.2 711 0.009603 177.4 711 0.009615 177.7 712 0.009653 177.9 714 0.009665 178.1 715 0.00969 178.4 717 0.009715 178.6 718 0.009739 178.8 719 0.009764 179.1 720 0.009789 179.3 721 0.009802 179.5 722 0.009826 179.8 724 0.009839 180 725 0.009864 180.2 726 0.009901 180.5 727 0.009926 180.7 728 0.009963 180.9 728 0.009975 181.2 729 0.009988 181.4 730 0.01001 181.6 731 0.01002 181.9 732 0.01004 182.1 732 0.01006 182.3 733 0.01007 182.6 734 0.0101 182.8 735 0.0101 183 736 0.01011 183.3 737 0.01014 183.5 737 0.01014 183.8 739 0.01015 184 740 0.01015 184.2 741 0.01016 184.5 742 0.01019 184.7 743 0.01019 184.9 743 0.0102 185.2 744 0.0102 185.4 744 0.01021 185.6 745 0.01022 185.9 746 0.01025 186.1 746 0.01025 186.3 747 0.01025 186.6 748 0.01026 186.8 749 0.01027 187 748 0.01026 187.3 749 0.01026 187.5 750 0.01029 187.7 752 0.01029 188 753 0.0103 188.2 754 0.01032 188.4 755 0.01035 188.7 756 0.01035 188.9 757 0.01037 189.1 758 0.01039 189.4 759 0.0104 189.6 761 0.01042 189.8 763 0.01045 190.1 763 0.01045 190.3 764 0.01045 190.5 766 0.01047 190.8 767 0.01048 191 768 0.0105 191.3 769 0.0105 191.5 770 0.01053 191.7 771 0.01056 192 771 0.01056 192.2 772 0.01056 192.4 775 0.01057 192.7 775 0.0106 192.9 776 0.0106 193.1 778 0.01062 193.4 778 0.01061 193.6 779 0.01065 193.8 780 0.01066 194.1 781 0.01066 194.3 782 0.01066 194.5 782 0.01068 194.8 783 0.0107 195 784 0.01072 195.2 785 0.01075 195.5 786 0.01076 195.7 787 0.01076 195.9 788 0.01076 196.2 789 0.01076 196.4 789 0.01078 196.6 791 0.01079 196.9 792 0.01081 197.1 793 0.01079 197.3 793 0.01079 197.6 795 0.01079 197.8 796 0.01081 198 796 0.01079 198.3 799 0.01079 198.5 798 0.01078 198.8 800 0.01078 199 800 0.01077 199.2 800 0.01075 199.5 801 0.01071 199.7 801 0.0107 199.9 801 0.0107 200.2 801 0.01066 200.4 801 0.01061 200.6 801 0.01058 200.9 802 0.01055 201.1 803 0.01048 201.3 804 0.01043 201.6 805 0.0104 201.8 805 0.01036 202 807 0.0103 202.3 807 0.01022 202.5 808 0.01016 202.7 809 0.0101 203 811 0.01005 203.2 811 0.009988 203.4 812 0.009901 203.7 812 0.009826 203.9 812 0.009752 204.1 813 0.009665 204.4 814 0.00959 204.6 814 0.009516 204.8 815 0.009454 205.1 817 0.009367 205.3 817 0.009305 205.5 818 0.009243 205.8 819 0.009193 206 821 0.009119 206.3 821 0.009069 206.5 823 0.009019 206.7 825 0.008932 207 826 0.00887 207.2 827 0.008833 207.4 828 0.008771 207.7 829 0.008709 207.9 831 0.008684 208.1 832 0.008635 208.4 834 0.008572 208.6 836 0.008535 208.8 836 0.00851 209.1 838 0.008473 209.3 839 0.008448 209.5 840 0.008448 209.8 842 0.008436 210 843 0.008423 210.2 843 0.008436 210.5 845 0.008448 210.7 847 0.008461 210.9 847 0.008498 211.2 848 0.00851 211.4 849 0.00851 211.6 850 0.008535 211.9 851 0.008548 212.1 852 0.008585 212.3 853 0.008597 212.6 853 0.00861 212.8 854 0.008635 213 855 0.008659 213.3 856 0.008684 213.5 857 0.008709 213.8 857 0.008709 214 857 0.008746 214.2 859 0.008759 214.5 859 0.008784 214.7 861 0.008796 214.9 861 0.008808 215.2 862 0.008833 215.4 862 0.008858 215.6 864 0.00887 215.9 865 0.008883 216.1 865 0.008908 216.3 867 0.00892 216.6 868 0.008932 216.8 868 0.008945 217 868 0.008957 217.3 869 0.00897 217.5 871 0.009007 217.7 872 0.009057 218 872 0.009069 218.2 873 0.009069 218.4 875 0.009106 218.7 875 0.009119 218.9 876 0.009156 219.1 878 0.009168 219.4 878 0.009193 219.6 879 0.00923 219.8 880 0.009255 220.1 881 0.009268 220.3 881 0.00928 220.5 882 0.00933 220.8 884 0.009342 221 884 0.009367 221.3 886 0.009392 221.5 886 0.009417 221.7 887 0.009429 222 889 0.009454 222.2 889 0.009479 222.4 890 0.009516 222.7 892 0.009541 222.9 892 0.009566 223.1 893 0.009603 223.4 894 0.009615 223.6 895 0.00964 223.8 897 0.009665 224.1 897 0.009677 224.3 898 0.009702 224.5 899 0.009727 224.8 900 0.009752 225 901 0.009802 225.2 903 0.009814 225.5 903 0.009826 225.7 904 0.009864 225.9 906 0.009901 226.2 906 0.009901 226.4 907 0.009913 226.6 907 0.009951 226.9 908 0.009963 227.1 909 0.009988 227.3 910 0.01001 227.6 911 0.01002 227.8 912 0.01005 228 913 0.0101 228.3 914 0.01012 228.5 915 0.01014 228.8 915 0.01014 229 917 0.01016 229.2 918 0.01019 229.5 918 0.01021 229.7 919 0.01025 229.9 920 0.01026 230.2 922 0.01029 230.4 922 0.0103 230.6 924 0.01032 230.9 925 0.01036 231.1 925 0.01039 231.3 926 0.01042 231.6 928 0.01045 231.8 929 0.01046 232 929 0.0105 232.3 930 0.0105 232.5 931 0.01052 232.7 932 0.01055 233 933 0.01056 233.2 934 0.0106 233.4 934 0.0106 233.7 936 0.01062 233.9 936 0.01065 234.1 937 0.01067 234.4 939 0.0107 234.6 940 0.01071 234.8 940 0.01075 235.1 941 0.01078 235.3 942 0.01079 235.5 943 0.01083 235.8 943 0.01086 236 945 0.01086 236.3 946 0.01089 236.5 947 0.01091 236.7 948 0.01094 237 949 0.01096 237.2 950 0.01097 237.4 950 0.01099 237.7 952 0.01103 237.9 953 0.01106 238.1 954 0.01107 238.4 954 0.01109 238.6 955 0.01112 238.8 956 0.01114 239.1 957 0.01115 239.3 958 0.01118 239.5 959 0.01119 239.8 960 0.01122 240 961 0.01125 240.2 962 0.01127 240.5 962 0.01128 240.7 964 0.0113 240.9 965 0.01132 241.2 965 0.01135 241.4 967 0.01138 241.6 968 0.0114 241.9 968 0.01142 242.1 968 0.01144 242.3 971 0.01147 242.6 972 0.01149 242.8 972 0.01151 243 973 0.01155 243.3 975 0.01156 243.5 975 0.01159 243.8 976 0.01163 244 977 0.01165 244.2 978 0.01166 244.5 979 0.0117 244.7 979 0.01171 244.9 980 0.01174 245.2 981 0.01178 245.4 983 0.01178 245.6 984 0.0118 245.9 984 0.01183 246.1 985 0.01185 246.3 986 0.01187 246.6 987 0.01189 246.8 988 0.01192 247 989 0.01195 247.3 990 0.01196 247.5 990 0.01199 247.7 990 0.01201 248 990 0.01206 248.2 992 0.01211 248.4 993 0.01215 248.7 994 0.01217 248.9 997 0.01221 249.1 998 0.01226 249.4 1000 0.0123 249.6 1001 0.01233 249.8 1002 0.01237 250.1 1003 0.01238 250.3 1004 0.01241 250.5 1005 0.01242 250.8 1006 0.01245 251 1007 0.01246 251.3 1007 0.01246 251.5 1008 0.01246 251.7 1008 0.01248 252 1008 0.01248 252.2 1009 0.0125 252.4 1009 0.01252 252.7 1011 0.01253 252.9 1011 0.01255 253.1 1012 0.01257 253.4 1012 0.01259 253.6 1014 0.01263 253.8 1015 0.01266 254.1 1015 0.01267 254.3 1015 0.01269 254.5 1018 0.01272 254.8 1019 0.01272 255 1019 0.01274 255.2 1022 0.01277 255.5 1023 0.01278 255.7 1024 0.01279 255.9 1026 0.01282 256.2 1026 0.01284 256.4 1028 0.01287 256.6 1028 0.01288 256.9 1029 0.01291 257.1 1029 0.01292 257.3 1030 0.01294 257.6 1031 0.01295 257.8 1033 0.01297 258 1033 0.01299 258.3 1033 0.01302 258.5 1033 0.01304 258.8 1035 0.01305 259 1036 0.01309 259.2 1036 0.0131 259.5 1037 0.01313 259.7 1038 0.01315 259.9 1040 0.01318 260.2 1040 0.0132 260.4 1040 0.01324 260.6 1042 0.01325 260.9 1043 0.01328 261.1 1043 0.01333 261.3 1043 0.01338 261.6 1044 0.01341 261.8 1047 0.01346 262 1048 0.01351 262.3 1049 0.01354 262.5 1051 0.01358 262.7 1051 0.01363 263 1053 0.01365 263.2 1054 0.01367 263.4 1054 0.01371 263.7 1056 0.01372 263.9 1057 0.01376 264.1 1058 0.01379 264.4 1059 0.01381 264.6 1059 0.01382 264.8 1061 0.01384 265.1 1061 0.01387 265.3 1062 0.01389 265.5 1064 0.01391 265.8 1065 0.01392 266 1065 0.01394 266.3 1066 0.01396 266.5 1067 0.01397 266.7 1068 0.01399 267 1068 0.01401 267.2 1069 0.01402 267.4 1070 0.01405 267.7 1072 0.01407 267.9 1072 0.01407 268.1 1072 0.0141 268.4 1073 0.01411 268.6 1075 0.01416 268.8 1076 0.01417 269.1 1076 0.01417 269.3 1077 0.0142 269.5 1078 0.01423 269.8 1079 0.01425 270 1080 0.01427 270.2 1080 0.01428 270.5 1082 0.0143 270.7 1083 0.01433 270.9 1084 0.01437 271.2 1085 0.0144 271.4 1086 0.01442 271.6 1087 0.01443 271.9 1088 0.01447 272.1 1090 0.01449 272.3 1090 0.01452 272.6 1092 0.01453 272.8 1093 0.01457 273 1094 0.01457 273.3 1094 0.01458 273.5 1094 0.01461 273.8 1097 0.01463 274 1097 0.01463 274.2 1097 0.01467 274.5 1099 0.01469 274.7 1099 0.01472 274.9 1100 0.01473 275.2 1100 0.01473 275.4 1101 0.01478 275.6 1102 0.01482 275.9 1103 0.01483 276.1 1104 0.01485 276.3 1105 0.01489 276.6 1107 0.0149 276.8 1108 0.01493 277 1109 0.01497 277.3 1109 0.01498 277.5 1110 0.01499 277.7 1111 0.01502 278 1111 0.01505 278.2 1112 0.01508 278.4 1114 0.0151 278.7 1115 0.01515 278.9 1115 0.01516 279.1 1117 0.0152 279.4 1117 0.0152 279.6 1119 0.01523 279.8 1119 0.01526 280.1 1119 0.01529 280.3 1122 0.01535 280.5 1122 0.01535 280.8 1124 0.01539 281 1125 0.01541 281.3 1126 0.01546 281.5 1127 0.01549 281.7 1126 0.01555 282 1128 0.01556 282.2 1129 0.01559 282.4 1130 0.01562 282.7 1131 0.01564 282.9 1132 0.01567 283.1 1133 0.01571 283.4 1134 0.01574 283.6 1135 0.01575 283.8 1136 0.01579 284.1 1137 0.01581 284.3 1137 0.01585 284.5 1138 0.01586 284.8 1140 0.01587 285 1140 0.0159 285.2 1142 0.01592 285.5 1142 0.01597 285.7 1143 0.016 285.9 1144 0.01602 286.2 1145 0.01606 286.4 1146 0.01608 286.6 1147 0.0161 286.9 1148 0.01615 287.1 1149 0.01617 287.3 1150 0.0162 287.6 1151 0.01622 287.8 1151 0.01626 288 1153 0.01628 288.3 1153 0.01631 288.5 1154 0.01633 288.8 1156 0.01637 289 1156 0.01639 289.2 1157 0.01642 289.5 1158 0.01646 289.7 1159 0.01648 289.9 1161 0.01651 290.2 1161 0.01652 290.4 1162 0.01656 290.6 1163 0.0166 290.9 1164 0.01662 291.1 1165 0.01665 291.3 1165 0.01667 291.6 1167 0.01669 291.8 1168 0.01672 292 1169 0.01675 292.3 1169 0.01677 292.5 1170 0.0168 292.7 1172 0.01683 293 1172 0.01685 293.2 1173 0.01688 293.4 1174 0.0169 293.7 1176 0.01692 293.9 1176 0.01695 294.1 1177 0.01696 294.4 1178 0.017 294.6 1179 0.01701 294.8 1180 0.01704 295.1 1181 0.01709 295.3 1181 0.01711 295.5 1183 0.01714 295.8 1183 0.01716 296 1184 0.01719 296.3 1186 0.01721 296.5 1187 0.01725 296.7 1187 0.01726 297 1188 0.01728 297.2 1189 0.01731 297.4 1190 0.01732 297.7 1192 0.01734 297.9 1192 0.01737 298.1 1194 0.01741 298.4 1194 0.0174 298.6 1194 0.01745 298.8 1196 0.01746 299.1 1197 0.0175 299.3 1197 0.01751 299.5 1199 0.01757 299.8 1200 0.01759 300 1201 0.0176 300.2 1201 0.01761 300.5 1201 0.01765 300.7 1201 0.01765 300.9 1201 0.01766 301.2 1201 0.01766 301.4 1201 0.01764 301.6 1201 0.01764 301.9 1201 0.01764 302.1 1201 0.01765 302.3 1200 0.01764 302.6 1200 0.01764 302.8 1200 0.01761 303 1200 0.01761 303.3 1200 0.01762 303.5 1200 0.01761 303.8 1199 0.0176 304 1199 0.0176 304.2 1199 0.01756 304.5 1199 0.01755 304.7 1199 0.01754 304.9 1199 0.01752 305.2 1199 0.01751 305.4 1199 0.01752 305.6 1199 0.01751 305.9 1199 0.01751 306.1 1199 0.01751 306.3 1199 0.01751 306.6 1199 0.01751 306.8 1199 0.01751 307 1199 0.01752 307.3 1199 0.01751 307.5 1199 0.01751 307.7 1199 0.01751 308 1199 0.01751 308.2 1199 0.01754 308.4 1199 0.01754 308.7 1199 0.01754 308.9 1199 0.01755 309.1 1199 0.01756 309.4 1199 0.01755 309.6 1199 0.01754 309.8 1199 0.01752 310.1 1199 0.01752 310.3 1199 0.01751 310.5 1199 0.01751 310.8 1199 0.01752 311 1199 0.01751 311.3 1199 0.01751 311.5 1199 0.01751 311.7 1199 0.01751 312 1199 0.01751 312.2 1199 0.01751 312.4 1199 0.01754 312.7 1199 0.01755 312.9 1199 0.01755 313.1 1199 0.01756 313.4 1199 0.01756 313.6 1200 0.01756 313.8 1200 0.01754 314.1 1199 0.01754 314.3 1199 0.01752 314.5 1199 0.01754 314.8 1199 0.01751 315 1199 0.01751 315.2 1199 0.01751 315.5 1198 0.01751 315.7 1197 0.01751 315.9 1197 0.01751 316.2 1197 0.01754 316.4 1197 0.01755 316.6 1198 0.01755 316.9 1199 0.01757 317.1 1199 0.0176 317.3 1198 0.0176 317.6 1200 0.01761 317.8 1201 0.01765 318 1201 0.01765 318.3 1200 0.01764 318.5 1199 0.01766 318.8 1199 0.01767 319 1200 0.01768 319.2 1200 0.01768 319.5 1200 0.01767 319.7 1200 0.01767 319.9 1200 0.01765 320.2 1200 0.01766 320.4 1200 0.01766 320.6 1200 0.01764 320.9 1200 0.01766 321.1 1200 0.01765 321.3 1200 0.01765 321.6 1201 0.01765 321.8 1200 0.01764 322 1200 0.01762 322.3 1199 0.01762 322.5 1199 0.01762 322.7 1199 0.01761 323 1199 0.01761 323.2 1199 0.0176 323.4 1198 0.0176 323.7 1199 0.0176 323.9 1198 0.0176 324.1 1198 0.01761 324.4 1198 0.01761 324.6 1199 0.01761 324.8 1199 0.01761 325.1 1198 0.01762 325.3 1199 0.01764 325.5 1199 0.01764 325.8 1199 0.01765 326 1199 0.01764 326.3 1199 0.01766 326.5 1199 0.01766 326.7 1200 0.01766 327 1198 0.01767 327.2 1197 0.01768 327.4 1198 0.01771 327.7 1199 0.01773 327.9 1199 0.01775 328.1 1199 0.01775 328.4 1199 0.01776 328.6 1200 0.01776 328.8 1200 0.01776 329.1 1199 0.01777 329.3 1199 0.0178 329.5 1200 0.01781 329.8 1200 0.01781 330 1200 0.01781 330.2 1200 0.01781 330.5 1200 0.01781 330.7 1200 0.01781 330.9 1201 0.0178 331.2 1201 0.01781 331.4 1201 0.01781 331.6 1201 0.01778 331.9 1200 0.01777 332.1 1200 0.01777 332.3 1199 0.01775 332.6 1199 0.01773 332.8 1199 0.01773 333 1199 0.01773 333.3 1199 0.01772 333.5 1199 0.01771 333.8 1199 0.01771 334 1199 0.01768 334.2 1199 0.0177 334.5 1199 0.0177 334.7 1199 0.01767 334.9 1199 0.01768 335.2 1199 0.01768 335.4 1199 0.01768 335.6 1199 0.01768 335.9 1199 0.01767 336.1 1200 0.01767 336.3 1199 0.01766 336.6 1199 0.01767 336.8 1199 0.01767 337 1199 0.01767 337.3 1199 0.01767 337.5 1199 0.01767 337.7 1199 0.01767 338 1199 0.01767 338.2 1199 0.01766 338.4 1199 0.01767 338.7 1199 0.01767 338.9 1200 0.01767 339.1 1200 0.01767 339.4 1199 0.01767 339.6 1199 0.01765 339.8 1200 0.01764 340.1 1199 0.01764 340.3 1199 0.01761 340.5 1199 0.01764 340.8 1199 0.01766 341 1199 0.01765 341.3 1199 0.01764 341.5 1199 0.01762 341.7 1199 0.01764 342 1199 0.01762 342.2 1199 0.01762 342.4 1199 0.01762 342.7 1198 0.01762 342.9 1199 0.01764 343.1 1199 0.01765 343.4 1199 0.01766 343.6 1199 0.01765 343.8 1199 0.01764 344.1 1199 0.01764 344.3 1199 0.01762 344.5 1199 0.01762 344.8 1200 0.01762 345 1199 0.01762 345.2 1199 0.01765 345.5 1199 0.01766 345.7 1199 0.01765 345.9 1199 0.01764 346.2 1200 0.01765 346.4 1199 0.01765 346.6 1199 0.01765 346.9 1199 0.01766 347.1 1199 0.01765 347.3 1199 0.01765 347.6 1199 0.01766 347.8 1199 0.01767 348 1200 0.01766 348.3 1199 0.01766 348.5 1199 0.01767 348.8 1199 0.01767 349 1199 0.01767 349.2 1199 0.01768 349.5 1199 0.0177 349.7 1199 0.0177 349.9 1199 0.01768 350.2 1199 0.01771 350.4 1200 0.01768 350.6 1199 0.0177 350.9 1200 0.01771 351.1 1200 0.01771 351.3 1200 0.01771 351.6 1200 0.01771 351.8 1200 0.01771 352 1199 0.01771 352.3 1200 0.01771 352.5 1200 0.01771 352.7 1200 0.0177 353 1200 0.01768 353.2 1200 0.0177 353.4 1200 0.0177 353.7 1200 0.0177 353.9 1200 0.0177 354.1 1200 0.01768 354.4 1199 0.0177 354.6 1200 0.0177 354.8 1199 0.01768 355.1 1199 0.01767 355.3 1200 0.01767 355.5 1199 0.01767 355.8 1199 0.01767 356 1200 0.01767 356.3 1199 0.01767 356.5 1199 0.01767 356.7 1200 0.01767 357 1199 0.01768 357.2 1199 0.01767 357.4 1199 0.01766 357.7 1199 0.01766 357.9 1199 0.01762 358.1 1199 0.01765 358.4 1199 0.01764 358.6 1199 0.01762 358.8 1199 0.01762 359.1 1199 0.01762 359.3 1199 0.01762 359.5 1199 0.01761 359.8 1199 0.01761 360 1199 0.01761 360.2 1199 0.01761 360.5 1199 0.01761 360.7 1199 0.01762 360.9 1199 0.01761 361.2 1199 0.01762 361.4 1199 0.01762 361.6 1200 0.01761 361.9 1199 0.01761 362.1 1199 0.01761 362.3 1199 0.01761 362.6 1199 0.01761 362.8 1199 0.01762 363 1199 0.01761 363.3 1199 0.01762 363.5 1199 0.01762 363.8 1199 0.01762 364 1199 0.01761 364.2 1200 0.01764 364.5 1199 0.01764 364.7 1200 0.01762 364.9 1200 0.01761 365.2 1200 0.01762 365.4 1200 0.01761 365.6 1199 0.01761 365.9 1199 0.01761 366.1 1199 0.01761 366.3 1199 0.01761 366.6 1199 0.01762 366.8 1199 0.01761 367 1199 0.01761 367.3 1199 0.01762 367.5 1199 0.01762 367.7 1199 0.01761 368 1199 0.01762 368.2 1200 0.01761 368.4 1199 0.01761 368.7 1200 0.01765 368.9 1199 0.01762 369.1 1199 0.01762 369.4 1199 0.01762 369.6 1200 0.01762 369.8 1199 0.01761 370.1 1199 0.01765 370.3 1199 0.01764 370.5 1199 0.01765 370.8 1199 0.01766 371 1199 0.01765 371.3 1200 0.01765 371.5 1199 0.01766 371.7 1199 0.01767 372 1199 0.01766 372.2 1199 0.01766 372.4 1199 0.01767 372.7 1199 0.01767 372.9 1199 0.01767 373.1 1199 0.01767 373.4 1199 0.01765 373.6 1199 0.01765 373.8 1199 0.01766 374.1 1199 0.01766 374.3 1199 0.01766 374.5 1199 0.01766 374.8 1199 0.01767 375 1200 0.01766 375.2 1200 0.01767 375.5 1199 0.01767 375.7 1200 0.01767 375.9 1199 0.01766 376.2 1200 0.01768 376.4 1199 0.01767 376.6 1199 0.01767 376.9 1199 0.01767 377.1 1199 0.01767 377.3 1199 0.01767 377.6 1199 0.01768 377.8 1199 0.01767 378 1199 0.01767 378.3 1199 0.01767 378.5 1199 0.01767 378.8 1199 0.01768 379 1199 0.01767 379.2 1200 0.01766 379.5 1200 0.01766 379.7 1200 0.01767 379.9 1200 0.01768 380.2 1199 0.01766 380.4 1200 0.01766 380.6 1200 0.01768 380.9 1199 0.01767 381.1 1199 0.01766 381.3 1199 0.01767 381.6 1199 0.01767 381.8 1199 0.01765 382 1199 0.01766 382.3 1199 0.01766 382.5 1199 0.01767 382.7 1200 0.0177 383 1200 0.01766 383.2 1200 0.01766 383.4 1199 0.01765 383.7 1199 0.01766 383.9 1200 0.01766 384.1 1200 0.01766 384.4 1199 0.01767 384.6 1199 0.01766 384.8 1199 0.01767 385.1 1199 0.01768 385.3 1199 0.01768 385.5 1200 0.01768 385.8 1199 0.01771 386 1199 0.0177 386.3 1200 0.0177 386.5 1200 0.0177 386.7 1199 0.01771 387 1199 0.01771 387.2 1199 0.0177 387.4 1199 0.0177 387.7 1199 0.01768 387.9 1199 0.01771 388.1 1199 0.01768 388.4 1200 0.0177 388.6 1199 0.01771 388.8 1199 0.0177 389.1 1199 0.01768 389.3 1199 0.0177 389.5 1199 0.01768 389.8 1199 0.0177 390 1199 0.01771 390.2 1199 0.0177 390.5 1199 0.01768 390.7 1200 0.0177 390.9 1200 0.0177 391.2 1199 0.01768 391.4 1200 0.01768 391.6 1200 0.01768 391.9 1200 0.01768 392.1 1199 0.01768 392.3 1199 0.01768 392.6 1199 0.01768 392.8 1199 0.01768 393 1199 0.01767 393.3 1199 0.01767 393.5 1199 0.01767 393.8 1199 0.01767 394 1200 0.01767 394.2 1199 0.01767 394.5 1200 0.01767 394.7 1199 0.01767 394.9 1199 0.0177 395.2 1200 0.01771 395.4 1199 0.01768 395.6 1199 0.01768 395.9 1199 0.01768 396.1 1200 0.01767 396.3 1199 0.01767 396.6 1199 0.01767 396.8 1199 0.01767 397 1199 0.01767 397.3 1199 0.01767 397.5 1200 0.01767 397.7 1199 0.01767 398 1199 0.01767 398.2 1199 0.01767 398.4 1199 0.01767 398.7 1200 0.01767 398.9 1200 0.01767 399.1 1200 0.01765 399.4 1200 0.01766 399.6 1199 0.01767 399.8 1199 0.01767 400.1 1199 0.01767 400.3 1199 0.01768 400.5 1199 0.01765 400.8 1199 0.01764 401 1199 0.01765 401.3 1199 0.01766 401.5 1199 0.01766 401.7 1199 0.01767 402 1199 0.01766 402.2 1199 0.01766 402.4 1199 0.01767 402.7 1199 0.01767 402.9 1199 0.01766 403.1 1199 0.01766 403.4 1199 0.01766 403.6 1200 0.01766 403.8 1199 0.01767 404.1 1199 0.01767 404.3 1199 0.01767 404.5 1199 0.01768 404.8 1199 0.01767 405 1199 0.01767 405.2 1200 0.01767 405.5 1200 0.01767 405.7 1200 0.01767 405.9 1199 0.01767 406.2 1200 0.01767 406.4 1199 0.01767 406.6 1200 0.01765 406.9 1199 0.01764 407.1 1200 0.01765 407.3 1200 0.01766 407.6 1200 0.01766 407.8 1200 0.01767 408 1199 0.01765 408.3 1200 0.01764 408.5 1200 0.01762 408.8 1200 0.01762 409 1200 0.01762 409.2 1200 0.01762 409.5 1200 0.01761 409.7 1200 0.01761 409.9 1199 0.0176 410.2 1199 0.0176 410.4 1199 0.01761 410.6 1199 0.01759 410.9 1199 0.0176 411.1 1199 0.01759 411.3 1199 0.01757 411.6 1199 0.01757 411.8 1199 0.01757 412 1199 0.0176 412.3 1199 0.01757 412.5 1199 0.01761 412.7 1199 0.01761 413 1199 0.01761 413.2 1199 0.01761 413.4 1199 0.0176 413.7 1199 0.01759 413.9 1199 0.01759 414.1 1199 0.01757 414.4 1200 0.01756 414.6 1199 0.01757 414.8 1200 0.01756 415.1 1200 0.01756 415.3 1199 0.01757 415.5 1200 0.01756 415.8 1199 0.01756 416 1200 0.01757 416.3 1199 0.01756 416.5 1199 0.01756 416.7 1200 0.01756 417 1199 0.01756 417.2 1199 0.01756 417.4 1200 0.01756 417.7 1199 0.01757 417.9 1199 0.01756 418.1 1200 0.01756 418.4 1199 0.01755 418.6 1199 0.01755 418.8 1200 0.01756 419.1 1200 0.01756 419.3 1199 0.01756 419.5 1199 0.01755 419.8 1199 0.01756 420 1199 0.01756 420.2 1199 0.01756 420.5 1199 0.01756 420.7 1199 0.01756 420.9 1199 0.01755 421.2 1199 0.01755 421.4 1199 0.01754 421.6 1199 0.01754 421.9 1200 0.01754 422.1 1199 0.01751 422.3 1200 0.01751 422.6 1199 0.01754 422.8 1199 0.01751 423 1199 0.01751 423.3 1200 0.01751 423.5 1199 0.01751 423.8 1200 0.01751 424 1200 0.01749 424.2 1200 0.01751 424.5 1200 0.01749 424.7 1199 0.0175 424.9 1199 0.01749 425.2 1199 0.0175 425.4 1200 0.01749 425.6 1199 0.0175 425.9 1200 0.01749 426.1 1199 0.01747 426.3 1199 0.01747 426.6 1199 0.01747 426.8 1199 0.01746 427 1199 0.01747 427.3 1199 0.0175 427.5 1199 0.0175 427.7 1200 0.0175 428 1199 0.01749 428.2 1199 0.01751 428.4 1199 0.01751 428.7 1200 0.01751 428.9 1199 0.01751 429.1 1199 0.01751 429.4 1199 0.01751 429.6 1200 0.0175 429.8 1199 0.0175 430.1 1199 0.01749 430.3 1200 0.01747 430.5 1199 0.01747 430.8 1199 0.01747 431 1199 0.01747 431.3 1199 0.01746 431.5 1200 0.01746 431.7 1200 0.01746 432 1199 0.01746 432.2 1199 0.01746 432.4 1199 0.01746 432.7 1199 0.01745 432.9 1199 0.01745 433.1 1200 0.01746 433.4 1199 0.01746 433.6 1199 0.01746 433.8 1199 0.01747 434.1 1199 0.01746 434.3 1199 0.01746 434.5 1199 0.01746 434.8 1199 0.01745 435 1199 0.01745 435.2 1200 0.01745 435.5 1199 0.01745 435.7 1199 0.01745 435.9 1199 0.01744 436.2 1199 0.01742 436.4 1200 0.01742 436.6 1199 0.01742 436.9 1199 0.01741 437.1 1199 0.01739 437.3 1199 0.0174 437.6 1199 0.01741 437.8 1199 0.01741 438 1199 0.0174 438.3 1199 0.01737 438.5 1199 0.01739 438.8 1199 0.0174 439 1199 0.0174 439.2 1199 0.01739 439.5 1199 0.0174 439.7 1199 0.01741 439.9 1199 0.01741 440.2 1199 0.01741 440.4 1200 0.01741 440.6 1199 0.01741 440.9 1199 0.01741 441.1 1199 0.01741 441.3 1199 0.01741 441.6 1199 0.01741 441.8 1199 0.01741 442 1199 0.01741 442.3 1200 0.01741 442.5 1199 0.01741 442.7 1199 0.01739 443 1199 0.01737 443.2 1199 0.01739 443.4 1199 0.01739 443.7 1199 0.0174 443.9 1199 0.01741 444.1 1199 0.01739 444.4 1199 0.0174 444.6 1199 0.01739 444.8 1199 0.0174 445.1 1199 0.0174 445.3 1199 0.01741 445.5 1200 0.01742 445.8 1200 0.01742 446 1200 0.01742 446.3 1200 0.01742 446.5 1200 0.01741 446.7 1200 0.01741 447 1200 0.01741 447.2 1199 0.01741 447.4 1199 0.01739 447.7 1199 0.01741 447.9 1199 0.0174 448.1 1199 0.01739 448.4 1199 0.01737 448.6 1199 0.01736 448.8 1199 0.01739 449.1 1199 0.01739 449.3 1199 0.0174 449.5 1199 0.01739 449.8 1199 0.0174 450 1199 0.0174 450.2 1199 0.01741 450.5 1199 0.01741 450.7 1199 0.0174 450.9 1199 0.0174 451.2 1199 0.01741 451.4 1199 0.01739 451.6 1199 0.0174 451.9 1199 0.0174 452.1 1199 0.0174 452.3 1199 0.0174 452.6 1200 0.0174 452.8 1200 0.0174 453 1199 0.0174 453.3 1200 0.0174 453.5 1199 0.01741 453.8 1199 0.01741 454 1199 0.01741 454.2 1199 0.01741 454.5 1200 0.01741 454.7 1200 0.01741 454.9 1199 0.01742 455.2 1200 0.01741 455.4 1199 0.01741 455.6 1199 0.01741 455.9 1199 0.01741 456.1 1199 0.01741 456.3 1199 0.01741 456.6 1199 0.01741 456.8 1199 0.01741 457 1200 0.0174 457.3 1199 0.0174 457.5 1199 0.01739 457.7 1199 0.01739 458 1199 0.0174 458.2 1199 0.0174 458.4 1199 0.01739 458.7 1199 0.0174 458.9 1199 0.01737 459.1 1199 0.01737 459.4 1199 0.0174 459.6 1199 0.0174 459.8 1200 0.0174 460.1 1199 0.0174 460.3 1199 0.0174 460.5 1199 0.01737 460.8 1199 0.01737 461 1199 0.01737 461.3 1200 0.01736 461.5 1199 0.01739 461.7 1199 0.01737 462 1199 0.01736 462.2 1200 0.01736 462.4 1199 0.01737 462.7 1199 0.01736 462.9 1199 0.01736 463.1 1199 0.01737 463.4 1199 0.01736 463.6 1199 0.01736 463.8 1199 0.01736 464.1 1199 0.01736 464.3 1199 0.01736 464.5 1199 0.01736 464.8 1199 0.01736 465 1199 0.01736 465.2 1199 0.01736 465.5 1199 0.01736 465.7 1199 0.01736 465.9 1199 0.01736 466.2 1199 0.01736 466.4 1199 0.01736 466.6 1199 0.01736 466.9 1199 0.01736 467.1 1200 0.01736 467.3 1199 0.01736 467.6 1199 0.01736 467.8 1199 0.01736 468 1200 0.01736 468.3 1199 0.01736 468.5 1199 0.01737 468.8 1199 0.01736 469 1200 0.01736 469.2 1199 0.01736 469.5 1200 0.01736 469.7 1199 0.01736 469.9 1199 0.01737 470.2 1199 0.01736 470.4 1199 0.01736 470.6 1199 0.01736 470.9 1200 0.01736 471.1 1199 0.01736 471.3 1199 0.01736 471.6 1199 0.01736 471.8 1199 0.01736 472 1199 0.01736 472.3 1199 0.01736 472.5 1199 0.01736 472.7 1199 0.01736 473 1199 0.01736 473.2 1199 0.01736 473.4 1199 0.01734 473.7 1199 0.01735 473.9 1199 0.01735 474.1 1199 0.01736 474.4 1199 0.01736 474.6 1200 0.01736 474.8 1199 0.01736 475.1 1199 0.01736 475.3 1199 0.01736 475.5 1199 0.01736 475.8 1199 0.01736 476 1199 0.01736 476.3 1199 0.01736 476.5 1199 0.01736 476.7 1199 0.01735 477 1199 0.01734 477.2 1199 0.01732 477.4 1199 0.01732 477.7 1199 0.01732 477.9 1199 0.01734 478.1 1199 0.01735 478.4 1199 0.01735 478.6 1199 0.01737 478.8 1199 0.01737 479.1 1199 0.01736 479.3 1200 0.01736 479.5 1199 0.01737 479.8 1199 0.01736 480 1199 0.01736 480.2 1199 0.01736 480.5 1199 0.01736 480.7 1199 0.01736 480.9 1199 0.01736 481.2 1199 0.01735 481.4 1199 0.01735 481.6 1200 0.01735 481.9 1199 0.01735 482.1 1199 0.01734 482.3 1199 0.01735 482.6 1200 0.01734 482.8 1199 0.01734 483 1199 0.01734 483.3 1200 0.01734 483.5 1199 0.01731 483.8 1200 0.01731 484 1199 0.01731 484.2 1199 0.01731 484.5 1199 0.01734 484.7 1199 0.01734 484.9 1199 0.01734 485.2 1199 0.01732 485.4 1199 0.01734 485.6 1199 0.01731 485.9 1199 0.01731 486.1 1199 0.01731 486.3 1199 0.01731 486.6 1199 0.01731 486.8 1199 0.01731 487 1199 0.01731 487.3 1199 0.01732 487.5 1199 0.01731 487.7 1200 0.0173 488 1199 0.0173 488.2 1199 0.01731 488.4 1199 0.01731 488.7 1199 0.01731 488.9 1199 0.0173 489.1 1200 0.0173 489.4 1199 0.0173 489.6 1199 0.0173 489.8 1199 0.01729 490.1 1199 0.01728 490.3 1199 0.01729 490.5 1199 0.01728 490.8 1199 0.01728 491 1199 0.01726 491.3 1199 0.01729 491.5 1199 0.01728 491.7 1199 0.01729 492 1199 0.0173 492.2 1199 0.0173 492.4 1199 0.01731 492.7 1200 0.0173 492.9 1199 0.01728 493.1 1199 0.01729 493.4 1199 0.0173 493.6 1199 0.01729 493.8 1199 0.01728 494.1 1199 0.01726 494.3 1199 0.01726 494.5 1199 0.01726 494.8 1199 0.01725 495 1199 0.01725 495.2 1199 0.01724 495.5 1199 0.01725 495.7 1200 0.01726 495.9 1199 0.01725 496.2 1200 0.01725 496.4 1199 0.01726 496.6 1200 0.01725 496.9 1199 0.01725 497.1 1199 0.01726 497.3 1199 0.01726 497.6 1199 0.01726 497.8 1199 0.01725 498 1199 0.01726 498.3 1199 0.01728 498.5 1199 0.01728 498.8 1200 0.01728 499 1199 0.01729 499.2 1199 0.01728 499.5 1199 0.01728 499.7 1199 0.01726 499.9 1199 0.01726 500.2 1199 0.01726 500.4 1199 0.01726 500.6 1199 0.01725 500.9 1199 0.01726 501.1 1199 0.01726 501.3 1199 0.01725 501.6 1199 0.01726 501.8 1199 0.01726 502 1200 0.01726 502.3 1199 0.01725 502.5 1199 0.01726 502.7 1199 0.01726 503 1199 0.01725 503.2 1199 0.01724 503.4 1199 0.01723 503.7 1199 0.01721 503.9 1199 0.01721 504.1 1199 0.01724 504.4 1199 0.01721 504.6 1199 0.01721 504.8 1199 0.01723 505.1 1200 0.01725 505.3 1200 0.01725 505.5 1199 0.01725 505.8 1199 0.01723 506 1200 0.01721 506.3 1199 0.01721 506.5 1200 0.01721 506.7 1199 0.01724 507 1199 0.01725 507.2 1199 0.01723 507.4 1199 0.01721 507.7 1200 0.01723 507.9 1200 0.01724 508.1 1199 0.01725 508.4 1200 0.01723 508.6 1199 0.01723 508.8 1199 0.01724 509.1 1199 0.01725 509.3 1199 0.01723 509.5 1199 0.01721 509.8 1200 0.01721 510 1199 0.01721 510.2 1199 0.01719 510.5 1199 0.01718 510.7 1199 0.01719 510.9 1199 0.0172 511.2 1199 0.01718 511.4 1199 0.01716 511.6 1199 0.01719 511.9 1199 0.01718 512.1 1199 0.01716 512.3 1199 0.01718 512.6 1199 0.01716 512.8 1199 0.01716 513 1199 0.01718 513.3 1199 0.01719 513.5 1199 0.01719 513.8 1199 0.01718 514 1199 0.01719 514.2 1199 0.01718 514.5 1199 0.01716 514.7 1199 0.01719 514.9 1199 0.01718 515.2 1199 0.01719 515.4 1199 0.01719 515.6 1199 0.01718 515.9 1199 0.01719 516.1 1199 0.01715 516.3 1199 0.01718 516.6 1199 0.01716 516.8 1199 0.01716 517 1200 0.01718 517.3 1199 0.01715 517.5 1199 0.01716 517.7 1199 0.01718 518 1200 0.01718 518.2 1199 0.01718 518.4 1199 0.01719 518.7 1199 0.01718 518.9 1199 0.01718 519.1 1199 0.01716 519.4 1199 0.01716 519.6 1199 0.01716 519.8 1199 0.01715 520.1 1200 0.01716 520.3 1199 0.01715 520.5 1199 0.01715 520.8 1199 0.01715 521 1199 0.01715 521.3 1199 0.01718 521.5 1199 0.01715 521.7 1199 0.01718 522 1199 0.01714 522.2 1199 0.01714 522.4 1199 0.01715 522.7 1199 0.01713 522.9 1199 0.01715 523.1 1199 0.01713 523.4 1199 0.01713 523.6 1200 0.01714 523.8 1199 0.01711 524.1 1199 0.01711 524.3 1199 0.01711 524.5 1199 0.01711 524.8 1199 0.01714 525 1199 0.01714 525.2 1199 0.01711 525.5 1199 0.01715 525.7 1199 0.01714 525.9 1199 0.01713 526.2 1199 0.01714 526.4 1199 0.01715 526.6 1199 0.01713 526.9 1199 0.01714 527.1 1199 0.01716 527.3 1199 0.01718 527.6 1199 0.01715 527.8 1199 0.01715 528 1199 0.01715 528.3 1199 0.01714 528.5 1199 0.0171 528.8 1199 0.0171 529 1199 0.01714 529.2 1199 0.01715 529.5 1200 0.01711 529.7 1199 0.01711 529.9 1199 0.01713 530.2 1199 0.01715 530.4 1199 0.01715 530.6 1200 0.01711 530.9 1199 0.01711 531.1 1199 0.01711 531.3 1199 0.01715 531.6 1199 0.01716 531.8 1199 0.01715 532 1199 0.01711 532.3 1199 0.0171 532.5 1199 0.01709 532.7 1199 0.01711 533 1199 0.01714 533.2 1199 0.01714 533.4 1200 0.01711 533.7 1199 0.01709 533.9 1200 0.01705 534.1 1199 0.01703 534.4 1199 0.01704 534.6 1199 0.01706 534.8 1199 0.0171 535.1 1199 0.01711 535.3 1199 0.01714 535.5 1199 0.01714 535.8 1199 0.01716 536 1199 0.01718 536.3 1199 0.01716 536.5 1199 0.01715 536.7 1199 0.01716 537 1200 0.01716 537.2 1199 0.01716 537.4 1199 0.01715 537.7 1200 0.01715 537.9 1199 0.01715 538.1 1199 0.01715 538.4 1199 0.01716 538.6 1200 0.01715 538.8 1199 0.01715 539.1 1199 0.01714 539.3 1199 0.01711 539.5 1199 0.01709 539.8 1200 0.01708 540 1199 0.01705 540.2 1199 0.01703 540.5 1199 0.01704 540.7 1199 0.01706 540.9 1199 0.0171 541.2 1199 0.0171 541.4 1199 0.01711 541.6 1199 0.01709 541.9 1199 0.01705 542.1 1199 0.01704 542.3 1199 0.01703 542.6 1199 0.01705 542.8 1200 0.01708 543 1199 0.01708 543.3 1199 0.01705 543.5 1199 0.01704 543.8 1199 0.01703 544 1199 0.01705 544.2 1199 0.01706 544.5 1199 0.01705 544.7 1199 0.01701 544.9 1199 0.017 545.2 1199 0.01701 545.4 1199 0.01703 545.6 1199 0.01704 545.9 1199 0.01703 546.1 1199 0.017 546.3 1199 0.01701 546.6 1199 0.01705 546.8 1199 0.01704 547 1199 0.017 547.3 1199 0.017 547.5 1199 0.01703 547.7 1200 0.01699 548 1199 0.01698 548.2 1199 0.017 548.4 1199 0.01701 548.7 1200 0.01696 548.9 1199 0.01696 549.1 1199 0.01699 549.4 1200 0.01698 549.6 1200 0.01698 549.8 1199 0.017 550.1 1199 0.017 550.3 1199 0.01698 550.5 1199 0.017 550.8 1199 0.01699 551 1199 0.01698 551.3 1200 0.01701 551.5 1200 0.017 551.7 1199 0.01701 552 1200 0.01703 552.2 1199 0.01699 552.4 1199 0.017 552.7 1199 0.01698 552.9 1200 0.01698 553.1 1199 0.01699 553.4 1199 0.01698 553.6 1199 0.017 553.8 1199 0.017 554.1 1199 0.01701 554.3 1199 0.01701 554.5 1199 0.01703 554.8 1199 0.01701 555 1199 0.017 555.2 1200 0.01698 555.5 1200 0.01695 555.7 1199 0.01694 555.9 1199 0.01694 556.2 1199 0.01693 556.4 1199 0.01694 556.6 1199 0.01695 556.9 1199 0.01696 557.1 1199 0.01696 557.3 1200 0.01698 557.6 1199 0.01698 557.8 1199 0.01696 558 1199 0.01699 558.3 1199 0.01696 558.5 1199 0.01698 558.8 1200 0.01696 559 1200 0.01696 559.2 1199 0.01698 559.5 1199 0.01696 559.7 1199 0.01696 559.9 1199 0.01696 560.2 1199 0.01695 560.4 1199 0.01696 560.6 1199 0.01695 560.9 1199 0.01694 561.1 1199 0.01694 561.3 1199 0.01694 561.6 1199 0.01695 561.8 1199 0.01695 562 1199 0.01695 562.3 1200 0.01695 562.5 1199 0.01694 562.7 1199 0.01694 563 1199 0.01694 563.2 1199 0.01694 563.4 1199 0.01695 563.7 1199 0.01693 563.9 1199 0.01694 564.1 1199 0.01694 564.4 1199 0.01693 564.6 1199 0.01694 564.8 1200 0.01695 565.1 1199 0.01693 565.3 1200 0.01692 565.5 1199 0.01692 565.8 1199 0.01692 566 1199 0.0169 566.3 1199 0.0169 566.5 1199 0.0169 566.7 1199 0.0169 567 1199 0.0169 567.2 1199 0.0169 567.4 1199 0.0169 567.7 1199 0.0169 567.9 1199 0.0169 568.1 1199 0.0169 568.4 1200 0.0169 568.6 1199 0.0169 568.8 1199 0.0169 569.1 1199 0.0169 569.3 1199 0.0169 569.5 1199 0.0169 569.8 1199 0.0169 570 1199 0.0169 570.2 1199 0.0169 570.5 1199 0.01689 570.7 1199 0.0169 570.9 1199 0.0169 571.2 1199 0.0169 571.4 1199 0.0169 571.6 1199 0.01693 571.9 1199 0.01692 572.1 1199 0.01693 572.3 1199 0.01692 572.6 1199 0.01692 572.8 1199 0.0169 573 1199 0.0169 573.3 1199 0.0169 573.5 1199 0.01689 573.8 1199 0.0169 574 1199 0.0169 574.2 1199 0.01689 574.5 1199 0.0169 574.7 1200 0.01692 574.9 1199 0.01692 575.2 1199 0.01694 575.4 1199 0.01695 575.6 1199 0.01695 575.9 1199 0.01695 576.1 1200 0.01695 576.3 1200 0.01692 576.6 1199 0.0169 576.8 1199 0.01692 577 1199 0.01692 577.3 1199 0.0169 577.5 1199 0.0169 577.7 1199 0.0169 578 1199 0.01689 578.2 1199 0.01687 578.4 1199 0.01687 578.7 1199 0.01688 578.9 1199 0.01688 579.1 1199 0.01689 579.4 1199 0.01689 579.6 1199 0.01689 579.8 1199 0.0169 580.1 1199 0.0169 580.3 1199 0.0169 580.5 1199 0.0169 580.8 1199 0.0169 581 1199 0.01689 581.3 1199 0.01688 581.5 1199 0.01689 581.7 1199 0.01689 582 1199 0.01689 582.2 1199 0.01689 582.4 1199 0.0169 582.7 1199 0.0169 582.9 1199 0.01692 583.1 1199 0.01694 583.4 1199 0.01692 583.6 1199 0.01692 583.8 1199 0.01694 584.1 1199 0.01694 584.3 1199 0.01695 584.5 1199 0.01693 584.8 1199 0.01692 585 1199 0.01692 585.2 1199 0.0169 585.5 1199 0.0169 585.7 1199 0.0169 585.9 1199 0.0169 586.2 1199 0.0169 586.4 1199 0.0169 586.6 1200 0.0169 586.9 1199 0.0169 587.1 1200 0.0169 587.3 1199 0.0169 587.6 1199 0.0169 587.8 1199 0.0169 588 1199 0.0169 588.3 1199 0.0169 588.5 1199 0.0169 588.8 1199 0.0169 589 1200 0.0169 589.2 1199 0.01688 589.5 1199 0.01687 589.7 1199 0.01685 589.9 1199 0.01685 590.2 1199 0.01685 590.4 1199 0.01687 590.6 1199 0.01688 590.9 1199 0.0169 591.1 1199 0.0169 591.3 1199 0.0169 591.6 1199 0.0169 591.8 1199 0.0169 592 1199 0.01689 592.3 1199 0.0169 592.5 1199 0.01692 592.7 1199 0.01689 593 1199 0.0169 593.2 1200 0.0169 593.4 1199 0.0169 593.7 1199 0.01689 593.9 1199 0.01688 594.1 1199 0.01689 594.4 1200 0.01687 594.6 1199 0.01687 594.8 1199 0.01687 595.1 1199 0.01685 595.3 1199 0.01685 595.5 1199 0.01685 595.8 1199 0.01685 596 1199 0.01685 596.3 1199 0.01684 596.5 1199 0.01685 596.7 1199 0.01685 597 1199 0.01683 597.2 1199 0.01682 597.4 1199 0.01682 597.7 1200 0.01682 597.9 1199 0.01684 598.1 1199 0.01687 598.4 1199 0.01688 598.6 1199 0.01688 598.8 1199 0.0169 599.1 1199 0.01689 599.3 1199 0.01687 599.5 1199 0.01685 599.8 1198 0.01685 600 1198 0.01685 600.2 1172 0.01685 600.5 1178 0.01692 600.7 1182 0.01696 600.9 1186 0.01705 601.2 1187 0.01715 601.4 1188 0.01721 601.6 1190 0.01728 601.9 1190 0.01734 602.1 1190 0.01736 602.3 1190 0.01739 602.6 1190 0.01739 602.8 1189 0.01739 603 1187 0.01739 603.3 1187 0.01737 603.5 1186 0.01736 603.8 1184 0.01736 604 1184 0.01734 604.2 1182 0.01734 604.5 1181 0.01729 604.7 1179 0.01725 604.9 1178 0.01721 605.2 1177 0.01719 605.4 1176 0.01715 605.6 1175 0.01711 605.9 1174 0.01709 606.1 1173 0.01705 606.3 1172 0.01701 606.6 1171 0.01698 606.8 1169 0.01696 607 1169 0.01694 607.3 1168 0.0169 607.5 1167 0.01685 607.7 1165 0.01682 608 1165 0.01677 608.2 1164 0.01674 608.4 1162 0.01672 608.7 1161 0.01672 608.9 1161 0.01669 609.1 1159 0.01667 609.4 1158 0.01665 609.6 1158 0.01662 609.8 1156 0.01658 610.1 1155 0.01656 610.3 1154 0.01654 610.5 1154 0.01651 610.8 1153 0.01648 611 1152 0.01646 611.3 1151 0.01643 611.5 1150 0.01641 611.7 1149 0.01637 612 1148 0.01636 612.2 1147 0.01633 612.4 1147 0.01631 612.7 1145 0.01627 612.9 1144 0.01624 613.1 1144 0.01622 613.4 1143 0.01618 613.6 1142 0.01616 613.8 1140 0.01616 614.1 1140 0.01612 614.3 1139 0.01611 614.5 1138 0.01608 614.8 1136 0.01606 615 1136 0.01605 615.2 1136 0.01601 615.5 1134 0.01597 615.7 1134 0.01596 615.9 1133 0.01593 616.2 1132 0.01591 616.4 1131 0.0159 616.6 1129 0.01587 616.9 1129 0.01584 617.1 1128 0.01581 617.3 1127 0.0158 617.6 1126 0.01576 617.8 1125 0.01572 618 1124 0.01571 618.3 1123 0.01569 618.5 1122 0.01565 618.8 1121 0.01565 619 1119 0.01562 619.2 1119 0.01559 619.5 1119 0.01555 619.7 1117 0.01552 619.9 1117 0.01551 620.2 1115 0.01548 620.4 1115 0.01546 620.6 1114 0.01543 620.9 1113 0.01541 621.1 1111 0.01538 621.3 1111 0.01535 621.6 1110 0.01533 621.8 1109 0.0153 622 1108 0.01526 622.3 1107 0.01523 622.5 1106 0.01519 622.7 1105 0.01518 623 1104 0.01515 623.2 1103 0.01512 623.4 1103 0.01509 623.7 1101 0.01507 623.9 1101 0.01504 624.1 1099 0.015 624.4 1099 0.01499 624.6 1098 0.01495 624.8 1097 0.01493 625.1 1096 0.0149 625.3 1095 0.01487 625.5 1094 0.01484 625.8 1093 0.01483 626 1093 0.0148 626.3 1092 0.01477 626.5 1090 0.01473 626.7 1090 0.01472 627 1088 0.01468 627.2 1087 0.01466 627.4 1086 0.01463 627.7 1086 0.01461 627.9 1085 0.01458 628.1 1084 0.01457 628.4 1083 0.01453 628.6 1082 0.01449 628.8 1082 0.01448 629.1 1080 0.01444 629.3 1079 0.01443 629.5 1078 0.0144 629.8 1077 0.01437 630 1076 0.01435 630.2 1075 0.01433 630.5 1074 0.0143 630.7 1073 0.01427 630.9 1072 0.01425 631.2 1072 0.0142 631.4 1071 0.01418 631.6 1069 0.01416 631.9 1068 0.01413 632.1 1068 0.0141 632.3 1067 0.01407 632.6 1065 0.01403 632.8 1065 0.01402 633 1065 0.01397 633.3 1063 0.01396 633.5 1061 0.01394 633.8 1061 0.01392 634 1060 0.0139 634.2 1059 0.01386 634.5 1058 0.01384 634.7 1057 0.01381 634.9 1056 0.01377 635.2 1055 0.01376 635.4 1054 0.01376 635.6 1054 0.01372 635.9 1053 0.0137 636.1 1052 0.01369 636.3 1051 0.01366 636.6 1050 0.01363 636.8 1049 0.01359 637 1048 0.01356 637.3 1047 0.01355 637.5 1046 0.01353 637.7 1044 0.0135 638 1043 0.01349 638.2 1043 0.01348 638.4 1043 0.01346 638.7 1042 0.01343 638.9 1041 0.0134 639.1 1040 0.01339 639.4 1039 0.01338 639.6 1037 0.01336 639.8 1036 0.01334 640.1 1036 0.01331 640.3 1035 0.01329 640.5 1034 0.01327 640.8 1034 0.01324 641 1032 0.01322 641.3 1031 0.01319 641.5 1030 0.01317 641.7 1029 0.01314 642 1028 0.01312 642.2 1028 0.01308 642.4 1026 0.01305 642.7 1026 0.01304 642.9 1024 0.013 643.1 1023 0.01299 643.4 1022 0.01297 643.6 1022 0.01294 643.8 1019 0.01292 644.1 1019 0.01289 644.3 1018 0.01287 644.5 1018 0.01284 644.8 1018 0.01284 645 1016 0.01283 645.2 1015 0.01279 645.5 1014 0.01278 645.7 1013 0.01276 645.9 1012 0.01273 646.2 1011 0.01272 646.4 1011 0.01272 646.6 1009 0.01272 646.9 1009 0.01271 647.1 1008 0.01269 647.3 1007 0.01267 647.6 1006 0.01266 647.8 1005 0.01262 648 1004 0.01259 648.3 1003 0.01258 648.5 1002 0.01253 648.8 1001 0.01251 649 1001 0.0125 649.2 1000 0.01247 649.5 999 0.01243 649.7 998 0.01241 649.9 997 0.01238 650.2 997 0.01235 650.4 995 0.01232 650.6 994 0.0123 650.9 993 0.01228 651.1 992 0.01226 651.3 992 0.01225 651.6 990 0.01222 651.8 989 0.0122 652 988 0.01217 652.3 987 0.01215 652.5 986 0.01214 652.7 986 0.0121 653 985 0.01209 653.2 984 0.01207 653.4 983 0.01205 653.7 982 0.01202 653.9 981 0.012 654.1 980 0.01197 654.4 979 0.01196 654.6 979 0.01195 654.8 977 0.01192 655.1 976 0.0119 655.3 975 0.01186 655.5 975 0.01185 655.8 974 0.01181 656 972 0.01179 656.3 972 0.01176 656.5 971 0.01174 656.7 969 0.01173 657 968 0.01169 657.2 968 0.01168 657.4 967 0.01165 657.7 966 0.01163 657.9 965 0.01161 658.1 965 0.0116 658.4 964 0.01156 658.6 962 0.01154 658.8 961 0.01153 659.1 961 0.01149 659.3 960 0.01145 659.5 959 0.01143 659.8 957 0.01139 660 957 0.01137 660.2 956 0.01133 660.5 955 0.01132 660.7 954 0.0113 660.9 953 0.01129 661.2 952 0.01127 661.4 950 0.01129 661.6 950 0.01127 661.9 949 0.01125 662.1 948 0.01124 662.3 947 0.01122 662.6 947 0.01119 662.8 946 0.01115 663 944 0.01113 663.3 943 0.01109 663.5 943 0.01107 663.8 942 0.01102 664 940 0.01099 664.2 940 0.01096 664.5 940 0.01094 664.7 939 0.01092 664.9 937 0.01089 665.2 936 0.01087 665.4 936 0.01086 665.6 934 0.01084 665.9 933 0.01082 666.1 932 0.01079 666.3 932 0.01077 666.6 930 0.01075 666.8 929 0.01072 667 929 0.0107 667.3 928 0.01067 667.5 927 0.01066 667.7 926 0.01065 668 925 0.01065 668.2 924 0.01061 668.4 923 0.0106 668.7 922 0.01058 668.9 922 0.01056 669.1 920 0.01052 669.4 919 0.0105 669.6 918 0.01048 669.8 917 0.01046 670.1 917 0.01042 670.3 915 0.0104 670.5 914 0.01036 670.8 914 0.01035 671 912 0.01032 671.3 911 0.0103 671.5 911 0.01029 671.7 910 0.01027 672 909 0.01025 672.2 908 0.01024 672.4 907 0.0102 672.7 906 0.01019 672.9 905 0.01015 673.1 904 0.01014 673.4 904 0.01012 673.6 903 0.0101 673.8 902 0.01009 674.1 901 0.01006 674.3 900 0.01004 674.5 899 0.01001 674.8 898 0.009988 675 897 0.009963 675.2 897 0.009938 675.5 895 0.009913 675.7 893 0.009888 675.9 893 0.009864 676.2 893 0.009839 676.4 891 0.009814 676.6 890 0.009789 676.9 889 0.009777 677.1 889 0.009752 677.3 888 0.009739 677.6 886 0.009715 677.8 886 0.00969 678 885 0.009653 678.3 883 0.00964 678.5 883 0.00959 678.8 882 0.009553 679 881 0.009541 679.2 880 0.009504 679.5 879 0.009479 679.7 878 0.009441 679.9 877 0.009441 680.2 876 0.009429 680.4 875 0.009404 680.6 874 0.009392 680.9 873 0.009355 681.1 872 0.00933 681.3 872 0.00933 681.6 871 0.009305 681.8 869 0.00928 682 868 0.009268 682.3 868 0.00923 682.5 867 0.009218 682.7 866 0.009206 683 865 0.009168 683.2 864 0.009144 683.4 863 0.009119 683.7 862 0.009081 683.9 861 0.009069 684.1 861 0.009057 684.4 859 0.009032 684.6 859 0.009007 684.8 858 0.009007 685.1 857 0.008982 685.3 856 0.008945 685.5 855 0.00892 685.8 854 0.008895 686 853 0.00887 686.3 852 0.008833 686.5 850 0.008821 686.7 850 0.008784 687 849 0.008746 687.2 848 0.008721 687.4 847 0.008709 687.7 847 0.008684 687.9 845 0.008659 688.1 844 0.008635 688.4 844 0.00861 688.6 843 0.008597 688.8 842 0.008585 689.1 840 0.00856 689.3 839 0.008548 689.5 839 0.008535 689.8 838 0.008498 690 836 0.008473 690.2 836 0.008448 690.5 835 0.008423 690.7 834 0.008374 690.9 833 0.008361 691.2 832 0.008324 691.4 831 0.008299 691.6 830 0.008275 691.9 829 0.00825 692.1 829 0.008237 692.3 828 0.008225 692.6 826 0.008212 692.8 826 0.0082 693 825 0.008163 693.3 824 0.00815 693.5 823 0.008138 693.8 821 0.008113 694 821 0.008088 694.2 819 0.008039 694.5 819 0.008026 694.7 818 0.008014 694.9 817 0.007989 695.2 817 0.007964 695.4 815 0.007914 695.6 814 0.00789 695.9 814 0.00789 696.1 813 0.007852 696.3 811 0.00784 696.6 811 0.007828 696.8 810 0.007803 697 809 0.007765 697.3 807 0.007741 697.5 807 0.007716 697.7 806 0.007679 698 805 0.007641 698.2 804 0.007641 698.4 803 0.007617 698.7 802 0.007567 698.9 801 0.007542 699.1 801 0.00753 699.4 801 0.007517 699.6 801 0.007492 699.8 801 0.00748 700.1 800 0.007468 700.3 800 0.007455 700.5 799 0.007418 700.8 798 0.007405 701 797 0.007368 701.3 796 0.007343 701.5 795 0.007319 701.7 794 0.007281 702 793 0.007244 702.2 793 0.007232 702.4 792 0.007219 702.7 791 0.007182 702.9 789 0.00717 703.1 789 0.007145 703.4 788 0.007095 703.6 787 0.007083 703.8 786 0.007045 704.1 785 0.007008 704.3 785 0.006983 704.5 784 0.006946 704.8 782 0.006921 705 781 0.006896 705.2 780 0.006872 705.5 779 0.006847 705.7 778 0.006822 705.9 777 0.006797 706.2 777 0.006772 706.4 775 0.006747 706.6 774 0.00671 706.9 773 0.006685 707.1 772 0.006648 707.3 771 0.006623 707.6 770 0.006611 707.8 769 0.006598 708 768 0.006574 708.3 768 0.006549 708.5 767 0.006549 708.8 765 0.006524 709 765 0.006512 709.2 764 0.006499 709.5 763 0.006474 709.7 762 0.006437 709.9 761 0.006412 710.2 761 0.006412 710.4 760 0.006375 710.6 759 0.00635 710.9 757 0.006338 711.1 757 0.006325 711.3 756 0.006313 711.6 755 0.006288 711.8 753 0.006263 712 753 0.006226 712.3 752 0.006226 712.5 751 0.006214 712.7 750 0.006164 713 749 0.006139 713.2 748 0.006114 713.4 746 0.006077 713.7 746 0.006065 713.9 745 0.00604 714.1 744 0.006015 714.4 743 0.00599 714.6 743 0.005953 714.8 742 0.005941 715.1 741 0.005903 715.3 739 0.005878 715.5 739 0.005854 715.8 738 0.005841 716 737 0.005816 716.3 736 0.005816 716.5 735 0.005779 716.7 734 0.005754 717 733 0.005729 717.2 732 0.005692 717.4 731 0.005667 717.7 730 0.00563 717.9 729 0.005605 718.1 728 0.00558 718.4 727 0.005556 718.6 726 0.005531 718.8 726 0.005506 719.1 725 0.005494 719.3 723 0.005481 719.5 722 0.005481 719.8 721 0.005444 720 721 0.005432 720.2 720 0.005394 720.5 719 0.005357 720.7 718 0.005369 720.9 718 0.005345 721.2 717 0.00532 721.4 715 0.00527 721.6 714 0.005245 721.9 714 0.005233 722.1 712 0.005233 722.3 711 0.005196 722.6 711 0.005183 722.8 710 0.005158 723 709 0.005134 723.3 708 0.005109 723.5 707 0.005096 723.8 706 0.005071 724 706 0.005059 724.2 705 0.005034 724.5 704 0.005022 724.7 704 0.005009 724.9 703 0.004985 725.2 703 0.00496 725.4 703 0.004985 725.6 703 0.004972 725.9 703 0.004972 726.1 702 0.00496 726.3 702 0.00496 726.6 701 0.004947 726.8 700 0.004935 727 699 0.00491 727.3 698 0.004885 727.5 696 0.004873 727.7 693 0.004848 728 692 0.004811 728.2 690 0.004786 728.4 688 0.004761 728.7 687 0.004749 728.9 685 0.004711 729.1 684 0.004674 729.4 683 0.004637 729.6 682 0.004612 729.8 681 0.004587 730.1 680 0.004575 730.3 679 0.00455 730.5 678 0.004538 730.8 677 0.004513 731 677 0.004488 731.3 675 0.004438 731.5 676 0.004426 731.7 675 0.004401 732 674 0.004389 732.2 673 0.004339 732.4 672 0.004327 732.7 671 0.004339 732.9 669 0.004314 733.1 668 0.004302 733.4 667 0.004277 733.6 666 0.004265 733.8 664 0.00424 734.1 664 0.004202 734.3 664 0.004165 734.5 664 0.00414 734.8 663 0.004116 735 662 0.004091 735.2 661 0.004066 735.5 660 0.004041 735.7 658 0.004016 735.9 657 0.003991 736.2 656 0.003967 736.4 654 0.003954 736.6 654 0.003929 736.9 653 0.003892 737.1 653 0.003867 737.3 651 0.003867 737.6 651 0.003842 737.8 650 0.003818 738.1 650 0.003793 738.3 649 0.003755 738.5 647 0.003731 738.8 646 0.003718 739 646 0.003681 739.2 643 0.003656 739.5 643 0.003631 739.7 642 0.003607 739.9 641 0.003569 740.2 639 0.003569 740.4 639 0.003557 740.6 638 0.003507 740.9 637 0.003482 741.1 636 0.003458 741.3 636 0.003445 741.6 635 0.003408 741.8 634 0.003383 742 634 0.003371 742.3 632 0.003333 742.5 631 0.003296 742.7 630 0.003271 743 629 0.003259 743.2 628 0.003246 743.4 627 0.003209 743.7 626 0.003184 743.9 625 0.00316 744.1 624 0.003147 744.4 624 0.003122 744.6 623 0.003098 744.8 622 0.003073 745.1 621 0.00306 745.3 620 0.003048 745.6 619 0.003011 745.8 617 0.002973 746 617 0.002973 746.3 616 0.002961 746.5 614 0.002949 746.7 614 0.002924 747 613 0.002899 747.2 612 0.002886 747.4 611 0.002862 747.7 610 0.002849 747.9 610 0.002812 748.1 608 0.002787 748.4 607 0.002762 748.6 607 0.002725 748.8 606 0.002688 749.1 605 0.002651 749.3 604 0.002638 749.5 603 0.002626 749.8 602 0.002601 750 601 0.002576 750.2 601 0.002564 750.5 600 0.002539 750.7 599 0.002514 750.9 598 0.002502 751.2 596 0.002464 751.4 596 0.00244 751.6 594 0.002402 751.9 594 0.002415 752.1 592 0.002377 752.3 592 0.002353 752.6 591 0.002328 752.8 590 0.002315 753.1 589 0.002303 753.3 589 0.002266 753.5 588 0.002253 753.8 587 0.002204 754 585 0.002166 754.2 585 0.002142 754.5 584 0.002117 754.7 583 0.002079 754.9 582 0.002067 755.2 580 0.002055 755.4 580 0.002017 755.6 579 0.002017 755.9 578 0.002005 756.1 577 0.001968 756.3 576 0.001955 756.6 575 0.001943 756.8 574 0.001906 757 574 0.001881 757.3 572 0.001868 757.5 571 0.001831 757.7 571 0.001806 758 569 0.001782 758.2 568 0.001757 758.4 567 0.001732 758.7 567 0.001719 758.9 565 0.001682 759.1 565 0.001657 759.4 564 0.001633 759.6 563 0.001595 759.8 562 0.001583 760.1 561 0.00157 760.3 560 0.001546 760.6 559 0.001508 760.8 558 0.001484 761 557 0.001484 761.3 557 0.001459 761.5 556 0.001434 761.7 555 0.001397 762 553 0.001372 762.2 553 0.001359 762.4 552 0.001335 762.7 550 0.001335 762.9 549 0.00131 763.1 549 0.001285 763.4 548 0.00126 763.6 546 0.00126 763.8 546 0.001223 764.1 545 0.00121 764.3 544 0.001173 764.5 543 0.001161 764.8 542 0.001136 765 542 0.001111 765.2 540 0.001074 765.5 539 0.001061 765.7 539 0.001037 765.9 538 0.001012 766.2 536 0.000987 766.4 536 0.0009622 766.6 535 0.0009373 766.9 534 0.0009001 767.1 533 0.0008628 767.3 532 0.0008504 767.6 531 0.0008256 767.8 530 0.0007883 768.1 529 0.0007635 768.3 528 0.0007263 768.5 528 0.0007014 768.8 527 0.0006766 769 525 0.0006642 769.2 524 0.0006518 769.5 524 0.0006394 769.7 522 0.0006021 769.9 521 0.0005897 770.2 521 0.0005649 770.4 520 0.0005525 770.6 519 0.0005276 770.9 518 0.0005152 771.1 517 0.0004656 771.3 517 0.0004531 771.6 515 0.0004159 771.8 514 0.0004035 772 514 0.0003787 772.3 513 0.0003787 772.5 511 0.0003538 772.7 510 0.000329 773 510 0.0003042 773.2 509 0.0002669 773.4 508 0.0002545 773.7 506 0.0002297 773.9 506 0.0002173 774.1 505 0.0001924 774.4 504 0.0001676 774.6 503 0.0001676 774.8 503 0.0001428 775.1 501 0.0001179 775.3 500 9.311e-05 775.6 499 5.587e-05 775.8 499 3.104e-05 776 497 3.104e-05 776.3 496 6.207e-06 776.5 496 6.207e-06 776.7 494 6.207e-06 777 493 6.207e-06 777.2 493 -6.207e-06 777.4 492 -4.345e-05 777.7 491 -6.828e-05 777.9 490 -8.07e-05 778.1 489 -8.07e-05 778.4 488 -0.0001055 778.6 488 -0.0001428 778.8 486 -0.00018 779.1 485 -0.0002173 779.3 485 -0.0002297 779.5 484 -0.0002669 779.8 483 -0.0002917 780 481 -0.0003166 780.2 481 -0.0003538 780.5 480 -0.0003662 780.7 479 -0.0003911 780.9 478 -0.0004283 781.2 477 -0.0004656 781.4 477 -0.0004904 781.6 475 -0.0005028 781.9 474 -0.00054 782.1 474 -0.00054 782.3 473 -0.0005897 782.6 471 -0.0006518 782.8 471 -0.0006642 783.1 469 -0.000689 783.3 469 -0.0007014 783.5 467 -0.0007139 783.8 467 -0.0007387 784 466 -0.0007635 784.2 465 -0.0007759 784.5 464 -0.0007883 784.7 463 -0.0007759 784.9 462 -0.0007883 785.2 461 -0.0007883 785.4 460 -0.0008256 785.6 460 -0.000838 785.9 458 -0.0008752 786.1 457 -0.0008877 786.3 456 -0.0009001 786.6 456 -0.0009373 786.8 455 -0.0009746 787 453 -0.001024 787.3 453 -0.001074 787.5 452 -0.001074 787.7 451 -0.001074 788 449 -0.001086 788.2 449 -0.001111 788.4 448 -0.001136 788.7 447 -0.001161 788.9 446 -0.001173 789.1 446 -0.001173 789.4 444 -0.001161 789.6 443 -0.001173 789.8 442 -0.001223 790.1 442 -0.001248 790.3 441 -0.001273 790.6 439 -0.001297 790.8 438 -0.001322 791 438 -0.001322 791.3 437 -0.001322 791.5 436 -0.001322 791.7 435 -0.001347 792 434 -0.001372 792.2 433 -0.001384 792.4 432 -0.001422 792.7 431 -0.001446 792.9 430 -0.001446 793.1 430 -0.001459 793.4 428 -0.001471 793.6 428 -0.001521 793.8 427 -0.001508 794.1 425 -0.001533 794.3 424 -0.00157 794.5 424 -0.001558 794.8 423 -0.001583 795 422 -0.001595 795.2 421 -0.001608 795.5 420 -0.00162 795.7 419 -0.001633 795.9 418 -0.001645 796.2 417 -0.001657 796.4 417 -0.001682 796.6 415 -0.001695 796.9 414 -0.001719 797.1 413 -0.001757 797.3 413 -0.001782 797.6 411 -0.001794 797.8 411 -0.001794 798.1 410 -0.001794 798.3 409 -0.001806 798.5 407 -0.001819 798.8 406 -0.001844 799 405 -0.001868 799.2 405 -0.001893 799.5 404 -0.001918 799.7 404 -0.001931 799.9 403 -0.001943 800.2 401 -0.001918 800.4 399 -0.001943 800.6 399 -0.001943 800.9 399 -0.001968 801.1 399 -0.001955 801.3 399 -0.002005 801.6 399 -0.002005 801.8 396 -0.002005 802 394 -0.002005 802.3 392 -0.002005 802.5 391 -0.002005 802.7 390 -0.002005 803 392 -0.002017 803.2 392 -0.002042 803.4 392 -0.002042 803.7 390 -0.00203 803.9 388 -0.002042 804.1 386 -0.002042 804.4 383 -0.00203 804.6 381 -0.002042 804.8 382 -0.002055 805.1 383 -0.002055 805.3 384 -0.002067 805.6 384 -0.002092 805.8 382 -0.002092 806 380 -0.002092 806.3 377 -0.002104 806.5 376 -0.002104 806.7 374 -0.002117 807 373 -0.002117 807.2 374 -0.002104 807.4 374 -0.002104 807.7 374 -0.002129 807.9 373 -0.002117 808.1 371 -0.002117 808.4 370 -0.002117 808.6 368 -0.002117 808.8 368 -0.002142 809.1 367 -0.002129 809.3 366 -0.002129 809.5 365 -0.002142 809.8 364 -0.002154 810 363 -0.002154 810.2 362 -0.002154 810.5 361 -0.002154 810.7 361 -0.002166 810.9 360 -0.002166 811.2 360 -0.002166 811.4 359 -0.002191 811.6 356 -0.002204 811.9 356 -0.002204 812.1 356 -0.002216 812.3 354 -0.002216 812.6 353 -0.002216 812.8 353 -0.002241 813.1 351 -0.002228 813.3 350 -0.002216 813.5 349 -0.002241 813.8 349 -0.002253 814 347 -0.002241 814.2 346 -0.002228 814.5 345 -0.002216 814.7 344 -0.002204 814.9 343 -0.002166 815.2 342 -0.002142 815.4 342 -0.002129 815.6 341 -0.002117 815.9 340 -0.002104 816.1 339 -0.002079 816.3 338 -0.00203 816.6 337 -0.002005 816.8 336 -0.001968 817 335 -0.001931 817.3 334 -0.001893 817.5 333 -0.001856 817.7 332 -0.001794 818 331 -0.001744 818.2 330 -0.001682 818.4 330 -0.00162 818.7 329 -0.001558 818.9 327 -0.001459 819.1 326 -0.001397 819.4 326 -0.001322 819.6 324 -0.001248 819.8 323 -0.001161 820.1 323 -0.001074 820.3 321 -0.0009746 820.6 320 -0.0008877 820.8 319 -0.0007883 821 318 -0.0007014 821.3 317 -0.0006021 821.5 317 -0.0005152 821.7 316 -0.0004283 822 315 -0.0003414 822.2 313 -0.0002669 822.4 313 -0.00018 822.7 312 -0.0001179 822.9 312 -3.104e-05 823.1 310 6.207e-06 823.4 309 5.587e-05 823.6 308 0.0001304 823.8 307 0.0002173 824.1 306 0.0002793 824.3 305 0.0003662 824.5 304 0.0004283 824.8 303 0.0004904 825 302 0.00054 825.2 301 0.0005897 825.5 300 0.0006518 825.7 299 0.0006766 825.9 299 0.0007139 826.2 299 0.0007387 826.4 297 0.0007635 826.6 295 0.0007883 826.9 295 0.0008256 827.1 294 0.0008628 827.3 292 0.0009125 827.6 292 0.0009249 827.8 292 0.0009497 828.1 290 0.0009746 828.3 289 0.0009994 828.5 288 0.001012 828.8 288 0.001024 829 286 0.001049 829.2 286 0.001061 829.5 285 0.001074 829.7 284 0.001099 829.9 283 0.001124 830.2 281 0.001136 830.4 281 0.001136 830.6 280 0.001161 830.9 279 0.001161 831.1 277 0.001198 831.3 277 0.00121 831.6 277 0.001248 831.8 275 0.00126 832 274 0.001297 832.3 274 0.00131 832.5 273 0.001322 832.7 272 0.001322 833 270 0.001322 833.2 270 0.001335 833.4 269 0.001335 833.7 267 0.001335 833.9 267 0.001347 834.1 266 0.001359 834.4 265 0.001372 834.6 264 0.001384 834.8 263 0.001409 835.1 263 0.001397 835.3 261 0.001397 835.6 260 0.001409 835.8 260 0.001409 836 259 0.001409 836.3 258 0.001422 836.5 256 0.001422 836.7 255 0.001422 837 254 0.001434 837.2 254 0.001422 837.4 253 0.001434 837.7 252 0.001446 837.9 252 0.001434 838.1 250 0.001434 838.4 249 0.001434 838.6 249 0.001434 838.8 248 0.001434 839.1 246 0.001434 839.3 245 0.001434 839.5 244 0.001434 839.8 243 0.001422 840 242 0.001397 840.2 242 0.001409 840.5 241 0.001409 840.7 240 0.001409 840.9 239 0.001397 841.2 237 0.001384 841.4 237 0.001372 841.6 235 0.001384 841.9 235 0.001359 842.1 234 0.001347 842.3 233 0.001347 842.6 231 0.001335 842.8 231 0.001335 843.1 231 0.00131 843.3 229 0.001297 843.5 228 0.001322 843.8 227 0.00131 844 227 0.001297 844.2 226 0.001297 844.5 224 0.001285 844.7 224 0.001297 844.9 224 0.001285 845.2 221 0.001285 845.4 221 0.001285 845.6 220 0.001273 845.9 219 0.001248 846.1 219 0.001248 846.3 217 0.001235 846.6 217 0.001235 846.8 216 0.001235 847 214 0.001223 847.3 213 0.001223 847.5 212 0.001223 847.7 211 0.00121 848 210 0.001198 848.2 210 0.001186 848.4 209 0.001161 848.7 208 0.001148 848.9 206 0.001148 849.1 205 0.001136 849.4 205 0.001124 849.6 204 0.001136 849.8 202 0.001136 850.1 202 0.001136 850.3 202 0.001136 850.6 201 0.001111 850.8 200 0.001099 851 199 0.001086 851.3 198 0.001086 851.5 197 0.001061 851.7 196 0.001061 852 195 0.001037 852.2 194 0.001024 852.4 193 0.0009994 852.7 192 0.000987 852.9 192 0.0009746 853.1 190 0.0009746 853.4 189 0.0009746 853.6 189 0.0009497 853.8 188 0.0009373 854.1 187 0.0009249 854.3 186 0.0009249 854.5 185 0.0009001 854.8 184 0.0008877 855 183 0.0008877 855.2 181 0.0008504 855.5 181 0.000838 855.7 180 0.000838 855.9 180 0.0008256 856.2 178 0.0008256 856.4 177 0.0008132 856.6 177 0.0007883 856.9 176 0.0007759 857.1 174 0.0007759 857.3 174 0.0007635 857.6 174 0.0007387 857.8 171 0.0007511 858.1 171 0.0007511 858.3 169 0.0007263 858.5 169 0.0007139 858.8 168 0.000689 859 166 0.000689 859.2 166 0.0006766 859.5 166 0.0006642 859.7 164 0.0006766 859.9 164 0.0006642 860.2 163 0.0006518 860.4 161 0.000627 860.6 161 0.000627 860.9 159 0.0006145 861.1 159 0.0005897 861.3 158 0.0005897 861.6 156 0.0006021 861.8 156 0.0005897 862 155 0.0005773 862.3 154 0.0005649 862.5 154 0.0005649 862.7 152 0.0005525 863 152 0.00054 863.2 150 0.0005276 863.4 149 0.0005028 863.7 149 0.0004904 863.9 147 0.000478 864.1 147 0.0004531 864.4 145 0.0004283 864.6 145 0.0004283 864.8 143 0.0004283 865.1 142 0.0004531 865.3 142 0.0004407 865.6 141 0.0004283 865.8 140 0.0004159 866 139 0.0004159 866.3 138 0.0003911 866.5 137 0.0003787 866.7 136 0.0003662 867 135 0.0003414 867.2 134 0.000329 867.4 134 0.000329 867.7 132 0.000329 867.9 131 0.0003166 868.1 131 0.0002917 868.4 130 0.0002669 868.6 129 0.0002669 868.8 127 0.0002669 869.1 127 0.0002669 869.3 126 0.0002669 869.5 125 0.0002421 869.8 124 0.0002297 870 123 0.0002297 870.2 121 0.0002173 870.5 121 0.0002048 870.7 120 0.00018 870.9 119 0.0001676 871.2 118 0.0001676 871.4 117 0.0001676 871.6 116 0.0001552 871.9 115 0.0001552 872.1 115 0.0001304 872.3 113 0.0001179 872.6 113 0.0001179 872.8 112 0.0001055 873.1 111 0.0001055 873.3 110 9.311e-05 873.5 109 6.828e-05 873.8 108 3.104e-05 874 108 1.862e-05 874.2 106 6.207e-06 874.5 106 6.207e-06 874.7 105 6.207e-06 874.9 104 6.207e-06 875.2 102 6.207e-06 875.4 102 6.207e-06 875.6 101 6.207e-06 875.9 100 6.207e-06 876.1 98 -1.862e-05 876.3 98 -3.104e-05 876.6 97 -3.104e-05 876.8 97 -4.345e-05 877 95 -4.345e-05 877.3 94 -4.345e-05 877.5 93 -4.345e-05 877.7 92 -5.587e-05 878 92 -5.587e-05 878.2 91 -8.07e-05 878.4 90 -8.07e-05 878.7 89 -9.311e-05 878.9 88 -9.311e-05 879.1 87 -0.0001055 879.4 87 -0.0001304 879.6 85 -0.0001304 879.8 84 -0.0001676 880.1 84 -0.0001924 880.3 83 -0.0002048 880.6 81 -0.0002048 880.8 81 -0.0002048 881 81 -0.0002048 881.3 80 -0.0002048 881.5 79 -0.0002297 881.7 77 -0.0002421 882 77 -0.0002545 882.2 76 -0.0002545 882.4 74 -0.0002545 882.7 74 -0.0002669 882.9 73 -0.0002917 883.1 73 -0.0003042 883.4 71 -0.0003042 883.6 70 -0.0003166 883.8 70 -0.0003166 884.1 68 -0.0003414 884.3 68 -0.0003414 884.5 67 -0.0003662 884.8 66 -0.0003662 885 65 -0.0003662 885.2 64 -0.0003911 885.5 63 -0.0004035 885.7 63 -0.0004159 885.9 62 -0.0004159 886.2 61 -0.0004283 886.4 59 -0.0004531 886.6 59 -0.0004531 886.9 58 -0.0004656 887.1 57 -0.0004904 887.3 56 -0.0005028 887.6 55 -0.0005028 887.8 55 -0.0005152 888.1 54 -0.0005152 888.3 53 -0.0005152 888.5 52 -0.0005276 888.8 52 -0.0005276 889 51 -0.0005276 889.2 50 -0.0005525 889.5 49 -0.0005649 889.7 48 -0.0005649 889.9 48 -0.0005773 890.2 48 -0.0005773 890.4 47 -0.0005773 890.6 46 -0.0006021 890.9 45 -0.0006145 891.1 44 -0.0006145 891.3 44 -0.000627 891.6 44 -0.0006518 891.8 43 -0.0006642 892 42 -0.0006642 892.3 42 -0.0006766 892.5 41 -0.0007014 892.7 41 -0.0007139 893 40 -0.0007263 893.2 39 -0.0007263 893.4 38 -0.0007263 893.7 38 -0.0007263 893.9 38 -0.0007263 894.1 37 -0.0007263 894.4 36 -0.0007387 894.6 36 -0.0007511 894.8 35 -0.0007635 895.1 34 -0.0007635 895.3 34 -0.0007759 895.6 34 -0.0007759 895.8 33 -0.0007883 896 33 -0.0008132 896.3 32 -0.0008256 896.5 31 -0.0008256 896.7 31 -0.000838 897 30 -0.0008504 897.2 30 -0.0008628 897.4 30 -0.0008752 897.7 30 -0.0008877 897.9 29 -0.0008752 898.1 29 -0.0008877 898.4 29 -0.0008877 898.6 28 -0.0008877 898.8 28 -0.0008752 899.1 27 -0.0008877 899.3 27 -0.0008877 899.5 27 -0.0008877 899.8 27 -0.0008877 900 27 -0.0008877 900.2 26 -0.0008752 900.5 26 -0.0009001 900.7 26 -0.0009125 900.9 26 -0.0009249 901.2 25 -0.0009249 901.4 24 -0.0009249 901.6 24 -0.0009249 901.9 24 -0.0009373 902.1 23 -0.0009373 902.3 23 -0.0009373 902.6 23 -0.0009373 902.8 23 -0.0009373 903.1 23 -0.0009497 903.3 23 -0.0009497 903.5 23 -0.0009249 903.8 23 -0.0009373 904 22 -0.0009373 904.2 22 -0.0009497 904.5 22 -0.0009622 904.7 22 -0.0009622 904.9 21 -0.0009746 905.2 21 -0.0009746 905.4 21 -0.0009746 905.6 21 -0.000987 905.9 21 -0.000987 906.1 20 -0.0009994 906.3 20 -0.0009994 906.6 20 -0.000987 906.8 20 -0.0009994 907 20 -0.0009994 907.3 20 -0.0009994 907.5 20 -0.0009994 907.7 20 -0.000987 908 19 -0.000987 908.2 19 -0.0009994 908.4 19 -0.0009994 908.7 19 -0.000987 908.9 19 -0.000987 909.1 19 -0.0009994 909.4 19 -0.0009994 909.6 19 -0.000987 909.8 18 -0.000987 910.1 18 -0.0009994 910.3 18 -0.0009994 910.6 18 -0.000987 910.8 18 -0.000987 911 18 -0.000987 911.3 18 -0.000987 911.5 18 -0.0009994 911.7 18 -0.001012 912 18 -0.001024 912.2 17 -0.001024 912.4 17 -0.001012 912.7 17 -0.001012 912.9 17 -0.001024 913.1 17 -0.001024 913.4 17 -0.001037 913.6 16 -0.001037 913.8 16 -0.001024 914.1 17 -0.001024 914.3 16 -0.001024 914.5 16 -0.001024 914.8 16 -0.001037 915 16 -0.001037 915.2 16 -0.001037 915.5 17 -0.001037 915.7 16 -0.001049 915.9 16 -0.001037 916.2 16 -0.001049 916.4 16 -0.001049 916.6 16 -0.001049 916.9 16 -0.001061 917.1 16 -0.001061 917.3 16 -0.001061 917.6 16 -0.001074 917.8 15 -0.001086 918.1 16 -0.001086 918.3 16 -0.001086 918.5 15 -0.001086 918.8 15 -0.001099 919 15 -0.001099 919.2 15 -0.001099 919.5 15 -0.001099 919.7 15 -0.001086 919.9 15 -0.001099 920.2 15 -0.001099 920.4 15 -0.001099 920.6 15 -0.001099 920.9 15 -0.001099 921.1 15 -0.001074 921.3 15 -0.001061 921.6 14 -0.001074 921.8 15 -0.001086 922 14 -0.001086 922.3 14 -0.001086 922.5 15 -0.001086 922.7 14 -0.001099 923 14 -0.001086 923.2 14 -0.001099 923.4 14 -0.001099 923.7 14 -0.001099 923.9 14 -0.001099 924.1 14 -0.001086 924.4 14 -0.001099 924.6 14 -0.001099 924.8 14 -0.001099 925.1 13 -0.001099 925.3 13 -0.001099 925.6 14 -0.001086 925.8 13 -0.001074 926 14 -0.001074 926.3 13 -0.001086 926.5 13 -0.001086 926.7 14 -0.001086 927 13 -0.001086 927.2 13 -0.001099 927.4 13 -0.001099 927.7 13 -0.001086 927.9 13 -0.001086 928.1 13 -0.001074 928.4 13 -0.001061 928.6 13 -0.001074 928.8 13 -0.001074 929.1 13 -0.001086 929.3 13 -0.001086 929.5 13 -0.001086 929.8 13 -0.001086 930 13 -0.001099 930.2 13 -0.001086 930.5 13 -0.001099 930.7 13 -0.001099 930.9 13 -0.001099 931.2 13 -0.001099 931.4 13 -0.001099 931.6 13 -0.001099 931.9 13 -0.001099 932.1 13 -0.001099 932.3 13 -0.001086 932.6 13 -0.001099 932.8 13 -0.001111 933.1 13 -0.001111 933.3 13 -0.001111 933.5 13 -0.001099 933.8 13 -0.001099 934 12 -0.001111 934.2 12 -0.001111 934.5 13 -0.001111 934.7 13 -0.001124 934.9 12 -0.001111 935.2 12 -0.001111 935.4 12 -0.001099 935.6 12 -0.001099 935.9 12 -0.001099 936.1 12 -0.001099 936.3 12 -0.001099 936.6 12 -0.001099 936.8 13 -0.001099 937 12 -0.001099 937.3 12 -0.001124 937.5 12 -0.001099 937.7 12 -0.001099 938 12 -0.001099 938.2 12 -0.001099 938.4 12 -0.001099 938.7 12 -0.001099 938.9 12 -0.001099 939.1 12 -0.001124 939.4 12 -0.001111 939.6 12 -0.001124 939.8 12 -0.001124 940.1 12 -0.001124 940.3 12 -0.001124 940.6 12 -0.001136 940.8 12 -0.001136 941 12 -0.001136 941.3 11 -0.001136 941.5 11 -0.001136 941.7 12 -0.001148 942 12 -0.001148 942.2 11 -0.001136 942.4 12 -0.001124 942.7 11 -0.001099 942.9 11 -0.001099 943.1 11 -0.001086 943.4 12 -0.001099 943.6 11 -0.001099 943.8 11 -0.001124 944.1 11 -0.001124 944.3 11 -0.001111 944.5 11 -0.001124 944.8 11 -0.001111 945 11 -0.001124 945.2 11 -0.001136 945.5 11 -0.001136 945.7 11 -0.001136 945.9 11 -0.001124 946.2 11 -0.001111 946.4 11 -0.001111 946.6 11 -0.001099 946.9 11 -0.001099 947.1 11 -0.001111 947.3 11 -0.001136 947.6 11 -0.001161 947.8 11 -0.001161 948.1 11 -0.001161 948.3 11 -0.001148 948.5 11 -0.001148 948.8 10 -0.001148 949 11 -0.001148 949.2 11 -0.001148 949.5 11 -0.001148 949.7 11 -0.001161 949.9 11 -0.001161 950.2 11 -0.001161 950.4 10 -0.001148 950.6 11 -0.001148 950.9 11 -0.001136 951.1 11 -0.001136 951.3 11 -0.001148 951.6 11 -0.001136 951.8 10 -0.001148 952 10 -0.001136 952.3 10 -0.001148 952.5 10 -0.001124 952.7 11 -0.001124 953 10 -0.001099 953.2 10 -0.001099 953.4 11 -0.001111 953.7 11 -0.001124 953.9 10 -0.001136 954.1 11 -0.001136 954.4 11 -0.001124 954.6 11 -0.001124 954.8 11 -0.001124 955.1 10 -0.001136 955.3 10 -0.001136 955.6 10 -0.001136 955.8 10 -0.001136 956 10 -0.001148 956.3 10 -0.001173 956.5 10 -0.001173 956.7 10 -0.001161 957 10 -0.001161 957.2 10 -0.001173 957.4 10 -0.001161 957.7 10 -0.001148 957.9 10 -0.001148 958.1 10 -0.001148 958.4 10 -0.001148 958.6 10 -0.001148 958.8 8 0.21 0.05 0.66 0.002 0.007 0.75 2.11 0.83 0.31 0 0.62 0 0 0 5 -1.858e-05 0 9 -3.096e-05 0.1611 8 -3.096e-05 0.3223 8 -3.096e-05 0.4834 8 -3.096e-05 0.6445 8 -3.096e-05 0.8057 7 -3.096e-05 0.9668 7 -5.573e-05 1.128 8 -5.573e-05 1.289 8 -6.811e-05 1.45 7 -6.811e-05 1.611 7 -6.811e-05 1.772 8 -6.811e-05 1.934 7 -8.049e-05 2.095 9 -6.811e-05 2.256 9 -6.811e-05 2.417 9 -3.096e-05 2.578 9 0.0002167 2.739 9 0.0002291 2.9 9 0.0001053 3.062 12 3.096e-05 3.223 13 6.192e-06 3.384 15 6.192e-06 3.545 16 6.192e-06 3.706 18 6.192e-06 3.867 20 6.192e-06 4.028 21 6.192e-06 4.189 23 1.858e-05 4.351 26 3.096e-05 4.512 27 6.811e-05 4.673 29 0.0001053 4.834 30 0.00013 4.995 34 0.0001424 5.156 35 0.0001796 5.317 37 0.0002043 5.479 39 0.0002291 5.64 41 0.0002662 5.801 43 0.0002786 5.962 44 0.0003034 6.123 46 0.0003282 6.284 47 0.0003653 6.445 49 0.0003901 6.606 51 0.0004025 6.768 52 0.0004396 6.929 53 0.0004396 7.09 54 0.000452 7.251 55 0.0004644 7.412 57 0.0004644 7.573 59 0.0004891 7.734 59 0.0005015 7.896 61 0.0005263 8.057 62 0.0005263 8.218 63 0.0005511 8.379 65 0.0005634 8.54 66 0.0005758 8.701 68 0.0006006 8.862 69 0.000613 9.024 71 0.0006254 9.185 71 0.0006377 9.346 73 0.0006377 9.507 74 0.0006501 9.668 76 0.0006501 9.829 77 0.0006501 9.99 78 0.0006749 10.15 80 0.0006749 10.31 81 0.0006997 10.47 82 0.0007244 10.63 84 0.0007244 10.8 84 0.0007492 10.96 86 0.000774 11.12 87 0.0007863 11.28 88 0.0007987 11.44 90 0.0008111 11.6 91 0.0008235 11.76 92 0.0008483 11.92 93 0.0008483 12.09 95 0.0008606 12.25 97 0.0008606 12.41 98 0.0008854 12.57 101 0.0009102 12.73 102 0.0009226 12.89 102 0.0009349 13.05 104 0.0009349 13.21 106 0.0009597 13.37 106 0.0009721 13.54 107 0.0009845 13.7 109 0.0009969 13.86 111 0.001022 14.02 112 0.001046 14.18 113 0.001071 14.34 115 0.001084 14.5 115 0.001071 14.66 117 0.001071 14.82 118 0.001096 14.99 120 0.001108 15.15 121 0.001133 15.31 121 0.001145 15.47 123 0.001158 15.63 124 0.001183 15.79 126 0.001195 15.95 127 0.001195 16.11 129 0.001207 16.27 130 0.00122 16.44 131 0.001245 16.6 132 0.001245 16.76 134 0.001257 16.92 134 0.001257 17.08 135 0.001269 17.24 137 0.001282 17.4 138 0.001294 17.56 140 0.001319 17.72 141 0.001344 17.89 142 0.001356 18.05 143 0.001368 18.21 145 0.001381 18.37 146 0.001381 18.53 146 0.001406 18.69 148 0.001418 18.85 150 0.001443 19.01 150 0.001467 19.17 152 0.00148 19.34 154 0.001492 19.5 156 0.001505 19.66 156 0.001517 19.82 157 0.001554 19.98 159 0.001591 20.14 160 0.001616 20.3 162 0.001628 20.46 163 0.001641 20.63 163 0.001641 20.79 165 0.001666 20.95 166 0.00169 21.11 168 0.001715 21.27 169 0.001727 21.43 170 0.00174 21.59 171 0.001765 21.75 172 0.001789 21.91 174 0.001789 22.08 175 0.001814 22.24 177 0.001839 22.4 178 0.001864 22.56 180 0.001913 22.72 181 0.001938 22.88 182 0.001963 23.04 184 0.001988 23.2 184 0.002037 23.36 187 0.002062 23.53 188 0.002087 23.69 189 0.002111 23.85 191 0.002136 24.01 191 0.002149 24.17 193 0.002149 24.33 194 0.002136 24.49 196 0.002149 24.65 196 0.002161 24.81 198 0.002186 24.98 199 0.00221 25.14 201 0.002223 25.3 201 0.002235 25.46 202 0.002248 25.62 204 0.00226 25.78 206 0.002285 25.94 206 0.002322 26.1 207 0.002347 26.26 209 0.002371 26.43 209 0.002384 26.59 212 0.002409 26.75 213 0.002433 26.91 213 0.002458 27.07 215 0.002483 27.23 216 0.002508 27.39 217 0.002508 27.55 219 0.002532 27.72 220 0.002557 27.88 221 0.002607 28.04 223 0.002631 28.2 224 0.002631 28.36 226 0.002656 28.52 227 0.002681 28.68 229 0.002706 28.84 231 0.002731 29 232 0.002755 29.17 234 0.002768 29.33 234 0.00278 29.49 236 0.002805 29.65 237 0.002817 29.81 238 0.00283 29.97 240 0.002842 30.13 242 0.002854 30.29 242 0.002867 30.45 243 0.002879 30.62 245 0.002879 30.78 246 0.002904 30.94 247 0.002916 31.1 249 0.002929 31.26 249 0.002953 31.42 251 0.002953 31.58 252 0.002978 31.74 253 0.002991 31.9 254 0.002991 32.07 256 0.003003 32.23 257 0.003003 32.39 259 0.003003 32.55 260 0.003003 32.71 262 0.00304 32.87 262 0.003053 33.03 264 0.003077 33.19 265 0.003102 33.35 266 0.003102 33.52 268 0.003127 33.68 268 0.003127 33.84 270 0.003139 34 271 0.003139 34.16 273 0.003152 34.32 274 0.003176 34.48 276 0.003176 34.64 277 0.003201 34.8 278 0.003226 34.97 279 0.003251 35.13 281 0.003263 35.29 281 0.003275 35.45 284 0.0033 35.61 285 0.0033 35.77 286 0.003325 35.93 287 0.003337 36.09 288 0.003362 36.26 289 0.003374 36.42 291 0.003374 36.58 292 0.003387 36.74 292 0.003387 36.9 293 0.003399 37.06 293 0.003424 37.22 296 0.003449 37.38 297 0.003474 37.54 299 0.003498 37.71 300 0.003511 37.87 301 0.003535 38.03 302 0.003573 38.19 304 0.003597 38.35 306 0.00361 38.51 307 0.003635 38.67 309 0.003647 38.83 310 0.003672 38.99 311 0.003696 39.16 313 0.003721 39.32 313 0.003746 39.48 315 0.003758 39.64 317 0.003771 39.8 318 0.003796 39.96 320 0.00382 40.12 320 0.003833 40.28 322 0.003833 40.44 324 0.003845 40.61 324 0.003882 40.77 327 0.003919 40.93 328 0.003944 41.09 328 0.003969 41.25 329 0.003981 41.41 331 0.003956 41.57 332 0.003956 41.73 334 0.003956 41.89 335 0.003956 42.06 336 0.003956 42.22 338 0.003969 42.38 339 0.003981 42.54 340 0.004006 42.7 342 0.004043 42.86 342 0.004056 43.02 344 0.004068 43.18 345 0.004093 43.35 346 0.004093 43.51 348 0.00413 43.67 349 0.004142 43.83 350 0.004155 43.99 353 0.004192 44.15 353 0.004217 44.31 354 0.004229 44.47 356 0.004241 44.63 357 0.004254 44.8 359 0.004291 44.96 360 0.004303 45.12 361 0.004328 45.28 362 0.00434 45.44 363 0.004365 45.6 365 0.004365 45.76 367 0.004353 45.92 368 0.00439 46.08 369 0.004427 46.25 370 0.004427 46.41 371 0.004415 46.57 374 0.004439 46.73 374 0.004464 46.89 376 0.004464 47.05 378 0.004489 47.21 379 0.004514 47.37 380 0.004539 47.53 381 0.004563 47.7 382 0.004563 47.86 384 0.0046 48.02 385 0.004613 48.18 386 0.004613 48.34 387 0.004638 48.5 388 0.004638 48.66 390 0.004662 48.82 392 0.004662 48.98 393 0.004662 49.15 393 0.004687 49.31 395 0.004687 49.47 396 0.004712 49.63 397 0.004737 49.79 399 0.004737 49.95 399 0.004749 50.11 401 0.004774 50.27 403 0.004786 50.43 403 0.004811 50.6 404 0.004823 50.76 406 0.004836 50.92 406 0.00486 51.08 409 0.004885 51.24 409 0.00491 51.4 411 0.004922 51.56 412 0.004935 51.72 413 0.00496 51.89 414 0.004984 52.05 416 0.005009 52.21 417 0.005034 52.37 418 0.005083 52.53 420 0.005108 52.69 421 0.005133 52.85 422 0.005158 53.01 424 0.00517 53.17 424 0.005182 53.34 426 0.005207 53.5 428 0.005232 53.66 429 0.005257 53.82 431 0.005282 53.98 431 0.005319 54.14 433 0.005343 54.3 435 0.005343 54.46 435 0.005381 54.62 437 0.005418 54.79 438 0.00543 54.95 439 0.005455 55.11 440 0.00548 55.27 442 0.005492 55.43 443 0.005529 55.59 445 0.005542 55.75 446 0.005554 55.91 447 0.005579 56.07 449 0.005616 56.24 450 0.005628 56.4 451 0.005665 56.56 453 0.005703 56.72 454 0.005727 56.88 455 0.005777 57.04 456 0.005802 57.2 457 0.005814 57.36 459 0.005839 57.52 460 0.005851 57.69 462 0.005876 57.85 462 0.005913 58.01 464 0.005938 58.17 465 0.005963 58.33 467 0.005987 58.49 468 0.006012 58.65 470 0.006037 58.81 471 0.006074 58.98 471 0.006099 59.14 473 0.006124 59.3 474 0.006136 59.46 476 0.006161 59.62 478 0.006185 59.78 478 0.006198 59.94 480 0.006223 60.1 481 0.006247 60.26 482 0.006272 60.43 484 0.006297 60.59 485 0.006322 60.75 486 0.006346 60.91 488 0.006371 61.07 489 0.006371 61.23 490 0.006396 61.39 492 0.006408 61.55 493 0.006433 61.71 494 0.00647 61.88 496 0.00647 62.04 496 0.006507 62.2 498 0.00652 62.36 499 0.006545 62.52 501 0.006569 62.68 502 0.006594 62.84 503 0.006607 63 504 0.006644 63.16 506 0.006656 63.33 507 0.006668 63.49 509 0.006706 63.65 510 0.006718 63.81 510 0.00673 63.97 512 0.006755 64.13 513 0.006768 64.29 515 0.00678 64.45 516 0.006805 64.61 517 0.006829 64.78 518 0.006842 64.94 520 0.006842 65.1 521 0.006854 65.26 522 0.006867 65.42 524 0.006879 65.58 524 0.006904 65.74 526 0.006916 65.9 528 0.006929 66.06 529 0.006953 66.23 531 0.006966 66.39 532 0.006978 66.55 534 0.007003 66.71 534 0.00704 66.87 535 0.007065 67.03 537 0.007077 67.19 539 0.007089 67.35 540 0.007102 67.52 540 0.007114 67.68 542 0.007127 67.84 543 0.007151 68 544 0.007164 68.16 546 0.007189 68.32 547 0.007189 68.48 549 0.007201 68.64 549 0.007226 68.8 551 0.007238 68.97 553 0.007263 69.13 554 0.007275 69.29 555 0.007288 69.45 556 0.0073 69.61 557 0.007325 69.77 559 0.007337 69.93 560 0.00735 70.09 562 0.007362 70.25 563 0.007374 70.42 565 0.007387 70.58 565 0.007411 70.74 567 0.007424 70.9 568 0.007436 71.06 570 0.007449 71.22 571 0.007461 71.38 571 0.007461 71.54 573 0.007511 71.7 574 0.007523 71.87 576 0.007548 72.03 578 0.007572 72.19 578 0.007585 72.35 580 0.007597 72.51 581 0.007634 72.67 582 0.007647 72.83 584 0.007672 72.99 585 0.007709 73.15 586 0.007721 73.32 588 0.007758 73.48 589 0.007758 73.64 590 0.007795 73.8 592 0.007808 73.96 593 0.007808 74.12 594 0.007832 74.28 596 0.007857 74.44 596 0.007894 74.61 599 0.007907 74.77 600 0.007907 74.93 601 0.007932 75.09 602 0.007956 75.25 603 0.007981 75.41 604 0.007993 75.57 606 0.008006 75.73 607 0.008031 75.89 608 0.008055 76.06 609 0.008093 76.22 610 0.008117 76.38 612 0.00813 76.54 612 0.008154 76.7 614 0.008154 76.86 615 0.008192 77.02 617 0.008229 77.18 618 0.008254 77.34 620 0.008291 77.51 621 0.008303 77.67 622 0.008291 77.83 624 0.008303 77.99 625 0.008328 78.15 626 0.00834 78.31 628 0.008353 78.47 628 0.008377 78.63 630 0.008402 78.79 631 0.008439 78.96 632 0.008452 79.12 634 0.008464 79.28 635 0.008464 79.44 636 0.008476 79.6 637 0.008501 79.76 639 0.008538 79.92 640 0.008551 80.08 642 0.008575 80.24 643 0.008588 80.41 645 0.008613 80.57 646 0.008637 80.73 648 0.008675 80.89 649 0.008699 81.05 650 0.008712 81.21 653 0.008724 81.37 653 0.008749 81.53 654 0.008774 81.69 656 0.008774 81.86 657 0.008786 82.02 659 0.008798 82.18 660 0.008823 82.34 660 0.008823 82.5 662 0.008848 82.66 663 0.00886 82.82 664 0.008848 82.98 666 0.008873 83.15 667 0.008885 83.31 668 0.008897 83.47 670 0.008922 83.63 671 0.008922 83.79 671 0.008947 83.95 673 0.008947 84.11 675 0.008972 84.27 676 0.008984 84.43 677 0.008997 84.6 678 0.009034 84.76 679 0.009058 84.92 681 0.009071 85.08 682 0.009083 85.24 684 0.009083 85.4 684 0.009108 85.56 686 0.00912 85.72 687 0.009133 85.88 689 0.009158 86.05 689 0.00917 86.21 691 0.009182 86.37 693 0.009195 86.53 693 0.009195 86.69 695 0.009195 86.85 696 0.009232 87.01 697 0.009244 87.17 700 0.009244 87.33 700 0.009269 87.5 701 0.009294 87.66 703 0.009318 87.82 703 0.009343 87.98 705 0.009368 88.14 706 0.00938 88.3 708 0.009393 88.46 709 0.009405 88.62 710 0.009418 88.78 711 0.009455 88.95 713 0.009479 89.11 714 0.009504 89.27 715 0.009517 89.43 717 0.009517 89.59 718 0.009529 89.75 719 0.009541 89.91 721 0.009541 90.07 722 0.009591 90.24 723 0.009603 90.4 725 0.00964 90.56 726 0.009678 90.72 728 0.00969 90.88 728 0.00969 91.04 729 0.009715 91.2 731 0.00974 91.36 732 0.009777 91.52 734 0.009789 91.69 735 0.009839 91.85 736 0.009851 92.01 737 0.009851 92.17 739 0.009863 92.33 740 0.009888 92.49 742 0.009913 92.65 743 0.009938 92.81 744 0.009962 92.97 745 0.009975 93.14 746 0.009987 93.3 748 0.01001 93.46 749 0.01004 93.62 750 0.01005 93.78 750 0.01007 93.94 753 0.01009 94.1 753 0.0101 94.26 753 0.01014 94.42 754 0.01016 94.59 756 0.01019 94.75 757 0.01021 94.91 757 0.01025 95.07 759 0.0103 95.23 759 0.01033 95.39 760 0.01037 95.55 761 0.0104 95.71 761 0.01042 95.87 762 0.01046 96.04 762 0.01048 96.2 762 0.01052 96.36 764 0.01057 96.52 764 0.01062 96.68 765 0.01066 96.84 765 0.01069 97 767 0.01073 97.16 768 0.01077 97.32 769 0.01083 97.49 771 0.01089 97.65 771 0.01094 97.81 774 0.011 97.97 775 0.01103 98.13 778 0.01108 98.29 779 0.01111 98.45 781 0.01115 98.61 782 0.01116 98.78 784 0.01121 98.94 786 0.01126 99.1 788 0.01129 99.26 790 0.01132 99.42 792 0.01135 99.58 793 0.0114 99.74 796 0.01142 99.9 798 0.01147 100.1 800 0.01151 100.2 801 0.01154 100.4 801 0.01156 100.5 801 0.01161 100.7 803 0.01162 100.9 804 0.01162 101 806 0.01167 101.2 807 0.01168 101.4 809 0.0117 101.5 809 0.0117 101.7 811 0.01168 101.8 812 0.01167 102 813 0.01163 102.2 814 0.0116 102.3 815 0.01156 102.5 817 0.01151 102.6 817 0.01149 102.8 818 0.01145 103 820 0.01137 103.1 821 0.01135 103.3 821 0.01131 103.4 823 0.01121 103.6 825 0.01114 103.8 825 0.01109 103.9 826 0.011 104.1 828 0.01093 104.3 829 0.01087 104.4 830 0.01077 104.6 831 0.01069 104.7 832 0.01063 104.9 834 0.01056 105.1 836 0.01047 105.2 837 0.0104 105.4 839 0.0103 105.5 840 0.01022 105.7 842 0.01016 105.9 843 0.01009 106 844 0.01001 106.2 847 0.009962 106.3 848 0.009901 106.5 850 0.009839 106.7 850 0.009789 106.8 853 0.00974 107 854 0.009702 107.2 856 0.009653 107.3 857 0.009616 107.5 859 0.009579 107.6 861 0.009541 107.8 863 0.009529 108 865 0.009517 108.1 868 0.009479 108.3 869 0.009479 108.4 872 0.009442 108.6 874 0.009442 108.8 876 0.009467 108.9 878 0.009479 109.1 879 0.009479 109.2 881 0.009467 109.4 882 0.009455 109.6 884 0.009467 109.7 886 0.009479 109.9 886 0.009479 110.1 887 0.009492 110.2 889 0.009504 110.4 890 0.009517 110.5 891 0.009517 110.7 892 0.009517 110.9 893 0.009517 111 893 0.009517 111.2 894 0.009529 111.3 896 0.009541 111.5 897 0.009566 111.7 897 0.009579 111.8 897 0.009591 112 898 0.009616 112.1 900 0.00964 112.3 900 0.00964 112.5 901 0.009653 112.6 901 0.009665 112.8 903 0.00969 113 904 0.00974 113.1 904 0.00974 113.3 906 0.009777 113.4 906 0.009801 113.6 907 0.009839 113.8 908 0.009863 113.9 909 0.009901 114.1 911 0.009925 114.2 911 0.009938 114.4 912 0.009962 114.6 914 0.01 114.7 915 0.01005 114.9 915 0.01007 115 917 0.01009 115.2 918 0.0101 115.4 919 0.01014 115.5 922 0.01017 115.7 922 0.01021 115.9 923 0.01023 116 925 0.01027 116.2 926 0.0103 116.3 928 0.01032 116.5 929 0.01035 116.7 930 0.01038 116.8 932 0.01043 117 933 0.01047 117.1 935 0.01048 117.3 936 0.01053 117.5 937 0.01056 117.6 939 0.01058 117.8 940 0.01059 118 942 0.01063 118.1 943 0.01068 118.3 944 0.01071 118.4 945 0.01073 118.6 947 0.01075 118.8 949 0.0108 118.9 950 0.01083 119.1 951 0.01087 119.2 953 0.01089 119.4 954 0.0109 119.6 956 0.01089 119.7 957 0.01092 119.9 959 0.01094 120 959 0.01097 120.2 961 0.011 120.4 962 0.01103 120.5 964 0.01104 120.7 965 0.01108 120.9 967 0.01109 121 968 0.01108 121.2 968 0.0111 121.3 970 0.01113 121.5 972 0.01118 121.7 972 0.0112 121.8 975 0.01123 122 975 0.01126 122.1 976 0.0113 122.3 978 0.01132 122.5 979 0.01137 122.6 981 0.0114 122.8 981 0.01144 122.9 983 0.0115 123.1 984 0.01151 123.3 985 0.01151 123.4 987 0.01152 123.6 988 0.01154 123.8 989 0.01155 123.9 990 0.01157 124.1 992 0.01161 124.2 993 0.01163 124.4 994 0.01165 124.6 995 0.01167 124.7 997 0.01172 124.9 998 0.01172 125 1000 0.01176 125.2 1001 0.0118 125.4 1001 0.01181 125.5 1003 0.01182 125.7 1004 0.01186 125.8 1005 0.01188 126 1006 0.01192 126.2 1008 0.01196 126.3 1009 0.01201 126.5 1010 0.01204 126.7 1011 0.01207 126.8 1012 0.01212 127 1014 0.01214 127.1 1015 0.01218 127.3 1015 0.0122 127.5 1017 0.01222 127.6 1018 0.01222 127.8 1018 0.01225 127.9 1020 0.01228 128.1 1022 0.01232 128.3 1022 0.01235 128.4 1023 0.01238 128.6 1024 0.01241 128.7 1025 0.01243 128.9 1026 0.01243 129.1 1026 0.01245 129.2 1028 0.01249 129.4 1029 0.01253 129.6 1031 0.01256 129.7 1031 0.0126 129.9 1033 0.01264 130 1034 0.01269 130.2 1036 0.01269 130.4 1037 0.01271 130.5 1039 0.01274 130.7 1040 0.01279 130.8 1042 0.01281 131 1043 0.01286 131.2 1045 0.01291 131.3 1047 0.01296 131.5 1048 0.01298 131.6 1050 0.01303 131.8 1051 0.01307 132 1053 0.01313 132.1 1054 0.01316 132.3 1056 0.01321 132.5 1058 0.01327 132.6 1059 0.01331 132.8 1061 0.01333 132.9 1062 0.01338 133.1 1064 0.01343 133.3 1066 0.01345 133.4 1067 0.01353 133.6 1068 0.01357 133.7 1070 0.0136 133.9 1072 0.01365 134.1 1072 0.0137 134.2 1073 0.01375 134.4 1075 0.0138 134.5 1076 0.01383 134.7 1078 0.01385 134.9 1079 0.01389 135 1081 0.0139 135.2 1082 0.01391 135.4 1083 0.01395 135.5 1084 0.01396 135.7 1085 0.014 135.8 1086 0.01404 136 1088 0.01406 136.2 1089 0.01411 136.3 1090 0.01416 136.5 1092 0.0142 136.6 1094 0.01425 136.8 1094 0.0143 137 1096 0.01433 137.1 1097 0.01437 137.3 1098 0.01441 137.4 1100 0.01443 137.6 1101 0.01446 137.8 1103 0.01448 137.9 1103 0.01452 138.1 1104 0.01457 138.3 1106 0.01459 138.4 1107 0.01463 138.6 1109 0.01467 138.7 1110 0.01469 138.9 1111 0.01474 139.1 1112 0.01478 139.2 1114 0.0148 139.4 1115 0.01482 139.5 1117 0.01484 139.7 1117 0.01487 139.9 1119 0.01489 140 1120 0.01494 140.2 1122 0.01499 140.3 1123 0.01503 140.5 1124 0.01506 140.7 1125 0.01509 140.8 1126 0.01511 141 1128 0.01514 141.2 1129 0.01516 141.3 1130 0.01519 141.5 1132 0.01521 141.6 1133 0.01524 141.8 1134 0.01526 142 1136 0.0153 142.1 1137 0.01534 142.3 1138 0.01537 142.4 1140 0.01539 142.6 1140 0.01541 142.8 1142 0.01546 142.9 1144 0.01546 143.1 1145 0.01547 143.2 1147 0.0155 143.4 1148 0.01553 143.6 1149 0.01556 143.7 1150 0.01557 143.9 1151 0.01558 144.1 1153 0.01561 144.2 1154 0.01563 144.4 1156 0.01566 144.5 1156 0.0157 144.7 1158 0.01572 144.9 1159 0.01576 145 1161 0.01578 145.2 1162 0.01581 145.3 1162 0.01583 145.5 1164 0.01586 145.7 1165 0.01588 145.8 1167 0.01588 146 1169 0.01592 146.1 1169 0.01596 146.3 1172 0.01598 146.5 1172 0.01601 146.6 1173 0.01601 146.8 1175 0.01602 147 1176 0.01603 147.1 1178 0.01606 147.3 1179 0.01607 147.4 1179 0.0161 147.6 1181 0.01614 147.8 1183 0.01619 147.9 1184 0.01623 148.1 1184 0.01627 148.2 1187 0.01628 148.4 1187 0.01632 148.6 1189 0.01633 148.7 1190 0.01638 148.9 1192 0.0164 149 1194 0.01644 149.2 1194 0.01648 149.4 1196 0.0165 149.5 1197 0.01653 149.7 1199 0.01656 149.9 1200 0.01659 150 1201 0.0166 150.2 1201 0.01661 150.3 1201 0.01662 150.5 1202 0.01662 150.7 1203 0.01664 150.8 1203 0.01666 151 1203 0.01666 151.1 1203 0.01665 151.3 1203 0.01667 151.5 1203 0.01667 151.6 1203 0.01666 151.8 1203 0.01665 151.9 1203 0.01662 152.1 1203 0.01661 152.3 1202 0.01661 152.4 1201 0.0166 152.6 1201 0.01656 152.8 1201 0.01656 152.9 1201 0.01655 153.1 1201 0.01653 153.2 1201 0.01651 153.4 1201 0.01651 153.6 1200 0.01653 153.7 1200 0.01653 153.9 1200 0.01653 154 1200 0.01655 154.2 1200 0.01655 154.4 1200 0.01655 154.5 1200 0.01653 154.7 1199 0.01651 154.8 1199 0.01649 155 1199 0.01648 155.2 1199 0.01651 155.3 1199 0.01653 155.5 1199 0.01656 155.7 1198 0.01654 155.8 1199 0.0165 156 1199 0.0165 156.1 1199 0.0165 156.3 1199 0.0165 156.5 1199 0.0165 156.6 1199 0.0165 156.8 1199 0.01649 156.9 1199 0.0165 157.1 1199 0.01648 157.3 1199 0.01648 157.4 1200 0.0165 157.6 1199 0.01651 157.8 1199 0.01651 157.9 1200 0.01651 158.1 1199 0.0165 158.2 1200 0.0165 158.4 1199 0.01648 158.6 1200 0.01645 158.7 1199 0.01643 158.9 1200 0.01643 159 1200 0.01643 159.2 1200 0.01643 159.4 1199 0.01643 159.5 1200 0.01644 159.7 1200 0.01645 159.8 1200 0.01648 160 1200 0.01648 160.2 1200 0.01648 160.3 1200 0.01648 160.5 1200 0.01648 160.7 1200 0.01644 160.8 1200 0.01643 161 1200 0.01641 161.1 1200 0.01641 161.3 1200 0.01641 161.5 1200 0.01643 161.6 1200 0.01643 161.8 1200 0.01643 161.9 1200 0.01643 162.1 1200 0.01644 162.3 1200 0.01644 162.4 1200 0.01644 162.6 1200 0.01644 162.7 1200 0.01644 162.9 1200 0.01644 163.1 1200 0.01643 163.2 1200 0.01641 163.4 1200 0.0164 163.6 1200 0.0164 163.7 1199 0.0164 163.9 1200 0.01638 164 1200 0.01638 164.2 1200 0.01635 164.4 1200 0.01633 164.5 1200 0.01634 164.7 1200 0.01633 164.8 1200 0.01633 165 1200 0.01633 165.2 1200 0.01632 165.3 1200 0.01633 165.5 1200 0.01633 165.6 1200 0.01633 165.8 1200 0.01634 166 1200 0.01633 166.1 1200 0.01633 166.3 1200 0.01634 166.5 1200 0.01633 166.6 1200 0.01634 166.8 1200 0.01634 166.9 1200 0.01635 167.1 1200 0.01635 167.3 1199 0.01635 167.4 1200 0.01635 167.6 1200 0.01633 167.7 1200 0.01633 167.9 1200 0.01632 168.1 1200 0.01632 168.2 1200 0.01633 168.4 1200 0.01633 168.5 1200 0.01633 168.7 1200 0.01632 168.9 1200 0.0163 169 1200 0.0163 169.2 1200 0.01632 169.4 1200 0.01633 169.5 1200 0.01635 169.7 1200 0.01638 169.8 1200 0.01638 170 1200 0.01638 170.2 1200 0.01636 170.3 1200 0.01638 170.5 1200 0.01639 170.6 1200 0.0164 170.8 1200 0.0164 171 1200 0.0164 171.1 1200 0.01639 171.3 1200 0.01639 171.4 1200 0.01639 171.6 1200 0.01639 171.8 1200 0.01639 171.9 1200 0.01639 172.1 1200 0.01639 172.3 1200 0.01639 172.4 1200 0.01639 172.6 1200 0.01639 172.7 1200 0.0164 172.9 1200 0.01641 173.1 1200 0.01643 173.2 1200 0.01644 173.4 1200 0.01646 173.5 1200 0.01648 173.7 1200 0.01651 173.9 1200 0.01651 174 1200 0.0165 174.2 1200 0.0165 174.3 1200 0.01648 174.5 1200 0.01646 174.7 1200 0.01646 174.8 1200 0.01644 175 1200 0.01646 175.2 1200 0.01648 175.3 1200 0.01648 175.5 1200 0.01648 175.6 1200 0.0165 175.8 1200 0.01651 176 1200 0.01653 176.1 1200 0.01653 176.3 1199 0.01653 176.4 1200 0.01653 176.6 1200 0.01654 176.8 1200 0.01654 176.9 1200 0.01655 177.1 1200 0.01654 177.2 1200 0.01654 177.4 1200 0.01655 177.6 1200 0.01655 177.7 1200 0.01654 177.9 1200 0.01656 178.1 1200 0.01656 178.2 1200 0.01655 178.4 1200 0.01658 178.5 1200 0.01658 178.7 1200 0.01656 178.9 1200 0.01658 179 1200 0.01658 179.2 1200 0.01656 179.3 1200 0.01658 179.5 1200 0.01658 179.7 1200 0.01659 179.8 1200 0.01659 180 1200 0.01658 180.1 1200 0.01658 180.3 1200 0.01658 180.5 1200 0.01659 180.6 1200 0.01659 180.8 1200 0.01658 181 1200 0.01659 181.1 1199 0.0166 181.3 1200 0.0166 181.4 1200 0.01658 181.6 1200 0.01658 181.8 1200 0.01658 181.9 1200 0.01658 182.1 1200 0.01658 182.2 1200 0.01656 182.4 1200 0.01655 182.6 1200 0.01653 182.7 1200 0.01653 182.9 1200 0.01653 183 1200 0.01653 183.2 1200 0.01653 183.4 1200 0.01653 183.5 1200 0.01653 183.7 1200 0.01654 183.9 1200 0.01654 184 1200 0.01653 184.2 1200 0.01651 184.3 1200 0.01651 184.5 1200 0.0165 184.7 1200 0.01649 184.8 1200 0.01648 185 1200 0.01648 185.1 1200 0.01648 185.3 1200 0.01648 185.5 1200 0.01645 185.6 1200 0.01643 185.8 1200 0.01643 185.9 1199 0.01641 186.1 1200 0.01643 186.3 1200 0.01644 186.4 1200 0.01646 186.6 1200 0.01648 186.8 1200 0.01648 186.9 1200 0.01648 187.1 1200 0.01649 187.2 1200 0.01649 187.4 1200 0.01648 187.6 1200 0.01648 187.7 1200 0.01644 187.9 1200 0.01644 188 1200 0.01645 188.2 1200 0.01644 188.4 1200 0.01644 188.5 1200 0.01643 188.7 1200 0.01641 188.8 1200 0.01641 189 1200 0.0164 189.2 1200 0.0164 189.3 1200 0.0164 189.5 1200 0.01641 189.7 1200 0.01641 189.8 1200 0.01638 190 1200 0.01638 190.1 1200 0.01639 190.3 1200 0.01638 190.5 1200 0.01639 190.6 1200 0.01639 190.8 1200 0.01639 190.9 1200 0.0164 191.1 1200 0.01639 191.3 1200 0.01639 191.4 1200 0.01639 191.6 1200 0.01639 191.7 1200 0.01638 191.9 1200 0.01638 192.1 1200 0.01635 192.2 1200 0.01636 192.4 1200 0.01638 192.6 1200 0.01638 192.7 1200 0.01638 192.9 1200 0.01638 193 1200 0.01638 193.2 1200 0.01635 193.4 1200 0.01636 193.5 1200 0.01635 193.7 1200 0.01635 193.8 1200 0.01638 194 1200 0.01635 194.2 1200 0.01636 194.3 1200 0.01638 194.5 1199 0.0164 194.6 1200 0.01641 194.8 1199 0.01643 195 1200 0.01643 195.1 1200 0.01643 195.3 1200 0.01641 195.5 1200 0.0164 195.6 1200 0.0164 195.8 1200 0.01639 195.9 1200 0.01639 196.1 1200 0.01639 196.3 1200 0.0164 196.4 1200 0.01641 196.6 1200 0.01643 196.7 1200 0.01643 196.9 1200 0.01641 197.1 1200 0.01643 197.2 1200 0.01643 197.4 1200 0.01643 197.6 1200 0.01643 197.7 1200 0.01644 197.9 1200 0.01644 198 1200 0.01644 198.2 1200 0.01644 198.4 1200 0.01644 198.5 1200 0.01644 198.7 1200 0.01643 198.8 1200 0.01641 199 1200 0.0164 199.2 1199 0.0164 199.3 1200 0.01639 199.5 1200 0.01639 199.6 1200 0.0164 199.8 1200 0.01641 200 1200 0.01641 200.1 1200 0.0164 200.3 1200 0.01639 200.5 1200 0.0164 200.6 1200 0.01641 200.8 1200 0.01641 200.9 1200 0.01641 201.1 1200 0.0164 201.3 1200 0.01638 201.4 1200 0.01638 201.6 1200 0.01635 201.7 1200 0.01638 201.9 1200 0.01638 202.1 1200 0.01635 202.2 1200 0.01635 202.4 1200 0.01635 202.5 1200 0.01635 202.7 1200 0.01635 202.9 1200 0.01638 203 1200 0.01638 203.2 1200 0.01638 203.4 1200 0.01638 203.5 1200 0.01636 203.7 1200 0.01634 203.8 1200 0.01633 204 1200 0.01632 204.2 1200 0.0163 204.3 1200 0.0163 204.5 1200 0.01632 204.6 1200 0.0163 204.8 1200 0.0163 205 1200 0.0163 205.1 1200 0.0163 205.3 1200 0.01632 205.4 1200 0.01633 205.6 1200 0.01632 205.8 1200 0.01633 205.9 1200 0.01632 206.1 1200 0.01632 206.3 1200 0.01633 206.4 1200 0.01633 206.6 1200 0.01633 206.7 1200 0.0163 206.9 1200 0.0163 207.1 1200 0.0163 207.2 1200 0.0163 207.4 1200 0.01629 207.5 1200 0.01629 207.7 1200 0.01629 207.9 1200 0.01629 208 1200 0.01629 208.2 1200 0.01629 208.3 1199 0.01628 208.5 1200 0.01628 208.7 1200 0.01628 208.8 1200 0.0163 209 1200 0.01632 209.2 1200 0.0163 209.3 1200 0.01628 209.5 1200 0.01627 209.6 1200 0.01623 209.8 1200 0.01623 210 1200 0.0162 210.1 1200 0.0162 210.3 1200 0.01623 210.4 1200 0.01628 210.6 1200 0.01629 210.8 1200 0.0163 210.9 1200 0.01632 211.1 1200 0.0163 211.2 1200 0.0163 211.4 1200 0.0163 211.6 1200 0.0163 211.7 1200 0.01628 211.9 1200 0.01627 212.1 1200 0.01623 212.2 1200 0.01625 212.4 1200 0.01628 212.5 1200 0.01628 212.7 1200 0.01629 212.9 1200 0.0163 213 1200 0.0163 213.2 1200 0.01633 213.3 1200 0.01633 213.5 1200 0.0163 213.7 1200 0.01632 213.8 1200 0.01633 214 1200 0.01632 214.1 1200 0.01632 214.3 1200 0.01633 214.5 1200 0.0163 214.6 1200 0.01633 214.8 1200 0.01634 215 1200 0.01634 215.1 1200 0.01633 215.3 1200 0.01633 215.4 1200 0.01634 215.6 1200 0.01635 215.8 1200 0.01635 215.9 1200 0.01634 216.1 1200 0.01634 216.2 1200 0.01634 216.4 1200 0.01633 216.6 1200 0.01635 216.7 1200 0.01638 216.9 1200 0.01638 217 1200 0.01638 217.2 1199 0.01638 217.4 1200 0.01638 217.5 1200 0.01636 217.7 1200 0.01638 217.9 1200 0.01638 218 1200 0.01638 218.2 1200 0.01641 218.3 1200 0.01641 218.5 1200 0.01643 218.7 1200 0.01643 218.8 1200 0.01644 219 1200 0.01644 219.1 1200 0.01644 219.3 1200 0.01644 219.5 1200 0.01645 219.6 1200 0.01648 219.8 1200 0.01648 219.9 1200 0.01649 220.1 1200 0.0165 220.3 1200 0.0165 220.4 1200 0.0165 220.6 1200 0.0165 220.8 1200 0.01651 220.9 1200 0.01653 221.1 1200 0.01653 221.2 1200 0.01653 221.4 1200 0.01653 221.6 1200 0.01654 221.7 1200 0.01653 221.9 1200 0.01653 222 1200 0.01653 222.2 1200 0.01653 222.4 1200 0.01654 222.5 1200 0.01655 222.7 1200 0.01655 222.8 1200 0.01656 223 1200 0.01655 223.2 1200 0.01655 223.3 1200 0.01658 223.5 1200 0.01656 223.7 1200 0.01656 223.8 1200 0.01658 224 1200 0.01656 224.1 1200 0.01658 224.3 1200 0.01659 224.5 1200 0.01658 224.6 1200 0.01659 224.8 1200 0.0166 224.9 1200 0.01659 225.1 1200 0.01658 225.3 1200 0.01658 225.4 1200 0.01658 225.6 1200 0.01658 225.7 1200 0.01659 225.9 1200 0.01659 226.1 1200 0.01659 226.2 1200 0.0166 226.4 1200 0.01658 226.6 1200 0.01658 226.7 1200 0.01656 226.9 1200 0.01656 227 1200 0.01655 227.2 1200 0.01656 227.4 1200 0.01658 227.5 1200 0.01658 227.7 1200 0.01658 227.8 1200 0.01656 228 1200 0.01656 228.2 1200 0.01656 228.3 1200 0.01655 228.5 1200 0.01654 228.6 1200 0.01655 228.8 1200 0.01655 229 1199 0.01654 229.1 1200 0.01655 229.3 1200 0.01653 229.5 1200 0.01651 229.6 1200 0.01651 229.8 1200 0.01653 229.9 1200 0.01651 230.1 1200 0.0165 230.3 1200 0.01649 230.4 1200 0.01649 230.6 1200 0.0165 230.7 1199 0.01648 230.9 1200 0.01648 231.1 1200 0.01646 231.2 1200 0.01648 231.4 1200 0.01646 231.5 1200 0.01646 231.7 1200 0.01645 231.9 1200 0.01645 232 1200 0.01645 232.2 1200 0.01644 232.4 1200 0.01644 232.5 1200 0.01645 232.7 1200 0.01643 232.8 1200 0.01643 233 1200 0.01641 233.2 1200 0.01643 233.3 1200 0.01644 233.5 1200 0.01645 233.6 1200 0.01643 233.8 1200 0.01641 234 1200 0.01641 234.1 1200 0.01641 234.3 1200 0.01643 234.4 1200 0.01641 234.6 1200 0.0164 234.8 1200 0.0164 234.9 1200 0.0164 235.1 1200 0.01639 235.3 1200 0.01639 235.4 1200 0.01639 235.6 1200 0.01639 235.7 1199 0.01639 235.9 1200 0.0164 236.1 1200 0.01639 236.2 1200 0.01639 236.4 1200 0.01639 236.5 1200 0.0164 236.7 1200 0.01641 236.9 1200 0.01641 237 1200 0.0164 237.2 1200 0.0164 237.4 1200 0.0164 237.5 1200 0.01639 237.7 1200 0.01639 237.8 1200 0.0164 238 1200 0.01639 238.2 1200 0.01641 238.3 1200 0.01641 238.5 1200 0.0164 238.6 1200 0.01639 238.8 1200 0.0164 239 1200 0.01639 239.1 1200 0.01639 239.3 1200 0.0164 239.4 1200 0.01639 239.6 1200 0.01639 239.8 1200 0.01639 239.9 1200 0.01639 240.1 1200 0.01638 240.3 1200 0.01639 240.4 1200 0.01639 240.6 1200 0.01639 240.7 1200 0.0164 240.9 1200 0.01641 241.1 1200 0.01641 241.2 1200 0.0164 241.4 1200 0.01639 241.5 1200 0.01639 241.7 1200 0.01639 241.9 1200 0.01639 242 1200 0.01639 242.2 1200 0.01639 242.3 1200 0.0164 242.5 1200 0.01641 242.7 1200 0.01641 242.8 1200 0.0164 243 1200 0.01643 243.2 1200 0.01641 243.3 1200 0.01641 243.5 1200 0.01643 243.6 1199 0.01641 243.8 1200 0.01641 244 1200 0.0164 244.1 1200 0.01641 244.3 1200 0.01641 244.4 1200 0.01641 244.6 1200 0.01641 244.8 1200 0.01643 244.9 1200 0.01643 245.1 1200 0.01643 245.2 1200 0.01641 245.4 1200 0.01641 245.6 1200 0.0164 245.7 1200 0.0164 245.9 1200 0.0164 246.1 1200 0.01639 246.2 1200 0.01639 246.4 1200 0.01643 246.5 1200 0.01641 246.7 1200 0.0164 246.9 1200 0.0164 247 1200 0.01639 247.2 1200 0.01639 247.3 1200 0.0164 247.5 1200 0.01638 247.7 1200 0.01638 247.8 1200 0.01638 248 1200 0.01639 248.1 1200 0.0164 248.3 1200 0.01638 248.5 1200 0.01635 248.6 1200 0.01638 248.8 1200 0.01638 249 1200 0.01639 249.1 1200 0.01643 249.3 1200 0.01644 249.4 1200 0.01641 249.6 1200 0.01638 249.8 1200 0.01633 249.9 1200 0.01633 250.1 1200 0.01636 250.2 1200 0.01633 250.4 1200 0.01633 250.6 1200 0.01633 250.7 1200 0.01633 250.9 1200 0.01632 251 1200 0.01633 251.2 1200 0.01633 251.4 1200 0.01633 251.5 1200 0.01634 251.7 1200 0.01633 251.9 1200 0.0163 252 1200 0.01628 252.2 1200 0.01628 252.3 1200 0.01629 252.5 1200 0.0163 252.7 1200 0.01629 252.8 1200 0.01628 253 1200 0.0163 253.1 1200 0.0163 253.3 1200 0.0163 253.5 1200 0.0163 253.6 1200 0.01628 253.8 1200 0.01627 253.9 1200 0.01627 254.1 1200 0.01625 254.3 1200 0.01628 254.4 1200 0.01628 254.6 1200 0.01628 254.8 1200 0.01628 254.9 1200 0.01629 255.1 1200 0.01628 255.2 1200 0.01628 255.4 1200 0.01628 255.6 1200 0.01628 255.7 1200 0.01628 255.9 1200 0.01628 256 1200 0.01628 256.2 1200 0.01627 256.4 1200 0.01628 256.5 1200 0.01628 256.7 1200 0.01625 256.8 1200 0.01628 257 1200 0.01628 257.2 1200 0.01628 257.3 1200 0.01629 257.5 1200 0.01628 257.7 1200 0.01628 257.8 1200 0.01628 258 1200 0.01628 258.1 1200 0.01628 258.3 1200 0.01628 258.5 1200 0.01628 258.6 1200 0.01627 258.8 1200 0.01628 258.9 1200 0.01628 259.1 1200 0.01628 259.3 1200 0.0163 259.4 1200 0.01633 259.6 1200 0.01633 259.7 1200 0.01632 259.9 1200 0.01633 260.1 1200 0.01633 260.2 1200 0.01635 260.4 1200 0.01635 260.6 1200 0.01634 260.7 1200 0.01635 260.9 1200 0.01635 261 1200 0.01634 261.2 1200 0.01634 261.4 1200 0.01634 261.5 1199 0.01633 261.7 1200 0.01633 261.8 1200 0.01633 262 1200 0.01634 262.2 1200 0.0163 262.3 1200 0.0163 262.5 1200 0.0163 262.6 1200 0.01633 262.8 1200 0.01635 263 1200 0.01638 263.1 1200 0.0164 263.3 1200 0.01641 263.5 1200 0.0164 263.6 1200 0.0164 263.8 1200 0.0164 263.9 1200 0.01641 264.1 1200 0.01641 264.3 1200 0.0164 264.4 1200 0.01639 264.6 1200 0.0164 264.7 1200 0.0164 264.9 1200 0.01639 265.1 1200 0.0164 265.2 1200 0.01643 265.4 1200 0.01643 265.5 1200 0.01644 265.7 1200 0.01646 265.9 1200 0.01645 266 1200 0.01645 266.2 1200 0.01648 266.4 1200 0.01648 266.5 1200 0.01648 266.7 1200 0.01649 266.8 1200 0.0165 267 1200 0.01648 267.2 1200 0.01648 267.3 1200 0.01648 267.5 1200 0.01648 267.6 1200 0.01649 267.8 1200 0.01649 268 1200 0.01649 268.1 1200 0.0165 268.3 1200 0.01651 268.4 1200 0.01651 268.6 1199 0.01651 268.8 1200 0.01653 268.9 1200 0.01653 269.1 1200 0.01654 269.3 1200 0.01651 269.4 1200 0.01651 269.6 1200 0.01653 269.7 1200 0.01653 269.9 1200 0.01651 270.1 1200 0.01653 270.2 1200 0.01651 270.4 1200 0.01653 270.5 1200 0.01653 270.7 1200 0.01653 270.9 1200 0.01653 271 1200 0.01654 271.2 1200 0.01654 271.3 1200 0.01654 271.5 1200 0.01654 271.7 1200 0.01654 271.8 1200 0.01654 272 1200 0.01655 272.2 1200 0.01653 272.3 1200 0.01653 272.5 1200 0.01651 272.6 1200 0.0165 272.8 1200 0.01651 273 1200 0.0165 273.1 1200 0.0165 273.3 1200 0.0165 273.4 1200 0.0165 273.6 1200 0.0165 273.8 1200 0.01653 273.9 1200 0.01651 274.1 1200 0.0165 274.3 1200 0.0165 274.4 1200 0.0165 274.6 1200 0.01651 274.7 1200 0.01653 274.9 1200 0.01651 275.1 1200 0.01648 275.2 1200 0.01645 275.4 1200 0.01643 275.5 1200 0.01643 275.7 1200 0.01641 275.9 1200 0.01643 276 1200 0.01644 276.2 1200 0.01645 276.3 1200 0.01645 276.5 1200 0.01644 276.7 1200 0.01643 276.8 1200 0.01643 277 1200 0.01644 277.2 1199 0.01643 277.3 1200 0.01644 277.5 1200 0.01644 277.6 1200 0.01644 277.8 1200 0.01644 278 1200 0.01644 278.1 1200 0.01644 278.3 1200 0.01644 278.4 1200 0.01644 278.6 1200 0.01643 278.8 1200 0.01641 278.9 1200 0.01641 279.1 1200 0.0164 279.2 1200 0.0164 279.4 1200 0.0164 279.6 1200 0.01639 279.7 1200 0.01639 279.9 1200 0.01639 280.1 1200 0.01639 280.2 1200 0.01639 280.4 1200 0.0164 280.5 1200 0.01641 280.7 1200 0.0164 280.9 1200 0.01641 281 1200 0.0164 281.2 1200 0.01639 281.3 1200 0.0164 281.5 1200 0.01638 281.7 1200 0.01638 281.8 1200 0.01636 282 1200 0.01638 282.1 1200 0.01636 282.3 1200 0.01636 282.5 1200 0.01635 282.6 1200 0.01635 282.8 1200 0.01634 283 1200 0.01633 283.1 1200 0.01634 283.3 1200 0.01635 283.4 1200 0.01635 283.6 1200 0.01634 283.8 1200 0.01635 283.9 1200 0.01635 284.1 1200 0.01634 284.2 1200 0.01635 284.4 1200 0.01635 284.6 1200 0.01638 284.7 1200 0.01638 284.9 1200 0.01638 285 1200 0.01638 285.2 1200 0.01638 285.4 1200 0.01635 285.5 1200 0.01636 285.7 1200 0.01638 285.9 1200 0.01635 286 1200 0.01635 286.2 1200 0.01635 286.3 1200 0.01634 286.5 1200 0.01634 286.7 1200 0.01635 286.8 1200 0.01634 287 1200 0.01634 287.1 1200 0.01634 287.3 1200 0.01634 287.5 1200 0.01633 287.6 1200 0.01635 287.8 1200 0.01635 287.9 1200 0.01638 288.1 1200 0.01638 288.3 1200 0.01638 288.4 1200 0.01635 288.6 1200 0.01635 288.8 1200 0.01635 288.9 1200 0.01635 289.1 1200 0.01635 289.2 1200 0.01634 289.4 1200 0.01633 289.6 1200 0.01633 289.7 1200 0.01633 289.9 1200 0.01633 290 1200 0.01634 290.2 1200 0.01633 290.4 1200 0.0163 290.5 1200 0.0163 290.7 1200 0.0163 290.8 1200 0.0163 291 1200 0.0163 291.2 1200 0.01629 291.3 1200 0.0163 291.5 1200 0.01633 291.7 1200 0.01636 291.8 1200 0.01638 292 1200 0.01639 292.1 1200 0.01638 292.3 1200 0.01636 292.5 1200 0.01636 292.6 1200 0.01634 292.8 1199 0.01633 292.9 1200 0.01632 293.1 1200 0.0163 293.3 1200 0.0163 293.4 1200 0.01632 293.6 1200 0.01633 293.7 1200 0.01635 293.9 1200 0.01635 294.1 1200 0.01635 294.2 1200 0.01634 294.4 1200 0.01636 294.6 1200 0.01638 294.7 1200 0.01638 294.9 1200 0.01636 295 1200 0.01635 295.2 1200 0.01635 295.4 1200 0.01635 295.5 1200 0.01633 295.7 1200 0.01633 295.8 1200 0.01633 296 1200 0.01633 296.2 1200 0.01633 296.3 1200 0.01633 296.5 1200 0.01633 296.6 1200 0.01634 296.8 1200 0.01633 297 1200 0.01633 297.1 1200 0.01632 297.3 1200 0.0163 297.5 1200 0.0163 297.6 1200 0.0163 297.8 1200 0.0163 297.9 1200 0.0163 298.1 1200 0.01632 298.3 1200 0.0163 298.4 1200 0.01632 298.6 1200 0.01633 298.7 1200 0.01633 298.9 1200 0.01633 299.1 1200 0.01632 299.2 1200 0.01628 299.4 1200 0.01628 299.5 1200 0.01628 299.7 1200 0.01628 299.9 1200 0.01625 300 1200 0.01623 300.2 1200 0.01622 300.4 1200 0.01622 300.5 1200 0.01623 300.7 1200 0.01623 300.8 1200 0.01623 301 1200 0.01623 301.2 1200 0.01625 301.3 1200 0.01625 301.5 1200 0.01628 301.6 1200 0.01625 301.8 1200 0.01627 302 1200 0.01625 302.1 1200 0.01624 302.3 1200 0.01625 302.4 1200 0.01624 302.6 1200 0.01623 302.8 1200 0.01624 302.9 1200 0.01623 303.1 1200 0.01623 303.3 1200 0.01624 303.4 1200 0.01623 303.6 1200 0.01623 303.7 1200 0.01624 303.9 1200 0.01623 304.1 1200 0.01623 304.2 1200 0.01624 304.4 1200 0.01625 304.5 1200 0.01627 304.7 1200 0.01628 304.9 1200 0.01627 305 1200 0.01625 305.2 1200 0.01625 305.3 1200 0.01623 305.5 1200 0.01622 305.7 1200 0.01622 305.8 1200 0.01622 306 1200 0.01623 306.2 1200 0.01623 306.3 1200 0.01623 306.5 1200 0.01623 306.6 1200 0.01623 306.8 1200 0.01623 307 1200 0.01623 307.1 1200 0.01623 307.3 1200 0.01619 307.4 1200 0.01618 307.6 1200 0.01617 307.8 1200 0.01617 307.9 1200 0.01618 308.1 1200 0.01618 308.2 1200 0.0162 308.4 1199 0.01623 308.6 1200 0.01627 308.7 1200 0.01628 308.9 1200 0.01629 309.1 1200 0.01628 309.2 1200 0.01625 309.4 1200 0.01624 309.5 1200 0.01623 309.7 1200 0.01623 309.9 1200 0.01625 310 1200 0.01628 310.2 1200 0.01629 310.3 1200 0.01632 310.5 1200 0.01632 310.7 1200 0.01633 310.8 1200 0.01633 311 1200 0.01633 311.1 1200 0.01633 311.3 1200 0.01635 311.5 1200 0.01635 311.6 1200 0.01635 311.8 1200 0.01635 312 1200 0.01635 312.1 1200 0.01635 312.3 1200 0.01638 312.4 1200 0.01635 312.6 1200 0.01636 312.8 1200 0.01638 312.9 1200 0.01638 313.1 1200 0.01638 313.2 1200 0.01639 313.4 1200 0.0164 313.6 1200 0.01641 313.7 1200 0.01643 313.9 1200 0.01643 314.1 1200 0.01643 314.2 1200 0.01641 314.4 1200 0.01643 314.5 1200 0.01643 314.7 1200 0.01643 314.9 1200 0.01643 315 1200 0.01644 315.2 1200 0.01646 315.3 1200 0.01645 315.5 1200 0.01646 315.7 1200 0.01648 315.8 1200 0.01648 316 1200 0.01649 316.1 1200 0.01649 316.3 1200 0.01648 316.5 1200 0.01648 316.6 1200 0.01645 316.8 1200 0.01648 317 1200 0.01648 317.1 1200 0.01648 317.3 1200 0.01649 317.4 1200 0.0165 317.6 1200 0.01651 317.8 1200 0.01653 317.9 1200 0.01654 318.1 1200 0.01655 318.2 1200 0.01653 318.4 1200 0.01654 318.6 1200 0.01655 318.7 1200 0.01655 318.9 1200 0.01655 319 1200 0.01655 319.2 1200 0.01655 319.4 1200 0.01655 319.5 1200 0.01655 319.7 1200 0.01651 319.9 1200 0.0165 320 1200 0.01648 320.2 1200 0.01646 320.3 1200 0.01646 320.5 1200 0.01648 320.7 1200 0.01651 320.8 1200 0.01653 321 1200 0.01653 321.1 1200 0.01653 321.3 1200 0.01653 321.5 1200 0.01654 321.6 1200 0.01653 321.8 1200 0.01653 321.9 1200 0.01654 322.1 1200 0.01653 322.3 1200 0.01653 322.4 1200 0.01653 322.6 1200 0.01653 322.8 1200 0.01654 322.9 1200 0.01655 323.1 1200 0.01655 323.2 1200 0.01655 323.4 1200 0.01658 323.6 1200 0.01658 323.7 1200 0.01655 323.9 1200 0.01654 324 1200 0.01653 324.2 1200 0.01653 324.4 1200 0.01651 324.5 1200 0.0165 324.7 1200 0.01648 324.8 1200 0.01648 325 1200 0.01648 325.2 1200 0.01648 325.3 1200 0.01648 325.5 1200 0.01645 325.7 1200 0.01645 325.8 1200 0.01645 326 1200 0.01644 326.1 1200 0.01644 326.3 1200 0.01645 326.5 1200 0.01645 326.6 1200 0.01648 326.8 1200 0.01646 326.9 1200 0.01645 327.1 1200 0.01645 327.3 1200 0.01645 327.4 1200 0.01644 327.6 1200 0.01643 327.7 1200 0.01643 327.9 1200 0.01641 328.1 1200 0.0164 328.2 1200 0.0164 328.4 1200 0.01639 328.6 1200 0.0164 328.7 1200 0.01638 328.9 1200 0.01638 329 1200 0.01635 329.2 1200 0.01635 329.4 1200 0.0163 329.5 1200 0.01628 329.7 1200 0.01628 329.8 1200 0.01628 330 1200 0.0163 330.2 1200 0.01633 330.3 1200 0.01635 330.5 1200 0.01635 330.6 1200 0.01639 330.8 1200 0.0164 331 1200 0.01641 331.1 1200 0.01643 331.3 1200 0.01643 331.5 1200 0.01641 331.6 1200 0.0164 331.8 1200 0.01638 331.9 1200 0.01638 332.1 1200 0.01641 332.3 1200 0.0164 332.4 1200 0.01638 332.6 1200 0.01638 332.7 1200 0.01636 332.9 1200 0.01635 333.1 1199 0.01635 333.2 1200 0.01634 333.4 1200 0.01634 333.5 1200 0.01635 333.7 1200 0.01634 333.9 1200 0.01634 334 1200 0.01634 334.2 1200 0.01634 334.4 1200 0.01634 334.5 1200 0.01634 334.7 1200 0.01634 334.8 1200 0.01635 335 1200 0.01635 335.2 1200 0.01635 335.3 1200 0.01635 335.5 1200 0.01634 335.6 1200 0.01635 335.8 1200 0.01633 336 1200 0.01634 336.1 1200 0.01634 336.3 1200 0.01634 336.4 1200 0.01635 336.6 1200 0.01633 336.8 1200 0.01633 336.9 1200 0.01632 337.1 1200 0.0163 337.3 1200 0.01632 337.4 1200 0.0163 337.6 1200 0.01629 337.7 1200 0.01629 337.9 1200 0.0163 338.1 1200 0.01629 338.2 1200 0.0163 338.4 1200 0.01632 338.5 1200 0.01632 338.7 1200 0.01633 338.9 1200 0.01634 339 1200 0.01635 339.2 1200 0.01638 339.3 1200 0.01638 339.5 1200 0.01638 339.7 1200 0.01639 339.8 1200 0.01638 340 1200 0.01636 340.2 1200 0.01638 340.3 1200 0.01638 340.5 1200 0.01638 340.6 1200 0.01639 340.8 1200 0.01639 341 1200 0.01638 341.1 1200 0.01639 341.3 1200 0.01639 341.4 1200 0.01639 341.6 1200 0.01638 341.8 1200 0.01639 341.9 1200 0.01639 342.1 1200 0.01639 342.2 1200 0.01639 342.4 1200 0.01638 342.6 1200 0.01639 342.7 1200 0.01639 342.9 1200 0.0164 343.1 1200 0.01639 343.2 1200 0.01638 343.4 1200 0.01635 343.5 1200 0.01634 343.7 1200 0.01633 343.9 1200 0.0163 344 1200 0.0163 344.2 1200 0.0163 344.3 1200 0.0163 344.5 1200 0.0163 344.7 1200 0.01632 344.8 1200 0.01633 345 1200 0.01633 345.1 1200 0.01633 345.3 1200 0.01633 345.5 1200 0.01633 345.6 1200 0.01632 345.8 1200 0.0163 346 1200 0.0163 346.1 1200 0.01633 346.3 1200 0.01633 346.4 1200 0.01632 346.6 1200 0.01632 346.8 1200 0.01632 346.9 1200 0.01633 347.1 1200 0.01633 347.2 1200 0.01633 347.4 1200 0.01633 347.6 1200 0.01633 347.7 1200 0.01633 347.9 1200 0.01634 348 1200 0.01633 348.2 1200 0.01634 348.4 1200 0.01633 348.5 1200 0.01632 348.7 1200 0.0163 348.9 1200 0.0163 349 1200 0.01633 349.2 1200 0.0163 349.3 1200 0.0163 349.5 1200 0.0163 349.7 1200 0.0163 349.8 1200 0.01628 350 1200 0.01628 350.1 1200 0.01625 350.3 1200 0.01623 350.5 1200 0.01622 350.6 1200 0.01622 350.8 1200 0.01623 350.9 1200 0.01623 351.1 1200 0.01623 351.3 1200 0.01623 351.4 1200 0.01625 351.6 1200 0.01624 351.8 1200 0.01623 351.9 1200 0.01622 352.1 1200 0.01622 352.2 1200 0.01622 352.4 1200 0.01622 352.6 1200 0.01622 352.7 1200 0.01623 352.9 1200 0.01623 353 1200 0.01623 353.2 1200 0.01623 353.4 1200 0.01624 353.5 1200 0.01623 353.7 1200 0.01623 353.9 1200 0.01623 354 1200 0.01623 354.2 1200 0.01622 354.3 1200 0.01619 354.5 1200 0.01619 354.7 1200 0.0162 354.8 1200 0.01622 355 1200 0.01623 355.1 1200 0.01623 355.3 1200 0.01623 355.5 1200 0.0162 355.6 1200 0.0162 355.8 1200 0.01622 355.9 1200 0.01622 356.1 1200 0.0162 356.3 1200 0.0162 356.4 1200 0.0162 356.6 1200 0.01622 356.8 1200 0.01622 356.9 1200 0.01622 357.1 1200 0.01622 357.2 1200 0.01622 357.4 1200 0.0162 357.6 1200 0.01619 357.7 1199 0.0162 357.9 1200 0.0162 358 1200 0.01622 358.2 1200 0.01623 358.4 1200 0.01623 358.5 1200 0.01623 358.7 1200 0.01623 358.8 1200 0.01623 359 1200 0.01623 359.2 1200 0.01623 359.3 1200 0.01623 359.5 1200 0.01624 359.7 1200 0.01624 359.8 1200 0.01623 360 1200 0.01623 360.1 1200 0.01623 360.3 1200 0.01623 360.5 1200 0.01622 360.6 1200 0.01622 360.8 1200 0.01623 360.9 1200 0.01623 361.1 1200 0.01623 361.3 1200 0.01623 361.4 1200 0.01623 361.6 1200 0.01623 361.7 1200 0.01625 361.9 1200 0.01627 362.1 1200 0.01625 362.2 1200 0.01625 362.4 1200 0.01627 362.6 1200 0.01628 362.7 1200 0.01628 362.9 1200 0.01628 363 1200 0.0163 363.2 1200 0.01632 363.4 1200 0.0163 363.5 1200 0.0163 363.7 1200 0.0163 363.8 1200 0.0163 364 1200 0.0163 364.2 1200 0.01632 364.3 1200 0.01632 364.5 1200 0.01633 364.6 1200 0.01633 364.8 1200 0.01633 365 1200 0.01633 365.1 1200 0.01634 365.3 1200 0.01633 365.5 1200 0.01635 365.6 1200 0.01636 365.8 1200 0.01638 365.9 1200 0.01638 366.1 1200 0.01638 366.3 1200 0.01638 366.4 1200 0.01638 366.6 1200 0.01635 366.7 1200 0.01635 366.9 1200 0.01635 367.1 1200 0.01638 367.2 1200 0.01636 367.4 1200 0.01635 367.5 1200 0.01635 367.7 1200 0.01635 367.9 1200 0.01635 368 1200 0.01638 368.2 1200 0.01638 368.4 1200 0.01638 368.5 1200 0.01638 368.7 1200 0.01638 368.8 1200 0.01639 369 1200 0.01639 369.2 1200 0.01639 369.3 1200 0.01639 369.5 1200 0.01638 369.6 1200 0.01639 369.8 1200 0.01639 370 1200 0.01639 370.1 1200 0.01639 370.3 1200 0.01639 370.4 1200 0.01639 370.6 1200 0.01641 370.8 1200 0.01641 370.9 1200 0.01643 371.1 1200 0.01643 371.3 1200 0.01644 371.4 1200 0.01648 371.6 1200 0.01648 371.7 1200 0.01649 371.9 1200 0.01649 372.1 1200 0.01648 372.2 1200 0.01648 372.4 1200 0.01648 372.5 1200 0.01648 372.7 1200 0.01644 372.9 1200 0.01644 373 1200 0.01644 373.2 1200 0.01644 373.3 1200 0.01643 373.5 1200 0.01643 373.7 1200 0.01643 373.8 1200 0.01643 374 1200 0.01644 374.2 1200 0.01646 374.3 1200 0.01648 374.5 1200 0.01648 374.6 1200 0.01648 374.8 1200 0.01649 375 1200 0.0165 375.1 1200 0.0165 375.3 1200 0.01648 375.4 1200 0.01648 375.6 1200 0.01646 375.8 1200 0.01645 375.9 1200 0.01648 376.1 1200 0.0165 376.2 1200 0.01648 376.4 1200 0.01648 376.6 1200 0.01645 376.7 1200 0.01648 376.9 1200 0.01648 377.1 1200 0.01648 377.2 1200 0.01648 377.4 1200 0.01648 377.5 1200 0.01648 377.7 1200 0.01646 377.9 1200 0.01646 378 1200 0.01645 378.2 1200 0.01644 378.3 1200 0.01643 378.5 1200 0.01641 378.7 1200 0.01641 378.8 1200 0.01639 379 1200 0.01638 379.1 1200 0.01638 379.3 1200 0.01639 379.5 1200 0.01639 379.6 1200 0.01639 379.8 1200 0.01639 380 1200 0.0164 380.1 1200 0.01639 380.3 1200 0.01638 380.4 1200 0.01638 380.6 1200 0.01638 380.8 1200 0.01638 380.9 1200 0.01639 381.1 1200 0.0164 381.2 1200 0.0164 381.4 1200 0.01638 381.6 1200 0.01638 381.7 1200 0.01635 381.9 1200 0.01634 382 1200 0.01633 382.2 1200 0.01632 382.4 1200 0.01633 382.5 1200 0.01632 382.7 1200 0.01632 382.9 1200 0.01633 383 1200 0.01633 383.2 1200 0.0163 383.3 1200 0.01628 383.5 1200 0.01629 383.7 1200 0.01628 383.8 1200 0.01627 384 1200 0.01628 384.1 1200 0.01628 384.3 1200 0.01628 384.5 1200 0.01628 384.6 1200 0.01625 384.8 1200 0.01628 384.9 1200 0.01629 385.1 1200 0.0163 385.3 1200 0.0163 385.4 1200 0.01632 385.6 1200 0.01633 385.8 1200 0.01634 385.9 1200 0.01633 386.1 1200 0.01633 386.2 1200 0.01632 386.4 1200 0.0163 386.6 1200 0.01633 386.7 1200 0.01632 386.9 1200 0.0163 387 1200 0.0163 387.2 1200 0.01628 387.4 1200 0.01627 387.5 1200 0.01627 387.7 1200 0.01627 387.8 1200 0.01627 388 1200 0.01625 388.2 1200 0.01628 388.3 1200 0.01628 388.5 1200 0.01628 388.7 1200 0.01628 388.8 1200 0.01629 389 1200 0.0163 389.1 1200 0.0163 389.3 1200 0.0163 389.5 1200 0.01632 389.6 1200 0.01633 389.8 1200 0.01633 389.9 1200 0.01633 390.1 1200 0.01633 390.3 1200 0.01632 390.4 1200 0.0163 390.6 1200 0.01632 390.7 1200 0.01633 390.9 1200 0.01633 391.1 1200 0.01633 391.2 1200 0.01633 391.4 1200 0.01633 391.6 1200 0.01633 391.7 1200 0.01632 391.9 1200 0.0163 392 1200 0.0163 392.2 1200 0.0163 392.4 1200 0.0163 392.5 1200 0.01629 392.7 1200 0.01629 392.8 1200 0.01629 393 1200 0.0163 393.2 1200 0.01632 393.3 1200 0.01632 393.5 1200 0.01633 393.7 1200 0.01633 393.8 1200 0.01632 394 1200 0.0163 394.1 1200 0.01628 394.3 1200 0.01628 394.5 1200 0.01627 394.6 1200 0.01625 394.8 1200 0.01627 394.9 1200 0.01628 395.1 1200 0.01628 395.3 1200 0.0163 395.4 1200 0.0163 395.6 1200 0.01632 395.7 1200 0.01633 395.9 1200 0.01633 396.1 1200 0.01632 396.2 1200 0.0163 396.4 1200 0.01629 396.6 1200 0.01628 396.7 1200 0.01625 396.9 1200 0.01625 397 1200 0.01627 397.2 1200 0.01627 397.4 1200 0.01628 397.5 1200 0.01628 397.7 1200 0.0163 397.8 1200 0.01632 398 1200 0.01632 398.2 1200 0.01633 398.3 1200 0.01633 398.5 1200 0.01633 398.6 1200 0.01633 398.8 1200 0.01632 399 1200 0.01633 399.1 1200 0.01632 399.3 1200 0.0163 399.5 1200 0.0163 399.6 1200 0.01628 399.8 1200 0.01628 399.9 1200 0.01625 400.1 1200 0.01625 400.3 1200 0.01625 400.4 1200 0.01625 400.6 1200 0.01624 400.7 1200 0.01623 400.9 1200 0.01625 401.1 1200 0.01625 401.2 1200 0.01625 401.4 1200 0.01628 401.5 1200 0.01628 401.7 1200 0.01628 401.9 1200 0.01628 402 1200 0.01628 402.2 1200 0.01628 402.4 1200 0.01629 402.5 1200 0.01628 402.7 1200 0.01625 402.8 1200 0.01625 403 1200 0.01625 403.2 1200 0.01625 403.3 1200 0.01625 403.5 1200 0.01628 403.6 1200 0.01628 403.8 1200 0.01627 404 1200 0.01625 404.1 1200 0.01623 404.3 1200 0.01622 404.4 1200 0.0162 404.6 1200 0.0162 404.8 1200 0.01619 404.9 1200 0.0162 405.1 1200 0.01622 405.3 1200 0.01623 405.4 1200 0.01622 405.6 1200 0.0162 405.7 1200 0.01622 405.9 1200 0.01623 406.1 1200 0.01623 406.2 1200 0.01625 406.4 1200 0.01625 406.5 1200 0.01628 406.7 1200 0.01625 406.9 1200 0.01625 407 1200 0.01625 407.2 1200 0.01623 407.3 1200 0.01623 407.5 1200 0.01623 407.7 1200 0.01622 407.8 1200 0.01622 408 1200 0.01623 408.2 1200 0.01623 408.3 1200 0.01623 408.5 1200 0.01622 408.6 1200 0.01623 408.8 1200 0.01623 409 1200 0.01623 409.1 1200 0.01622 409.3 1200 0.01622 409.4 1199 0.0162 409.6 1200 0.0162 409.8 1200 0.01619 409.9 1200 0.01619 410.1 1200 0.0162 410.2 1200 0.0162 410.4 1200 0.0162 410.6 1200 0.01618 410.7 1200 0.01618 410.9 1200 0.01618 411.1 1200 0.01619 411.2 1200 0.01618 411.4 1200 0.01618 411.5 1200 0.01619 411.7 1200 0.0162 411.9 1200 0.0162 412 1200 0.01618 412.2 1200 0.01618 412.3 1200 0.01615 412.5 1200 0.01613 412.7 1200 0.01613 412.8 1200 0.01613 413 1200 0.01613 413.1 1200 0.01613 413.3 1200 0.01615 413.5 1200 0.01618 413.6 1200 0.0162 413.8 1200 0.01619 414 1200 0.01618 414.1 1200 0.01618 414.3 1200 0.01615 414.4 1200 0.01615 414.6 1200 0.01617 414.8 1200 0.01615 414.9 1200 0.01617 415.1 1200 0.01617 415.2 1200 0.01617 415.4 1200 0.01615 415.6 1200 0.01618 415.7 1200 0.01617 415.9 1200 0.01615 416 1200 0.01615 416.2 1200 0.01614 416.4 1200 0.01614 416.5 1200 0.01614 416.7 1200 0.01614 416.9 1200 0.01615 417 1200 0.01615 417.2 1200 0.01618 417.3 1200 0.01618 417.5 1200 0.0162 417.7 1200 0.01622 417.8 1200 0.01623 418 1200 0.01623 418.1 1200 0.01623 418.3 1200 0.01623 418.5 1199 0.01623 418.6 1200 0.01623 418.8 1200 0.01624 418.9 1200 0.01624 419.1 1200 0.01625 419.3 1200 0.01628 419.4 1200 0.01628 419.6 1200 0.01628 419.8 1200 0.01629 419.9 1200 0.0163 420.1 1200 0.0163 420.2 1200 0.0163 420.4 1200 0.01632 420.6 1200 0.01632 420.7 1200 0.0163 420.9 1200 0.0163 421 1200 0.0163 421.2 1200 0.0163 421.4 1200 0.01632 421.5 1200 0.0163 421.7 1200 0.0163 421.8 1200 0.0163 422 1200 0.0163 422.2 1200 0.01632 422.3 1200 0.01633 422.5 1200 0.01633 422.7 1200 0.01633 422.8 1200 0.01633 423 1200 0.01633 423.1 1200 0.01633 423.3 1200 0.01634 423.5 1200 0.01634 423.6 1200 0.01633 423.8 1200 0.01634 423.9 1200 0.01634 424.1 1200 0.01634 424.3 1200 0.01635 424.4 1200 0.01636 424.6 1200 0.01638 424.7 1200 0.01638 424.9 1200 0.01638 425.1 1200 0.01636 425.2 1200 0.01638 425.4 1200 0.01638 425.6 1200 0.01635 425.7 1200 0.01638 425.9 1200 0.01638 426 1200 0.01638 426.2 1200 0.0164 426.4 1200 0.01641 426.5 1200 0.01641 426.7 1200 0.0164 426.8 1200 0.01639 427 1200 0.01638 427.2 1200 0.01638 427.3 1200 0.01639 427.5 1199 0.0164 427.6 1200 0.01641 427.8 1200 0.01643 428 1200 0.01644 428.1 1200 0.01643 428.3 1200 0.01643 428.5 1200 0.01644 428.6 1200 0.01644 428.8 1200 0.01644 428.9 1200 0.01648 429.1 1200 0.01648 429.3 1200 0.01648 429.4 1200 0.0165 429.6 1200 0.01649 429.7 1200 0.01648 429.9 1200 0.01649 430.1 1200 0.0165 430.2 1200 0.01649 430.4 1200 0.01648 430.6 1200 0.01646 430.7 1200 0.01646 430.9 1200 0.01648 431 1200 0.01648 431.2 1200 0.01645 431.4 1200 0.01645 431.5 1200 0.01645 431.7 1200 0.01644 431.8 1200 0.01644 432 1200 0.01644 432.2 1200 0.01644 432.3 1200 0.01644 432.5 1200 0.01645 432.6 1200 0.01648 432.8 1200 0.01645 433 1200 0.01645 433.1 1200 0.01645 433.3 1200 0.01644 433.5 1200 0.01644 433.6 1200 0.01644 433.8 1200 0.01644 433.9 1200 0.01645 434.1 1200 0.01648 434.3 1200 0.01646 434.4 1200 0.01645 434.6 1200 0.01645 434.7 1200 0.01645 434.9 1200 0.01644 435.1 1200 0.01643 435.2 1200 0.01644 435.4 1200 0.01644 435.5 1200 0.01644 435.7 1200 0.01643 435.9 1200 0.01641 436 1200 0.0164 436.2 1200 0.01643 436.4 1200 0.01643 436.5 1199 0.01643 436.7 1200 0.01641 436.8 1200 0.01641 437 1200 0.01641 437.2 1200 0.0164 437.3 1200 0.0164 437.5 1200 0.01639 437.6 1200 0.01638 437.8 1200 0.01638 438 1200 0.01635 438.1 1200 0.01636 438.3 1200 0.01638 438.4 1200 0.01638 438.6 1200 0.01638 438.8 1200 0.01638 438.9 1200 0.01639 439.1 1200 0.01638 439.3 1200 0.01635 439.4 1200 0.01636 439.6 1200 0.01635 439.7 1200 0.01635 439.9 1200 0.01635 440.1 1200 0.01635 440.2 1200 0.01634 440.4 1200 0.01634 440.5 1200 0.01635 440.7 1200 0.01634 440.9 1200 0.01634 441 1200 0.01634 441.2 1200 0.01634 441.3 1200 0.01634 441.5 1200 0.01633 441.7 1200 0.01632 441.8 1200 0.0163 442 1200 0.0163 442.2 1200 0.0163 442.3 1200 0.01632 442.5 1200 0.01632 442.6 1200 0.0163 442.8 1200 0.0163 443 1200 0.01629 443.1 1200 0.01629 443.3 1200 0.0163 443.4 1200 0.01629 443.6 1200 0.01629 443.8 1200 0.0163 443.9 1200 0.01628 444.1 1200 0.01629 444.2 1200 0.01629 444.4 1200 0.01629 444.6 1200 0.0163 444.7 1200 0.0163 444.9 1200 0.01632 445.1 1200 0.0163 445.2 1200 0.01632 445.4 1200 0.01632 445.5 1199 0.0163 445.7 1200 0.0163 445.9 1200 0.0163 446 1200 0.0163 446.2 1200 0.01629 446.3 1200 0.01629 446.5 1200 0.01629 446.7 1200 0.01629 446.8 1200 0.01629 447 1200 0.0163 447.1 1200 0.01629 447.3 1200 0.01628 447.5 1200 0.01629 447.6 1200 0.01629 447.8 1200 0.01628 448 1200 0.01629 448.1 1200 0.01629 448.3 1200 0.01628 448.4 1200 0.01629 448.6 1200 0.01629 448.8 1200 0.01629 448.9 1200 0.01629 449.1 1200 0.01629 449.2 1200 0.01629 449.4 1200 0.01628 449.6 1200 0.01629 449.7 1199 0.01628 449.9 1199 0.01629 450 1198 0.01629 450.2 1198 0.01628 450.4 1197 0.01627 450.5 1187 0.01625 450.7 1187 0.01677 450.9 1187 0.01726 451 1187 0.01695 451.2 1185 0.01672 451.3 1184 0.01656 451.5 1184 0.01644 451.7 1182 0.01633 451.8 1181 0.01625 452 1179 0.0162 452.1 1179 0.01617 452.3 1178 0.01614 452.5 1176 0.01608 452.6 1175 0.01603 452.8 1174 0.01598 452.9 1173 0.01597 453.1 1172 0.01597 453.3 1171 0.01596 453.4 1169 0.01593 453.6 1169 0.01592 453.8 1167 0.01591 453.9 1165 0.01588 454.1 1164 0.01586 454.2 1163 0.01583 454.4 1162 0.0158 454.6 1161 0.01577 454.7 1159 0.01575 454.9 1158 0.01572 455 1157 0.01568 455.2 1156 0.01565 455.4 1154 0.01562 455.5 1153 0.01558 455.7 1153 0.01558 455.8 1152 0.01555 456 1151 0.01551 456.2 1150 0.0155 456.3 1149 0.01547 456.5 1148 0.01545 456.7 1148 0.01544 456.8 1147 0.01539 457 1145 0.01536 457.1 1144 0.01531 457.3 1144 0.01529 457.5 1142 0.01529 457.6 1140 0.01524 457.8 1139 0.01521 457.9 1137 0.01519 458.1 1137 0.01519 458.3 1136 0.01513 458.4 1134 0.01508 458.6 1131 0.01504 458.7 1130 0.01501 458.9 1129 0.01497 459.1 1128 0.0149 459.2 1125 0.01484 459.4 1123 0.0148 459.6 1122 0.01478 459.7 1121 0.01473 459.9 1119 0.01469 460 1117 0.01467 460.2 1115 0.01462 460.4 1114 0.01456 460.5 1112 0.01454 460.7 1111 0.01449 460.8 1109 0.01445 461 1108 0.01442 461.2 1106 0.01438 461.3 1104 0.01435 461.5 1103 0.0143 461.6 1101 0.01427 461.8 1100 0.01425 462 1098 0.0142 462.1 1097 0.01416 462.3 1097 0.01414 462.5 1094 0.0141 462.6 1094 0.01409 462.8 1092 0.01405 462.9 1090 0.014 463.1 1090 0.01399 463.3 1088 0.01397 463.4 1087 0.01394 463.6 1086 0.0139 463.7 1084 0.01385 463.9 1083 0.01383 464.1 1082 0.01379 464.2 1080 0.01373 464.4 1079 0.0137 464.5 1078 0.01368 464.7 1076 0.01365 464.9 1075 0.01362 465 1075 0.0136 465.2 1073 0.01358 465.4 1072 0.01355 465.5 1071 0.01354 465.7 1069 0.01352 465.8 1068 0.01347 466 1067 0.01343 466.2 1065 0.01338 466.3 1065 0.01331 466.5 1063 0.01326 466.6 1062 0.01324 466.8 1061 0.01321 467 1059 0.01318 467.1 1058 0.01314 467.3 1057 0.01311 467.4 1056 0.01306 467.6 1054 0.01305 467.8 1053 0.01301 467.9 1052 0.01297 468.1 1050 0.01293 468.3 1049 0.01291 468.4 1047 0.01291 468.6 1047 0.01288 468.7 1045 0.01285 468.9 1043 0.01281 469.1 1043 0.01276 469.2 1041 0.01274 469.4 1040 0.0127 469.5 1038 0.01269 469.7 1037 0.01269 469.9 1036 0.01269 470 1034 0.01269 470.2 1034 0.01266 470.4 1032 0.01265 470.5 1031 0.0126 470.7 1029 0.01254 470.8 1028 0.01248 471 1026 0.01245 471.2 1025 0.0124 471.3 1025 0.01238 471.5 1023 0.01235 471.6 1022 0.01232 471.8 1020 0.01229 472 1018 0.01227 472.1 1018 0.01227 472.3 1016 0.01225 472.4 1015 0.01222 472.6 1014 0.0122 472.8 1012 0.01218 472.9 1011 0.01213 473.1 1009 0.0121 473.3 1008 0.01207 473.4 1007 0.01204 473.6 1006 0.01202 473.7 1004 0.01198 473.9 1003 0.01198 474.1 1002 0.01196 474.2 1001 0.01191 474.4 1000 0.01188 474.5 998 0.01186 474.7 997 0.01182 474.9 997 0.0118 475 994 0.01176 475.2 993 0.01172 475.3 993 0.01168 475.5 990 0.01167 475.7 990 0.01162 475.8 988 0.01157 476 987 0.01156 476.2 986 0.01154 476.3 984 0.01152 476.5 984 0.01151 476.6 982 0.0115 476.8 980 0.01146 477 979 0.01142 477.1 978 0.01137 477.3 976 0.01135 477.4 976 0.01132 477.6 975 0.0113 477.8 972 0.01128 477.9 972 0.01125 478.1 970 0.01124 478.2 969 0.0112 478.4 968 0.01116 478.6 967 0.01113 478.7 965 0.01113 478.9 964 0.01111 479.1 962 0.01108 479.2 961 0.01105 479.4 960 0.01104 479.5 959 0.011 479.7 957 0.01098 479.9 956 0.01095 480 954 0.01092 480.2 953 0.01089 480.3 953 0.01088 480.5 950 0.01083 480.7 950 0.0108 480.8 948 0.01078 481 947 0.01077 481.1 946 0.01075 481.3 943 0.01073 481.5 943 0.01071 481.6 942 0.01067 481.8 940 0.01064 482 939 0.01062 482.1 937 0.01058 482.3 936 0.01057 482.4 935 0.01053 482.6 934 0.01048 482.8 932 0.01046 482.9 931 0.01043 483.1 929 0.01042 483.2 929 0.01038 483.4 928 0.01036 483.6 926 0.01032 483.7 925 0.01028 483.9 923 0.01023 484 922 0.0102 484.2 922 0.01017 484.4 919 0.01015 484.5 918 0.01012 484.7 917 0.01011 484.9 915 0.0101 485 914 0.0101 485.2 913 0.01009 485.3 912 0.01006 485.5 910 0.01004 485.7 909 0.01001 485.8 907 0.009987 486 906 0.009975 486.1 904 0.009962 486.3 903 0.009938 486.5 903 0.009901 486.6 900 0.009888 486.8 900 0.009863 486.9 899 0.009839 487.1 897 0.009814 487.3 896 0.009789 487.4 894 0.009764 487.6 893 0.009702 487.8 892 0.009678 487.9 890 0.00964 488.1 889 0.009579 488.2 888 0.009541 488.4 887 0.009517 488.6 886 0.009492 488.7 884 0.009479 488.9 882 0.009455 489 881 0.00943 489.2 880 0.009405 489.4 879 0.00938 489.5 878 0.009368 489.7 876 0.009343 489.8 875 0.009306 490 874 0.009257 490.2 872 0.009219 490.3 871 0.009195 490.5 869 0.00917 490.7 868 0.009158 490.8 867 0.009145 491 865 0.009096 491.1 864 0.009071 491.3 864 0.009046 491.5 862 0.009021 491.6 861 0.008997 491.8 859 0.008997 491.9 858 0.008947 492.1 857 0.008922 492.3 856 0.008897 492.4 854 0.008848 492.6 853 0.008811 492.7 851 0.008774 492.9 850 0.008749 493.1 848 0.008724 493.2 847 0.008687 493.4 847 0.00865 493.6 845 0.008625 493.7 843 0.008613 493.9 842 0.0086 494 841 0.008575 494.2 840 0.008551 494.4 838 0.008514 494.5 837 0.008476 494.7 836 0.008402 494.8 834 0.008377 495 834 0.00834 495.2 832 0.008291 495.3 831 0.008241 495.5 829 0.008204 495.6 828 0.008154 495.8 826 0.008117 496 825 0.00808 496.1 824 0.008043 496.3 823 0.008006 496.5 821 0.007993 496.6 820 0.007956 496.8 818 0.007932 496.9 818 0.007919 497.1 817 0.00787 497.3 815 0.007857 497.4 814 0.007845 497.6 812 0.00782 497.7 811 0.007795 497.9 809 0.007758 498.1 809 0.007721 498.2 807 0.007696 498.4 806 0.007659 498.5 804 0.00761 498.7 803 0.007572 498.9 802 0.007523 499 801 0.007473 499.2 801 0.007436 499.4 801 0.007399 499.5 801 0.007387 499.7 800 0.007337 499.8 798 0.0073 500 796 0.007275 500.2 796 0.007238 500.3 794 0.007213 500.5 793 0.007176 500.6 792 0.007151 500.8 790 0.007127 501 789 0.007114 501.1 788 0.007065 501.3 787 0.007015 501.4 786 0.007003 501.6 784 0.006978 501.8 783 0.006941 501.9 782 0.006904 502.1 780 0.006867 502.3 779 0.006817 502.4 778 0.006792 502.6 776 0.006743 502.7 775 0.006706 502.9 774 0.006656 503.1 772 0.006619 503.2 771 0.006582 503.4 770 0.006569 503.5 768 0.006532 503.7 768 0.00652 503.9 765 0.00647 504 765 0.006458 504.2 764 0.006421 504.3 762 0.006384 504.5 761 0.006371 504.7 760 0.006346 504.8 758 0.006322 505 757 0.006297 505.2 756 0.006272 505.3 754 0.006235 505.5 753 0.00621 505.6 751 0.006185 505.8 750 0.006136 506 749 0.006099 506.1 747 0.006074 506.3 746 0.006037 506.4 746 0.006012 506.6 743 0.005975 506.8 743 0.005963 506.9 741 0.00595 507.1 740 0.005913 507.2 739 0.005888 507.4 737 0.005864 507.6 736 0.005851 507.7 735 0.005826 507.9 734 0.005789 508.1 732 0.005752 508.2 731 0.005727 508.4 729 0.00569 508.5 728 0.005653 508.7 727 0.005616 508.9 725 0.005591 509 725 0.005529 509.2 723 0.005492 509.3 721 0.005455 509.5 720 0.005418 509.7 719 0.005381 509.8 718 0.005331 510 718 0.005282 510.2 715 0.005269 510.3 714 0.005232 510.5 712 0.005195 510.6 711 0.00517 510.8 710 0.005133 511 709 0.005108 511.1 707 0.005083 511.3 706 0.005071 511.4 704 0.005046 511.6 703 0.005021 511.8 702 0.005009 511.9 701 0.004984 512.1 700 0.00496 512.2 698 0.004935 512.4 697 0.004922 512.6 696 0.004898 512.7 694 0.004885 512.9 693 0.004836 513.1 692 0.004799 513.2 690 0.004786 513.4 689 0.004761 513.5 688 0.004749 513.7 686 0.004737 513.9 685 0.004687 514 684 0.004638 514.2 682 0.004613 514.3 681 0.004588 514.5 680 0.004563 514.7 679 0.004539 514.8 678 0.004501 515 676 0.004489 515.1 675 0.004464 515.3 674 0.004464 515.5 672 0.004452 515.6 671 0.004452 515.8 669 0.004427 516 668 0.004415 516.1 668 0.00439 516.3 665 0.00434 516.4 664 0.004303 516.6 663 0.004278 516.8 662 0.004241 516.9 660 0.004217 517.1 659 0.004167 517.2 658 0.00413 517.4 657 0.004093 517.6 655 0.004043 517.7 654 0.004018 517.9 653 0.003994 518 651 0.003956 518.2 650 0.003944 518.4 649 0.003919 518.5 647 0.003919 518.7 646 0.003895 518.9 645 0.00387 519 643 0.003857 519.2 643 0.00382 519.3 641 0.003783 519.5 639 0.003758 519.7 639 0.003746 519.8 637 0.003709 520 635 0.003696 520.1 635 0.003684 520.3 633 0.003647 520.5 632 0.003622 520.6 631 0.003597 520.8 629 0.003548 520.9 628 0.003523 521.1 627 0.003498 521.3 625 0.003449 521.4 624 0.003449 521.6 623 0.003424 521.8 621 0.003399 521.9 619 0.003362 522.1 619 0.00335 522.2 617 0.003325 522.4 615 0.003313 522.6 615 0.003263 522.7 614 0.003213 522.9 612 0.003164 523 612 0.003127 523.2 609 0.003102 523.4 609 0.003065 523.5 607 0.003028 523.7 606 0.002978 523.8 604 0.002941 524 603 0.002916 524.2 601 0.002904 524.3 601 0.002854 524.5 601 0.00283 524.7 598 0.002805 524.8 597 0.00278 525 596 0.002743 525.1 594 0.002718 525.3 593 0.002706 525.5 593 0.002669 525.6 590 0.002656 525.8 590 0.002619 525.9 589 0.002594 526.1 587 0.002582 526.3 586 0.002545 526.4 584 0.002508 526.6 582 0.002495 526.7 582 0.00247 526.9 581 0.002458 527.1 578 0.002446 527.2 579 0.002409 527.4 576 0.002384 527.6 574 0.002359 527.7 574 0.002322 527.9 572 0.002285 528 571 0.002248 528.2 571 0.002198 528.4 568 0.002161 528.5 567 0.002124 528.7 567 0.002062 528.8 565 0.002037 529 564 0.002 529.2 564 0.001963 529.3 560 0.001938 529.5 560 0.001901 529.6 559 0.001888 529.8 556 0.001864 530 556 0.001839 530.1 556 0.001814 530.3 553 0.001814 530.5 553 0.001777 530.6 551 0.001752 530.8 548 0.001715 530.9 549 0.001678 531.1 546 0.001653 531.3 544 0.001641 531.4 545 0.001591 531.6 542 0.001579 531.7 540 0.001566 531.9 542 0.001529 532.1 539 0.001517 532.2 537 0.001505 532.4 537 0.001467 532.5 534 0.001418 532.7 534 0.001381 532.9 533 0.001306 533 530 0.001245 533.2 531 0.00122 533.4 528 0.00122 533.5 526 0.001207 533.7 528 0.001195 533.8 524 0.00117 534 523 0.001158 534.2 524 0.001121 534.3 519 0.001096 534.5 520 0.001071 534.6 518 0.001034 534.8 515 0.001022 535 517 0.0009845 535.1 514 0.0009473 535.3 513 0.0009226 535.4 513 0.000873 535.6 509 0.0008606 535.8 510 0.0008235 535.9 508 0.000774 536.1 506 0.0007492 536.3 506 0.0006873 536.4 503 0.0006501 536.6 503 0.0006254 536.7 503 0.0005882 536.9 499 0.0005634 537.1 499 0.0005263 537.2 497 0.0005263 537.4 496 0.0005139 537.5 496 0.0004891 537.7 492 0.0004768 537.9 492 0.000452 538 492 0.0004025 538.2 489 0.0003529 538.3 489 0.0003282 538.5 487 0.0003034 538.7 485 0.000291 538.8 485 0.0002786 539 481 0.0002539 539.2 482 0.0002291 539.3 481 0.0002043 539.5 478 0.0001548 539.6 479 0.00013 539.8 476 9.288e-05 540 476 6.811e-05 540.1 474 5.573e-05 540.3 471 5.573e-05 540.4 472 3.096e-05 540.6 469 1.858e-05 540.8 469 6.192e-06 540.9 468 6.192e-06 541.1 465 6.192e-06 541.2 467 6.192e-06 541.4 463 -6.192e-06 541.6 462 -4.334e-05 541.7 462 -6.811e-05 541.9 459 -6.811e-05 542.1 460 -9.288e-05 542.2 456 -0.0001176 542.4 456 -0.00013 542.5 455 -0.0001672 542.7 453 -0.0002167 542.9 453 -0.0002539 543 449 -0.0002662 543.2 449 -0.000291 543.3 448 -0.0003034 543.5 447 -0.0003282 543.7 446 -0.0003405 543.8 444 -0.0003529 544 442 -0.0003653 544.1 442 -0.0003777 544.3 440 -0.0004272 544.5 439 -0.000452 544.6 438 -0.0004644 544.8 437 -0.0004768 545 435 -0.0005139 545.1 434 -0.0005263 545.3 432 -0.0005634 545.4 431 -0.0005758 545.6 430 -0.0006006 545.8 429 -0.000613 545.9 428 -0.0006501 546.1 426 -0.0006749 546.2 425 -0.000712 546.4 424 -0.0007368 546.6 422 -0.0007616 546.7 421 -0.000774 546.9 420 -0.0007863 547 418 -0.0007987 547.2 417 -0.0008235 547.4 415 -0.0008483 547.5 415 -0.000873 547.7 413 -0.0008978 547.9 412 -0.0009102 548 410 -0.0009349 548.2 409 -0.0009597 548.3 407 -0.0009597 548.5 406 -0.0009969 548.7 406 -0.001009 548.8 404 -0.001022 549 403 -0.001046 549.1 402 -0.001059 549.3 401 -0.001059 549.5 399 -0.001071 549.6 399 -0.001084 549.8 398 -0.001084 550 396 -0.001108 550.1 395 -0.001121 550.3 393 -0.001121 550.4 392 -0.001133 550.6 391 -0.001133 550.8 390 -0.001145 550.9 388 -0.001158 551.1 387 -0.001158 551.2 386 -0.001158 551.4 385 -0.00117 551.6 384 -0.00117 551.7 382 -0.001183 551.9 381 -0.001183 552 380 -0.001183 552.2 379 -0.001158 552.4 378 -0.001183 552.5 376 -0.001183 552.7 374 -0.001158 552.9 374 -0.001158 553 372 -0.001145 553.2 371 -0.001133 553.3 370 -0.001121 553.5 369 -0.001108 553.7 368 -0.001084 553.8 367 -0.001071 554 365 -0.001059 554.1 363 -0.001034 554.3 363 -0.001009 554.5 361 -0.0009721 554.6 360 -0.0009349 554.8 359 -0.0009102 554.9 358 -0.0008483 555.1 356 -0.0007987 555.3 356 -0.0007492 555.4 354 -0.000712 555.6 353 -0.0006625 555.8 352 -0.0006006 555.9 350 -0.0005263 556.1 349 -0.0004644 556.2 349 -0.0003777 556.4 349 -0.0003034 556.6 348 -0.0002291 556.7 346 -0.0001672 556.9 345 -8.049e-05 557 343 -1.858e-05 557.2 342 6.192e-06 557.4 340 6.811e-05 557.5 338 0.0001796 557.7 337 0.0002786 557.8 335 0.0003777 558 334 0.0004644 558.2 331 0.0005634 558.3 331 0.0006501 558.5 328 0.0007368 558.7 327 0.0008111 558.8 324 0.0008854 559 323 0.0009597 559.1 321 0.001034 559.3 320 0.001096 559.5 318 0.00117 559.6 317 0.001245 559.8 315 0.001306 559.9 313 0.001381 560.1 312 0.00143 560.3 310 0.001467 560.4 309 0.001529 560.6 307 0.001579 560.7 306 0.001616 560.9 304 0.001666 561.1 302 0.001727 561.2 302 0.001765 561.4 300 0.001789 561.6 299 0.001802 561.7 298 0.001814 561.9 296 0.001839 562 295 0.001851 562.2 293 0.001876 562.4 292 0.001901 562.5 290 0.001913 562.7 288 0.001938 562.8 288 0.00195 563 287 0.001963 563.2 286 0.001988 563.3 285 0.002 563.5 284 0.002012 563.6 283 0.002012 563.8 282 0.002025 564 281 0.002025 564.1 280 0.002025 564.3 279 0.002012 564.5 278 0.002012 564.6 277 0.001988 564.8 276 0.001975 564.9 274 0.001963 565.1 273 0.00195 565.3 272 0.001938 565.4 270 0.001938 565.6 269 0.001938 565.7 268 0.001938 565.9 267 0.001926 566.1 265 0.001913 566.2 265 0.001913 566.4 263 0.001913 566.5 262 0.001901 566.7 260 0.001901 566.9 259 0.001888 567 257 0.001913 567.2 256 0.001901 567.4 256 0.001888 567.5 254 0.001913 567.7 252 0.001888 567.8 251 0.001876 568 249 0.001864 568.2 249 0.001851 568.3 247 0.001839 568.5 246 0.001814 568.6 245 0.001814 568.8 243 0.001789 569 242 0.001789 569.1 241 0.001765 569.3 240 0.001765 569.4 238 0.00174 569.6 237 0.001715 569.8 235 0.00169 569.9 234 0.001666 570.1 234 0.001653 570.3 231 0.001653 570.4 231 0.001616 570.6 229 0.001616 570.7 228 0.001591 570.9 227 0.001579 571.1 226 0.001566 571.2 224 0.001566 571.4 223 0.001554 571.5 221 0.001542 571.7 220 0.001542 571.9 219 0.001529 572 218 0.001529 572.2 217 0.001517 572.3 215 0.00148 572.5 213 0.001467 572.7 213 0.001467 572.8 212 0.001467 573 209 0.001467 573.2 209 0.001467 573.3 207 0.001443 573.5 206 0.001418 573.6 205 0.001381 573.8 203 0.001368 574 202 0.001344 574.1 201 0.001331 574.3 201 0.001294 574.4 199 0.001282 574.6 198 0.001269 574.8 196 0.001282 574.9 195 0.001269 575.1 193 0.001269 575.2 192 0.001269 575.4 191 0.001282 575.6 190 0.001294 575.7 188 0.001294 575.9 187 0.001269 576.1 187 0.001269 576.2 184 0.001245 576.4 184 0.00122 576.5 181 0.001207 576.7 181 0.00117 576.9 179 0.001158 577 177 0.001158 577.2 177 0.001121 577.3 175 0.001108 577.5 174 0.001096 577.7 174 0.001059 577.8 171 0.001022 578 170 0.0009845 578.1 169 0.0009597 578.3 167 0.0009226 578.5 166 0.0009102 578.6 165 0.0008978 578.8 163 0.0008854 579 163 0.000873 579.1 160 0.0008978 579.3 159 0.0009226 579.4 159 0.0009597 579.6 157 0.0009721 579.8 156 0.0009597 579.9 155 0.0009721 580.1 154 0.0009721 580.2 152 0.0009349 580.4 150 0.0009226 580.6 149 0.0008978 580.7 148 0.000873 580.9 147 0.0008483 581 146 0.0008235 581.2 145 0.0008235 581.4 143 0.0008235 581.5 141 0.0008235 581.7 140 0.0008359 581.9 139 0.0008235 582 138 0.000774 582.2 137 0.0007368 582.3 135 0.0007244 582.5 134 0.000712 582.7 132 0.0006873 582.8 131 0.0006749 583 131 0.0006625 583.1 129 0.0006501 583.3 127 0.0006377 583.5 126 0.0006254 583.6 126 0.0006006 583.8 124 0.0005882 583.9 123 0.0005758 584.1 121 0.0005758 584.3 120 0.0005634 584.4 120 0.0005758 584.6 118 0.0005634 584.8 116 0.0005634 584.9 115 0.0005511 585.1 115 0.0005387 585.2 114 0.0005263 585.4 113 0.0005263 585.6 112 0.0005387 585.7 111 0.0005634 585.9 109 0.0005634 586 109 0.0005511 586.2 107 0.0005015 586.4 106 0.000452 586.5 105 0.0004272 586.7 102 0.0004148 586.9 102 0.0004148 587 101 0.0004148 587.2 100 0.0004025 587.3 99 0.0004025 587.5 98 0.0003901 587.7 97 0.0003777 587.8 96 0.0003653 588 95 0.0003653 588.1 93 0.0003529 588.3 91 0.0003282 588.5 91 0.0003034 588.6 90 0.000291 588.8 88 0.0002786 588.9 88 0.0002662 589.1 87 0.0002662 589.3 85 0.0002662 589.4 84 0.0002415 589.6 84 0.0002291 589.8 81 0.0002291 589.9 81 0.0002167 590.1 81 0.0002167 590.2 79 0.0002043 590.4 77 0.0001919 590.6 77 0.0001796 590.7 76 0.0001672 590.9 74 0.0001672 591 74 0.0001672 591.2 73 0.0001548 591.4 72 0.0001424 591.5 71 0.0001176 591.7 70 9.288e-05 591.8 69 8.049e-05 592 68 6.811e-05 592.2 67 3.096e-05 592.3 66 6.192e-06 592.5 66 6.192e-06 592.7 65 6.192e-06 592.8 63 6.192e-06 593 63 6.192e-06 593.1 62 6.192e-06 593.3 61 6.192e-06 593.5 60 6.192e-06 593.6 59 6.192e-06 593.8 59 6.192e-06 593.9 58 -1.858e-05 594.1 56 -3.096e-05 594.3 56 -5.573e-05 594.4 55 -6.811e-05 594.6 55 -8.049e-05 594.7 54 -9.288e-05 594.9 54 -9.288e-05 595.1 52 -0.0001176 595.2 52 -0.0001176 595.4 51 -0.0001176 595.6 51 -0.00013 595.7 49 -0.0001176 595.9 49 -0.0001176 596 49 -0.0001176 596.2 48 -0.00013 596.4 48 -0.00013 596.5 48 -0.00013 596.7 47 -0.00013 596.8 46 -0.0001424 597 46 -0.0001672 597.2 45 -0.0001919 597.3 45 -0.0001919 597.5 45 -0.0002043 597.6 44 -0.0001919 597.8 43 -0.0001796 598 43 -0.0001672 598.1 43 -0.0001796 598.3 42 -0.0001919 598.5 41 -0.0002043 598.6 41 -0.0002043 598.8 41 -0.0002167 598.9 41 -0.0002291 599.1 40 -0.0002539 599.3 40 -0.0002786 599.4 39 -0.0003529 599.6 39 -0.0003653 599.7 38 -0.0004025 599.9 38 -0.0004148 600.1 37 -0.0004148 600.2 38 -0.0004396 600.4 37 -0.0004272 600.5 37 -0.0003901 600.7 36 -0.0003653 600.9 36 -0.0003653 601 36 -0.0003405 601.2 36 -0.0003405 601.4 35 -0.0003282 601.5 35 -0.0003282 601.7 34 -0.0003282 601.8 34 -0.0003282 602 34 -0.0003405 602.2 34 -0.0003529 602.3 34 -0.0003529 602.5 34 -0.0003405 602.6 33 -0.0003405 602.8 33 -0.0003282 603 32 -0.0003405 603.1 32 -0.0003529 603.3 32 -0.0003653 603.4 31 -0.0003777 603.6 31 -0.0003901 603.8 30 -0.0004025 603.9 30 -0.0003901 604.1 30 -0.0003901 604.3 30 -0.0003901 604.4 30 -0.0004148 604.6 30 -0.000452 604.7 30 -0.0004891 604.9 30 -0.0005139 605.1 30 -0.0005263 605.2 29 -0.0005263 605.4 29 -0.0005263 605.5 29 -0.0005263 605.7 29 -0.0005015 605.9 29 -0.0004891 606 29 -0.0004891 606.2 27 -0.0004768 606.3 27 -0.0004768 606.5 27 -0.0004768 606.7 27 -0.0004768 606.8 27 -0.0004644 607 27 -0.0004644 607.2 27 -0.0004644 607.3 27 -0.0004768 607.5 27 -0.0005015 607.6 27 -0.0005263 607.8 27 -0.0005387 608 27 -0.0005387 608.1 26 -0.0005139 608.3 26 -0.0005139 608.4 27 -0.0004891 608.6 26 -0.0004644 608.8 26 -0.0004644 608.9 26 -0.0004768 609.1 25 -0.0005139 609.2 26 -0.0005263 609.4 25 -0.0005387 609.6 25 -0.0005387 609.7 24 -0.0005387 609.9 24 -0.0005263 610.1 24 -0.0005263 610.2 24 -0.0005263 610.4 24 -0.0005263 610.5 24 -0.0005263 610.7 24 -0.0005139 610.9 24 -0.0005015 611 24 -0.0005139 611.2 24 -0.0005263 611.3 23 -0.0005263 611.5 24 -0.0005263 611.7 23 -0.0005263 611.8 23 -0.0005263 612 23 -0.0005263 612.1 23 -0.0005139 612.3 23 -0.0005139 612.5 23 -0.0005139 612.6 23 -0.0005139 612.8 23 -0.0005015 613 23 -0.0004891 613.1 23 -0.0005015 613.3 23 -0.0005139 613.4 23 -0.0005263 613.6 22 -0.0005387 613.8 22 -0.0005634 613.9 21 -0.0005634 614.1 22 -0.0005634 614.2 21 -0.0005511 614.4 22 -0.0005387 614.6 21 -0.0005387 614.7 21 -0.0005263 614.9 21 -0.0005263 615 21 -0.0005263 615.2 21 -0.0005263 615.4 21 -0.0005263 615.5 21 -0.0005263 615.7 21 -0.0005263 615.9 21 -0.0005139 616 21 -0.0005139 616.2 20 -0.0005139 616.3 21 -0.0005263 616.5 21 -0.0005139 616.7 20 -0.0005263 616.8 21 -0.0005263 617 20 -0.0005139 617.1 20 -0.0005015 617.3 20 -0.0005139 617.5 20 -0.0005139 617.6 20 -0.0005015 617.8 20 -0.0004891 617.9 20 -0.0004891 618.1 20 -0.0004768 618.3 20 -0.0004768 618.4 20 -0.0004891 618.6 20 -0.0004768 618.8 19 -0.0004644 618.9 20 -0.0004768 619.1 19 -0.0004768 619.2 19 -0.0004768 619.4 19 -0.0004768 619.6 19 -0.0004768 619.7 19 -0.0004768 619.9 19 -0.0004891 620 19 -0.0005015 620.2 19 -0.0004891 620.4 19 -0.0004891 620.5 18 -0.0005139 620.7 19 -0.0005015 620.8 18 -0.0005015 621 18 -0.0005139 621.2 19 -0.0005015 621.3 18 -0.0004891 621.5 18 -0.0004891 621.7 18 -0.0004891 621.8 18 -0.0004768 622 18 -0.0004768 622.1 18 -0.0004768 622.3 18 -0.0004768 622.5 18 -0.0004768 622.6 18 -0.0004644 622.8 18 -0.000452 622.9 18 -0.0004396 623.1 18 -0.0004396 623.3 18 -0.0004272 623.4 18 -0.0004148 623.6 18 -0.0004025 623.7 18 -0.0003901 623.9 18 -0.0003901 624.1 17 -0.0003901 624.2 18 -0.0004148 624.4 17 -0.0004272 624.6 17 -0.000452 624.7 17 -0.000452 624.9 17 -0.0004396 625 17 -0.0004272 625.2 17 -0.0004148 625.4 17 -0.0003901 625.5 17 -0.0003901 625.7 17 -0.0003901 625.8 17 -0.0004148 626 17 -0.0004272 626.2 16 -0.0004272 626.3 17 -0.0004396 626.5 16 -0.000452 626.7 16 -0.0004396 626.8 16 -0.0004272 627 16 -0.0004272 627.1 16 -0.0004272 627.3 16 -0.0004148 627.5 16 -0.0003901 627.6 16 -0.0003901 627.8 16 -0.0004025 627.9 16 -0.0004148 628.1 16 -0.0003901 628.3 16 -0.0004025 628.4 16 -0.0004148 628.6 16 -0.0004148 628.7 16 -0.0004148 628.9 16 -0.0004148 629.1 16 -0.0003777 629.2 16 -0.0003653 629.4 16 -0.0003529 629.6 16 -0.0003405 629.7 16 -0.0003405 629.9 16 -0.0003653 630 16 -0.0003777 630.2 16 -0.0003901 630.4 16 -0.0004148 630.5 16 -0.0003901 630.7 16 -0.0003901 630.8 16 -0.0004025 631 15 -0.0004148 631.2 16 -0.0004148 631.3 16 -0.0004148 631.5 16 -0.0004025 631.6 15 -0.0003901 631.8 15 -0.0003777 632 15 -0.0003653 632.1 15 -0.0003529 632.3 16 -0.0003405 632.5 16 -0.0003158 632.6 15 -0.0003158 632.8 15 -0.0003158 632.9 15 -0.0003158 633.1 16 -0.0003158 633.3 15 -0.0003282 633.4 15 -0.0003282 633.6 15 -0.0003405 633.7 15 -0.0003653 633.9 15 -0.0003529 634.1 15 -0.0003653 634.2 15 -0.0003653 634.4 15 -0.0003653 634.5 15 -0.0003653 634.7 15 -0.0003777 634.9 15 -0.0003653 635 15 -0.0003653 635.2 15 -0.0003653 635.4 15 -0.0003653 635.5 15 -0.0003653 635.7 15 -0.0003653 635.8 15 -0.0003777 636 15 -0.0003653 636.2 15 -0.0003653 636.3 15 -0.0003653 636.5 15 -0.0003653 636.6 15 -0.0003777 636.8 15 -0.0003901 637 15 -0.0003901 637.1 15 -0.0003901 637.3 15 -0.0004025 637.4 15 -0.0004148 637.6 15 -0.0004148 637.8 15 -0.0004148 637.9 15 -0.0004148 638.1 15 -0.0004148 638.3 15 -0.0004272 638.4 14 -0.0004396 638.6 15 -0.0004272 638.7 15 -0.0004272 638.9 15 -0.0004396 639.1 15 -0.000452 639.2 14 -0.0004644 639.4 14 -0.0004644 639.5 14 -0.0004644 639.7 14 -0.0004644 639.9 14 -0.000452 640 14 -0.0004644 640.2 14 -0.0004644 640.3 14 -0.0004644 640.5 14 -0.0004644 640.7 14 -0.0004891 640.8 14 -0.0004891 641 14 -0.0005139 641.2 13 -0.0005139 641.3 14 -0.0005139 641.5 14 -0.0005263 641.6 13 -0.0005139 641.8 13 -0.0005015 642 13 -0.0004891 642.1 13 -0.0004891 642.3 13 -0.0004891 642.4 13 -0.0004768 642.6 13 -0.0004891 642.8 13 -0.0005015 642.9 13 -0.0005139 643.1 13 -0.0005139 643.2 13 -0.0005263 643.4 13 -0.0005263 643.6 13 -0.0005139 643.7 13 -0.0005015 643.9 13 -0.0005139 644.1 13 -0.0005263 644.2 13 -0.0005387 644.4 13 -0.0005634 644.5 13 -0.0005511 644.7 13 -0.0005387 644.9 13 -0.0005387 645 13 -0.0005387 645.2 13 -0.0005263 645.3 13 -0.0005263 645.5 13 -0.0005387 645.7 13 -0.0005511 645.8 13 -0.0005634 646 13 -0.0005634 646.1 13 -0.0005387 646.3 13 -0.0005634 646.5 13 -0.0005634 646.6 13 -0.0005387 646.8 13 -0.0005387 647 13 -0.0005263 647.1 13 -0.0005263 647.3 13 -0.0005263 647.4 13 -0.0005387 647.6 13 -0.0005263 647.8 13 -0.0005263 647.9 13 -0.0005263 648.1 14 -0.0005263 648.2 13 -0.0005387 648.4 13 -0.0005634 648.6 13 -0.0005634 648.7 13 -0.0005634 648.9 13 -0.0005634 649 13 -0.0005758 649.2 13 -0.0005758 649.4 13 -0.0005758 649.5 13 -0.0005758 649.7 13 -0.0005758 649.9 13 -0.0005758 650 13 -0.0005511 650.2 13 -0.0005387 650.3 13 -0.0005387 650.5 13 -0.0005511 650.7 13 -0.0005882 650.8 13 -0.000613 651 13 -0.0006377 651.1 13 -0.0006625 651.3 13 -0.0006873 651.5 13 -0.0006873 651.6 13 -0.0006873 651.8 13 -0.000712 651.9 13 -0.0007244 652.1 13 -0.000712 652.3 13 -0.0006997 652.4 13 -0.0006501 652.6 13 -0.000613 652.8 13 -0.0005758 652.9 13 -0.0005758 653.1 13 -0.0005882 653.2 13 -0.0006006 653.4 13 -0.000613 653.6 13 -0.000613 653.7 13 -0.0006006 653.9 13 -0.000613 654 13 -0.0006254 654.2 13 -0.000613 654.4 13 -0.0006254 654.5 13 -0.0006254 654.7 13 -0.0006254 654.8 13 -0.0006377 655 12 -0.0006254 655.2 12 -0.000613 655.3 13 -0.0006006 655.5 13 -0.0005882 655.7 13 -0.0005882 655.8 12 -0.0005882 656 13 -0.0005882 656.1 12 -0.0005882 656.3 13 -0.0005882 656.5 13 -0.0005758 656.6 12 -0.0005634 656.8 13 -0.0005634 656.9 12 -0.0005758 657.1 12 -0.0005758 657.3 12 -0.0005634 657.4 13 -0.0005634 657.6 13 -0.0005882 657.7 12 -0.0006006 657.9 13 -0.000613 658.1 13 -0.0005882 658.2 12 -0.0005758 658.4 12 -0.0005634 658.6 12 -0.0005758 658.7 13 -0.0005882 658.9 12 -0.0005882 659 13 -0.0006006 659.2 12 -0.0005634 659.4 16 0.21 0.05 0.66 0.002 0.007 0.75 2.11 0.83 0.31 0 0.62 0 0 0 6 6.184e-06 0 8 6.184e-06 0.1245 8 6.184e-06 0.249 8 -1.855e-05 0.3735 8 -3.092e-05 0.4981 8 -4.329e-05 0.6226 9 -5.565e-05 0.7471 9 -6.802e-05 0.8716 9 -6.802e-05 0.9961 9 -3.092e-05 1.121 9 6.184e-06 1.245 9 6.184e-06 1.37 9 6.184e-06 1.494 10 6.184e-06 1.619 11 6.184e-06 1.743 12 6.184e-06 1.868 14 6.184e-06 1.992 16 6.184e-06 2.117 18 6.184e-06 2.241 20 6.184e-06 2.366 23 6.184e-06 2.49 25 1.855e-05 2.615 27 5.565e-05 2.739 30 8.039e-05 2.864 34 0.0001299 2.988 36 0.000167 3.113 39 0.0002041 3.237 41 0.0002288 3.362 45 0.0002535 3.486 48 0.0002535 3.611 50 0.0002906 3.735 52 0.0003277 3.86 55 0.0003772 3.984 59 0.0004267 4.109 61 0.0004762 4.233 63 0.0005009 4.358 66 0.000538 4.482 68 0.0005627 4.607 71 0.0005998 4.731 73 0.0006246 4.856 75 0.0006369 4.981 78 0.0006493 5.105 81 0.000674 5.23 83 0.0007111 5.354 85 0.0007606 5.479 87 0.0007977 5.603 90 0.0008225 5.728 91 0.0008472 5.852 93 0.0008719 5.977 95 0.0008967 6.101 98 0.0009214 6.226 99 0.0009461 6.35 102 0.0009585 6.475 104 0.0009709 6.599 106 0.00102 6.724 108 0.001045 6.848 109 0.001057 6.973 112 0.001082 7.097 113 0.001107 7.222 115 0.001144 7.346 117 0.001156 7.471 119 0.001181 7.595 121 0.001206 7.72 123 0.001218 7.844 126 0.001243 7.969 127 0.00128 8.093 130 0.001317 8.218 131 0.001342 8.342 134 0.001354 8.467 135 0.001379 8.591 137 0.001379 8.716 139 0.001391 8.84 141 0.001416 8.965 143 0.001441 9.089 145 0.001453 9.214 146 0.001503 9.338 149 0.00154 9.463 151 0.001589 9.588 152 0.001614 9.712 155 0.001639 9.837 157 0.001651 9.961 159 0.001639 10.09 161 0.001639 10.21 163 0.001639 10.33 165 0.001651 10.46 167 0.001688 10.58 168 0.001713 10.71 171 0.001787 10.83 173 0.001837 10.96 174 0.001837 11.08 177 0.001849 11.21 179 0.001849 11.33 181 0.001837 11.46 183 0.001886 11.58 184 0.001911 11.7 187 0.001948 11.83 188 0.001985 11.95 190 0.001985 12.08 192 0.00201 12.2 194 0.002034 12.33 196 0.002034 12.45 199 0.002059 12.58 201 0.002084 12.7 202 0.002096 12.82 204 0.002109 12.95 206 0.002133 13.07 208 0.002146 13.2 209 0.002183 13.32 212 0.00222 13.45 214 0.002245 13.57 217 0.002269 13.7 218 0.002307 13.82 220 0.002331 13.95 221 0.002356 14.07 224 0.002368 14.19 226 0.002368 14.32 227 0.002393 14.44 231 0.00243 14.57 232 0.002467 14.69 234 0.002504 14.82 237 0.002529 14.94 238 0.002554 15.07 240 0.002591 15.19 243 0.002628 15.32 245 0.002641 15.44 246 0.002678 15.56 248 0.002702 15.69 251 0.002727 15.81 252 0.002752 15.94 255 0.002777 16.06 256 0.002801 16.19 259 0.002801 16.31 261 0.002826 16.44 263 0.002826 16.56 265 0.002851 16.68 267 0.002875 16.81 269 0.002913 16.93 271 0.002937 17.06 273 0.002962 17.18 274 0.002987 17.31 277 0.002999 17.43 279 0.002999 17.56 281 0.002999 17.68 282 0.003024 17.81 285 0.003073 17.93 287 0.00311 18.05 289 0.003172 18.18 292 0.003197 18.3 293 0.003222 18.43 295 0.003234 18.55 297 0.003271 18.68 299 0.003296 18.8 301 0.003333 18.93 302 0.003383 19.05 305 0.003395 19.18 307 0.003432 19.3 309 0.003444 19.42 311 0.003469 19.55 313 0.003494 19.67 315 0.003506 19.8 317 0.003531 19.92 319 0.003568 20.05 321 0.003593 20.17 323 0.00363 20.3 325 0.003667 20.42 328 0.003692 20.54 329 0.003729 20.67 331 0.003754 20.79 334 0.003778 20.92 335 0.003815 21.04 337 0.003853 21.17 339 0.003877 21.29 342 0.00389 21.42 343 0.003927 21.54 345 0.003951 21.67 347 0.003964 21.79 349 0.003989 21.91 352 0.004013 22.04 353 0.004038 22.16 356 0.004063 22.29 357 0.004075 22.41 359 0.0041 22.54 362 0.004112 22.66 363 0.004137 22.79 365 0.004162 22.91 367 0.004199 23.03 369 0.004236 23.16 371 0.004285 23.28 374 0.004335 23.41 376 0.00436 23.53 378 0.004372 23.66 379 0.00436 23.78 381 0.004372 23.91 384 0.004409 24.03 385 0.004421 24.16 388 0.004434 24.28 390 0.004471 24.4 392 0.004496 24.53 393 0.00452 24.65 396 0.004557 24.78 397 0.004607 24.9 399 0.004632 25.03 401 0.004669 25.15 403 0.004706 25.28 405 0.004731 25.4 406 0.004768 25.53 409 0.004805 25.65 410 0.00483 25.77 412 0.004867 25.9 414 0.004904 26.02 417 0.004941 26.15 418 0.004966 26.27 420 0.004978 26.4 422 0.00499 26.52 424 0.005015 26.65 427 0.00504 26.77 428 0.005077 26.89 430 0.005102 27.02 432 0.005139 27.14 434 0.005151 27.27 437 0.005201 27.39 438 0.005225 27.52 440 0.005275 27.64 442 0.0053 27.77 444 0.005337 27.89 446 0.005361 28.02 448 0.005386 28.14 450 0.005399 28.26 453 0.005411 28.39 454 0.005423 28.51 456 0.005473 28.64 459 0.00551 28.76 460 0.005535 28.89 462 0.005559 29.01 465 0.005609 29.14 467 0.005646 29.26 468 0.005671 29.39 471 0.005695 29.51 472 0.005732 29.63 474 0.00577 29.76 477 0.005807 29.88 478 0.005856 30.01 481 0.005881 30.13 482 0.00593 30.26 485 0.005967 30.38 487 0.006005 30.51 489 0.006029 30.63 491 0.006054 30.75 492 0.006066 30.88 494 0.006079 31 497 0.006116 31.13 499 0.006153 31.25 501 0.00619 31.38 503 0.006227 31.5 504 0.006264 31.63 506 0.006301 31.75 509 0.006301 31.88 510 0.006351 32 512 0.006363 32.12 515 0.0064 32.25 517 0.006437 32.37 518 0.006474 32.5 521 0.006512 32.62 523 0.006536 32.75 524 0.006561 32.87 527 0.006586 33 528 0.006598 33.12 531 0.006635 33.24 532 0.00666 33.37 534 0.006709 33.49 537 0.006722 33.62 539 0.006759 33.74 540 0.006784 33.87 542 0.006808 33.99 545 0.006833 34.12 546 0.006895 34.24 549 0.006932 34.37 551 0.006957 34.49 553 0.006969 34.61 554 0.007006 34.74 557 0.007031 34.86 559 0.007068 34.99 561 0.007093 35.11 562 0.007142 35.24 565 0.007155 35.36 567 0.007192 35.49 568 0.007204 35.61 571 0.007229 35.74 573 0.007266 35.86 574 0.007291 35.98 577 0.007303 36.11 578 0.00734 36.23 581 0.007353 36.36 583 0.007402 36.48 585 0.007414 36.61 587 0.007452 36.73 589 0.007501 36.86 591 0.00755 36.98 593 0.007575 37.1 595 0.0076 37.23 596 0.007625 37.35 599 0.007649 37.48 601 0.007687 37.6 603 0.007699 37.73 604 0.007736 37.85 606 0.007773 37.98 609 0.007823 38.1 610 0.00786 38.23 612 0.007922 38.35 614 0.007983 38.47 617 0.008045 38.6 618 0.008082 38.72 621 0.008132 38.85 622 0.008144 38.97 625 0.008144 39.1 626 0.008119 39.22 628 0.008132 39.35 631 0.008144 39.47 632 0.008169 39.6 634 0.008194 39.72 636 0.008231 39.84 639 0.008255 39.97 640 0.008305 40.09 643 0.00833 40.22 644 0.008354 40.34 646 0.008379 40.47 649 0.008416 40.59 650 0.008441 40.72 653 0.008503 40.84 655 0.00854 40.96 656 0.008577 41.09 659 0.008602 41.21 660 0.008626 41.34 662 0.008639 41.46 665 0.008676 41.59 667 0.008688 41.71 668 0.008738 41.84 671 0.008763 41.96 672 0.008787 42.09 675 0.008824 42.21 677 0.008849 42.33 678 0.008874 42.46 681 0.008923 42.58 683 0.008936 42.71 685 0.00896 42.83 687 0.008985 42.96 689 0.009022 43.08 691 0.009047 43.21 693 0.009084 43.33 695 0.009134 43.46 696 0.009158 43.58 699 0.009195 43.7 701 0.00922 43.83 703 0.009245 43.95 704 0.009282 44.08 707 0.009307 44.2 709 0.009331 44.33 711 0.009356 44.45 712 0.009381 44.58 714 0.009418 44.7 717 0.009443 44.82 718 0.00948 44.95 720 0.009505 45.07 721 0.009542 45.2 724 0.009579 45.32 726 0.009604 45.45 728 0.009628 45.57 729 0.009665 45.7 730 0.009678 45.82 731 0.009702 45.95 733 0.009715 46.07 734 0.009752 46.19 736 0.009777 46.32 737 0.009814 46.44 739 0.009839 46.57 740 0.009876 46.69 742 0.009888 46.82 743 0.009937 46.94 745 0.009975 47.07 746 0.01002 47.19 748 0.01007 47.31 749 0.01011 47.44 750 0.01016 47.56 751 0.01018 47.69 753 0.01022 47.81 753 0.01026 47.94 754 0.0103 48.06 755 0.01036 48.19 756 0.01041 48.31 757 0.01044 48.44 759 0.01048 48.56 760 0.01052 48.68 761 0.01056 48.81 763 0.01062 48.93 765 0.01064 49.06 767 0.01068 49.18 769 0.01072 49.31 771 0.01077 49.43 775 0.01083 49.56 777 0.01088 49.68 780 0.01095 49.81 782 0.01103 49.93 786 0.0111 50.05 788 0.01114 50.18 791 0.0112 50.3 793 0.01125 50.43 796 0.0113 50.55 800 0.01135 50.68 801 0.01141 50.8 801 0.01145 50.93 803 0.01152 51.05 806 0.01156 51.17 808 0.01161 51.3 810 0.01164 51.42 812 0.01168 51.55 814 0.01169 51.67 817 0.01169 51.8 818 0.01169 51.92 821 0.01164 52.05 822 0.01159 52.17 825 0.0115 52.3 828 0.01141 52.42 830 0.01127 52.54 833 0.01116 52.67 836 0.011 52.79 839 0.01085 52.92 843 0.01068 53.04 846 0.01051 53.17 849 0.01033 53.29 853 0.01018 53.42 856 0.01002 53.54 859 0.0099 53.67 862 0.009789 53.79 865 0.009702 53.91 868 0.009616 54.04 870 0.009554 54.16 873 0.009517 54.29 875 0.009505 54.41 878 0.009505 54.54 880 0.009529 54.66 882 0.009529 54.79 884 0.009554 54.91 886 0.009566 55.03 889 0.009591 55.16 890 0.009628 55.28 892 0.009665 55.41 893 0.009678 55.53 896 0.009702 55.66 897 0.009727 55.78 898 0.009727 55.91 900 0.009752 56.03 901 0.009789 56.16 903 0.009826 56.28 904 0.009863 56.4 906 0.009888 56.53 907 0.009925 56.65 909 0.009962 56.78 911 0.01002 56.9 912 0.01006 57.03 914 0.01011 57.15 915 0.01015 57.28 917 0.01021 57.4 918 0.01026 57.53 920 0.01032 57.65 922 0.01038 57.77 923 0.01042 57.9 925 0.01047 58.02 927 0.01053 58.15 929 0.01057 58.27 931 0.01061 58.4 932 0.01065 58.52 934 0.01068 58.65 936 0.01072 58.77 938 0.01075 58.89 940 0.01078 59.02 942 0.01083 59.14 943 0.01089 59.27 946 0.01095 59.39 948 0.01103 59.52 950 0.01109 59.64 951 0.01116 59.77 954 0.01122 59.89 956 0.01131 60.02 958 0.01138 60.14 960 0.01143 60.26 962 0.01151 60.39 964 0.01152 60.51 966 0.01152 60.64 968 0.01156 60.76 970 0.01159 60.89 972 0.01166 61.01 975 0.01172 61.14 976 0.01178 61.26 979 0.01184 61.38 981 0.0119 61.51 983 0.01195 61.63 984 0.01202 61.76 986 0.01206 61.88 989 0.01213 62.01 990 0.01215 62.13 993 0.0122 62.26 996 0.01225 62.38 997 0.0123 62.51 998 0.01234 62.63 1001 0.01239 62.75 1003 0.01242 62.88 1004 0.01249 63 1006 0.01253 63.13 1008 0.0126 63.25 1011 0.01265 63.38 1012 0.01267 63.5 1015 0.0127 63.63 1017 0.01274 63.75 1018 0.01282 63.88 1021 0.01288 64 1023 0.01292 64.12 1025 0.01293 64.25 1026 0.01294 64.37 1028 0.01299 64.5 1031 0.01304 64.62 1033 0.01312 64.75 1035 0.01318 64.87 1036 0.01324 65 1039 0.01329 65.12 1040 0.01334 65.24 1043 0.01339 65.37 1044 0.01344 65.49 1047 0.01349 65.62 1049 0.01354 65.74 1050 0.01361 65.87 1053 0.01366 65.99 1054 0.01372 66.12 1057 0.01376 66.24 1059 0.01381 66.37 1061 0.01385 66.49 1062 0.0139 66.61 1065 0.01396 66.74 1067 0.01401 66.86 1068 0.01407 66.99 1071 0.01413 67.11 1072 0.01417 67.24 1075 0.01422 67.36 1078 0.01425 67.49 1079 0.01432 67.61 1081 0.01435 67.74 1083 0.0144 67.86 1085 0.01444 67.98 1087 0.01448 68.11 1089 0.01453 68.23 1091 0.01458 68.36 1094 0.01462 68.48 1095 0.01469 68.61 1097 0.01475 68.73 1099 0.01481 68.86 1101 0.01485 68.98 1103 0.01491 69.1 1105 0.01493 69.23 1107 0.01498 69.35 1109 0.01502 69.48 1111 0.01506 69.6 1113 0.01511 69.73 1115 0.01518 69.85 1117 0.01521 69.98 1119 0.01527 70.1 1122 0.01532 70.23 1123 0.01537 70.35 1125 0.01542 70.47 1128 0.01545 70.6 1129 0.01552 70.72 1131 0.01556 70.85 1133 0.01561 70.97 1135 0.01566 71.1 1137 0.01571 71.22 1140 0.01575 71.35 1142 0.0158 71.47 1144 0.01585 71.59 1145 0.0159 71.72 1147 0.01596 71.84 1150 0.01601 71.97 1151 0.01603 72.09 1154 0.01611 72.22 1155 0.01616 72.34 1158 0.01621 72.47 1159 0.01624 72.59 1162 0.01631 72.72 1164 0.01636 72.84 1165 0.01641 72.96 1168 0.01646 73.09 1169 0.0165 73.21 1172 0.01657 73.34 1173 0.01663 73.46 1176 0.01668 73.59 1178 0.01671 73.71 1179 0.01675 73.84 1181 0.01679 73.96 1184 0.01683 74.09 1186 0.0169 74.21 1187 0.01695 74.33 1190 0.017 74.46 1192 0.01709 74.58 1194 0.01715 74.71 1196 0.0172 74.83 1198 0.01727 74.96 1200 0.01728 75.08 1201 0.01733 75.21 1201 0.01737 75.33 1202 0.01738 75.45 1203 0.01741 75.58 1204 0.01744 75.7 1204 0.01747 75.83 1204 0.01747 75.95 1204 0.01747 76.08 1205 0.01747 76.2 1205 0.01744 76.33 1205 0.01743 76.45 1205 0.01743 76.58 1205 0.01742 76.7 1205 0.01741 76.82 1205 0.0174 76.95 1204 0.01738 77.07 1204 0.01736 77.2 1204 0.01736 77.32 1204 0.01736 77.45 1204 0.01736 77.57 1203 0.01738 77.7 1203 0.01738 77.82 1203 0.01738 77.95 1203 0.01738 78.07 1201 0.01737 78.19 1201 0.01736 78.32 1201 0.01735 78.44 1201 0.01732 78.57 1201 0.01728 78.69 1201 0.01726 78.82 1201 0.01725 78.94 1200 0.01726 79.07 1200 0.01726 79.19 1200 0.01728 79.31 1200 0.01727 79.44 1199 0.01728 79.56 1200 0.01728 79.69 1199 0.01727 79.81 1199 0.01726 79.94 1199 0.01726 80.06 1198 0.01725 80.19 1199 0.01725 80.31 1198 0.01725 80.44 1199 0.01722 80.56 1198 0.01722 80.68 1198 0.01722 80.81 1198 0.01722 80.93 1198 0.01723 81.06 1198 0.01725 81.18 1198 0.01725 81.31 1198 0.01725 81.43 1198 0.01725 81.56 1198 0.01727 81.68 1198 0.01727 81.81 1198 0.01727 81.93 1198 0.01728 82.05 1198 0.01727 82.18 1198 0.01727 82.3 1198 0.01725 82.43 1199 0.01723 82.55 1198 0.01722 82.68 1198 0.01721 82.8 1198 0.01722 82.93 1199 0.01722 83.05 1199 0.01723 83.17 1199 0.01723 83.3 1199 0.01722 83.42 1199 0.01723 83.55 1199 0.01725 83.67 1199 0.01723 83.8 1199 0.01725 83.92 1199 0.01725 84.05 1199 0.01723 84.17 1199 0.01723 84.3 1199 0.01725 84.42 1199 0.01726 84.54 1199 0.01726 84.67 1199 0.01726 84.79 1199 0.01725 84.92 1199 0.01725 85.04 1199 0.01727 85.17 1199 0.01727 85.29 1199 0.01728 85.42 1199 0.01728 85.54 1199 0.01728 85.66 1199 0.01728 85.79 1200 0.0173 85.91 1199 0.01728 86.04 1199 0.01728 86.16 1200 0.01727 86.29 1199 0.01727 86.41 1199 0.01725 86.54 1200 0.01725 86.66 1199 0.01725 86.79 1199 0.01725 86.91 1199 0.01725 87.03 1199 0.01725 87.16 1200 0.01725 87.28 1199 0.01723 87.41 1199 0.01725 87.53 1199 0.01725 87.66 1199 0.01725 87.78 1199 0.01727 87.91 1199 0.01727 88.03 1199 0.01727 88.16 1199 0.0173 88.28 1199 0.0173 88.4 1199 0.0173 88.53 1199 0.01728 88.65 1199 0.01726 88.78 1199 0.01725 88.9 1199 0.01725 89.03 1199 0.01725 89.15 1199 0.01725 89.28 1199 0.01725 89.4 1199 0.01725 89.52 1199 0.01725 89.65 1199 0.01725 89.77 1199 0.01726 89.9 1199 0.01728 90.02 1199 0.01727 90.15 1199 0.01727 90.27 1199 0.01726 90.4 1199 0.01725 90.52 1199 0.01725 90.65 1199 0.01723 90.77 1199 0.01722 90.89 1199 0.01723 91.02 1199 0.01723 91.14 1199 0.01723 91.27 1199 0.01723 91.39 1199 0.01721 91.52 1199 0.0172 91.64 1199 0.01721 91.77 1199 0.01721 91.89 1199 0.0172 92.02 1199 0.0172 92.14 1199 0.0172 92.26 1199 0.0172 92.39 1199 0.0172 92.51 1199 0.0172 92.64 1199 0.0172 92.76 1199 0.01718 92.89 1199 0.01717 93.01 1199 0.01716 93.14 1198 0.01716 93.26 1199 0.01715 93.38 1199 0.01715 93.51 1199 0.01715 93.63 1199 0.01714 93.76 1200 0.01712 93.88 1199 0.01714 94.01 1199 0.01715 94.13 1199 0.01715 94.26 1199 0.01715 94.38 1199 0.01714 94.51 1199 0.01712 94.63 1199 0.0171 94.75 1199 0.01712 94.88 1199 0.01715 95 1199 0.01715 95.13 1199 0.01715 95.25 1199 0.01715 95.38 1199 0.01714 95.5 1199 0.01715 95.63 1199 0.01716 95.75 1199 0.01715 95.88 1199 0.01714 96 1199 0.01712 96.12 1199 0.01711 96.25 1199 0.01711 96.37 1199 0.0171 96.5 1199 0.0171 96.62 1199 0.0171 96.75 1199 0.0171 96.87 1199 0.0171 97 1199 0.01712 97.12 1199 0.01714 97.24 1200 0.01712 97.37 1199 0.01711 97.49 1199 0.0171 97.62 1199 0.0171 97.74 1199 0.01709 97.87 1198 0.01707 97.99 1199 0.01706 98.12 1199 0.01706 98.24 1199 0.01706 98.37 1199 0.01707 98.49 1199 0.0171 98.61 1199 0.0171 98.74 1199 0.0171 98.86 1199 0.01709 98.99 1199 0.01707 99.11 1199 0.01707 99.24 1199 0.01707 99.36 1199 0.01709 99.49 1199 0.0171 99.61 1199 0.0171 99.73 1199 0.01711 99.86 1199 0.01711 99.98 1199 0.0171 100.1 1199 0.0171 100.2 1199 0.01707 100.4 1199 0.0171 100.5 1199 0.01712 100.6 1199 0.01712 100.7 1199 0.0171 100.9 1199 0.0171 101 1199 0.01709 101.1 1199 0.01707 101.2 1199 0.01709 101.4 1199 0.01707 101.5 1199 0.01709 101.6 1199 0.01707 101.7 1199 0.01706 101.9 1199 0.01705 102 1199 0.01705 102.1 1199 0.01706 102.2 1199 0.01706 102.3 1199 0.01707 102.5 1199 0.01709 102.6 1199 0.01707 102.7 1199 0.01709 102.8 1199 0.01709 103 1199 0.01707 103.1 1199 0.01709 103.2 1199 0.01709 103.3 1199 0.01709 103.5 1199 0.01709 103.6 1199 0.01707 103.7 1199 0.01706 103.8 1199 0.01706 104 1199 0.01705 104.1 1199 0.01706 104.2 1199 0.01706 104.3 1199 0.01705 104.5 1199 0.01705 104.6 1199 0.01706 104.7 1199 0.01707 104.8 1199 0.01707 105 1199 0.01709 105.1 1199 0.0171 105.2 1199 0.0171 105.3 1199 0.0171 105.5 1199 0.01709 105.6 1199 0.01707 105.7 1199 0.01705 105.8 1199 0.01704 106 1199 0.01701 106.1 1199 0.01699 106.2 1199 0.01697 106.3 1199 0.01697 106.5 1199 0.01697 106.6 1199 0.01697 106.7 1199 0.017 106.8 1199 0.01702 107 1199 0.01704 107.1 1199 0.01705 107.2 1199 0.01705 107.3 1199 0.01705 107.5 1199 0.01704 107.6 1199 0.01702 107.7 1199 0.01701 107.8 1199 0.01704 108 1199 0.01704 108.1 1199 0.01702 108.2 1200 0.01704 108.3 1199 0.01704 108.5 1199 0.01701 108.6 1199 0.01701 108.7 1199 0.01702 108.8 1199 0.01702 108.9 1199 0.01702 109.1 1199 0.01704 109.2 1199 0.01701 109.3 1199 0.01701 109.4 1199 0.01702 109.6 1199 0.01701 109.7 1199 0.01701 109.8 1199 0.01701 109.9 1199 0.017 110.1 1199 0.017 110.2 1199 0.01702 110.3 1199 0.017 110.4 1199 0.017 110.6 1199 0.017 110.7 1199 0.017 110.8 1199 0.017 110.9 1199 0.017 111.1 1199 0.017 111.2 1199 0.01699 111.3 1199 0.01699 111.4 1199 0.01699 111.6 1199 0.01699 111.7 1199 0.01699 111.8 1199 0.017 111.9 1199 0.01699 112.1 1199 0.01699 112.2 1199 0.01701 112.3 1199 0.01699 112.4 1199 0.01697 112.6 1199 0.01697 112.7 1199 0.01695 112.8 1199 0.01695 112.9 1199 0.01695 113.1 1199 0.01695 113.2 1199 0.01696 113.3 1199 0.01697 113.4 1199 0.01697 113.6 1199 0.01696 113.7 1199 0.01695 113.8 1200 0.01696 113.9 1199 0.01696 114.1 1199 0.01696 114.2 1199 0.01695 114.3 1199 0.01695 114.4 1199 0.01695 114.6 1199 0.01695 114.7 1199 0.01695 114.8 1199 0.01695 114.9 1199 0.01694 115.1 1199 0.01695 115.2 1199 0.01694 115.3 1199 0.01694 115.4 1199 0.01694 115.5 1199 0.01694 115.7 1199 0.01694 115.8 1199 0.01695 115.9 1199 0.01695 116 1199 0.01696 116.2 1199 0.01696 116.3 1200 0.01695 116.4 1199 0.01695 116.5 1199 0.01693 116.7 1199 0.01693 116.8 1199 0.01693 116.9 1200 0.01694 117 1199 0.01693 117.2 1199 0.01693 117.3 1199 0.01691 117.4 1199 0.0169 117.5 1199 0.0169 117.7 1199 0.0169 117.8 1199 0.01693 117.9 1199 0.01691 118 1199 0.01693 118.2 1199 0.01693 118.3 1199 0.01693 118.4 1199 0.01693 118.5 1199 0.01694 118.7 1199 0.01693 118.8 1199 0.01693 118.9 1199 0.01693 119 1199 0.0169 119.2 1199 0.01691 119.3 1199 0.01693 119.4 1199 0.01693 119.5 1199 0.01693 119.7 1199 0.01693 119.8 1199 0.01693 119.9 1199 0.01691 120 1199 0.01691 120.2 1199 0.01691 120.3 1199 0.01691 120.4 1199 0.01691 120.5 1199 0.01693 120.7 1199 0.01691 120.8 1199 0.0169 120.9 1199 0.0169 121 1199 0.0169 121.2 1199 0.01689 121.3 1199 0.0169 121.4 1199 0.01689 121.5 1199 0.01689 121.6 1199 0.01689 121.8 1199 0.01689 121.9 1199 0.01689 122 1199 0.01688 122.1 1199 0.01689 122.3 1199 0.01689 122.4 1199 0.01689 122.5 1199 0.01689 122.6 1199 0.01686 122.8 1199 0.01685 122.9 1199 0.01685 123 1199 0.01685 123.1 1199 0.01684 123.3 1199 0.01685 123.4 1199 0.01685 123.5 1199 0.01688 123.6 1199 0.0169 123.8 1200 0.01691 123.9 1199 0.01693 124 1199 0.01696 124.1 1199 0.01699 124.3 1199 0.01696 124.4 1199 0.01696 124.5 1199 0.01693 124.6 1199 0.0169 124.8 1199 0.01688 124.9 1199 0.01685 125 1199 0.01684 125.1 1198 0.01683 125.3 1199 0.01683 125.4 1199 0.01683 125.5 1199 0.01683 125.6 1199 0.01684 125.8 1199 0.01685 125.9 1199 0.01685 126 1199 0.01684 126.1 1199 0.01681 126.3 1199 0.01679 126.4 1199 0.01679 126.5 1199 0.0168 126.6 1199 0.0168 126.8 1200 0.01681 126.9 1199 0.01681 127 1199 0.01679 127.1 1199 0.01679 127.3 1199 0.0168 127.4 1199 0.0168 127.5 1199 0.01681 127.6 1199 0.01683 127.8 1199 0.01684 127.9 1199 0.01685 128 1199 0.01686 128.1 1199 0.01688 128.2 1199 0.01688 128.4 1199 0.01689 128.5 1199 0.0169 128.6 1199 0.01689 128.7 1199 0.0169 128.9 1199 0.0169 129 1199 0.0169 129.1 1199 0.0169 129.2 1199 0.0169 129.4 1199 0.0169 129.5 1199 0.01691 129.6 1199 0.01691 129.7 1199 0.0169 129.9 1199 0.0169 130 1199 0.0169 130.1 1199 0.01689 130.2 1199 0.01689 130.4 1199 0.01689 130.5 1199 0.01689 130.6 1199 0.0169 130.7 1199 0.0169 130.9 1199 0.0169 131 1199 0.0169 131.1 1199 0.0169 131.2 1199 0.01689 131.4 1199 0.01689 131.5 1199 0.01689 131.6 1199 0.01688 131.7 1199 0.01686 131.9 1199 0.01688 132 1199 0.01688 132.1 1199 0.01689 132.2 1199 0.0169 132.4 1198 0.01689 132.5 1199 0.01688 132.6 1199 0.01685 132.7 1199 0.01685 132.9 1199 0.01686 133 1199 0.01688 133.1 1199 0.01688 133.2 1199 0.01688 133.4 1199 0.01688 133.5 1199 0.01688 133.6 1199 0.01689 133.7 1199 0.01688 133.9 1199 0.01685 134 1199 0.01683 134.1 1199 0.01683 134.2 1199 0.0168 134.3 1199 0.0168 134.5 1199 0.0168 134.6 1199 0.0168 134.7 1199 0.01681 134.8 1199 0.01683 135 1199 0.01684 135.1 1199 0.01685 135.2 1199 0.01688 135.3 1200 0.01689 135.5 1199 0.0169 135.6 1199 0.01691 135.7 1199 0.0169 135.8 1199 0.01691 136 1199 0.01691 136.1 1199 0.0169 136.2 1199 0.0169 136.3 1199 0.0169 136.5 1199 0.0169 136.6 1199 0.01689 136.7 1200 0.01689 136.8 1199 0.01689 137 1199 0.01689 137.1 1199 0.01688 137.2 1199 0.01688 137.3 1199 0.01686 137.5 1199 0.01688 137.6 1199 0.01689 137.7 1199 0.01689 137.8 1199 0.0169 138 1199 0.0169 138.1 1199 0.0169 138.2 1199 0.01689 138.3 1199 0.0169 138.5 1199 0.01689 138.6 1199 0.01689 138.7 1199 0.01689 138.8 1199 0.01689 139 1199 0.01689 139.1 1199 0.0169 139.2 1199 0.01693 139.3 1199 0.01693 139.5 1199 0.01691 139.6 1199 0.01691 139.7 1199 0.01691 139.8 1199 0.01691 140 1199 0.01691 140.1 1199 0.0169 140.2 1199 0.01691 140.3 1199 0.01693 140.5 1199 0.01693 140.6 1199 0.01691 140.7 1199 0.01691 140.8 1199 0.0169 140.9 1199 0.0169 141.1 1199 0.0169 141.2 1199 0.01691 141.3 1199 0.01691 141.4 1199 0.01691 141.6 1199 0.01693 141.7 1199 0.01693 141.8 1199 0.01694 141.9 1199 0.01694 142.1 1199 0.01695 142.2 1199 0.01695 142.3 1199 0.01696 142.4 1199 0.01696 142.6 1199 0.01697 142.7 1199 0.01699 142.8 1200 0.01697 142.9 1199 0.01697 143.1 1199 0.01694 143.2 1199 0.01691 143.3 1200 0.01693 143.4 1199 0.01693 143.6 1200 0.01695 143.7 1199 0.01696 143.8 1199 0.01697 143.9 1199 0.01699 144.1 1200 0.01695 144.2 1199 0.01694 144.3 1199 0.01693 144.4 1200 0.01691 144.6 1199 0.01691 144.7 1200 0.01691 144.8 1199 0.01691 144.9 1199 0.01693 145.1 1199 0.01695 145.2 1199 0.01695 145.3 1200 0.01695 145.4 1199 0.01695 145.6 1199 0.01695 145.7 1199 0.01694 145.8 1200 0.01694 145.9 1199 0.01695 146.1 1200 0.01694 146.2 1199 0.01694 146.3 1199 0.01695 146.4 1199 0.01694 146.6 1199 0.01694 146.7 1199 0.01694 146.8 1199 0.01694 146.9 1200 0.01694 147 1199 0.01695 147.2 1199 0.01694 147.3 1199 0.01694 147.4 1199 0.01695 147.5 1200 0.01696 147.7 1199 0.01695 147.8 1199 0.01695 147.9 1199 0.01695 148 1199 0.01694 148.2 1199 0.01695 148.3 1199 0.01694 148.4 1199 0.01694 148.5 1200 0.01695 148.7 1199 0.01694 148.8 1199 0.01694 148.9 1199 0.01694 149 1199 0.01694 149.2 1199 0.01694 149.3 1199 0.01694 149.4 1199 0.01694 149.5 1199 0.01694 149.7 1199 0.01694 149.8 1199 0.01694 149.9 1199 0.01694 150 1199 0.01694 150.2 1199 0.01695 150.3 1199 0.01693 150.4 1199 0.01691 150.5 1199 0.01691 150.7 1199 0.0169 150.8 1199 0.0169 150.9 1199 0.01691 151 1199 0.01693 151.2 1199 0.01695 151.3 1199 0.01695 151.4 1199 0.01696 151.5 1199 0.01696 151.7 1199 0.01699 151.8 1199 0.01695 151.9 1199 0.01694 152 1199 0.01691 152.2 1199 0.0169 152.3 1199 0.01688 152.4 1199 0.01688 152.5 1200 0.01689 152.7 1199 0.01691 152.8 1199 0.01694 152.9 1199 0.01695 153 1199 0.01695 153.2 1199 0.01695 153.3 1199 0.01694 153.4 1199 0.01695 153.5 1199 0.01695 153.6 1199 0.01694 153.8 1199 0.01694 153.9 1199 0.01694 154 1199 0.01694 154.1 1199 0.01694 154.3 1199 0.01694 154.4 1200 0.01694 154.5 1199 0.01694 154.6 1199 0.01695 154.8 1199 0.01694 154.9 1199 0.01694 155 1199 0.01694 155.1 1199 0.01693 155.3 1199 0.01691 155.4 1199 0.01691 155.5 1199 0.0169 155.6 1199 0.0169 155.8 1200 0.0169 155.9 1199 0.0169 156 1199 0.0169 156.1 1199 0.01693 156.3 1199 0.01691 156.4 1199 0.0169 156.5 1199 0.0169 156.6 1199 0.0169 156.8 1199 0.0169 156.9 1199 0.0169 157 1199 0.01689 157.1 1199 0.01689 157.3 1199 0.01688 157.4 1200 0.01688 157.5 1199 0.01688 157.6 1199 0.01688 157.8 1199 0.01688 157.9 1199 0.01688 158 1199 0.01689 158.1 1199 0.0169 158.3 1199 0.0169 158.4 1199 0.01691 158.5 1199 0.01691 158.6 1199 0.0169 158.8 1199 0.0169 158.9 1199 0.0169 159 1199 0.0169 159.1 1199 0.0169 159.3 1199 0.01689 159.4 1199 0.0169 159.5 1199 0.0169 159.6 1199 0.01693 159.8 1199 0.01691 159.9 1199 0.01694 160 1199 0.01693 160.1 1200 0.01693 160.2 1199 0.01693 160.4 1199 0.01694 160.5 1199 0.01694 160.6 1199 0.01693 160.7 1199 0.01694 160.9 1199 0.01694 161 1199 0.01693 161.1 1199 0.01693 161.2 1199 0.01691 161.4 1199 0.0169 161.5 1200 0.0169 161.6 1199 0.01689 161.7 1200 0.0169 161.9 1199 0.01691 162 1199 0.0169 162.1 1199 0.0169 162.2 1199 0.0169 162.4 1200 0.01691 162.5 1200 0.01691 162.6 1199 0.01691 162.7 1200 0.0169 162.9 1199 0.01689 163 1199 0.0169 163.1 1200 0.01689 163.2 1199 0.01689 163.4 1199 0.0169 163.5 1199 0.01689 163.6 1199 0.01689 163.7 1200 0.01689 163.9 1200 0.01689 164 1199 0.01689 164.1 1199 0.01689 164.2 1199 0.01689 164.4 1199 0.01689 164.5 1199 0.01689 164.6 1199 0.01689 164.7 1199 0.0169 164.9 1200 0.01691 165 1199 0.01689 165.1 1200 0.01688 165.2 1199 0.01689 165.4 1199 0.0169 165.5 1199 0.0169 165.6 1199 0.0169 165.7 1199 0.01689 165.9 1199 0.01689 166 1199 0.01689 166.1 1199 0.01686 166.2 1199 0.01685 166.3 1199 0.01685 166.5 1199 0.01685 166.6 1200 0.01685 166.7 1199 0.01686 166.8 1199 0.01685 167 1199 0.01685 167.1 1199 0.01685 167.2 1199 0.01686 167.3 1199 0.01686 167.5 1199 0.01688 167.6 1199 0.01688 167.7 1199 0.01688 167.8 1199 0.01688 168 1200 0.01686 168.1 1199 0.01685 168.2 1199 0.01685 168.3 1199 0.01685 168.5 1199 0.01681 168.6 1199 0.01683 168.7 1200 0.01683 168.8 1198 0.01683 169 1199 0.01683 169.1 1199 0.01681 169.2 1199 0.0168 169.3 1199 0.0168 169.5 1199 0.0168 169.6 1199 0.0168 169.7 1199 0.01681 169.8 1199 0.01681 170 1199 0.01683 170.1 1199 0.01683 170.2 1199 0.01683 170.3 1199 0.01683 170.5 1199 0.01683 170.6 1199 0.01685 170.7 1199 0.01685 170.8 1199 0.01685 171 1199 0.01685 171.1 1199 0.01685 171.2 1199 0.01686 171.3 1199 0.01685 171.5 1199 0.01685 171.6 1200 0.01685 171.7 1199 0.01685 171.8 1199 0.01685 172 1199 0.01686 172.1 1199 0.01685 172.2 1199 0.01685 172.3 1199 0.01686 172.5 1199 0.01685 172.6 1199 0.01685 172.7 1199 0.01685 172.8 1199 0.01685 172.9 1199 0.01685 173.1 1199 0.01685 173.2 1199 0.01688 173.3 1199 0.01686 173.4 1199 0.01686 173.6 1199 0.01686 173.7 1199 0.01686 173.8 1199 0.01686 173.9 1199 0.01688 174.1 1199 0.01685 174.2 1199 0.01684 174.3 1199 0.01684 174.4 1199 0.01683 174.6 1199 0.01683 174.7 1199 0.01683 174.8 1200 0.01683 174.9 1199 0.01684 175.1 1199 0.01684 175.2 1199 0.01685 175.3 1199 0.01685 175.4 1199 0.01686 175.6 1199 0.01685 175.7 1199 0.01683 175.8 1199 0.01683 175.9 1199 0.01679 176.1 1199 0.01676 176.2 1199 0.01679 176.3 1199 0.01681 176.4 1199 0.01683 176.6 1199 0.01685 176.7 1199 0.01685 176.8 1199 0.01684 176.9 1199 0.01685 177.1 1199 0.01684 177.2 1199 0.01685 177.3 1199 0.01685 177.4 1199 0.01685 177.6 1199 0.01685 177.7 1199 0.01684 177.8 1199 0.01683 177.9 1199 0.01684 178.1 1199 0.01685 178.2 1199 0.01685 178.3 1200 0.01684 178.4 1199 0.01683 178.6 1199 0.01681 178.7 1199 0.01681 178.8 1199 0.01684 178.9 1199 0.01684 179 1199 0.01683 179.2 1200 0.01683 179.3 1200 0.0168 179.4 1199 0.0168 179.5 1199 0.0168 179.7 1199 0.0168 179.8 1199 0.01681 179.9 1200 0.01683 180 1199 0.01681 180.2 1199 0.0168 180.3 1199 0.01681 180.4 1199 0.0168 180.5 1200 0.01679 180.7 1199 0.0168 180.8 1199 0.01679 180.9 1199 0.01679 181 1199 0.0168 181.2 1199 0.01679 181.3 1199 0.0168 181.4 1199 0.01681 181.5 1199 0.0168 181.7 1199 0.01679 181.8 1199 0.0168 181.9 1199 0.01681 182 1199 0.01681 182.2 1199 0.01683 182.3 1200 0.01681 182.4 1199 0.0168 182.5 1199 0.01681 182.7 1199 0.01681 182.8 1200 0.01681 182.9 1200 0.01681 183 1199 0.01681 183.2 1199 0.01681 183.3 1199 0.01683 183.4 1199 0.01681 183.5 1199 0.01681 183.7 1199 0.01681 183.8 1199 0.01681 183.9 1199 0.01681 184 1199 0.0168 184.2 1200 0.0168 184.3 1199 0.0168 184.4 1199 0.0168 184.5 1199 0.01679 184.7 1199 0.01679 184.8 1199 0.0168 184.9 1199 0.01681 185 1199 0.01681 185.2 1199 0.01683 185.3 1199 0.01681 185.4 1199 0.01684 185.5 1199 0.01684 185.6 1199 0.01684 185.8 1199 0.01684 185.9 1199 0.01683 186 1199 0.01681 186.1 1200 0.01681 186.3 1199 0.01681 186.4 1200 0.01681 186.5 1199 0.01683 186.6 1199 0.01683 186.8 1199 0.01683 186.9 1199 0.01683 187 1200 0.01681 187.1 1200 0.01681 187.3 1199 0.01681 187.4 1199 0.01681 187.5 1199 0.0168 187.6 1199 0.0168 187.8 1200 0.0168 187.9 1199 0.0168 188 1199 0.01679 188.1 1200 0.01679 188.3 1199 0.01679 188.4 1200 0.01679 188.5 1199 0.01679 188.6 1199 0.01679 188.8 1200 0.01679 188.9 1199 0.01679 189 1199 0.01678 189.1 1199 0.01679 189.3 1199 0.01679 189.4 1199 0.0168 189.5 1199 0.0168 189.6 1199 0.0168 189.8 1199 0.0168 189.9 1199 0.01679 190 1199 0.01679 190.1 1199 0.01679 190.3 1199 0.01679 190.4 1199 0.0168 190.5 1199 0.0168 190.6 1199 0.0168 190.8 1199 0.0168 190.9 1199 0.0168 191 1199 0.01679 191.1 1199 0.01679 191.3 1199 0.0168 191.4 1199 0.0168 191.5 1199 0.01683 191.6 1199 0.01684 191.8 1199 0.01685 191.9 1199 0.01684 192 1199 0.01684 192.1 1199 0.01681 192.2 1199 0.01681 192.4 1199 0.01683 192.5 1200 0.01683 192.6 1199 0.0168 192.7 1199 0.0168 192.9 1199 0.01679 193 1199 0.01679 193.1 1199 0.0168 193.2 1199 0.01679 193.4 1199 0.01679 193.5 1199 0.01679 193.6 1199 0.01679 193.7 1200 0.0168 193.9 1199 0.01681 194 1200 0.0168 194.1 1199 0.0168 194.2 1199 0.0168 194.4 1199 0.01679 194.5 1199 0.0168 194.6 1199 0.01681 194.7 1200 0.0168 194.9 1199 0.0168 195 1199 0.0168 195.1 1199 0.01679 195.2 1199 0.0168 195.4 1199 0.01681 195.5 1200 0.01683 195.6 1199 0.01683 195.7 1199 0.01683 195.9 1199 0.01683 196 1199 0.0168 196.1 1199 0.0168 196.2 1199 0.01679 196.4 1199 0.01678 196.5 1199 0.01676 196.6 1199 0.01675 196.7 1199 0.01675 196.9 1199 0.01675 197 1199 0.01675 197.1 1199 0.01676 197.2 1199 0.01678 197.4 1199 0.01678 197.5 1199 0.01678 197.6 1199 0.01679 197.7 1200 0.01678 197.9 1199 0.01678 198 1199 0.01679 198.1 1199 0.01679 198.2 1199 0.01679 198.3 1199 0.01679 198.5 1199 0.01679 198.6 1199 0.01679 198.7 1199 0.01679 198.8 1199 0.01679 199 1200 0.0168 199.1 1199 0.0168 199.2 1199 0.0168 199.3 1200 0.0168 199.5 1199 0.0168 199.6 1199 0.0168 199.7 1199 0.01681 199.8 1200 0.01684 200 1199 0.01684 200.1 1199 0.0168 200.2 1199 0.0168 200.3 1199 0.01678 200.5 1200 0.01676 200.6 1200 0.0168 200.7 1199 0.01681 200.8 1199 0.01681 201 1199 0.0168 201.1 1199 0.01676 201.2 1199 0.01675 201.3 1200 0.01675 201.5 1199 0.01675 201.6 1199 0.01676 201.7 1200 0.0168 201.8 1199 0.0168 202 1199 0.0168 202.1 1199 0.01683 202.2 1199 0.01681 202.3 1199 0.0168 202.5 1199 0.0168 202.6 1199 0.0168 202.7 1199 0.01679 202.8 1199 0.0168 203 1200 0.01678 203.1 1199 0.01676 203.2 1200 0.01676 203.3 1199 0.01676 203.5 1199 0.01678 203.6 1200 0.01679 203.7 1199 0.01679 203.8 1199 0.01678 204 1199 0.0168 204.1 1199 0.0168 204.2 1199 0.0168 204.3 1199 0.01683 204.5 1199 0.01681 204.6 1199 0.0168 204.7 1199 0.0168 204.8 1199 0.01679 204.9 1199 0.0168 205.1 1199 0.01681 205.2 1199 0.01683 205.3 1199 0.01683 205.4 1200 0.01683 205.6 1199 0.01683 205.7 1199 0.01681 205.8 1199 0.01681 205.9 1199 0.01681 206.1 1200 0.01681 206.2 1199 0.01683 206.3 1199 0.01683 206.4 1199 0.01681 206.6 1199 0.0168 206.7 1199 0.01681 206.8 1199 0.01681 206.9 1199 0.01683 207.1 1199 0.01683 207.2 1199 0.01683 207.3 1200 0.01683 207.4 1199 0.01681 207.6 1199 0.01681 207.7 1199 0.01683 207.8 1199 0.01681 207.9 1199 0.0168 208.1 1199 0.01681 208.2 1199 0.01681 208.3 1200 0.01681 208.4 1199 0.01683 208.6 1199 0.01683 208.7 1199 0.01684 208.8 1199 0.01683 208.9 1199 0.01681 209.1 1199 0.0168 209.2 1199 0.0168 209.3 1199 0.0168 209.4 1199 0.01681 209.6 1199 0.01684 209.7 1199 0.01685 209.8 1199 0.01685 209.9 1199 0.01688 210.1 1199 0.01686 210.2 1199 0.01688 210.3 1199 0.01689 210.4 1199 0.01688 210.6 1199 0.01688 210.7 1199 0.01689 210.8 1199 0.01688 210.9 1199 0.01689 211 1199 0.0169 211.2 1199 0.0169 211.3 1199 0.0169 211.4 1199 0.0169 211.5 1199 0.0169 211.7 1199 0.01689 211.8 1199 0.01688 211.9 1199 0.01686 212 1199 0.01683 212.2 1199 0.0168 212.3 1199 0.01683 212.4 1199 0.01683 212.5 1199 0.01684 212.7 1199 0.01685 212.8 1199 0.01686 212.9 1199 0.01686 213 1199 0.01688 213.2 1199 0.01688 213.3 1199 0.01688 213.4 1199 0.01689 213.5 1199 0.01689 213.7 1199 0.01688 213.8 1199 0.01689 213.9 1199 0.01689 214 1199 0.01689 214.2 1199 0.0169 214.3 1199 0.0169 214.4 1199 0.0169 214.5 1200 0.0169 214.7 1199 0.01689 214.8 1199 0.01688 214.9 1200 0.01688 215 1199 0.01685 215.2 1199 0.01685 215.3 1199 0.01688 215.4 1199 0.01688 215.5 1199 0.01688 215.7 1199 0.01688 215.8 1199 0.01688 215.9 1200 0.01689 216 1199 0.0169 216.2 1199 0.0169 216.3 1199 0.0169 216.4 1200 0.0169 216.5 1200 0.0169 216.7 1199 0.01689 216.8 1199 0.01689 216.9 1199 0.0169 217 1199 0.0169 217.2 1199 0.01691 217.3 1200 0.01691 217.4 1199 0.0169 217.5 1199 0.01688 217.6 1199 0.01688 217.8 1199 0.01688 217.9 1199 0.0169 218 1200 0.01693 218.1 1199 0.01694 218.3 1199 0.01695 218.4 1199 0.01695 218.5 1199 0.01695 218.6 1200 0.01693 218.8 1199 0.01693 218.9 1200 0.01693 219 1200 0.01693 219.1 1199 0.01694 219.3 1199 0.01693 219.4 1199 0.01694 219.5 1199 0.01694 219.6 1200 0.01694 219.8 1199 0.01695 219.9 1199 0.01695 220 1199 0.01695 220.1 1199 0.01695 220.3 1199 0.01695 220.4 1199 0.01693 220.5 1199 0.01691 220.6 1199 0.0169 220.8 1199 0.0169 220.9 1199 0.0169 221 1199 0.0169 221.1 1199 0.01691 221.3 1199 0.01691 221.4 1199 0.01693 221.5 1199 0.01693 221.6 1199 0.01693 221.8 1199 0.01693 221.9 1199 0.01693 222 1199 0.01693 222.1 1199 0.01693 222.3 1199 0.01693 222.4 1199 0.01691 222.5 1199 0.01691 222.6 1199 0.01693 222.8 1199 0.01693 222.9 1199 0.01693 223 1199 0.01691 223.1 1199 0.01691 223.3 1199 0.01691 223.4 1199 0.01693 223.5 1199 0.01693 223.6 1199 0.01693 223.7 1199 0.01695 223.9 1199 0.01695 224 1199 0.01696 224.1 1199 0.01697 224.2 1199 0.01697 224.4 1199 0.01697 224.5 1200 0.01699 224.6 1199 0.01697 224.7 1199 0.01697 224.9 1199 0.01696 225 1199 0.01695 225.1 1199 0.01695 225.2 1199 0.01695 225.4 1199 0.01695 225.5 1200 0.01695 225.6 1199 0.01697 225.7 1199 0.01697 225.9 1200 0.01697 226 1199 0.01697 226.1 1199 0.01699 226.2 1199 0.01697 226.4 1199 0.01699 226.5 1199 0.017 226.6 1199 0.01699 226.7 1199 0.01699 226.9 1200 0.017 227 1199 0.017 227.1 1199 0.01701 227.2 1199 0.01702 227.4 1199 0.01704 227.5 1199 0.01705 227.6 1199 0.01705 227.7 1199 0.01705 227.9 1199 0.01704 228 1199 0.01702 228.1 1199 0.01701 228.2 1199 0.017 228.4 1199 0.017 228.5 1199 0.017 228.6 1199 0.01699 228.7 1199 0.01697 228.9 1199 0.01697 229 1199 0.01699 229.1 1199 0.017 229.2 1199 0.017 229.4 1200 0.017 229.5 1200 0.017 229.6 1199 0.01697 229.7 1199 0.01697 229.9 1199 0.01699 230 1199 0.017 230.1 1199 0.01701 230.2 1199 0.01701 230.3 1199 0.01701 230.5 1199 0.017 230.6 1199 0.017 230.7 1199 0.01701 230.8 1199 0.01701 231 1199 0.01701 231.1 1200 0.01702 231.2 1199 0.01702 231.3 1199 0.01704 231.5 1199 0.01704 231.6 1199 0.01701 231.7 1200 0.017 231.8 1199 0.017 232 1199 0.01701 232.1 1199 0.01701 232.2 1199 0.01701 232.3 1199 0.017 232.5 1200 0.017 232.6 1200 0.01702 232.7 1199 0.01701 232.8 1199 0.017 233 1199 0.01701 233.1 1199 0.01702 233.2 1199 0.01702 233.3 1199 0.01704 233.5 1199 0.01702 233.6 1200 0.01704 233.7 1200 0.01704 233.8 1200 0.01704 234 1200 0.01704 234.1 1199 0.01705 234.2 1199 0.01704 234.3 1199 0.01704 234.5 1199 0.01705 234.6 1199 0.01706 234.7 1199 0.01705 234.8 1199 0.01705 235 1200 0.01705 235.1 1199 0.01705 235.2 1199 0.01705 235.3 1199 0.01705 235.5 1199 0.01705 235.6 1199 0.01707 235.7 1199 0.01705 235.8 1200 0.01705 236 1200 0.01705 236.1 1199 0.01705 236.2 1199 0.01705 236.3 1199 0.01705 236.5 1199 0.01705 236.6 1200 0.01706 236.7 1200 0.01706 236.8 1199 0.01705 236.9 1199 0.01706 237.1 1199 0.01707 237.2 1199 0.01706 237.3 1199 0.01705 237.4 1199 0.01705 237.6 1199 0.01704 237.7 1200 0.01702 237.8 1199 0.01702 237.9 1199 0.01702 238.1 1199 0.01704 238.2 1199 0.01705 238.3 1200 0.01706 238.4 1199 0.01706 238.6 1199 0.01709 238.7 1199 0.01707 238.8 1199 0.01707 238.9 1200 0.01707 239.1 1200 0.01705 239.2 1199 0.01705 239.3 1199 0.01705 239.4 1199 0.01705 239.6 1199 0.01705 239.7 1199 0.01705 239.8 1199 0.01705 239.9 1199 0.01707 240.1 1199 0.01707 240.2 1199 0.01707 240.3 1200 0.01709 240.4 1199 0.0171 240.6 1199 0.0171 240.7 1199 0.0171 240.8 1199 0.01707 240.9 1199 0.01707 241.1 1199 0.01706 241.2 1199 0.01705 241.3 1199 0.01706 241.4 1199 0.01705 241.6 1199 0.01705 241.7 1200 0.01705 241.8 1200 0.01705 241.9 1199 0.01705 242.1 1199 0.01706 242.2 1199 0.01707 242.3 1199 0.01709 242.4 1199 0.01711 242.6 1199 0.01712 242.7 1199 0.01714 242.8 1199 0.01712 242.9 1199 0.01711 243 1199 0.01709 243.2 1199 0.01709 243.3 1199 0.01709 243.4 1199 0.01709 243.5 1199 0.0171 243.7 1199 0.01709 243.8 1199 0.01709 243.9 1199 0.01709 244 1199 0.01709 244.2 1199 0.0171 244.3 1199 0.0171 244.4 1199 0.01711 244.5 1199 0.0171 244.7 1199 0.0171 244.8 1199 0.0171 244.9 1200 0.0171 245 1199 0.01709 245.2 1199 0.01711 245.3 1199 0.01711 245.4 1199 0.01712 245.5 1199 0.01716 245.7 1199 0.01714 245.8 1199 0.01712 245.9 1200 0.01712 246 1199 0.01711 246.2 1199 0.01711 246.3 1199 0.01711 246.4 1199 0.01711 246.5 1200 0.01711 246.7 1199 0.01711 246.8 1199 0.01711 246.9 1199 0.0171 247 1199 0.0171 247.2 1199 0.01709 247.3 1199 0.01707 247.4 1199 0.01707 247.5 1199 0.01709 247.7 1199 0.0171 247.8 1199 0.0171 247.9 1199 0.0171 248 1199 0.01711 248.2 1199 0.01714 248.3 1199 0.01716 248.4 1200 0.01718 248.5 1199 0.01718 248.7 1199 0.01717 248.8 1199 0.01715 248.9 1199 0.01711 249 1199 0.01709 249.2 1199 0.01709 249.3 1199 0.01707 249.4 1199 0.01709 249.5 1199 0.01709 249.6 1199 0.01709 249.8 1199 0.0171 249.9 1199 0.01711 250 1199 0.01711 250.1 1200 0.01712 250.3 1199 0.01712 250.4 1199 0.01714 250.5 1199 0.01712 250.6 1200 0.01711 250.8 1199 0.01712 250.9 1200 0.01712 251 1200 0.01712 251.1 1199 0.01711 251.3 1199 0.0171 251.4 1199 0.01711 251.5 1200 0.01711 251.6 1199 0.01712 251.8 1199 0.01714 251.9 1200 0.01712 252 1199 0.01714 252.1 1199 0.01715 252.3 1199 0.01715 252.4 1199 0.01716 252.5 1199 0.01717 252.6 1199 0.01717 252.8 1199 0.01718 252.9 1200 0.01718 253 1200 0.01716 253.1 1199 0.01714 253.3 1199 0.01711 253.4 1199 0.01709 253.5 1200 0.01707 253.6 1199 0.01707 253.8 1199 0.01706 253.9 1199 0.01705 254 1200 0.01705 254.1 1199 0.01705 254.3 1200 0.01706 254.4 1199 0.01707 254.5 1199 0.01707 254.6 1199 0.01707 254.8 1199 0.01709 254.9 1199 0.01709 255 1200 0.01709 255.1 1199 0.01709 255.3 1199 0.01709 255.4 1199 0.01709 255.5 1199 0.01707 255.6 1200 0.01705 255.7 1200 0.01704 255.9 1199 0.01704 256 1199 0.01705 256.1 1199 0.01705 256.2 1199 0.01709 256.4 1199 0.01709 256.5 1199 0.01709 256.6 1199 0.01709 256.7 1199 0.01709 256.9 1199 0.01709 257 1199 0.01709 257.1 1200 0.01709 257.2 1199 0.01707 257.4 1200 0.01707 257.5 1200 0.01709 257.6 1199 0.01706 257.7 1199 0.01706 257.9 1199 0.01707 258 1199 0.01707 258.1 1200 0.01707 258.2 1199 0.01707 258.4 1199 0.01707 258.5 1199 0.01706 258.6 1199 0.01707 258.7 1199 0.01707 258.9 1199 0.01706 259 1199 0.01706 259.1 1199 0.01707 259.2 1199 0.01707 259.4 1199 0.01706 259.5 1199 0.01706 259.6 1199 0.01705 259.7 1199 0.01705 259.9 1199 0.01705 260 1199 0.01705 260.1 1199 0.01705 260.2 1199 0.01705 260.4 1199 0.01706 260.5 1199 0.01705 260.6 1199 0.01705 260.7 1199 0.01705 260.9 1199 0.01705 261 1199 0.01705 261.1 1199 0.01705 261.2 1199 0.01702 261.4 1199 0.01702 261.5 1199 0.017 261.6 1199 0.01697 261.7 1199 0.01696 261.9 1199 0.01695 262 1199 0.01695 262.1 1199 0.01694 262.2 1199 0.01695 262.3 1199 0.01696 262.5 1199 0.01697 262.6 1200 0.017 262.7 1199 0.01701 262.8 1199 0.01701 263 1199 0.01701 263.1 1199 0.01702 263.2 1199 0.01702 263.3 1199 0.01702 263.5 1199 0.01702 263.6 1199 0.01701 263.7 1199 0.01702 263.8 1199 0.01702 264 1199 0.01701 264.1 1199 0.01701 264.2 1199 0.01701 264.3 1199 0.01704 264.5 1199 0.01702 264.6 1199 0.01702 264.7 1199 0.01702 264.8 1199 0.01701 265 1199 0.01702 265.1 1199 0.01702 265.2 1199 0.01702 265.3 1200 0.01702 265.5 1199 0.01704 265.6 1200 0.01704 265.7 1199 0.01702 265.8 1199 0.01704 266 1200 0.01704 266.1 1199 0.01702 266.2 1200 0.01702 266.3 1200 0.01701 266.5 1199 0.017 266.6 1199 0.017 266.7 1199 0.017 266.8 1199 0.017 267 1199 0.017 267.1 1199 0.017 267.2 1200 0.01701 267.3 1199 0.017 267.5 1200 0.017 267.6 1199 0.017 267.7 1199 0.01699 267.8 1199 0.017 268 1199 0.017 268.1 1199 0.01699 268.2 1199 0.01701 268.3 1200 0.017 268.5 1200 0.01697 268.6 1200 0.01695 268.7 1199 0.01691 268.8 1199 0.01694 268.9 1199 0.01695 269.1 1200 0.01696 269.2 1199 0.01696 269.3 1199 0.01697 269.4 1199 0.01697 269.6 1199 0.01699 269.7 1200 0.01697 269.8 1199 0.01699 269.9 1200 0.01699 270.1 1199 0.017 270.2 1199 0.01701 270.3 1199 0.01702 270.4 1199 0.01701 270.6 1200 0.017 270.7 1199 0.017 270.8 1199 0.01699 270.9 1199 0.01697 271.1 1199 0.01696 271.2 1199 0.01696 271.3 1199 0.01696 271.4 1200 0.01697 271.6 1199 0.01697 271.7 1199 0.01697 271.8 1199 0.01699 271.9 1199 0.01699 272.1 1200 0.01699 272.2 1199 0.01699 272.3 1199 0.01699 272.4 1199 0.01699 272.6 1199 0.01699 272.7 1199 0.01697 272.8 1200 0.01696 272.9 1199 0.01697 273.1 1199 0.01697 273.2 1199 0.01696 273.3 1200 0.01696 273.4 1199 0.01695 273.6 1199 0.01695 273.7 1199 0.01694 273.8 1199 0.01693 273.9 1199 0.01691 274.1 1199 0.0169 274.2 1199 0.0169 274.3 1199 0.0169 274.4 1199 0.0169 274.6 1199 0.01689 274.7 1199 0.0169 274.8 1199 0.01689 274.9 1199 0.0169 275 1199 0.01691 275.2 1199 0.01693 275.3 1199 0.01695 275.4 1199 0.01696 275.5 1200 0.01696 275.7 1199 0.01697 275.8 1199 0.01699 275.9 1199 0.01697 276 1199 0.01697 276.2 1200 0.01699 276.3 1199 0.01699 276.4 1199 0.01699 276.5 1199 0.01699 276.7 1199 0.017 276.8 1199 0.01697 276.9 1199 0.01695 277 1199 0.01695 277.2 1199 0.01693 277.3 1199 0.0169 277.4 1199 0.0169 277.5 1199 0.01689 277.7 1199 0.0169 277.8 1199 0.01693 277.9 1199 0.01694 278 1199 0.01694 278.2 1199 0.01693 278.3 1199 0.01691 278.4 1199 0.01693 278.5 1199 0.01693 278.7 1199 0.01694 278.8 1199 0.01695 278.9 1199 0.01695 279 1199 0.01695 279.2 1199 0.01695 279.3 1199 0.01695 279.4 1199 0.01695 279.5 1199 0.01694 279.7 1199 0.01694 279.8 1199 0.01695 279.9 1199 0.01694 280 1199 0.01694 280.2 1200 0.01695 280.3 1199 0.01694 280.4 1200 0.01694 280.5 1199 0.01693 280.7 1199 0.0169 280.8 1199 0.01693 280.9 1199 0.01693 281 1200 0.01693 281.2 1199 0.01693 281.3 1199 0.01693 281.4 1199 0.01694 281.5 1199 0.01693 281.6 1199 0.01694 281.8 1199 0.01695 281.9 1199 0.01695 282 1199 0.01696 282.1 1199 0.01697 282.3 1199 0.01697 282.4 1199 0.01697 282.5 1199 0.01696 282.6 1199 0.01696 282.8 1199 0.01695 282.9 1200 0.01695 283 1199 0.01695 283.1 1199 0.01695 283.3 1199 0.01694 283.4 1199 0.01695 283.5 1199 0.01695 283.6 1200 0.01696 283.8 1199 0.01695 283.9 1199 0.01694 284 1199 0.01693 284.1 1199 0.01691 284.3 1199 0.01691 284.4 1199 0.01691 284.5 1199 0.01693 284.6 1200 0.01694 284.8 1199 0.01695 284.9 1200 0.01694 285 1199 0.01693 285.1 1199 0.01691 285.3 1199 0.01691 285.4 1199 0.0169 285.5 1200 0.0169 285.6 1199 0.01693 285.8 1199 0.01694 285.9 1200 0.0169 286 1200 0.01689 286.1 1199 0.01691 286.3 1200 0.01691 286.4 1199 0.01693 286.5 1199 0.01695 286.6 1199 0.01695 286.8 1199 0.01694 286.9 1200 0.01691 287 1199 0.0169 287.1 1199 0.0169 287.3 1200 0.01691 287.4 1200 0.01691 287.5 1199 0.01693 287.6 1199 0.01693 287.7 1199 0.01693 287.9 1199 0.01691 288 1199 0.0169 288.1 1200 0.01693 288.2 1199 0.01693 288.4 1199 0.01693 288.5 1199 0.01693 288.6 1199 0.01691 288.7 1200 0.01691 288.9 1200 0.01693 289 1200 0.01691 289.1 1199 0.01691 289.2 1199 0.0169 289.4 1199 0.0169 289.5 1200 0.0169 289.6 1199 0.01689 289.7 1199 0.01689 289.9 1200 0.01689 290 1200 0.01689 290.1 1200 0.01688 290.2 1199 0.01688 290.4 1199 0.01688 290.5 1199 0.0169 290.6 1199 0.0169 290.7 1199 0.01693 290.9 1199 0.01695 291 1199 0.01695 291.1 1199 0.01695 291.2 1199 0.01696 291.4 1199 0.01697 291.5 1199 0.01695 291.6 1199 0.01694 291.7 1199 0.01691 291.9 1199 0.01689 292 1199 0.0169 292.1 1199 0.01689 292.2 1199 0.0169 292.4 1199 0.01691 292.5 1199 0.0169 292.6 1199 0.0169 292.7 1200 0.01691 292.9 1199 0.01691 293 1199 0.0169 293.1 1199 0.0169 293.2 1199 0.0169 293.4 1199 0.0169 293.5 1199 0.0169 293.6 1199 0.0169 293.7 1199 0.0169 293.9 1199 0.01691 294 1199 0.01695 294.1 1199 0.01695 294.2 1199 0.01695 294.3 1199 0.01697 294.5 1199 0.01697 294.6 1200 0.01695 294.7 1199 0.01695 294.8 1199 0.01694 295 1199 0.01691 295.1 1199 0.01691 295.2 1199 0.0169 295.3 1199 0.0169 295.5 1199 0.01691 295.6 1199 0.01691 295.7 1199 0.01693 295.8 1199 0.01693 296 1200 0.01693 296.1 1199 0.01694 296.2 1199 0.01694 296.3 1199 0.01695 296.5 1199 0.01695 296.6 1199 0.01695 296.7 1199 0.01695 296.8 1199 0.01695 297 1199 0.01695 297.1 1199 0.0169 297.2 1199 0.01685 297.3 1200 0.01683 297.5 1199 0.0168 297.6 1199 0.01683 297.7 1199 0.01685 297.8 1199 0.01691 298 1199 0.01694 298.1 1199 0.01695 298.2 1199 0.01696 298.3 1199 0.01695 298.5 1199 0.01695 298.6 1199 0.01695 298.7 1199 0.01695 298.8 1199 0.01697 299 1199 0.017 299.1 1199 0.017 299.2 1199 0.017 299.3 1199 0.017 299.5 1200 0.017 299.6 1200 0.01697 299.7 1199 0.01697 299.8 1199 0.01697 300 1199 0.01699 300.1 1199 0.01699 300.2 1199 0.01697 300.3 1200 0.01695 300.4 1199 0.01695 300.6 1199 0.01695 300.7 1199 0.01694 300.8 1199 0.01695 300.9 1199 0.01694 301.1 1199 0.01694 301.2 1200 0.01693 301.3 1199 0.01693 301.4 1199 0.01689 301.6 1199 0.01686 301.7 1200 0.01684 301.8 1199 0.0168 301.9 1200 0.0168 302.1 1200 0.01681 302.2 1199 0.01683 302.3 1199 0.01683 302.4 1199 0.01686 302.6 1199 0.0169 302.7 1199 0.01691 302.8 1199 0.01694 302.9 1199 0.01695 303.1 1199 0.01696 303.2 1199 0.017 303.3 1199 0.01701 303.4 1199 0.01702 303.6 1199 0.01702 303.7 1199 0.01705 303.8 1199 0.01705 303.9 1200 0.01705 304.1 1200 0.01705 304.2 1199 0.01701 304.3 1199 0.01699 304.4 1199 0.01696 304.6 1199 0.01695 304.7 1199 0.01695 304.8 1199 0.01695 304.9 1199 0.01695 305.1 1200 0.01695 305.2 1199 0.01696 305.3 1200 0.01696 305.4 1199 0.01696 305.6 1199 0.01697 305.7 1199 0.01695 305.8 1199 0.01695 305.9 1200 0.01695 306.1 1200 0.01695 306.2 1199 0.01696 306.3 1199 0.01697 306.4 1199 0.01697 306.6 1199 0.01699 306.7 1199 0.01699 306.8 1200 0.01697 306.9 1199 0.01696 307 1199 0.01696 307.2 1200 0.01697 307.3 1199 0.01696 307.4 1199 0.01695 307.5 1199 0.01695 307.7 1199 0.01695 307.8 1199 0.01695 307.9 1199 0.01696 308 1199 0.01697 308.2 1200 0.01697 308.3 1199 0.01699 308.4 1200 0.01699 308.5 1199 0.01699 308.7 1199 0.01699 308.8 1199 0.017 308.9 1200 0.017 309 1199 0.017 309.2 1200 0.01699 309.3 1199 0.01697 309.4 1200 0.01699 309.5 1199 0.017 309.7 1199 0.017 309.8 1200 0.017 309.9 1199 0.017 310 1199 0.017 310.2 1199 0.017 310.3 1199 0.017 310.4 1200 0.01699 310.5 1199 0.01699 310.7 1199 0.017 310.8 1199 0.01699 310.9 1199 0.01699 311 1199 0.017 311.2 1199 0.01699 311.3 1199 0.01699 311.4 1199 0.01699 311.5 1199 0.017 311.7 1200 0.017 311.8 1199 0.01699 311.9 1199 0.017 312 1199 0.01699 312.2 1199 0.01699 312.3 1199 0.017 312.4 1199 0.01697 312.5 1199 0.01696 312.7 1199 0.01697 312.8 1200 0.01697 312.9 1199 0.01696 313 1199 0.01696 313.2 1199 0.01695 313.3 1199 0.01695 313.4 1199 0.01695 313.5 1199 0.01695 313.6 1200 0.01695 313.8 1199 0.01696 313.9 1199 0.01699 314 1199 0.017 314.1 1199 0.017 314.3 1199 0.017 314.4 1199 0.017 314.5 1199 0.01699 314.6 1199 0.01699 314.8 1199 0.01699 314.9 1199 0.01699 315 1200 0.01699 315.1 1200 0.017 315.3 1199 0.017 315.4 1199 0.01699 315.5 1199 0.01697 315.6 1199 0.01696 315.8 1199 0.01695 315.9 1199 0.01695 316 1199 0.01697 316.1 1199 0.01697 316.3 1200 0.017 316.4 1200 0.01701 316.5 1199 0.017 316.6 1200 0.01699 316.8 1199 0.017 316.9 1199 0.017 317 1199 0.017 317.1 1199 0.017 317.3 1199 0.017 317.4 1199 0.017 317.5 1199 0.017 317.6 1199 0.017 317.8 1199 0.01699 317.9 1200 0.01696 318 1199 0.01697 318.1 1199 0.01697 318.3 1199 0.01699 318.4 1199 0.01699 318.5 1200 0.01697 318.6 1199 0.01696 318.8 1199 0.01695 318.9 1200 0.01695 319 1199 0.01695 319.1 1199 0.01697 319.3 1199 0.01697 319.4 1199 0.01697 319.5 1199 0.01699 319.6 1199 0.01699 319.7 1199 0.01699 319.9 1200 0.01699 320 1199 0.01699 320.1 1200 0.01699 320.2 1199 0.01697 320.4 1199 0.01697 320.5 1200 0.01695 320.6 1199 0.01695 320.7 1200 0.01696 320.9 1199 0.01697 321 1200 0.01697 321.1 1200 0.01699 321.2 1199 0.01699 321.4 1200 0.01699 321.5 1199 0.01699 321.6 1200 0.01699 321.7 1200 0.01699 321.9 1199 0.01699 322 1199 0.01697 322.1 1199 0.01696 322.2 1199 0.01697 322.4 1199 0.01697 322.5 1200 0.01699 322.6 1199 0.01699 322.7 1199 0.01699 322.9 1199 0.01699 323 1199 0.01699 323.1 1199 0.01697 323.2 1199 0.01697 323.4 1200 0.01695 323.5 1199 0.01695 323.6 1200 0.01695 323.7 1199 0.01693 323.9 1199 0.01693 324 1199 0.01693 324.1 1200 0.01693 324.2 1199 0.01693 324.4 1199 0.01695 324.5 1199 0.01696 324.6 1199 0.01699 324.7 1200 0.01699 324.9 1199 0.01699 325 1199 0.01699 325.1 1199 0.01697 325.2 1199 0.01697 325.4 1199 0.01697 325.5 1199 0.01697 325.6 1199 0.01696 325.7 1199 0.01695 325.9 1199 0.01695 326 1199 0.01694 326.1 1199 0.01695 326.2 1199 0.01695 326.3 1200 0.01696 326.5 1199 0.01696 326.6 1200 0.01696 326.7 1199 0.01695 326.8 1199 0.01697 327 1199 0.01697 327.1 1199 0.01697 327.2 1200 0.01697 327.3 1199 0.01696 327.5 1199 0.01695 327.6 1200 0.01697 327.7 1199 0.01697 327.8 1199 0.01696 328 1200 0.01696 328.1 1199 0.01695 328.2 1199 0.01695 328.3 1199 0.01695 328.5 1199 0.01695 328.6 1200 0.01695 328.7 1199 0.01694 328.8 1199 0.01695 329 1200 0.01694 329.1 1199 0.01694 329.2 1199 0.01695 329.3 1199 0.01694 329.5 1199 0.01693 329.6 1200 0.01691 329.7 1199 0.01693 329.8 1199 0.01695 330 1199 0.01695 330.1 1199 0.01696 330.2 1199 0.01696 330.3 1199 0.01697 330.5 1199 0.01697 330.6 1199 0.01696 330.7 1199 0.01696 330.8 1199 0.01697 331 1199 0.01696 331.1 1199 0.01695 331.2 1199 0.01695 331.3 1199 0.01693 331.5 1200 0.0169 331.6 1199 0.01689 331.7 1199 0.01688 331.8 1199 0.01686 332 1199 0.01689 332.1 1199 0.0169 332.2 1199 0.0169 332.3 1199 0.01689 332.4 1199 0.0169 332.6 1199 0.01691 332.7 1199 0.01691 332.8 1199 0.01693 332.9 1199 0.01693 333.1 1199 0.01693 333.2 1199 0.01694 333.3 1199 0.01694 333.4 1199 0.01694 333.6 1199 0.01694 333.7 1199 0.01694 333.8 1199 0.01694 333.9 1199 0.01694 334.1 1199 0.01694 334.2 1199 0.01695 334.3 1199 0.01693 334.4 1199 0.01693 334.6 1199 0.01691 334.7 1199 0.0169 334.8 1199 0.01691 334.9 1199 0.01691 335.1 1199 0.01691 335.2 1199 0.01693 335.3 1199 0.01694 335.4 1199 0.01693 335.6 1199 0.01693 335.7 1199 0.01691 335.8 1199 0.01691 335.9 1200 0.01691 336.1 1200 0.01691 336.2 1199 0.0169 336.3 1199 0.01691 336.4 1199 0.01693 336.6 1199 0.0169 336.7 1199 0.0169 336.8 1199 0.0169 336.9 1199 0.0169 337.1 1200 0.0169 337.2 1199 0.0169 337.3 1200 0.01691 337.4 1199 0.01691 337.6 1199 0.01693 337.7 1199 0.01695 337.8 1199 0.01694 337.9 1200 0.01691 338.1 1199 0.01691 338.2 1199 0.0169 338.3 1199 0.0169 338.4 1199 0.0169 338.6 1199 0.01688 338.7 1200 0.01685 338.8 1200 0.01684 338.9 1199 0.01685 339 1200 0.01685 339.2 1199 0.01685 339.3 1199 0.01688 339.4 1199 0.01688 339.5 1200 0.01689 339.7 1199 0.0169 339.8 1200 0.0169 339.9 1200 0.0169 340 1199 0.01689 340.2 1199 0.0169 340.3 1199 0.0169 340.4 1199 0.0169 340.5 1200 0.0169 340.7 1199 0.0169 340.8 1199 0.0169 340.9 1200 0.0169 341 1199 0.01689 341.2 1200 0.01689 341.3 1199 0.01688 341.4 1199 0.01688 341.5 1199 0.0169 341.7 1199 0.01689 341.8 1199 0.0169 341.9 1200 0.01689 342 1199 0.01689 342.2 1199 0.01689 342.3 1199 0.01686 342.4 1200 0.01688 342.5 1199 0.01688 342.7 1199 0.01688 342.8 1199 0.01688 342.9 1199 0.01686 343 1199 0.01684 343.2 1199 0.01684 343.3 1199 0.01684 343.4 1199 0.01684 343.5 1199 0.01684 343.7 1199 0.01683 343.8 1200 0.01684 343.9 1200 0.0168 344 1199 0.01679 344.2 1199 0.01679 344.3 1199 0.0168 344.4 1199 0.0168 344.5 1200 0.01681 344.7 1199 0.01683 344.8 1199 0.01681 344.9 1199 0.01683 345 1199 0.01683 345.2 1199 0.01683 345.3 1199 0.01684 345.4 1199 0.01685 345.5 1200 0.01685 345.6 1200 0.01685 345.8 1199 0.01685 345.9 1199 0.01686 346 1199 0.01686 346.1 1199 0.01685 346.3 1199 0.01686 346.4 1199 0.01686 346.5 1199 0.01686 346.6 1199 0.01685 346.8 1199 0.01688 346.9 1199 0.01689 347 1200 0.01688 347.1 1199 0.01688 347.3 1199 0.01688 347.4 1199 0.01688 347.5 1199 0.01688 347.6 1199 0.01686 347.8 1199 0.01685 347.9 1199 0.01688 348 1199 0.01686 348.1 1199 0.01685 348.3 1199 0.01686 348.4 1199 0.01688 348.5 1199 0.01685 348.6 1199 0.01685 348.8 1199 0.01688 348.9 1199 0.01688 349 1199 0.01686 349.1 1200 0.01686 349.3 1199 0.01686 349.4 1200 0.01688 349.5 1199 0.01688 349.6 1199 0.01688 349.8 1199 0.01689 349.9 1199 0.01689 350 1199 0.01689 350.1 1199 0.01688 350.3 1199 0.01685 350.4 1199 0.01685 350.5 1200 0.01685 350.6 1199 0.01685 350.8 1200 0.01685 350.9 1199 0.01685 351 1199 0.01685 351.1 1199 0.01684 351.3 1200 0.01686 351.4 1199 0.01686 351.5 1199 0.01685 351.6 1199 0.01685 351.7 1199 0.01688 351.9 1199 0.01686 352 1199 0.01685 352.1 1200 0.01686 352.2 1199 0.01686 352.4 1199 0.01688 352.5 1199 0.01688 352.6 1199 0.01688 352.7 1200 0.01685 352.9 1199 0.01686 353 1200 0.01688 353.1 1199 0.01686 353.2 1199 0.01685 353.4 1200 0.01685 353.5 1199 0.01683 353.6 1200 0.0168 353.7 1199 0.0168 353.9 1199 0.01679 354 1199 0.01676 354.1 1199 0.01675 354.2 1199 0.01675 354.4 1199 0.01675 354.5 1200 0.01676 354.6 1199 0.01675 354.7 1199 0.01675 354.9 1199 0.01675 355 1199 0.01676 355.1 1200 0.01679 355.2 1199 0.0168 355.4 1199 0.01681 355.5 1199 0.01684 355.6 1199 0.01683 355.7 1199 0.01681 355.9 1199 0.01684 356 1199 0.01685 356.1 1199 0.01688 356.2 1199 0.01689 356.4 1200 0.01689 356.5 1199 0.01689 356.6 1199 0.0169 356.7 1199 0.01691 356.9 1199 0.0169 357 1199 0.0169 357.1 1199 0.0169 357.2 1199 0.0169 357.4 1199 0.01689 357.5 1199 0.01688 357.6 1199 0.01686 357.7 1199 0.01684 357.9 1199 0.01681 358 1199 0.01683 358.1 1199 0.01683 358.2 1199 0.01683 358.3 1199 0.01683 358.5 1199 0.01684 358.6 1200 0.01684 358.7 1199 0.01683 358.8 1199 0.01685 359 1199 0.01685 359.1 1199 0.01685 359.2 1200 0.01685 359.3 1199 0.01685 359.5 1199 0.01684 359.6 1199 0.01683 359.7 1199 0.01685 359.8 1199 0.01685 360 1199 0.01685 360.1 1199 0.01688 360.2 1199 0.01688 360.3 1199 0.01688 360.5 1200 0.01685 360.6 1199 0.01685 360.7 1199 0.01683 360.8 1199 0.01681 361 1199 0.01684 361.1 1199 0.01685 361.2 1199 0.01685 361.3 1199 0.01686 361.5 1200 0.01685 361.6 1199 0.01685 361.7 1199 0.01685 361.8 1199 0.01685 362 1199 0.01685 362.1 1199 0.01688 362.2 1199 0.01688 362.3 1199 0.01688 362.5 1199 0.01688 362.6 1199 0.01689 362.7 1199 0.01689 362.8 1199 0.01689 363 1199 0.0169 363.1 1199 0.01693 363.2 1199 0.01695 363.3 1199 0.01695 363.5 1200 0.01694 363.6 1199 0.01691 363.7 1199 0.01688 363.8 1199 0.01686 364 1199 0.01685 364.1 1199 0.01685 364.2 1199 0.01684 364.3 1199 0.01685 364.4 1199 0.01685 364.6 1199 0.01684 364.7 1199 0.01683 364.8 1199 0.01683 364.9 1199 0.01683 365.1 1199 0.01684 365.2 1199 0.01685 365.3 1199 0.01688 365.4 1199 0.01689 365.6 1199 0.01688 365.7 1199 0.01688 365.8 1199 0.01685 365.9 1199 0.01684 366.1 1199 0.01683 366.2 1199 0.01683 366.3 1199 0.01683 366.4 1199 0.01685 366.6 1200 0.01684 366.7 1200 0.01684 366.8 1199 0.01683 366.9 1199 0.01685 367.1 1199 0.01685 367.2 1199 0.01685 367.3 1199 0.01688 367.4 1199 0.01688 367.6 1199 0.01685 367.7 1200 0.01686 367.8 1199 0.01688 367.9 1200 0.01688 368.1 1199 0.01688 368.2 1199 0.01689 368.3 1199 0.01688 368.4 1199 0.01688 368.6 1199 0.01688 368.7 1199 0.01686 368.8 1199 0.01688 368.9 1199 0.01688 369.1 1200 0.01689 369.2 1199 0.01688 369.3 1199 0.01689 369.4 1199 0.01689 369.6 1199 0.01688 369.7 1199 0.01686 369.8 1199 0.01688 369.9 1200 0.01688 370.1 1199 0.01688 370.2 1199 0.01689 370.3 1199 0.01689 370.4 1199 0.01689 370.6 1199 0.01689 370.7 1199 0.01689 370.8 1199 0.01689 370.9 1199 0.01689 371 1199 0.01689 371.2 1199 0.01689 371.3 1199 0.01689 371.4 1199 0.01688 371.5 1199 0.01688 371.7 1199 0.01685 371.8 1200 0.01685 371.9 1199 0.01685 372 1199 0.01685 372.2 1200 0.01685 372.3 1199 0.01685 372.4 1200 0.01685 372.5 1199 0.01686 372.7 1199 0.01689 372.8 1199 0.0169 372.9 1199 0.0169 373 1199 0.01691 373.2 1200 0.01695 373.3 1199 0.01696 373.4 1199 0.01695 373.5 1199 0.01693 373.7 1199 0.01691 373.8 1199 0.01691 373.9 1199 0.0169 374 1199 0.0169 374.2 1199 0.01691 374.3 1199 0.01691 374.4 1199 0.01691 374.5 1199 0.0169 374.7 1199 0.0169 374.8 1199 0.0169 374.9 1198 0.01689 375 1197 0.01685 375.2 1197 0.01685 375.3 1195 0.01686 375.4 1194 0.01684 375.5 1191 0.0168 375.7 1179 0.01676 375.8 1176 0.01675 375.9 1177 0.01675 376 1176 0.01675 376.2 1176 0.01674 376.3 1175 0.01671 376.4 1174 0.0167 376.5 1172 0.01669 376.7 1171 0.01664 376.8 1169 0.01659 376.9 1168 0.01654 377 1166 0.01649 377.1 1165 0.01647 377.3 1163 0.01642 377.4 1161 0.01638 377.5 1159 0.01634 377.6 1158 0.01629 377.8 1157 0.01624 377.9 1156 0.0162 378 1154 0.01615 378.1 1153 0.01611 378.3 1151 0.01606 378.4 1150 0.01601 378.5 1149 0.01596 378.6 1147 0.01594 378.8 1144 0.01592 378.9 1144 0.01589 379 1142 0.01586 379.1 1140 0.01582 379.3 1137 0.01576 379.4 1136 0.0157 379.5 1134 0.01565 379.6 1130 0.01558 379.8 1125 0.01553 379.9 1119 0.01549 380 1117 0.01544 380.1 1112 0.01542 380.3 1110 0.01539 380.4 1107 0.01537 380.5 1105 0.01533 380.6 1103 0.01532 380.8 1101 0.01529 380.9 1099 0.01527 381 1097 0.01522 381.1 1095 0.01514 381.3 1092 0.01509 381.4 1090 0.01502 381.5 1088 0.01497 381.6 1086 0.01495 381.8 1084 0.0149 381.9 1082 0.01484 382 1081 0.01479 382.1 1078 0.01476 382.3 1077 0.01472 382.4 1073 0.01472 382.5 1073 0.01471 382.6 1069 0.01467 382.8 1068 0.01465 382.9 1067 0.01462 383 1062 0.01456 383.1 1065 0.0145 383.3 1058 0.01446 383.4 1059 0.01441 383.5 1056 0.01437 383.6 1053 0.01433 383.7 1055 0.01428 383.9 1047 0.01424 384 1050 0.01418 384.1 1045 0.01414 384.2 1043 0.01406 384.4 1044 0.01401 384.5 1037 0.01397 384.6 1040 0.01393 384.7 1036 0.0139 384.9 1033 0.01386 385 1034 0.01381 385.1 1026 0.01376 385.2 1031 0.01372 385.4 1025 0.01371 385.5 1023 0.01365 385.6 1024 0.0136 385.7 1017 0.01355 385.9 1021 0.01352 386 1014 0.01347 386.1 1014 0.01343 386.2 1014 0.01339 386.4 1007 0.01335 386.5 1011 0.01329 386.6 1004 0.01324 386.7 1004 0.01319 386.9 1003 0.01313 387 997 0.01309 387.1 1001 0.01304 387.2 993 0.013 387.4 994 0.01294 387.5 994 0.01289 387.6 986 0.01284 387.7 992 0.01279 387.9 984 0.01276 388 984 0.01272 388.1 984 0.0127 388.2 977 0.01267 388.4 982 0.01267 388.5 973 0.01266 388.6 975 0.01261 388.7 975 0.01257 388.9 967 0.01249 389 972 0.01241 389.1 963 0.01236 389.2 965 0.01231 389.4 964 0.01227 389.5 957 0.01225 389.6 962 0.0122 389.7 953 0.01216 389.9 955 0.01213 390 954 0.01209 390.1 947 0.01204 390.2 953 0.012 390.3 942 0.01195 390.5 946 0.01192 390.6 943 0.01188 390.7 937 0.01184 390.8 943 0.01179 391 932 0.01173 391.1 937 0.01167 391.2 932 0.01162 391.3 929 0.01158 391.5 932 0.01155 391.6 922 0.01152 391.7 928 0.0115 391.8 920 0.01146 392 919 0.01142 392.1 920 0.01136 392.2 912 0.01131 392.3 918 0.01125 392.5 909 0.01121 392.6 912 0.01115 392.7 907 0.01109 392.8 905 0.01101 393 907 0.01095 393.1 899 0.01091 393.2 904 0.0109 393.3 894 0.01091 393.5 899 0.0109 393.6 893 0.01088 393.7 892 0.01082 393.8 893 0.01075 394 885 0.0107 394.1 890 0.01064 394.2 881 0.01061 394.3 886 0.01057 394.5 878 0.01053 394.6 879 0.01049 394.7 876 0.01044 394.8 872 0.01041 395 875 0.01035 395.1 867 0.0103 395.2 872 0.01021 395.3 862 0.01017 395.5 867 0.01012 395.6 859 0.01009 395.7 861 0.01002 395.8 857 0.009987 396 854 0.009962 396.1 857 0.009937 396.2 849 0.009888 396.3 854 0.009863 396.4 844 0.009814 396.6 850 0.009764 396.7 840 0.009727 396.8 845 0.009702 396.9 837 0.009665 397.1 840 0.009628 397.2 834 0.009566 397.3 834 0.009505 397.4 832 0.009467 397.6 828 0.00943 397.7 830 0.009381 397.8 823 0.009344 397.9 828 0.009294 398.1 818 0.00927 398.2 824 0.009208 398.3 814 0.009158 398.4 820 0.009096 398.6 809 0.009047 398.7 816 0.00901 398.8 806 0.008985 398.9 811 0.008936 399.1 803 0.008886 399.2 806 0.008837 399.3 801 0.0088 399.4 802 0.008763 399.6 800 0.008738 399.7 801 0.008688 399.8 796 0.008639 399.9 797 0.008589 400.1 793 0.00854 400.2 793 0.00849 400.3 789 0.008441 400.4 789 0.008404 400.6 785 0.008342 400.7 785 0.008293 400.8 781 0.008255 400.9 781 0.008231 401.1 776 0.008169 401.2 777 0.008119 401.3 772 0.00807 401.4 774 0.00802 401.6 768 0.007971 401.7 770 0.007946 401.8 764 0.007897 401.9 767 0.007847 402.1 759 0.007798 402.2 763 0.007748 402.3 755 0.007711 402.4 759 0.007687 402.6 750 0.007625 402.7 755 0.007588 402.8 746 0.007538 402.9 750 0.007501 403 744 0.007452 403.2 744 0.007414 403.3 742 0.007365 403.4 739 0.007328 403.5 739 0.007291 403.7 734 0.007254 403.8 736 0.007204 403.9 729 0.007155 404 732 0.007118 404.2 725 0.007068 404.3 728 0.007019 404.4 721 0.006969 404.5 723 0.00692 404.7 718 0.00687 404.8 717 0.006833 404.9 717 0.006796 405 711 0.006747 405.2 714 0.006697 405.3 706 0.00666 405.4 711 0.006611 405.5 703 0.006598 405.7 706 0.006561 405.8 700 0.006536 405.9 700 0.006474 406 698 0.0064 406.2 694 0.006338 406.3 696 0.006301 406.4 689 0.00624 406.5 693 0.006202 406.7 685 0.006153 406.8 688 0.006116 406.9 682 0.006079 407 681 0.006054 407.2 680 0.006017 407.3 676 0.005992 407.4 677 0.005955 407.5 672 0.005918 407.7 671 0.005856 407.8 669 0.005794 407.9 667 0.005732 408 667 0.005683 408.2 662 0.005621 408.3 662 0.005559 408.4 659 0.005535 408.5 658 0.00551 408.7 656 0.005473 408.8 653 0.005436 408.9 653 0.005386 409 647 0.005349 409.1 649 0.0053 409.3 644 0.00525 409.4 643 0.005213 409.5 643 0.005176 409.6 638 0.005126 409.8 639 0.005077 409.9 634 0.005015 410 634 0.004966 410.1 631 0.004916 410.3 629 0.004879 410.4 628 0.004842 410.5 625 0.004805 410.6 623 0.004768 410.8 621 0.004718 410.9 619 0.004681 411 617 0.004619 411.1 615 0.004557 411.3 614 0.004508 411.4 611 0.004471 411.5 609 0.004421 411.6 607 0.00436 411.8 606 0.004323 411.9 603 0.004285 412 601 0.004236 412.1 600 0.004199 412.3 598 0.004149 412.4 596 0.0041 412.5 593 0.00405 412.6 592 0.004013 412.8 590 0.003951 412.9 588 0.003902 413 586 0.003853 413.1 584 0.003828 413.3 582 0.003766 413.4 579 0.003716 413.5 578 0.003667 413.6 576 0.003618 413.8 573 0.003568 413.9 571 0.003531 414 569 0.003457 414.1 567 0.003407 414.3 565 0.003358 414.4 564 0.003308 414.5 561 0.003247 414.6 559 0.003197 414.8 557 0.003172 414.9 556 0.003148 415 554 0.003098 415.1 551 0.003061 415.3 549 0.003024 415.4 546 0.002974 415.5 546 0.0029 415.6 543 0.002851 415.7 542 0.002789 415.9 539 0.002739 416 537 0.00269 416.1 535 0.002653 416.2 534 0.002603 416.4 532 0.002579 416.5 529 0.002542 416.6 528 0.002504 416.7 525 0.002467 416.9 524 0.00243 417 521 0.002406 417.1 520 0.002356 417.2 518 0.002319 417.4 517 0.002269 417.5 515 0.002232 417.6 514 0.002171 417.7 511 0.002109 417.9 510 0.002034 418 506 0.001985 418.1 505 0.001911 418.2 503 0.001849 418.4 501 0.001812 418.5 499 0.001787 418.6 498 0.001713 418.7 496 0.001651 418.9 493 0.001577 419 492 0.00154 419.1 490 0.001466 419.2 488 0.001404 419.4 485 0.001342 419.5 484 0.00128 419.6 481 0.001218 419.7 478 0.001169 419.9 476 0.001082 420 474 0.00102 420.1 471 0.0009585 420.2 469 0.000909 420.4 467 0.0008348 420.5 464 0.000773 420.6 463 0.0006988 420.7 460 0.0006246 420.9 458 0.0005627 421 456 0.0005133 421.1 454 0.0004638 421.2 452 0.0004143 421.4 449 0.0003525 421.5 449 0.000303 421.6 446 0.0002659 421.7 443 0.0002164 421.9 442 0.0001546 422 441 9.276e-05 422.1 438 5.565e-05 422.2 437 6.184e-06 422.3 435 6.184e-06 422.5 433 6.184e-06 422.6 431 -3.092e-05 422.7 430 -8.039e-05 422.8 428 -0.0001422 423 426 -0.0001917 423.1 424 -0.0002288 423.2 422 -0.0002783 423.3 419 -0.0003277 423.5 418 -0.0003648 423.6 416 -0.000402 423.7 413 -0.0004638 423.8 412 -0.0004885 424 410 -0.0005504 424.1 409 -0.0005875 424.2 406 -0.0006493 424.3 404 -0.0006864 424.5 403 -0.0007482 424.6 401 -0.0007977 424.7 399 -0.0008225 424.8 396 -0.0008472 425 394 -0.0008967 425.1 392 -0.0009214 425.2 391 -0.0009585 425.3 388 -0.0009956 425.5 387 -0.001045 425.6 385 -0.001082 425.7 382 -0.001095 425.8 381 -0.001119 426 379 -0.001156 426.1 377 -0.001169 426.2 374 -0.001218 426.3 373 -0.001255 426.5 371 -0.00128 426.6 369 -0.001305 426.7 368 -0.001317 426.8 367 -0.001317 427 364 -0.001317 427.1 363 -0.001317 427.2 360 -0.001342 427.3 359 -0.001367 427.5 358 -0.001379 427.6 356 -0.001391 427.7 355 -0.001391 427.8 354 -0.001404 428 353 -0.001416 428.1 351 -0.001391 428.2 349 -0.001367 428.3 348 -0.001354 428.4 347 -0.00133 428.6 345 -0.001292 428.7 344 -0.001255 428.8 342 -0.001218 428.9 342 -0.001193 429.1 340 -0.001169 429.2 338 -0.001132 429.3 337 -0.001107 429.4 335 -0.00107 429.6 334 -0.00102 429.7 332 -0.0009585 429.8 331 -0.0008596 429.9 329 -0.000773 430.1 328 -0.0006246 430.2 326 -0.0005009 430.3 324 -0.0003772 430.4 322 -0.0002783 430.6 320 -0.000167 430.7 319 -9.276e-05 430.8 317 6.184e-06 430.9 316 6.184e-06 431.1 313 0.0001051 431.2 312 0.0001917 431.3 311 0.000303 431.4 310 0.0003896 431.6 307 0.0004762 431.7 306 0.0005627 431.8 302 0.0006493 431.9 301 0.0007111 432.1 299 0.000773 432.2 296 0.0008348 432.3 294 0.0008967 432.4 292 0.0009338 432.6 291 0.0009709 432.7 288 0.001008 432.8 286 0.001057 432.9 284 0.001107 433.1 281 0.001181 433.2 279 0.001243 433.3 277 0.001292 433.4 274 0.001317 433.6 273 0.001367 433.7 270 0.001391 433.8 267 0.001391 433.9 264 0.001404 434.1 262 0.001404 434.2 259 0.001416 434.3 256 0.001416 434.4 254 0.001441 434.6 252 0.001466 434.7 249 0.00149 434.8 246 0.00149 434.9 243 0.00149 435 242 0.00149 435.2 239 0.001466 435.3 236 0.001453 435.4 234 0.001441 435.5 231 0.001416 435.7 229 0.001416 435.8 227 0.001404 435.9 224 0.001379 436 221 0.001367 436.2 218 0.001354 436.3 217 0.00133 436.4 214 0.001317 436.5 211 0.001317 436.7 209 0.001305 436.8 206 0.001292 436.9 205 0.001268 437 202 0.001243 437.2 201 0.001243 437.3 199 0.001218 437.4 196 0.001169 437.5 193 0.001132 437.7 191 0.001132 437.8 190 0.001119 437.9 188 0.00107 438 185 0.00102 438.2 183 0.0009832 438.3 181 0.0009585 438.4 179 0.0009585 438.5 177 0.0009338 438.7 174 0.0008843 438.8 173 0.0008596 438.9 171 0.0008348 439 168 0.0008225 439.2 166 0.0008225 439.3 164 0.0008225 439.4 162 0.0007977 439.5 160 0.000773 439.7 159 0.0007235 439.8 156 0.000674 439.9 154 0.0006493 440 152 0.0006246 440.2 151 0.0005875 440.3 149 0.0005875 440.4 147 0.0005751 440.5 145 0.0005627 440.7 143 0.0005504 440.8 142 0.0005256 440.9 140 0.0005009 441 139 0.0004762 441.1 137 0.0004638 441.3 136 0.0004638 441.4 134 0.0004638 441.5 132 0.0004514 441.6 131 0.0004391 441.8 129 0.0004267 441.9 127 0.0004143 442 127 0.0003896 442.1 124 0.0003648 442.3 123 0.0003401 442.4 122 0.0003277 442.5 121 0.000303 442.6 119 0.0002906 442.8 118 0.0002906 442.9 116 0.0002783 443 116 0.0002535 443.1 115 0.0002288 443.3 113 0.0002288 443.4 112 0.0002164 443.5 110 0.0002041 443.6 110 0.0001917 443.8 109 0.0001793 443.9 108 0.0001793 444 106 0.0001793 444.1 106 0.000167 444.3 104 0.0001299 444.4 104 0.0001175 444.5 102 0.0001051 444.6 102 9.276e-05 444.8 100 0.0001051 444.9 99 9.276e-05 445 98 8.039e-05 445.1 98 5.565e-05 445.3 97 1.855e-05 445.4 96 6.184e-06 445.5 95 6.184e-06 445.6 94 6.184e-06 445.8 93 6.184e-06 445.9 92 6.184e-06 446 91 6.184e-06 446.1 91 6.184e-06 446.3 90 6.184e-06 446.4 89 6.184e-06 446.5 88 6.184e-06 446.6 88 6.184e-06 446.8 87 6.184e-06 446.9 86 -6.184e-06 447 85 -3.092e-05 447.1 84 -4.329e-05 447.3 84 -5.565e-05 447.4 84 -6.802e-05 447.5 83 -5.565e-05 447.6 83 -6.802e-05 447.7 81 -6.802e-05 447.9 81 -8.039e-05 448 81 -8.039e-05 448.1 80 -6.802e-05 448.2 79 -6.802e-05 448.4 78 -6.802e-05 448.5 77 -8.039e-05 448.6 77 -0.0001175 448.7 76 -0.0001422 448.9 76 -0.0001546 449 75 -0.000167 449.1 74 -0.0001793 449.2 74 -0.0001793 449.4 73 -0.0001917 449.5 73 -0.0002041 449.6 72 -0.0002164 449.7 72 -0.0002288 449.9 71 -0.0002288 450 71 -0.0002412 450.1 70 -0.0002412 450.2 70 -0.0002535 450.4 69 -0.0002535 450.5 69 -0.0002535 450.6 68 -0.0002535 450.7 68 -0.0002659 450.9 67 -0.0002659 451 66 -0.0002783 451.1 66 -0.0002906 451.2 66 -0.000303 451.4 65 -0.000303 451.5 65 -0.000303 451.6 65 -0.000303 451.7 64 -0.000303 451.9 63 -0.000303 452 63 -0.0003154 452.1 63 -0.0003277 452.2 63 -0.0003277 452.4 63 -0.0003154 452.5 62 -0.0003277 452.6 62 -0.0003401 452.7 61 -0.0003525 452.9 61 -0.0003525 453 60 -0.0003648 453.1 59 -0.0003772 453.2 59 -0.000402 453.4 59 -0.0004143 453.5 59 -0.0004143 453.6 59 -0.0004143 453.7 59 -0.0004143 453.8 59 -0.0004143 454 58 -0.0004267 454.1 57 -0.0004267 454.2 56 -0.0004514 454.3 56 -0.0004514 454.5 56 -0.0004514 454.6 55 -0.0004514 454.7 55 -0.0004514 454.8 55 -0.0004391 455 55 -0.0004514 455.1 55 -0.0004514 455.2 54 -0.0004514 455.3 54 -0.0004638 455.5 54 -0.0004638 455.6 54 -0.0004638 455.7 53 -0.0004762 455.8 54 -0.0004885 456 52 -0.0005009 456.1 52 -0.0005009 456.2 52 -0.0005133 456.3 52 -0.0005009 456.5 52 -0.0005133 456.6 52 -0.0005256 456.7 51 -0.000538 456.8 51 -0.0005256 457 51 -0.0005256 457.1 50 -0.0005256 457.2 49 -0.0005256 457.3 49 -0.0005256 457.5 49 -0.0005256 457.6 49 -0.0005256 457.7 49 -0.0005256 457.8 48 -0.0005133 458 48 -0.0005133 458.1 48 -0.0005133 458.2 48 -0.0005256 458.3 48 -0.0005133 458.5 48 -0.0005256 458.6 48 -0.0005256 458.7 47 -0.0005133 458.8 47 -0.0005133 459 47 -0.0005133 459.1 46 -0.0005133 459.2 46 -0.0005256 459.3 46 -0.0005133 459.5 46 -0.0005133 459.6 46 -0.0005133 459.7 45 -0.0005256 459.8 45 -0.000538 460 45 -0.000538 460.1 45 -0.000538 460.2 45 -0.0005627 460.3 44 -0.0005627 460.4 44 -0.0005627 460.6 44 -0.0005627 460.7 44 -0.0005627 460.8 43 -0.0005627 460.9 43 -0.0005627 461.1 43 -0.0005627 461.2 43 -0.0005627 461.3 43 -0.0005627 461.4 43 -0.0005627 461.6 42 -0.0005627 461.7 42 -0.0005751 461.8 42 -0.0005875 461.9 41 -0.0005998 462.1 41 -0.0006122 462.2 41 -0.0006122 462.3 41 -0.0006122 462.4 41 -0.0006122 462.6 41 -0.0006246 462.7 41 -0.0006246 462.8 41 -0.0006246 462.9 40 -0.0006246 463.1 40 -0.0006122 463.2 40 -0.0006246 463.3 40 -0.0006246 463.4 40 -0.0006246 463.6 40 -0.0006246 463.7 40 -0.0006246 463.8 39 -0.0006246 463.9 39 -0.0006369 464.1 39 -0.0006493 464.2 39 -0.0006617 464.3 39 -0.0006617 464.4 38 -0.0006617 464.6 38 -0.0006617 464.7 38 -0.0006988 464.8 38 -0.0007235 464.9 38 -0.0007359 465.1 38 -0.0007359 465.2 38 -0.0007606 465.3 38 -0.0007606 465.4 38 -0.0007482 465.6 38 -0.0007482 465.7 37 -0.0007359 465.8 37 -0.0007359 465.9 37 -0.0007482 466.1 37 -0.0007606 466.2 37 -0.0007359 466.3 36 -0.0007359 466.4 36 -0.0007359 466.6 36 -0.0007359 466.7 36 -0.0007111 466.8 36 -0.0007111 466.9 36 -0.0006988 467 36 -0.0006988 467.2 36 -0.0007111 467.3 35 -0.0007111 467.4 34 -0.0007111 467.5 35 -0.0007235 467.7 35 -0.0007359 467.8 35 -0.0007482 467.9 34 -0.0007606 468 34 -0.0007606 468.2 34 -0.0007606 468.3 34 -0.0007606 468.4 34 -0.0007606 468.5 34 -0.0007606 468.7 34 -0.0007606 468.8 34 -0.0007482 468.9 34 -0.0007359 469 34 -0.0007359 469.2 34 -0.0007359 469.3 34 -0.0007111 469.4 34 -0.0007111 469.5 33 -0.0007111 469.7 33 -0.0007235 469.8 33 -0.0007235 469.9 32 -0.0007235 470 33 -0.0007235 470.2 32 -0.0007235 470.3 32 -0.0007235 470.4 32 -0.0007235 470.5 32 -0.0007235 470.7 31 -0.0007235 470.8 31 -0.0007359 470.9 31 -0.0007482 471 31 -0.0007606 471.2 31 -0.0007606 471.3 31 -0.0007606 471.4 31 -0.000773 471.5 31 -0.0007853 471.7 30 -0.0007977 471.8 30 -0.0008101 471.9 30 -0.0008101 472 30 -0.0007977 472.2 30 -0.0007853 472.3 30 -0.000773 472.4 30 -0.0007606 472.5 30 -0.0007482 472.7 30 -0.0007606 472.8 30 -0.0007606 472.9 30 -0.000773 473 30 -0.0007977 473.1 30 -0.0007977 473.3 30 -0.0008101 473.4 30 -0.0008101 473.5 30 -0.0008101 473.6 30 -0.0008101 473.8 30 -0.0007977 473.9 30 -0.000773 474 30 -0.0007482 474.1 29 -0.0007359 474.3 29 -0.0007359 474.4 29 -0.0007359 474.5 29 -0.0007482 474.6 29 -0.0007606 474.8 29 -0.0007606 474.9 28 -0.0007606 475 29 -0.000773 475.1 28 -0.0007606 475.3 28 -0.000773 475.4 28 -0.0007606 475.5 27 -0.0007606 475.6 27 -0.0007482 475.8 27 -0.0007359 475.9 27 -0.0007482 476 27 -0.0007606 476.1 27 -0.0007606 476.3 27 -0.000773 476.4 27 -0.000773 476.5 27 -0.0007853 476.6 27 -0.000773 476.8 27 -0.000773 476.9 27 -0.0007606 477 27 -0.0007606 477.1 27 -0.0007606 477.3 27 -0.000773 477.4 27 -0.0007606 477.5 27 -0.000773 477.6 27 -0.000773 477.8 27 -0.000773 477.9 27 -0.000773 478 27 -0.000773 478.1 26 -0.000773 478.3 26 -0.000773 478.4 26 -0.000773 478.5 26 -0.0007853 478.6 26 -0.000773 478.8 26 -0.000773 478.9 26 -0.000773 479 26 -0.000773 479.1 26 -0.000773 479.3 26 -0.000773 479.4 26 -0.000773 479.5 25 -0.000773 479.6 26 -0.000773 479.7 26 -0.0007606 479.9 25 -0.0007606 480 25 -0.0007606 480.1 25 -0.0007606 480.2 24 -0.0007606 480.4 25 -0.0007482 480.5 24 -0.000773 480.6 24 -0.0007853 480.7 24 -0.0007977 480.9 24 -0.0008101 481 25 -0.0008101 481.1 24 -0.0008225 481.2 24 -0.0008101 481.4 24 -0.0007977 481.5 24 -0.0007977 481.6 24 -0.0007853 481.7 23 -0.0007853 481.9 24 -0.0007977 482 24 -0.0007853 482.1 24 -0.0007853 482.2 23 -0.0007977 482.4 23 -0.0007977 482.5 23 -0.0007853 482.6 23 -0.0007606 482.7 23 -0.0007606 482.9 23 -0.0007606 483 23 -0.0007606 483.1 23 -0.0007606 483.2 23 -0.0007853 483.4 23 -0.0008101 483.5 23 -0.0008225 483.6 23 -0.0008225 483.7 23 -0.0008225 483.9 23 -0.0008225 484 23 -0.0008348 484.1 23 -0.0008225 484.2 23 -0.0008101 484.4 23 -0.0008101 484.5 23 -0.0008101 484.6 23 -0.0008101 484.7 23 -0.0008225 484.9 23 -0.0008225 485 23 -0.0008225 485.1 23 -0.0008225 485.2 23 -0.0008225 485.4 23 -0.0008225 485.5 22 -0.0008225 485.6 23 -0.0008101 485.7 22 -0.0008101 485.8 22 -0.0008101 486 22 -0.0008225 486.1 22 -0.0008225 486.2 23 -0.0008225 486.3 22 -0.0008225 486.5 22 -0.0008225 486.6 21 -0.0008225 486.7 21 -0.0008225 486.8 21 -0.0008225 487 21 -0.0008225 487.1 21 -0.0008225 487.2 22 -0.0008225 487.3 21 -0.0008101 487.5 21 -0.0008101 487.6 21 -0.0008101 487.7 21 -0.0008225 487.8 21 -0.0008225 488 21 -0.0008225 488.1 21 -0.0008225 488.2 21 -0.0008225 488.3 21 -0.0008348 488.5 21 -0.0008225 488.6 21 -0.0008101 488.7 21 -0.0008101 488.8 21 -0.0008101 489 21 -0.0008225 489.1 21 -0.0008225 489.2 21 -0.0008225 489.3 21 -0.0008225 489.5 21 -0.0008225 489.6 21 -0.0008348 489.7 20 -0.0008225 489.8 20 -0.0008101 490 20 -0.0008101 490.1 20 -0.0008101 490.2 20 -0.0008225 490.3 20 -0.0008225 490.5 20 -0.0008225 490.6 20 -0.0008225 490.7 20 -0.0008225 490.8 20 -0.0008101 491 20 -0.0007977 491.1 20 -0.0007977 491.2 20 -0.0007977 491.3 20 -0.0008101 491.5 20 -0.0008101 491.6 20 -0.0008225 491.7 19 -0.0008101 491.8 20 -0.0007977 492 20 -0.0007977 492.1 19 -0.000773 492.2 19 -0.0007977 492.3 20 -0.0008101 492.4 20 -0.0007853 492.6 19 -0.000773 492.7 19 -0.0007853 492.8 19 -0.0007977 492.9 19 -0.0008101 493.1 19 -0.0008101 493.2 19 -0.0008225 493.3 19 -0.0008225 493.4 19 -0.0008225 493.6 19 -0.0008225 493.7 19 -0.0008225 493.8 19 -0.0008225 493.9 19 -0.0008225 494.1 19 -0.0008225 494.2 19 -0.0008348 494.3 19 -0.0008225 494.4 19 -0.0008101 494.6 18 -0.0008101 494.7 19 -0.0008101 494.8 19 -0.0008225 494.9 18 -0.0008225 495.1 18 -0.0008225 495.2 18 -0.0008225 495.3 19 -0.0008225 495.4 18 -0.0008225 495.6 18 -0.0008348 495.7 19 -0.0008225 495.8 18 -0.0008225 495.9 18 -0.0008101 496.1 18 -0.0008225 496.2 18 -0.0008348 496.3 18 -0.0008596 496.4 18 -0.0008719 496.6 18 -0.0008967 496.7 18 -0.0009214 496.8 18 -0.0009214 496.9 18 -0.000909 497.1 18 -0.0008967 497.2 18 -0.0008719 497.3 18 -0.0008472 497.4 18 -0.0008225 497.6 18 -0.0008225 497.7 18 -0.0008101 497.8 18 -0.0008101 497.9 18 -0.0008225 498.1 18 -0.0008225 498.2 18 -0.0008225 498.3 18 -0.0008225 498.4 17 -0.0008596 498.6 18 -0.0008596 498.7 17 -0.0008596 498.8 18 -0.0008596 498.9 17 -0.0008472 499 17 -0.0008472 499.2 17 -0.0008348 499.3 17 -0.0008348 499.4 17 -0.0008472 499.5 18 -0.0008596 499.7 17 -0.0008719 499.8 17 -0.0008967 499.9 17 -0.000909 500 17 -0.0008967 500.2 17 -0.0008967 500.3 17 -0.000909 500.4 17 -0.000909 500.5 17 -0.0008719 500.7 17 -0.0008596 500.8 17 -0.0008596 500.9 16 -0.0008596 501 17 -0.0008596 501.2 17 -0.0008596 501.3 16 -0.0008596 501.4 16 -0.0008719 501.5 16 -0.0008719 501.7 16 -0.0008719 501.8 16 -0.0008596 501.9 16 -0.0008596 502 16 -0.0008348 502.2 16 -0.0008348 502.3 16 -0.0008348 502.4 16 -0.0008348 502.5 16 -0.0008348 502.7 16 -0.0008348 502.8 16 -0.0008225 502.9 16 -0.0008225 503 16 -0.0008348 503.2 16 -0.0008472 503.3 16 -0.0008472 503.4 16 -0.0008596 503.5 16 -0.0008596 503.7 17 -0.0008596 503.8 16 -0.0008719 503.9 16 -0.0008719 504 16 -0.0008719 504.2 16 -0.0008719 504.3 16 -0.0008719 504.4 16 -0.0008719 504.5 16 -0.0008719 504.7 16 -0.0008843 504.8 16 -0.0008719 504.9 16 -0.0008719 505 16 -0.0008719 505.1 16 -0.0008719 505.3 16 -0.0008843 505.4 16 -0.0008843 505.5 16 -0.0008719 505.6 16 -0.0008843 505.8 16 -0.0008719 505.9 16 -0.0008719 506 16 -0.0008719 506.1 16 -0.0008843 506.3 16 -0.0008843 506.4 16 -0.0008967 506.5 16 -0.000909 506.6 16 -0.0009214 506.8 16 -0.000909 506.9 16 -0.000909 507 16 -0.0008967 507.1 16 -0.0008967 507.3 16 -0.0008843 507.4 16 -0.0008843 507.5 15 -0.0008967 507.6 16 -0.0008967 507.8 15 -0.000909 507.9 15 -0.0009214 508 16 -0.0009214 508.1 15 -0.0009214 508.3 15 -0.0009214 508.4 16 -0.0009338 508.5 15 -0.0009461 508.6 15 -0.0009338 508.8 16 -0.0009338 508.9 15 -0.0009338 509 15 -0.0009338 509.1 15 -0.0009338 509.3 15 -0.0009214 509.4 15 -0.000909 509.5 32 0.21 0.05 0.66 0.002 0.007 0.75 2.11 0.83 0.31 0 0.62 0 0 0 5 -1.857e-05 0 6 -6.191e-06 0.106 7 6.191e-06 0.2119 6 6.191e-06 0.3179 6 6.191e-06 0.4238 7 -6.191e-06 0.5298 8 -1.857e-05 0.6357 9 -4.334e-05 0.7417 10 -6.81e-05 0.8477 13 -5.572e-05 0.9536 15 -5.572e-05 1.06 18 -3.095e-05 1.166 20 -6.191e-06 1.271 23 6.191e-06 1.377 27 6.191e-06 1.483 30 6.191e-06 1.589 34 1.857e-05 1.695 38 4.334e-05 1.801 41 8.048e-05 1.907 46 0.00013 2.013 50 0.0001672 2.119 54 0.0002167 2.225 59 0.0002538 2.331 63 0.0003034 2.437 67 0.0003405 2.543 71 0.00039 2.649 76 0.0004396 2.755 81 0.0004767 2.861 84 0.0005386 2.967 89 0.0005881 3.073 93 0.0006253 3.179 97 0.0006748 3.285 101 0.0007243 3.391 106 0.0007739 3.497 109 0.000811 3.603 113 0.0008729 3.709 118 0.0009224 3.814 121 0.000972 3.92 126 0.001009 4.026 129 0.001059 4.132 134 0.001096 4.238 137 0.001145 4.344 141 0.001195 4.45 144 0.001232 4.556 148 0.001269 4.662 152 0.001306 4.768 156 0.001331 4.874 159 0.001368 4.98 163 0.001405 5.086 166 0.001455 5.192 169 0.001492 5.298 173 0.001542 5.404 177 0.001591 5.51 180 0.001616 5.616 184 0.001665 5.722 187 0.001727 5.828 190 0.001814 5.934 193 0.001913 6.04 197 0.002024 6.146 201 0.002111 6.252 203 0.00221 6.357 206 0.002297 6.463 210 0.002371 6.569 213 0.002433 6.675 217 0.002483 6.781 220 0.00252 6.887 224 0.002557 6.993 227 0.002606 7.099 231 0.002656 7.205 234 0.002693 7.311 237 0.00273 7.417 242 0.002767 7.523 245 0.002804 7.629 248 0.002842 7.735 252 0.002891 7.841 256 0.002928 7.947 259 0.002978 8.053 262 0.003027 8.159 265 0.003077 8.265 269 0.003126 8.371 273 0.003176 8.477 276 0.003225 8.583 280 0.00325 8.689 284 0.0033 8.795 287 0.003337 8.9 290 0.003362 9.006 293 0.003399 9.112 297 0.003448 9.218 300 0.003498 9.324 304 0.003535 9.43 307 0.003585 9.536 311 0.003634 9.642 314 0.003696 9.748 318 0.003745 9.854 321 0.003795 9.96 324 0.003845 10.07 328 0.003894 10.17 331 0.003931 10.28 334 0.003968 10.38 338 0.00403 10.49 342 0.00408 10.6 345 0.004154 10.7 349 0.004241 10.81 353 0.004303 10.91 356 0.004389 11.02 360 0.004476 11.13 363 0.004501 11.23 367 0.004513 11.34 370 0.004526 11.44 374 0.004526 11.55 378 0.004526 11.66 381 0.004538 11.76 384 0.00455 11.87 388 0.00455 11.97 392 0.004563 12.08 395 0.004575 12.19 398 0.0046 12.29 401 0.004625 12.4 404 0.004662 12.5 407 0.004687 12.61 411 0.004724 12.71 414 0.004761 12.82 417 0.00481 12.93 421 0.004835 13.03 424 0.004885 13.14 428 0.004934 13.24 431 0.004971 13.35 435 0.005021 13.46 438 0.005058 13.56 442 0.005107 13.67 445 0.005132 13.77 449 0.005194 13.88 453 0.005244 13.99 456 0.005306 14.09 460 0.005392 14.2 464 0.005467 14.3 467 0.005541 14.41 470 0.005615 14.52 474 0.005677 14.62 477 0.005751 14.73 480 0.005801 14.83 484 0.005875 14.94 487 0.005912 15.05 490 0.005974 15.15 494 0.006024 15.26 497 0.006073 15.36 501 0.006123 15.47 504 0.006172 15.58 507 0.006222 15.68 510 0.006271 15.79 515 0.006321 15.89 518 0.006346 16 521 0.006408 16.11 524 0.006457 16.21 528 0.006507 16.32 532 0.006544 16.42 535 0.006593 16.53 539 0.006655 16.64 542 0.006692 16.74 546 0.006767 16.85 549 0.006804 16.95 553 0.006853 17.06 557 0.006903 17.17 560 0.006952 17.27 564 0.007002 17.38 567 0.007027 17.48 571 0.007089 17.59 574 0.007126 17.69 578 0.007163 17.8 581 0.007212 17.91 585 0.007262 18.01 588 0.007311 18.12 591 0.007349 18.22 595 0.007411 18.33 598 0.00746 18.44 601 0.00751 18.54 604 0.007559 18.65 608 0.007621 18.75 611 0.007671 18.86 614 0.007732 18.97 618 0.007794 19.07 621 0.007856 19.18 625 0.007906 19.28 628 0.007943 19.39 632 0.008005 19.5 635 0.008067 19.6 639 0.008116 19.71 642 0.008178 19.81 646 0.008228 19.92 650 0.00829 20.03 653 0.008339 20.13 656 0.008389 20.24 660 0.008426 20.34 663 0.008475 20.45 667 0.008512 20.56 670 0.008574 20.66 674 0.008624 20.77 677 0.008661 20.87 681 0.008711 20.98 684 0.008748 21.09 687 0.008797 21.19 690 0.008847 21.3 693 0.008896 21.4 697 0.008933 21.51 700 0.008971 21.62 704 0.009045 21.72 707 0.009082 21.83 711 0.009144 21.93 714 0.009193 22.04 718 0.009255 22.15 721 0.00933 22.25 725 0.009379 22.36 728 0.009441 22.46 730 0.009503 22.57 732 0.00954 22.68 736 0.009577 22.78 737 0.009614 22.89 739 0.009639 22.99 741 0.009676 23.1 743 0.009738 23.2 746 0.009763 23.31 749 0.009837 23.42 751 0.009887 23.52 753 0.009949 23.63 753 0.01001 23.73 754 0.01007 23.84 756 0.01013 23.95 757 0.0102 24.05 760 0.01027 24.16 761 0.01031 24.26 764 0.01038 24.37 765 0.01047 24.48 768 0.01054 24.58 770 0.01063 24.69 772 0.01068 24.79 775 0.01079 24.9 779 0.01087 25.01 782 0.01098 25.11 786 0.01108 25.22 790 0.01117 25.32 793 0.01129 25.43 799 0.01137 25.54 801 0.01148 25.64 803 0.01157 25.75 807 0.01168 25.85 812 0.01178 25.96 815 0.01188 26.07 820 0.01199 26.17 824 0.01209 26.28 828 0.01215 26.38 832 0.01221 26.49 837 0.01213 26.6 842 0.01205 26.7 847 0.01188 26.81 853 0.01169 26.91 860 0.0115 27.02 867 0.01126 27.13 872 0.01108 27.23 879 0.01091 27.34 885 0.0108 27.44 891 0.01073 27.55 897 0.01065 27.66 903 0.01063 27.76 907 0.01063 27.87 912 0.01064 27.97 918 0.01068 28.08 922 0.0107 28.18 927 0.01078 28.29 931 0.01084 28.4 935 0.0109 28.5 939 0.01098 28.61 943 0.01103 28.71 947 0.01109 28.82 950 0.01114 28.93 953 0.01122 29.03 956 0.01127 29.14 959 0.01135 29.24 962 0.01142 29.35 965 0.01148 29.46 968 0.01156 29.56 972 0.01163 29.67 974 0.01168 29.77 978 0.01174 29.88 980 0.01181 29.99 983 0.01187 30.09 986 0.01193 30.2 988 0.01202 30.3 991 0.01208 30.41 994 0.01217 30.52 997 0.01224 30.62 1000 0.01234 30.73 1003 0.01241 30.83 1005 0.01249 30.94 1008 0.01256 31.05 1011 0.01264 31.15 1014 0.01269 31.26 1017 0.0127 31.36 1019 0.01277 31.47 1022 0.01285 31.58 1026 0.01292 31.68 1029 0.01301 31.79 1032 0.01309 31.89 1036 0.01317 32 1038 0.01324 32.11 1042 0.01334 32.21 1045 0.0134 32.32 1048 0.0135 32.42 1051 0.01358 32.53 1054 0.01368 32.64 1058 0.01377 32.74 1061 0.01385 32.85 1065 0.01397 32.95 1068 0.01405 33.06 1072 0.01415 33.16 1075 0.01422 33.27 1078 0.01432 33.38 1081 0.01439 33.48 1085 0.01448 33.59 1089 0.01459 33.69 1092 0.01467 33.8 1096 0.01478 33.91 1099 0.01486 34.01 1103 0.01496 34.12 1106 0.01505 34.22 1110 0.01514 34.33 1114 0.01524 34.44 1118 0.01531 34.54 1121 0.01541 34.65 1125 0.01548 34.75 1128 0.01558 34.86 1132 0.01568 34.97 1135 0.01579 35.07 1139 0.01589 35.18 1143 0.01598 35.28 1147 0.01608 35.39 1150 0.01615 35.5 1153 0.01626 35.6 1157 0.01635 35.71 1160 0.01642 35.81 1164 0.01652 35.92 1168 0.01661 36.03 1172 0.01672 36.13 1175 0.01681 36.24 1178 0.01689 36.34 1181 0.01697 36.45 1185 0.01706 36.56 1188 0.01712 36.66 1192 0.0172 36.77 1195 0.01729 36.87 1199 0.01737 36.98 1201 0.01746 37.09 1203 0.01754 37.19 1205 0.0176 37.3 1207 0.01765 37.4 1208 0.0177 37.51 1209 0.01774 37.62 1211 0.01776 37.72 1212 0.0178 37.83 1212 0.01781 37.93 1213 0.01784 38.04 1213 0.01786 38.14 1214 0.01786 38.25 1214 0.01786 38.36 1214 0.01786 38.46 1214 0.01786 38.57 1214 0.01786 38.67 1214 0.01785 38.78 1213 0.01784 38.89 1212 0.01781 38.99 1212 0.01779 39.1 1212 0.01776 39.2 1212 0.01774 39.31 1211 0.0177 39.42 1211 0.01769 39.52 1209 0.01766 39.63 1209 0.01766 39.73 1208 0.01765 39.84 1208 0.01764 39.95 1207 0.01763 40.05 1206 0.01763 40.16 1206 0.01764 40.26 1205 0.01763 40.37 1204 0.01761 40.48 1204 0.0176 40.58 1204 0.01758 40.69 1203 0.01756 40.79 1203 0.01753 40.9 1202 0.01751 41.01 1201 0.0175 41.11 1201 0.0175 41.22 1201 0.01749 41.32 1201 0.01749 41.43 1201 0.01748 41.54 1200 0.01746 41.64 1200 0.01745 41.75 1200 0.01744 41.85 1200 0.01744 41.96 1199 0.01743 42.07 1199 0.01743 42.17 1198 0.01742 42.28 1198 0.01742 42.38 1198 0.0174 42.49 1197 0.01739 42.6 1198 0.01739 42.7 1197 0.01739 42.81 1197 0.01737 42.91 1198 0.01738 43.02 1197 0.01737 43.12 1197 0.01737 43.23 1197 0.01737 43.34 1197 0.01737 43.44 1197 0.01737 43.55 1197 0.01737 43.65 1197 0.01737 43.76 1197 0.01737 43.87 1197 0.01737 43.97 1197 0.01737 44.08 1197 0.01737 44.18 1197 0.01737 44.29 1197 0.01737 44.4 1197 0.01738 44.5 1197 0.01739 44.61 1197 0.0174 44.71 1197 0.0174 44.82 1197 0.0174 44.93 1198 0.0174 45.03 1198 0.01742 45.14 1198 0.01742 45.24 1198 0.0174 45.35 1198 0.01742 45.46 1198 0.01742 45.56 1198 0.01742 45.67 1198 0.01742 45.77 1198 0.01739 45.88 1198 0.01739 45.99 1198 0.0174 46.09 1199 0.0174 46.2 1199 0.0174 46.3 1199 0.0174 46.41 1198 0.01742 46.52 1199 0.01742 46.62 1199 0.01743 46.73 1199 0.01743 46.83 1199 0.01743 46.94 1199 0.01742 47.05 1199 0.01742 47.15 1199 0.01742 47.26 1199 0.01743 47.36 1199 0.01744 47.47 1199 0.01744 47.58 1200 0.01744 47.68 1199 0.01746 47.79 1199 0.01746 47.89 1199 0.01748 48 1199 0.01748 48.1 1199 0.01746 48.21 1199 0.01746 48.32 1199 0.01744 48.42 1199 0.01743 48.53 1199 0.01742 48.63 1200 0.0174 48.74 1199 0.01739 48.85 1199 0.01738 48.95 1200 0.01738 49.06 1199 0.01738 49.16 1199 0.01737 49.27 1200 0.01737 49.38 1199 0.01737 49.48 1199 0.01737 49.59 1199 0.01737 49.69 1200 0.01738 49.8 1199 0.01738 49.91 1199 0.01739 50.01 1200 0.0174 50.12 1199 0.0174 50.22 1199 0.0174 50.33 1200 0.0174 50.44 1200 0.0174 50.54 1200 0.01742 50.65 1200 0.01743 50.75 1199 0.01744 50.86 1199 0.01743 50.97 1199 0.01742 51.07 1200 0.01742 51.18 1200 0.01743 51.28 1200 0.01743 51.39 1200 0.01742 51.5 1200 0.01742 51.6 1200 0.01742 51.71 1200 0.01742 51.81 1199 0.0174 51.92 1200 0.01739 52.03 1200 0.01739 52.13 1199 0.0174 52.24 1199 0.0174 52.34 1199 0.0174 52.45 1199 0.0174 52.56 1200 0.0174 52.66 1199 0.01742 52.77 1200 0.0174 52.87 1199 0.0174 52.98 1199 0.01742 53.08 1200 0.01742 53.19 1199 0.0174 53.3 1199 0.0174 53.4 1199 0.01739 53.51 1199 0.0174 53.61 1199 0.0174 53.72 1199 0.0174 53.83 1199 0.01739 53.93 1200 0.01738 54.04 1199 0.0174 54.14 1200 0.0174 54.25 1199 0.0174 54.36 1199 0.0174 54.46 1199 0.0174 54.57 1199 0.01742 54.67 1199 0.01742 54.78 1199 0.0174 54.89 1199 0.01742 54.99 1199 0.01742 55.1 1199 0.01742 55.2 1199 0.01742 55.31 1200 0.01742 55.42 1199 0.01742 55.52 1200 0.01742 55.63 1199 0.01742 55.73 1199 0.01743 55.84 1199 0.01743 55.95 1199 0.01743 56.05 1199 0.01743 56.16 1199 0.01743 56.26 1199 0.01743 56.37 1199 0.01743 56.48 1200 0.01742 56.58 1199 0.01742 56.69 1199 0.0174 56.79 1199 0.01739 56.9 1199 0.01739 57.01 1199 0.01738 57.11 1199 0.01738 57.22 1199 0.01737 57.32 1199 0.01737 57.43 1199 0.01737 57.54 1199 0.01737 57.64 1199 0.01737 57.75 1199 0.01737 57.85 1199 0.01737 57.96 1199 0.01739 58.06 1200 0.01738 58.17 1200 0.01739 58.28 1200 0.0174 58.38 1200 0.0174 58.49 1200 0.01742 58.59 1200 0.0174 58.7 1200 0.01739 58.81 1200 0.01738 58.91 1200 0.01738 59.02 1199 0.01738 59.12 1199 0.01738 59.23 1200 0.01737 59.34 1199 0.01737 59.44 1199 0.01737 59.55 1199 0.01737 59.65 1199 0.01738 59.76 1199 0.01739 59.87 1199 0.01738 59.97 1199 0.01738 60.08 1199 0.01737 60.18 1199 0.01737 60.29 1199 0.01738 60.4 1199 0.01739 60.5 1199 0.01739 60.61 1199 0.01739 60.71 1199 0.01737 60.82 1198 0.01738 60.93 1199 0.01738 61.03 1199 0.01737 61.14 1199 0.01735 61.24 1199 0.01734 61.35 1199 0.01734 61.46 1199 0.01735 61.56 1199 0.01737 61.67 1199 0.01735 61.77 1199 0.01735 61.88 1199 0.01737 61.99 1199 0.01737 62.09 1199 0.01737 62.2 1199 0.01738 62.3 1199 0.01739 62.41 1199 0.01739 62.52 1199 0.0174 62.62 1199 0.0174 62.73 1199 0.0174 62.83 1199 0.01739 62.94 1199 0.01738 63.05 1199 0.01738 63.15 1199 0.01737 63.26 1199 0.01738 63.36 1199 0.01737 63.47 1199 0.01737 63.57 1200 0.01739 63.68 1199 0.01739 63.79 1199 0.01739 63.89 1199 0.01738 64 1199 0.01738 64.1 1199 0.01739 64.21 1199 0.0174 64.32 1199 0.0174 64.42 1199 0.01742 64.53 1200 0.0174 64.63 1199 0.0174 64.74 1199 0.0174 64.85 1199 0.01739 64.95 1199 0.01739 65.06 1199 0.0174 65.16 1200 0.0174 65.27 1199 0.0174 65.38 1199 0.0174 65.48 1199 0.01742 65.59 1200 0.01742 65.69 1199 0.0174 65.8 1199 0.01742 65.91 1199 0.01742 66.01 1199 0.01742 66.12 1199 0.01743 66.22 1199 0.01742 66.33 1199 0.01742 66.44 1199 0.01742 66.54 1199 0.01742 66.65 1199 0.0174 66.75 1199 0.01742 66.86 1199 0.01742 66.97 1200 0.01742 67.07 1200 0.01742 67.18 1199 0.0174 67.28 1199 0.01739 67.39 1199 0.0174 67.5 1199 0.0174 67.6 1199 0.0174 67.71 1199 0.0174 67.81 1199 0.01742 67.92 1199 0.0174 68.03 1199 0.01739 68.13 1199 0.01738 68.24 1199 0.01738 68.34 1199 0.01738 68.45 1199 0.01737 68.55 1199 0.01737 68.66 1199 0.01738 68.77 1199 0.01739 68.87 1199 0.01739 68.98 1199 0.01738 69.08 1200 0.01738 69.19 1200 0.01739 69.3 1199 0.01739 69.4 1199 0.01739 69.51 1199 0.01739 69.61 1199 0.01738 69.72 1200 0.01737 69.83 1199 0.01737 69.93 1199 0.01737 70.04 1199 0.01737 70.14 1199 0.01737 70.25 1199 0.01737 70.36 1199 0.01737 70.46 1199 0.01737 70.57 1199 0.01737 70.67 1199 0.01739 70.78 1199 0.01739 70.89 1199 0.01739 70.99 1199 0.0174 71.1 1199 0.0174 71.2 1199 0.0174 71.31 1199 0.0174 71.42 1199 0.01739 71.52 1199 0.01739 71.63 1200 0.01738 71.73 1199 0.01738 71.84 1200 0.01737 71.95 1199 0.01737 72.05 1200 0.01738 72.16 1199 0.01739 72.26 1199 0.0174 72.37 1199 0.01742 72.48 1199 0.01742 72.58 1200 0.0174 72.69 1200 0.0174 72.79 1200 0.0174 72.9 1200 0.0174 73.01 1200 0.01742 73.11 1200 0.0174 73.22 1200 0.01742 73.32 1200 0.01742 73.43 1200 0.01742 73.53 1200 0.01742 73.64 1200 0.01742 73.75 1200 0.01742 73.85 1200 0.01743 73.96 1200 0.01743 74.06 1200 0.01742 74.17 1200 0.01742 74.28 1200 0.0174 74.38 1200 0.0174 74.49 1200 0.0174 74.59 1200 0.01742 74.7 1200 0.01742 74.81 1200 0.01742 74.91 1200 0.01742 75.02 1200 0.01742 75.12 1200 0.01742 75.23 1200 0.0174 75.34 1200 0.01739 75.44 1199 0.01739 75.55 1200 0.0174 75.65 1200 0.0174 75.76 1200 0.01742 75.87 1199 0.0174 75.97 1199 0.01739 76.08 1199 0.01739 76.18 1199 0.0174 76.29 1199 0.0174 76.4 1199 0.0174 76.5 1199 0.01742 76.61 1199 0.0174 76.71 1199 0.0174 76.82 1199 0.01742 76.93 1199 0.0174 77.03 1199 0.01739 77.14 1200 0.01739 77.24 1199 0.0174 77.35 1198 0.0174 77.46 1199 0.01739 77.56 1199 0.01739 77.67 1199 0.01739 77.77 1199 0.01739 77.88 1199 0.01739 77.99 1199 0.01739 78.09 1199 0.01739 78.2 1199 0.0174 78.3 1199 0.01742 78.41 1199 0.01742 78.51 1199 0.01742 78.62 1199 0.0174 78.73 1200 0.0174 78.83 1199 0.01739 78.94 1199 0.01738 79.04 1199 0.01738 79.15 1199 0.01737 79.26 1199 0.01737 79.36 1199 0.01737 79.47 1199 0.01737 79.57 1199 0.01737 79.68 1199 0.01737 79.79 1199 0.01737 79.89 1200 0.01739 80 1199 0.0174 80.1 1199 0.0174 80.21 1199 0.01742 80.32 1199 0.01742 80.42 1199 0.01742 80.53 1199 0.01742 80.63 1199 0.01743 80.74 1199 0.01743 80.85 1199 0.01744 80.95 1199 0.01744 81.06 1199 0.01744 81.16 1199 0.01744 81.27 1199 0.01744 81.38 1199 0.01743 81.48 1200 0.01742 81.59 1200 0.01742 81.69 1199 0.0174 81.8 1199 0.0174 81.91 1199 0.01742 82.01 1199 0.01742 82.12 1199 0.01743 82.22 1199 0.01743 82.33 1200 0.01743 82.44 1199 0.01743 82.54 1199 0.01743 82.65 1200 0.01743 82.75 1199 0.01743 82.86 1199 0.01744 82.97 1200 0.01745 83.07 1199 0.01743 83.18 1199 0.01743 83.28 1199 0.01744 83.39 1199 0.01744 83.49 1200 0.01744 83.6 1199 0.01743 83.71 1199 0.01743 83.81 1200 0.01743 83.92 1199 0.01743 84.02 1200 0.01743 84.13 1200 0.01744 84.24 1199 0.01745 84.34 1199 0.01744 84.45 1199 0.01744 84.55 1199 0.01744 84.66 1199 0.01744 84.77 1199 0.01745 84.87 1199 0.01745 84.98 1199 0.01745 85.08 1199 0.01745 85.19 1200 0.01746 85.3 1199 0.01746 85.4 1199 0.01746 85.51 1199 0.01746 85.61 1199 0.01746 85.72 1199 0.01746 85.83 1199 0.01749 85.93 1199 0.01749 86.04 1199 0.01748 86.14 1199 0.01746 86.25 1199 0.01746 86.36 1199 0.01746 86.46 1199 0.01746 86.57 1199 0.01744 86.67 1199 0.01745 86.78 1199 0.01745 86.89 1199 0.01746 86.99 1199 0.01748 87.1 1199 0.01748 87.2 1199 0.01746 87.31 1200 0.01746 87.42 1200 0.01746 87.52 1199 0.01746 87.63 1199 0.01746 87.73 1199 0.01746 87.84 1199 0.01746 87.95 1198 0.01746 88.05 1199 0.01746 88.16 1200 0.01746 88.26 1199 0.01746 88.37 1199 0.01746 88.47 1199 0.01744 88.58 1199 0.01744 88.69 1199 0.01745 88.79 1199 0.01746 88.9 1199 0.01745 89 1200 0.01746 89.11 1199 0.01746 89.22 1199 0.01746 89.32 1199 0.01746 89.43 1199 0.01744 89.53 1199 0.01744 89.64 1199 0.01744 89.75 1200 0.01745 89.85 1199 0.01743 89.96 1199 0.01742 90.06 1199 0.0174 90.17 1199 0.01742 90.28 1199 0.0174 90.38 1199 0.0174 90.49 1199 0.01739 90.59 1199 0.01739 90.7 1199 0.01738 90.81 1199 0.01738 90.91 1199 0.01738 91.02 1199 0.01737 91.12 1199 0.01737 91.23 1200 0.01737 91.34 1199 0.01737 91.44 1199 0.01737 91.55 1199 0.01737 91.65 1199 0.01737 91.76 1199 0.01737 91.87 1199 0.01737 91.97 1199 0.01737 92.08 1199 0.01737 92.18 1199 0.01737 92.29 1199 0.01737 92.4 1199 0.01737 92.5 1199 0.01737 92.61 1199 0.01738 92.71 1200 0.01739 92.82 1199 0.01742 92.93 1199 0.01743 93.03 1199 0.01745 93.14 1199 0.01746 93.24 1199 0.01746 93.35 1199 0.01746 93.45 1200 0.01746 93.56 1199 0.01746 93.67 1199 0.01746 93.77 1199 0.01745 93.88 1199 0.01744 93.98 1199 0.01746 94.09 1199 0.01746 94.2 1200 0.01746 94.3 1199 0.01745 94.41 1199 0.01744 94.51 1199 0.01745 94.62 1199 0.01745 94.73 1199 0.01746 94.83 1199 0.01749 94.94 1199 0.01749 95.04 1199 0.01749 95.15 1199 0.01749 95.26 1200 0.01749 95.36 1199 0.01749 95.47 1199 0.01746 95.57 1199 0.01746 95.68 1199 0.01746 95.79 1199 0.01746 95.89 1199 0.01748 96 1199 0.01746 96.1 1199 0.01746 96.21 1199 0.01749 96.32 1199 0.01749 96.42 1199 0.01751 96.53 1200 0.01751 96.63 1199 0.01751 96.74 1199 0.01751 96.85 1198 0.01751 96.95 1199 0.01751 97.06 1199 0.01751 97.16 1200 0.01751 97.27 1199 0.01751 97.38 1199 0.01751 97.48 1199 0.0175 97.59 1199 0.0175 97.69 1199 0.01749 97.8 1200 0.01748 97.91 1200 0.01746 98.01 1199 0.01746 98.12 1199 0.01746 98.22 1199 0.01746 98.33 1200 0.01748 98.43 1199 0.01749 98.54 1199 0.01749 98.65 1199 0.0175 98.75 1199 0.0175 98.86 1199 0.01749 98.96 1199 0.01749 99.07 1199 0.01749 99.18 1199 0.0175 99.28 1199 0.0175 99.39 1199 0.0175 99.49 1199 0.0175 99.6 1199 0.01749 99.71 1199 0.01749 99.81 1199 0.0175 99.92 1199 0.01749 100 1200 0.0175 100.1 1199 0.01749 100.2 1199 0.01749 100.3 1200 0.01749 100.4 1199 0.0175 100.6 1199 0.01749 100.7 1200 0.01749 100.8 1199 0.01749 100.9 1199 0.01749 101 1199 0.01749 101.1 1199 0.01746 101.2 1199 0.01746 101.3 1199 0.01749 101.4 1199 0.01749 101.5 1199 0.0175 101.6 1199 0.0175 101.7 1199 0.0175 101.8 1199 0.01751 101.9 1199 0.01751 102 1199 0.01751 102.1 1199 0.01751 102.2 1199 0.0175 102.4 1199 0.01749 102.5 1199 0.01749 102.6 1199 0.01749 102.7 1199 0.01748 102.8 1199 0.01746 102.9 1198 0.01746 103 1199 0.01749 103.1 1199 0.0175 103.2 1199 0.0175 103.3 1199 0.0175 103.4 1199 0.0175 103.5 1199 0.01749 103.6 1199 0.01749 103.7 1199 0.01749 103.8 1199 0.01746 103.9 1200 0.01749 104.1 1199 0.01749 104.2 1199 0.01749 104.3 1199 0.0175 104.4 1200 0.0175 104.5 1199 0.01751 104.6 1200 0.01754 104.7 1199 0.01753 104.8 1199 0.01754 104.9 1200 0.01751 105 1199 0.01751 105.1 1199 0.01751 105.2 1199 0.01749 105.3 1199 0.01748 105.4 1199 0.01748 105.5 1199 0.01746 105.6 1199 0.01746 105.7 1200 0.01748 105.9 1199 0.01749 106 1200 0.01751 106.1 1199 0.01751 106.2 1199 0.01754 106.3 1199 0.01754 106.4 1199 0.01754 106.5 1199 0.01754 106.6 1200 0.01754 106.7 1199 0.01754 106.8 1200 0.01755 106.9 1199 0.01754 107 1199 0.01754 107.1 1200 0.01754 107.2 1199 0.01753 107.3 1200 0.01751 107.4 1199 0.01751 107.5 1199 0.0175 107.7 1199 0.01749 107.8 1199 0.01749 107.9 1199 0.01746 108 1199 0.01746 108.1 1199 0.01745 108.2 1199 0.01746 108.3 1200 0.01746 108.4 1199 0.01746 108.5 1199 0.01749 108.6 1199 0.01749 108.7 1199 0.0175 108.8 1199 0.01749 108.9 1199 0.01749 109 1199 0.01749 109.1 1199 0.01748 109.2 1199 0.01749 109.3 1199 0.01749 109.5 1199 0.01749 109.6 1200 0.01751 109.7 1199 0.01751 109.8 1199 0.01753 109.9 1199 0.01751 110 1200 0.01751 110.1 1200 0.01751 110.2 1200 0.01751 110.3 1199 0.01751 110.4 1200 0.0175 110.5 1199 0.01749 110.6 1199 0.01746 110.7 1199 0.01746 110.8 1199 0.01744 110.9 1199 0.01744 111 1199 0.01744 111.1 1198 0.01744 111.3 1199 0.01745 111.4 1199 0.01746 111.5 1199 0.01746 111.6 1199 0.01746 111.7 1199 0.01749 111.8 1199 0.01749 111.9 1198 0.0175 112 1199 0.01749 112.1 1199 0.01749 112.2 1199 0.01749 112.3 1199 0.01749 112.4 1199 0.01749 112.5 1199 0.01749 112.6 1199 0.01749 112.7 1199 0.01749 112.8 1199 0.01748 113 1199 0.01746 113.1 1199 0.01746 113.2 1199 0.01746 113.3 1199 0.01746 113.4 1200 0.01744 113.5 1199 0.01745 113.6 1199 0.01745 113.7 1199 0.01746 113.8 1199 0.01746 113.9 1200 0.01746 114 1199 0.01746 114.1 1199 0.01746 114.2 1199 0.01746 114.3 1200 0.01744 114.4 1199 0.01744 114.5 1199 0.01745 114.6 1200 0.01746 114.8 1199 0.01746 114.9 1199 0.01746 115 1200 0.01746 115.1 1199 0.01746 115.2 1199 0.01746 115.3 1199 0.01746 115.4 1199 0.01746 115.5 1199 0.01744 115.6 1199 0.01744 115.7 1200 0.01744 115.8 1200 0.01743 115.9 1199 0.01743 116 1199 0.01743 116.1 1199 0.01742 116.2 1199 0.01742 116.3 1199 0.01742 116.4 1199 0.01744 116.6 1199 0.01744 116.7 1199 0.01743 116.8 1199 0.01743 116.9 1199 0.01743 117 1199 0.01744 117.1 1200 0.01745 117.2 1199 0.01744 117.3 1199 0.01743 117.4 1199 0.01742 117.5 1199 0.01742 117.6 1199 0.0174 117.7 1199 0.01742 117.8 1199 0.01742 117.9 1199 0.01742 118 1199 0.01742 118.1 1199 0.0174 118.2 1200 0.0174 118.4 1199 0.0174 118.5 1199 0.01742 118.6 1199 0.01744 118.7 1199 0.01746 118.8 1199 0.01746 118.9 1199 0.01745 119 1199 0.01744 119.1 1199 0.01744 119.2 1200 0.01743 119.3 1199 0.01744 119.4 1199 0.01744 119.5 1199 0.01744 119.6 1199 0.01744 119.7 1199 0.01743 119.8 1199 0.01743 119.9 1199 0.01742 120.1 1199 0.01743 120.2 1199 0.01744 120.3 1199 0.01744 120.4 1199 0.01742 120.5 1199 0.01742 120.6 1199 0.01742 120.7 1199 0.01742 120.8 1199 0.01743 120.9 1199 0.01743 121 1199 0.01744 121.1 1199 0.01743 121.2 1199 0.01743 121.3 1199 0.01745 121.4 1199 0.01744 121.5 1199 0.01744 121.6 1199 0.01743 121.7 1199 0.01743 121.9 1199 0.01742 122 1199 0.0174 122.1 1198 0.01742 122.2 1199 0.01742 122.3 1199 0.0174 122.4 1200 0.01739 122.5 1200 0.01738 122.6 1199 0.01738 122.7 1199 0.01739 122.8 1199 0.01739 122.9 1199 0.0174 123 1199 0.0174 123.1 1199 0.0174 123.2 1199 0.01742 123.3 1200 0.01742 123.4 1199 0.0174 123.5 1199 0.01739 123.7 1199 0.01739 123.8 1199 0.01738 123.9 1200 0.01738 124 1199 0.01739 124.1 1199 0.01739 124.2 1199 0.01739 124.3 1199 0.01739 124.4 1199 0.01739 124.5 1199 0.01739 124.6 1200 0.0174 124.7 1199 0.01739 124.8 1199 0.01739 124.9 1200 0.01739 125 1199 0.01739 125.1 1199 0.01739 125.2 1199 0.01739 125.3 1199 0.01738 125.5 1199 0.0174 125.6 1199 0.0174 125.7 1200 0.01739 125.8 1200 0.01739 125.9 1199 0.01738 126 1199 0.01738 126.1 1199 0.01737 126.2 1199 0.01735 126.3 1200 0.01734 126.4 1200 0.01737 126.5 1199 0.01738 126.6 1199 0.01738 126.7 1199 0.01737 126.8 1199 0.01737 126.9 1199 0.01739 127 1199 0.01739 127.1 1199 0.01739 127.3 1200 0.01739 127.4 1199 0.0174 127.5 1199 0.01742 127.6 1199 0.01742 127.7 1199 0.01742 127.8 1199 0.01742 127.9 1199 0.01742 128 1200 0.01742 128.1 1200 0.0174 128.2 1199 0.01738 128.3 1199 0.01737 128.4 1199 0.01737 128.5 1199 0.01734 128.6 1199 0.01735 128.7 1199 0.01737 128.8 1199 0.01737 129 1199 0.01737 129.1 1199 0.01737 129.2 1200 0.01738 129.3 1199 0.01738 129.4 1200 0.01737 129.5 1200 0.01735 129.6 1200 0.01737 129.7 1200 0.01735 129.8 1199 0.01737 129.9 1200 0.01737 130 1199 0.01737 130.1 1199 0.01737 130.2 1200 0.01737 130.3 1200 0.01737 130.4 1200 0.01739 130.5 1200 0.01738 130.6 1200 0.01737 130.8 1200 0.01737 130.9 1199 0.01737 131 1199 0.01737 131.1 1200 0.01737 131.2 1200 0.01737 131.3 1199 0.01739 131.4 1199 0.01739 131.5 1199 0.01738 131.6 1199 0.01737 131.7 1199 0.01737 131.8 1199 0.01737 131.9 1199 0.01738 132 1199 0.01738 132.1 1199 0.01738 132.2 1200 0.01735 132.3 1199 0.01734 132.4 1200 0.01732 132.6 1199 0.01732 132.7 1199 0.01733 132.8 1199 0.01733 132.9 1199 0.01733 133 1199 0.01733 133.1 1199 0.01733 133.2 1199 0.01734 133.3 1199 0.01734 133.4 1199 0.01734 133.5 1199 0.01733 133.6 1199 0.01733 133.7 1199 0.01733 133.8 1199 0.01732 133.9 1199 0.01732 134 1199 0.01732 134.1 1199 0.01732 134.2 1199 0.01733 134.4 1199 0.01732 134.5 1199 0.01732 134.6 1199 0.01729 134.7 1199 0.01729 134.8 1199 0.01728 134.9 1200 0.01729 135 1199 0.0173 135.1 1199 0.01732 135.2 1199 0.01734 135.3 1199 0.01737 135.4 1200 0.01739 135.5 1199 0.0174 135.6 1199 0.01739 135.7 1199 0.01738 135.8 1199 0.01737 135.9 1199 0.01735 136.1 1200 0.01734 136.2 1199 0.01734 136.3 1199 0.01733 136.4 1199 0.01734 136.5 1199 0.01735 136.6 1199 0.01734 136.7 1200 0.01735 136.8 1199 0.01735 136.9 1199 0.01734 137 1200 0.01734 137.1 1199 0.01732 137.2 1199 0.01729 137.3 1199 0.01729 137.4 1199 0.01727 137.5 1199 0.01729 137.6 1199 0.0173 137.7 1200 0.01733 137.9 1200 0.01735 138 1199 0.01737 138.1 1199 0.01737 138.2 1199 0.01737 138.3 1199 0.01737 138.4 1199 0.01737 138.5 1199 0.01734 138.6 1199 0.01732 138.7 1200 0.01729 138.8 1200 0.01727 138.9 1199 0.01727 139 1199 0.01725 139.1 1200 0.01727 139.2 1199 0.01727 139.3 1199 0.01724 139.4 1199 0.01723 139.5 1200 0.01723 139.7 1199 0.01724 139.8 1199 0.01725 139.9 1199 0.01725 140 1199 0.01725 140.1 1199 0.01727 140.2 1199 0.01729 140.3 1200 0.0173 140.4 1199 0.01732 140.5 1199 0.01732 140.6 1200 0.01733 140.7 1199 0.01734 140.8 1199 0.01733 140.9 1199 0.01732 141 1199 0.01732 141.1 1199 0.01732 141.2 1199 0.01729 141.3 1199 0.01729 141.5 1199 0.01729 141.6 1199 0.0173 141.7 1200 0.01732 141.8 1199 0.0173 141.9 1199 0.0173 142 1200 0.01729 142.1 1199 0.01728 142.2 1199 0.01729 142.3 1199 0.01727 142.4 1199 0.01727 142.5 1199 0.01727 142.6 1199 0.01724 142.7 1200 0.01724 142.8 1200 0.01725 142.9 1199 0.01724 143 1199 0.01724 143.1 1199 0.01723 143.3 1199 0.01723 143.4 1199 0.01725 143.5 1199 0.01725 143.6 1199 0.01725 143.7 1200 0.01724 143.8 1199 0.01724 143.9 1199 0.01723 144 1199 0.01724 144.1 1200 0.01725 144.2 1199 0.01725 144.3 1200 0.01725 144.4 1200 0.01727 144.5 1200 0.01727 144.6 1199 0.01728 144.7 1200 0.01728 144.8 1200 0.01727 145 1199 0.01727 145.1 1199 0.01727 145.2 1199 0.01729 145.3 1199 0.01729 145.4 1199 0.01729 145.5 1199 0.01729 145.6 1199 0.01727 145.7 1199 0.01727 145.8 1199 0.01728 145.9 1200 0.01727 146 1199 0.01724 146.1 1199 0.01722 146.2 1199 0.01722 146.3 1199 0.01722 146.4 1199 0.01722 146.5 1199 0.0172 146.6 1199 0.01722 146.8 1199 0.01723 146.9 1199 0.01722 147 1200 0.0172 147.1 1199 0.0172 147.2 1199 0.0172 147.3 1199 0.0172 147.4 1199 0.01722 147.5 1200 0.01723 147.6 1200 0.01724 147.7 1199 0.01727 147.8 1199 0.01727 147.9 1199 0.01727 148 1199 0.01727 148.1 1199 0.01727 148.2 1200 0.01727 148.3 1200 0.01725 148.4 1200 0.01724 148.6 1199 0.01724 148.7 1199 0.01725 148.8 1199 0.01725 148.9 1199 0.01723 149 1199 0.01723 149.1 1199 0.01723 149.2 1199 0.01724 149.3 1200 0.01723 149.4 1199 0.01722 149.5 1199 0.0172 149.6 1199 0.01722 149.7 1199 0.01722 149.8 1200 0.01719 149.9 1199 0.01718 150 1199 0.0172 150.1 1199 0.01722 150.2 1199 0.01723 150.4 1199 0.01723 150.5 1199 0.01723 150.6 1200 0.01723 150.7 1200 0.01723 150.8 1199 0.01723 150.9 1199 0.01722 151 1199 0.01722 151.1 1200 0.01723 151.2 1200 0.01723 151.3 1199 0.01723 151.4 1200 0.01723 151.5 1199 0.0172 151.6 1199 0.0172 151.7 1199 0.01718 151.8 1199 0.01718 151.9 1200 0.01719 152 1199 0.0172 152.2 1199 0.01722 152.3 1199 0.01723 152.4 1199 0.01723 152.5 1199 0.01723 152.6 1199 0.01723 152.7 1199 0.01723 152.8 1199 0.01723 152.9 1199 0.01724 153 1200 0.01725 153.1 1199 0.01725 153.2 1199 0.01723 153.3 1199 0.01722 153.4 1199 0.01722 153.5 1199 0.0172 153.6 1200 0.01719 153.7 1199 0.01719 153.9 1199 0.0172 154 1199 0.01722 154.1 1200 0.01723 154.2 1199 0.01722 154.3 1199 0.01722 154.4 1199 0.01723 154.5 1200 0.01723 154.6 1199 0.01724 154.7 1199 0.01723 154.8 1199 0.01722 154.9 1199 0.01722 155 1199 0.01719 155.1 1200 0.0172 155.2 1200 0.01722 155.3 1199 0.01723 155.4 1199 0.01724 155.5 1199 0.01724 155.7 1199 0.01723 155.8 1199 0.01723 155.9 1199 0.01722 156 1199 0.01722 156.1 1199 0.01722 156.2 1199 0.01718 156.3 1199 0.01718 156.4 1199 0.01719 156.5 1199 0.0172 156.6 1199 0.01722 156.7 1199 0.01723 156.8 1199 0.01723 156.9 1199 0.01724 157 1199 0.01724 157.1 1199 0.01724 157.2 1199 0.01727 157.3 1199 0.01724 157.5 1200 0.01724 157.6 1199 0.01724 157.7 1199 0.01723 157.8 1199 0.01724 157.9 1199 0.01724 158 1200 0.01723 158.1 1199 0.01723 158.2 1199 0.01722 158.3 1199 0.01722 158.4 1199 0.01723 158.5 1199 0.01725 158.6 1199 0.01727 158.7 1199 0.01727 158.8 1200 0.01725 158.9 1199 0.01725 159 1199 0.01725 159.1 1200 0.01725 159.3 1200 0.01724 159.4 1199 0.01723 159.5 1199 0.01723 159.6 1200 0.01723 159.7 1199 0.01723 159.8 1200 0.01722 159.9 1200 0.0172 160 1199 0.01719 160.1 1199 0.0172 160.2 1199 0.0172 160.3 1199 0.01722 160.4 1199 0.01723 160.5 1199 0.01723 160.6 1199 0.01723 160.7 1200 0.01722 160.8 1199 0.01722 161 1199 0.01722 161.1 1200 0.01723 161.2 1199 0.01723 161.3 1200 0.01724 161.4 1200 0.01724 161.5 1199 0.01724 161.6 1199 0.01723 161.7 1199 0.01723 161.8 1199 0.01722 161.9 1200 0.01722 162 1200 0.01722 162.1 1200 0.01722 162.2 1199 0.01722 162.3 1199 0.01719 162.4 1199 0.01718 162.5 1199 0.01718 162.6 1200 0.01718 162.8 1199 0.0172 162.9 1199 0.01722 163 1199 0.01722 163.1 1199 0.01722 163.2 1199 0.0172 163.3 1199 0.01719 163.4 1199 0.01719 163.5 1199 0.01719 163.6 1199 0.0172 163.7 1199 0.0172 163.8 1199 0.01722 163.9 1199 0.01719 164 1200 0.01718 164.1 1199 0.01718 164.2 1199 0.01719 164.3 1199 0.01719 164.4 1200 0.01719 164.6 1200 0.01718 164.7 1199 0.01717 164.8 1199 0.01717 164.9 1199 0.01718 165 1199 0.01718 165.1 1200 0.01718 165.2 1200 0.01717 165.3 1199 0.01715 165.4 1200 0.01715 165.5 1199 0.01714 165.6 1199 0.01714 165.7 1199 0.01714 165.8 1199 0.01714 165.9 1199 0.01715 166 1199 0.01717 166.1 1200 0.01717 166.2 1199 0.01719 166.4 1200 0.01719 166.5 1199 0.01718 166.6 1200 0.01718 166.7 1199 0.01717 166.8 1200 0.01717 166.9 1199 0.01718 167 1199 0.01719 167.1 1199 0.01719 167.2 1200 0.01719 167.3 1199 0.0172 167.4 1200 0.01722 167.5 1199 0.01722 167.6 1200 0.01724 167.7 1200 0.01724 167.8 1199 0.01723 167.9 1200 0.01723 168 1199 0.01722 168.2 1199 0.0172 168.3 1199 0.0172 168.4 1200 0.01718 168.5 1199 0.01718 168.6 1199 0.01718 168.7 1199 0.01717 168.8 1199 0.01717 168.9 1199 0.01717 169 1200 0.01717 169.1 1199 0.01718 169.2 1199 0.01718 169.3 1199 0.01717 169.4 1200 0.01717 169.5 1199 0.01717 169.6 1199 0.01717 169.7 1200 0.01718 169.9 1199 0.0172 170 1199 0.01722 170.1 1199 0.01723 170.2 1199 0.01723 170.3 1200 0.01723 170.4 1200 0.01725 170.5 1199 0.01723 170.6 1200 0.01722 170.7 1199 0.0172 170.8 1199 0.01719 170.9 1199 0.01719 171 1199 0.01718 171.1 1199 0.01718 171.2 1199 0.01718 171.3 1200 0.01718 171.4 1199 0.01719 171.5 1199 0.01718 171.7 1199 0.01717 171.8 1200 0.01718 171.9 1200 0.01719 172 1200 0.0172 172.1 1200 0.0172 172.2 1199 0.0172 172.3 1199 0.0172 172.4 1199 0.0172 172.5 1199 0.0172 172.6 1200 0.01722 172.7 1200 0.0172 172.8 1199 0.0172 172.9 1199 0.0172 173 1199 0.01719 173.1 1200 0.01719 173.2 1200 0.0172 173.3 1200 0.01719 173.5 1200 0.0172 173.6 1200 0.0172 173.7 1199 0.01722 173.8 1200 0.01723 173.9 1200 0.01722 174 1199 0.0172 174.1 1200 0.0172 174.2 1200 0.01718 174.3 1199 0.01719 174.4 1199 0.01718 174.5 1199 0.01719 174.6 1200 0.0172 174.7 1199 0.01722 174.8 1199 0.01722 174.9 1200 0.0172 175 1199 0.01719 175.1 1199 0.01719 175.3 1200 0.01718 175.4 1199 0.01717 175.5 1199 0.01717 175.6 1199 0.01717 175.7 1199 0.01717 175.8 1200 0.01717 175.9 1199 0.01718 176 1199 0.01719 176.1 1200 0.01718 176.2 1199 0.01719 176.3 1200 0.0172 176.4 1199 0.0172 176.5 1200 0.0172 176.6 1200 0.01719 176.7 1199 0.01718 176.8 1199 0.01719 176.9 1199 0.01719 177.1 1199 0.0172 177.2 1199 0.01718 177.3 1200 0.01717 177.4 1200 0.01717 177.5 1199 0.01717 177.6 1199 0.01718 177.7 1199 0.01719 177.8 1199 0.01719 177.9 1200 0.01719 178 1199 0.0172 178.1 1200 0.01719 178.2 1199 0.0172 178.3 1199 0.0172 178.4 1199 0.0172 178.5 1199 0.01722 178.6 1200 0.01723 178.8 1199 0.01723 178.9 1199 0.01723 179 1200 0.01722 179.1 1199 0.01722 179.2 1199 0.01722 179.3 1199 0.01722 179.4 1200 0.0172 179.5 1199 0.01718 179.6 1199 0.01718 179.7 1200 0.01717 179.8 1200 0.01717 179.9 1199 0.01717 180 1200 0.01717 180.1 1199 0.01717 180.2 1200 0.01717 180.3 1199 0.01717 180.4 1199 0.01717 180.6 1199 0.01718 180.7 1199 0.01718 180.8 1200 0.0172 180.9 1199 0.01722 181 1200 0.01722 181.1 1200 0.0172 181.2 1199 0.01718 181.3 1199 0.01717 181.4 1199 0.01717 181.5 1200 0.01717 181.6 1199 0.01718 181.7 1199 0.01719 181.8 1200 0.01719 181.9 1199 0.0172 182 1199 0.0172 182.1 1199 0.01719 182.2 1199 0.01719 182.4 1200 0.01718 182.5 1200 0.01718 182.6 1199 0.01717 182.7 1200 0.01718 182.8 1199 0.01719 182.9 1200 0.01718 183 1200 0.01719 183.1 1200 0.01719 183.2 1199 0.0172 183.3 1199 0.0172 183.4 1199 0.0172 183.5 1200 0.0172 183.6 1200 0.0172 183.7 1200 0.0172 183.8 1200 0.01722 183.9 1199 0.0172 184 1200 0.01718 184.2 1200 0.01719 184.3 1200 0.01719 184.4 1200 0.0172 184.5 1200 0.0172 184.6 1199 0.0172 184.7 1200 0.0172 184.8 1199 0.0172 184.9 1199 0.0172 185 1199 0.01722 185.1 1199 0.01722 185.2 1200 0.01722 185.3 1199 0.0172 185.4 1199 0.01719 185.5 1199 0.01718 185.6 1199 0.01717 185.7 1199 0.01717 185.9 1200 0.01715 186 1199 0.01715 186.1 1199 0.01715 186.2 1200 0.01717 186.3 1200 0.01717 186.4 1200 0.01715 186.5 1199 0.01717 186.6 1199 0.01717 186.7 1199 0.01717 186.8 1200 0.01717 186.9 1199 0.01718 187 1199 0.01718 187.1 1199 0.01718 187.2 1199 0.01717 187.3 1199 0.01717 187.4 1199 0.01717 187.5 1200 0.01717 187.7 1200 0.01714 187.8 1199 0.01714 187.9 1199 0.01714 188 1199 0.01715 188.1 1199 0.01715 188.2 1199 0.01715 188.3 1199 0.01715 188.4 1200 0.01715 188.5 1199 0.01717 188.6 1199 0.01717 188.7 1200 0.01718 188.8 1199 0.01718 188.9 1200 0.01719 189 1199 0.01719 189.1 1199 0.01718 189.2 1199 0.01717 189.3 1200 0.01717 189.5 1200 0.01717 189.6 1199 0.01717 189.7 1199 0.01717 189.8 1200 0.01717 189.9 1200 0.01718 190 1199 0.01719 190.1 1200 0.01719 190.2 1199 0.01719 190.3 1199 0.01719 190.4 1199 0.01718 190.5 1199 0.01717 190.6 1200 0.01717 190.7 1199 0.01717 190.8 1199 0.01715 190.9 1199 0.01714 191 1200 0.01714 191.1 1199 0.01715 191.3 1199 0.01715 191.4 1199 0.01717 191.5 1200 0.01715 191.6 1200 0.01715 191.7 1199 0.01715 191.8 1199 0.01717 191.9 1199 0.01717 192 1199 0.01717 192.1 1199 0.01717 192.2 1200 0.01717 192.3 1199 0.01718 192.4 1199 0.01717 192.5 1199 0.01718 192.6 1200 0.01717 192.7 1199 0.01714 192.8 1200 0.01715 192.9 1200 0.01714 193.1 1199 0.01714 193.2 1199 0.01715 193.3 1200 0.01714 193.4 1199 0.01717 193.5 1199 0.01717 193.6 1199 0.01718 193.7 1200 0.01717 193.8 1200 0.01717 193.9 1200 0.01718 194 1199 0.01719 194.1 1200 0.01718 194.2 1199 0.01718 194.3 1200 0.01718 194.4 1199 0.01718 194.5 1200 0.01718 194.6 1200 0.01719 194.8 1199 0.0172 194.9 1199 0.0172 195 1200 0.0172 195.1 1199 0.0172 195.2 1199 0.01722 195.3 1200 0.01723 195.4 1200 0.01723 195.5 1199 0.01722 195.6 1200 0.0172 195.7 1200 0.0172 195.8 1199 0.01719 195.9 1199 0.0172 196 1199 0.0172 196.1 1200 0.0172 196.2 1199 0.0172 196.3 1199 0.01719 196.4 1200 0.01719 196.6 1199 0.01719 196.7 1199 0.01719 196.8 1200 0.01719 196.9 1200 0.01719 197 1199 0.01718 197.1 1199 0.01718 197.2 1199 0.01717 197.3 1199 0.01717 197.4 1200 0.01717 197.5 1200 0.01717 197.6 1199 0.01715 197.7 1199 0.01714 197.8 1199 0.01712 197.9 1199 0.01711 198 1200 0.01711 198.1 1199 0.01711 198.2 1200 0.01711 198.4 1199 0.01711 198.5 1199 0.01711 198.6 1200 0.01709 198.7 1199 0.01708 198.8 1200 0.01708 198.9 1200 0.01707 199 1199 0.01707 199.1 1199 0.01704 199.2 1199 0.01704 199.3 1199 0.01702 199.4 1200 0.01701 199.5 1200 0.01701 199.6 1200 0.01701 199.7 1199 0.01703 199.8 1199 0.01706 199.9 1199 0.01709 200 1199 0.01709 200.2 1200 0.01711 200.3 1199 0.01714 200.4 1200 0.01715 200.5 1200 0.01717 200.6 1199 0.01717 200.7 1199 0.01717 200.8 1199 0.01717 200.9 1200 0.01717 201 1200 0.01718 201.1 1200 0.01719 201.2 1200 0.01718 201.3 1200 0.01717 201.4 1200 0.01717 201.5 1199 0.01717 201.6 1200 0.01717 201.7 1199 0.01717 201.8 1200 0.01717 202 1200 0.01717 202.1 1199 0.01715 202.2 1200 0.01717 202.3 1200 0.01717 202.4 1200 0.01717 202.5 1200 0.01717 202.6 1200 0.01715 202.7 1200 0.01717 202.8 1200 0.01717 202.9 1200 0.01717 203 1200 0.01717 203.1 1199 0.01717 203.2 1199 0.01714 203.3 1200 0.01714 203.4 1200 0.01714 203.5 1199 0.01714 203.7 1200 0.01714 203.8 1199 0.01714 203.9 1200 0.01715 204 1199 0.01717 204.1 1200 0.01715 204.2 1200 0.01717 204.3 1200 0.01715 204.4 1200 0.01714 204.5 1199 0.01714 204.6 1199 0.01714 204.7 1199 0.01714 204.8 1199 0.01714 204.9 1199 0.01714 205 1200 0.01715 205.1 1200 0.01715 205.2 1199 0.01717 205.3 1199 0.01717 205.5 1199 0.01715 205.6 1199 0.01715 205.7 1200 0.01714 205.8 1199 0.01713 205.9 1200 0.01714 206 1199 0.01714 206.1 1200 0.01714 206.2 1199 0.01714 206.3 1199 0.01713 206.4 1199 0.01714 206.5 1200 0.01714 206.6 1199 0.01714 206.7 1200 0.01713 206.8 1199 0.01714 206.9 1199 0.01717 207 1199 0.01717 207.1 1200 0.01717 207.3 1200 0.01717 207.4 1199 0.01719 207.5 1200 0.01718 207.6 1199 0.01717 207.7 1199 0.01717 207.8 1199 0.01718 207.9 1200 0.01717 208 1200 0.01714 208.1 1199 0.01712 208.2 1199 0.01709 208.3 1199 0.01709 208.4 1199 0.01709 208.5 1199 0.01708 208.6 1200 0.01709 208.7 1200 0.01709 208.8 1199 0.01712 208.9 1199 0.01713 209.1 1199 0.01712 209.2 1200 0.01712 209.3 1200 0.01712 209.4 1199 0.01713 209.5 1200 0.01714 209.6 1200 0.01714 209.7 1199 0.01715 209.8 1199 0.01717 209.9 1200 0.01717 210 1199 0.01717 210.1 1200 0.01717 210.2 1199 0.01717 210.3 1199 0.01717 210.4 1200 0.01715 210.5 1199 0.01715 210.6 1200 0.01714 210.8 1200 0.01712 210.9 1199 0.01712 211 1199 0.01712 211.1 1200 0.01712 211.2 1199 0.01712 211.3 1199 0.01712 211.4 1199 0.01712 211.5 1200 0.01712 211.6 1199 0.01713 211.7 1200 0.01714 211.8 1199 0.01714 211.9 1199 0.01714 212 1200 0.01714 212.1 1199 0.01714 212.2 1200 0.01715 212.3 1199 0.01715 212.4 1199 0.01715 212.6 1200 0.01715 212.7 1199 0.01714 212.8 1199 0.01714 212.9 1199 0.01713 213 1200 0.01713 213.1 1199 0.01712 213.2 1200 0.01712 213.3 1199 0.01712 213.4 1200 0.01711 213.5 1200 0.01707 213.6 1199 0.01707 213.7 1199 0.01708 213.8 1199 0.01709 213.9 1200 0.01711 214 1200 0.01712 214.1 1199 0.01712 214.2 1199 0.01714 214.4 1199 0.01714 214.5 1199 0.01712 214.6 1200 0.01712 214.7 1200 0.01709 214.8 1199 0.01707 214.9 1199 0.01708 215 1200 0.01709 215.1 1199 0.01709 215.2 1199 0.01709 215.3 1200 0.01709 215.4 1200 0.01708 215.5 1199 0.01709 215.6 1199 0.01709 215.7 1199 0.01709 215.8 1199 0.01709 215.9 1200 0.01709 216 1199 0.01711 216.2 1199 0.01711 216.3 1199 0.01711 216.4 1200 0.01711 216.5 1199 0.01711 216.6 1199 0.01709 216.7 1200 0.01709 216.8 1200 0.01708 216.9 1200 0.01707 217 1200 0.01707 217.1 1199 0.01708 217.2 1199 0.01709 217.3 1199 0.01708 217.4 1200 0.01707 217.5 1200 0.01708 217.6 1200 0.01709 217.7 1199 0.01709 217.8 1200 0.01709 218 1199 0.01709 218.1 1199 0.01709 218.2 1200 0.01708 218.3 1200 0.01709 218.4 1200 0.01709 218.5 1200 0.01709 218.6 1199 0.01709 218.7 1200 0.01711 218.8 1200 0.01711 218.9 1199 0.01711 219 1200 0.01711 219.1 1199 0.01711 219.2 1200 0.01711 219.3 1200 0.01711 219.4 1200 0.01712 219.5 1200 0.01711 219.7 1199 0.01711 219.8 1200 0.01711 219.9 1199 0.01712 220 1200 0.01711 220.1 1200 0.01709 220.2 1199 0.01708 220.3 1199 0.01709 220.4 1199 0.01709 220.5 1199 0.01711 220.6 1199 0.01711 220.7 1200 0.01709 220.8 1199 0.01709 220.9 1200 0.01708 221 1199 0.01707 221.1 1200 0.01707 221.2 1200 0.01704 221.3 1199 0.01704 221.5 1199 0.01703 221.6 1199 0.01702 221.7 1200 0.01702 221.8 1199 0.01702 221.9 1199 0.01702 222 1199 0.01703 222.1 1199 0.01704 222.2 1199 0.01703 222.3 1200 0.01702 222.4 1199 0.01702 222.5 1199 0.01702 222.6 1199 0.01702 222.7 1199 0.01704 222.8 1199 0.01707 222.9 1199 0.01707 223 1199 0.01707 223.1 1200 0.01709 223.3 1199 0.01709 223.4 1199 0.01709 223.5 1199 0.01709 223.6 1199 0.01709 223.7 1199 0.01709 223.8 1199 0.01708 223.9 1200 0.01709 224 1199 0.01708 224.1 1199 0.01709 224.2 1199 0.01708 224.3 1199 0.01707 224.4 1199 0.01707 224.5 1200 0.01707 224.6 1199 0.01707 224.7 1199 0.01708 224.8 1200 0.01709 224.9 1200 0.01709 225.1 1199 0.01709 225.2 1200 0.01708 225.3 1199 0.01708 225.4 1199 0.01707 225.5 1199 0.01707 225.6 1199 0.01707 225.7 1199 0.01707 225.8 1200 0.01707 225.9 1199 0.01707 226 1199 0.01707 226.1 1200 0.01706 226.2 1199 0.01703 226.3 1200 0.01702 226.4 1199 0.01701 226.5 1199 0.01699 226.6 1199 0.01701 226.8 1199 0.01701 226.9 1199 0.01702 227 1200 0.01702 227.1 1199 0.01703 227.2 1199 0.01704 227.3 1199 0.01704 227.4 1200 0.01703 227.5 1200 0.01702 227.6 1199 0.01703 227.7 1199 0.01706 227.8 1200 0.01706 227.9 1199 0.01707 228 1199 0.01707 228.1 1200 0.01707 228.2 1200 0.01707 228.3 1200 0.01707 228.4 1199 0.01707 228.6 1199 0.01707 228.7 1199 0.01707 228.8 1199 0.01707 228.9 1200 0.01706 229 1199 0.01706 229.1 1200 0.01706 229.2 1199 0.01706 229.3 1199 0.01707 229.4 1200 0.01707 229.5 1199 0.01706 229.6 1199 0.01707 229.7 1200 0.01706 229.8 1199 0.01707 229.9 1200 0.01706 230 1199 0.01706 230.1 1199 0.01706 230.2 1200 0.01704 230.4 1199 0.01704 230.5 1200 0.01704 230.6 1199 0.01704 230.7 1199 0.01704 230.8 1200 0.01704 230.9 1199 0.01704 231 1200 0.01704 231.1 1200 0.01703 231.2 1199 0.01704 231.3 1199 0.01704 231.4 1199 0.01703 231.5 1200 0.01703 231.6 1200 0.01704 231.7 1200 0.01704 231.8 1200 0.01707 231.9 1199 0.01707 232 1199 0.01707 232.2 1200 0.01704 232.3 1199 0.01702 232.4 1199 0.01702 232.5 1199 0.01701 232.6 1200 0.01702 232.7 1199 0.01702 232.8 1199 0.01701 232.9 1200 0.01702 233 1200 0.01702 233.1 1200 0.01704 233.2 1199 0.01704 233.3 1199 0.01704 233.4 1199 0.01703 233.5 1199 0.01702 233.6 1199 0.01702 233.7 1199 0.01702 233.8 1200 0.01701 234 1200 0.01701 234.1 1199 0.01698 234.2 1199 0.01698 234.3 1199 0.01697 234.4 1199 0.01697 234.5 1200 0.01694 234.6 1199 0.01694 234.7 1200 0.01694 234.8 1199 0.01697 234.9 1199 0.01697 235 1199 0.01697 235.1 1199 0.01697 235.2 1199 0.01698 235.3 1199 0.01699 235.4 1200 0.01699 235.5 1199 0.01699 235.7 1200 0.01701 235.8 1200 0.01701 235.9 1199 0.01701 236 1199 0.01702 236.1 1199 0.01701 236.2 1200 0.01701 236.3 1200 0.01701 236.4 1200 0.01701 236.5 1200 0.01702 236.6 1199 0.01699 236.7 1199 0.01701 236.8 1199 0.01701 236.9 1199 0.01701 237 1199 0.01701 237.1 1199 0.01701 237.2 1200 0.01701 237.3 1200 0.01701 237.5 1199 0.01701 237.6 1199 0.01701 237.7 1199 0.01701 237.8 1200 0.01701 237.9 1200 0.01701 238 1199 0.01701 238.1 1200 0.01701 238.2 1199 0.01701 238.3 1199 0.01701 238.4 1200 0.01701 238.5 1200 0.01701 238.6 1200 0.01701 238.7 1199 0.01701 238.8 1199 0.01702 238.9 1200 0.01701 239 1199 0.01699 239.1 1200 0.01698 239.3 1199 0.01697 239.4 1199 0.01697 239.5 1199 0.01697 239.6 1199 0.01697 239.7 1199 0.01699 239.8 1199 0.01699 239.9 1200 0.01699 240 1200 0.01699 240.1 1199 0.01701 240.2 1200 0.01701 240.3 1200 0.01701 240.4 1199 0.01699 240.5 1200 0.01698 240.6 1200 0.01698 240.7 1199 0.01697 240.8 1200 0.01697 240.9 1200 0.01697 241.1 1200 0.01697 241.2 1199 0.01697 241.3 1199 0.01696 241.4 1200 0.01697 241.5 1200 0.01697 241.6 1199 0.01698 241.7 1199 0.01697 241.8 1200 0.01697 241.9 1199 0.01697 242 1199 0.01697 242.1 1199 0.01697 242.2 1199 0.01697 242.3 1199 0.01696 242.4 1200 0.01697 242.5 1199 0.01697 242.6 1200 0.01697 242.7 1199 0.01697 242.9 1200 0.01697 243 1199 0.01697 243.1 1199 0.01697 243.2 1199 0.01697 243.3 1199 0.01697 243.4 1199 0.01697 243.5 1199 0.01697 243.6 1200 0.01697 243.7 1199 0.01696 243.8 1200 0.01696 243.9 1199 0.01696 244 1200 0.01696 244.1 1199 0.01696 244.2 1200 0.01696 244.3 1200 0.01697 244.4 1200 0.01697 244.6 1200 0.01698 244.7 1199 0.01699 244.8 1199 0.01699 244.9 1200 0.01699 245 1200 0.01699 245.1 1200 0.01699 245.2 1200 0.01698 245.3 1199 0.01697 245.4 1200 0.01697 245.5 1199 0.01697 245.6 1199 0.01698 245.7 1200 0.01699 245.8 1199 0.01698 245.9 1200 0.01699 246 1200 0.01699 246.1 1199 0.01699 246.2 1199 0.01699 246.4 1199 0.01699 246.5 1200 0.01701 246.6 1200 0.01701 246.7 1199 0.01701 246.8 1200 0.01701 246.9 1199 0.01701 247 1200 0.01701 247.1 1199 0.01701 247.2 1199 0.01701 247.3 1199 0.01702 247.4 1199 0.01701 247.5 1199 0.01699 247.6 1199 0.01699 247.7 1199 0.01697 247.8 1199 0.01697 247.9 1199 0.01694 248 1199 0.01694 248.2 1200 0.01693 248.3 1199 0.01693 248.4 1199 0.01694 248.5 1199 0.01693 248.6 1200 0.01692 248.7 1199 0.01692 248.8 1199 0.01693 248.9 1200 0.01694 249 1199 0.01694 249.1 1199 0.01694 249.2 1199 0.01694 249.3 1199 0.01694 249.4 1200 0.01697 249.5 1200 0.01697 249.6 1199 0.01697 249.7 1199 0.01698 249.8 1199 0.01699 250 1199 0.01701 250.1 1199 0.01702 250.2 1200 0.01702 250.3 1200 0.01702 250.4 1200 0.01702 250.5 1200 0.01701 250.6 1199 0.01702 250.7 1199 0.01702 250.8 1199 0.01703 250.9 1199 0.01702 251 1200 0.01701 251.1 1200 0.01699 251.2 1199 0.01697 251.3 1200 0.01694 251.4 1199 0.01694 251.5 1199 0.01693 251.7 1200 0.01694 251.8 1200 0.01696 251.9 1200 0.01697 252 1199 0.01697 252.1 1199 0.01698 252.2 1199 0.01697 252.3 1199 0.01697 252.4 1199 0.01697 252.5 1199 0.01697 252.6 1199 0.01697 252.7 1200 0.01697 252.8 1199 0.01697 252.9 1199 0.01697 253 1200 0.01697 253.1 1199 0.01698 253.2 1200 0.01698 253.3 1199 0.01699 253.5 1200 0.01699 253.6 1199 0.01701 253.7 1200 0.01702 253.8 1199 0.01702 253.9 1199 0.01702 254 1200 0.01699 254.1 1200 0.01697 254.2 1200 0.01694 254.3 1199 0.01693 254.4 1199 0.01694 254.5 1200 0.01694 254.6 1199 0.01697 254.7 1200 0.01697 254.8 1199 0.01697 254.9 1199 0.01697 255 1199 0.01696 255.1 1200 0.01692 255.3 1199 0.01692 255.4 1199 0.01689 255.5 1199 0.01689 255.6 1199 0.01692 255.7 1200 0.01693 255.8 1200 0.01694 255.9 1200 0.01697 256 1199 0.01697 256.1 1200 0.01698 256.2 1199 0.01698 256.3 1200 0.01699 256.4 1199 0.01699 256.5 1200 0.01698 256.6 1199 0.01698 256.7 1199 0.01697 256.8 1199 0.01697 256.9 1200 0.01697 257.1 1200 0.01697 257.2 1199 0.01697 257.3 1200 0.01697 257.4 1199 0.01697 257.5 1200 0.01697 257.6 1200 0.01694 257.7 1199 0.01697 257.8 1200 0.01697 257.9 1200 0.01697 258 1200 0.01698 258.1 1199 0.01698 258.2 1199 0.01698 258.3 1200 0.01697 258.4 1200 0.01696 258.5 1200 0.01696 258.6 1200 0.01694 258.7 1200 0.01697 258.9 1199 0.01697 259 1199 0.01699 259.1 1200 0.01702 259.2 1200 0.01703 259.3 1199 0.01704 259.4 1199 0.01704 259.5 1200 0.01703 259.6 1200 0.01703 259.7 1199 0.01702 259.8 1200 0.01699 259.9 1199 0.01699 260 1199 0.01698 260.1 1199 0.01698 260.2 1199 0.01698 260.3 1199 0.01699 260.4 1200 0.01698 260.6 1199 0.01697 260.7 1200 0.01698 260.8 1199 0.01698 260.9 1200 0.01699 261 1199 0.01701 261.1 1199 0.01699 261.2 1200 0.01699 261.3 1200 0.01701 261.4 1200 0.01699 261.5 1200 0.01698 261.6 1199 0.01698 261.7 1199 0.01699 261.8 1200 0.01699 261.9 1200 0.01698 262 1199 0.01697 262.1 1199 0.01698 262.2 1200 0.01699 262.4 1200 0.01698 262.5 1200 0.01697 262.6 1199 0.01697 262.7 1200 0.01697 262.8 1199 0.01697 262.9 1199 0.01697 263 1199 0.01696 263.1 1200 0.01697 263.2 1199 0.01697 263.3 1199 0.01697 263.4 1200 0.01697 263.5 1199 0.01697 263.6 1199 0.01699 263.7 1200 0.01698 263.8 1199 0.01697 263.9 1200 0.01696 264 1199 0.01694 264.2 1200 0.01694 264.3 1199 0.01693 264.4 1199 0.01694 264.5 1200 0.01697 264.6 1199 0.01697 264.7 1199 0.01698 264.8 1199 0.01699 264.9 1199 0.01701 265 1200 0.01702 265.1 1199 0.01699 265.2 1200 0.01699 265.3 1200 0.01699 265.4 1200 0.01699 265.5 1200 0.01701 265.6 1199 0.01699 265.7 1200 0.01699 265.8 1199 0.01699 266 1199 0.01697 266.1 1200 0.01697 266.2 1199 0.01697 266.3 1200 0.01696 266.4 1199 0.01694 266.5 1200 0.01694 266.6 1200 0.01694 266.7 1199 0.01694 266.8 1200 0.01697 266.9 1199 0.01701 267 1199 0.01698 267.1 1200 0.01697 267.2 1199 0.01697 267.3 1200 0.01696 267.4 1200 0.01696 267.5 1200 0.01697 267.6 1200 0.01697 267.8 1199 0.01698 267.9 1200 0.01701 268 1199 0.01702 268.1 1200 0.01701 268.2 1200 0.01701 268.3 1199 0.01697 268.4 1200 0.01697 268.5 1199 0.01697 268.6 1200 0.01698 268.7 1200 0.01697 268.8 1200 0.01697 268.9 1200 0.01697 269 1199 0.01697 269.1 1199 0.01697 269.2 1199 0.01697 269.3 1200 0.01697 269.5 1200 0.01701 269.6 1200 0.01702 269.7 1200 0.01701 269.8 1199 0.01699 269.9 1199 0.01698 270 1200 0.01699 270.1 1199 0.01701 270.2 1200 0.01701 270.3 1200 0.01702 270.4 1199 0.01702 270.5 1199 0.01701 270.6 1199 0.01699 270.7 1199 0.01698 270.8 1200 0.01697 270.9 1200 0.01697 271 1199 0.01697 271.1 1199 0.01697 271.3 1199 0.01697 271.4 1199 0.01697 271.5 1199 0.01696 271.6 1199 0.01697 271.7 1199 0.01698 271.8 1200 0.01699 271.9 1199 0.01701 272 1200 0.01699 272.1 1200 0.01701 272.2 1199 0.01701 272.3 1200 0.01701 272.4 1199 0.01699 272.5 1200 0.01698 272.6 1199 0.01699 272.7 1199 0.01699 272.8 1199 0.01701 272.9 1199 0.01702 273.1 1200 0.01702 273.2 1200 0.01702 273.3 1199 0.01702 273.4 1199 0.01702 273.5 1200 0.01702 273.6 1200 0.01701 273.7 1200 0.01701 273.8 1199 0.01702 273.9 1200 0.01701 274 1199 0.01701 274.1 1199 0.01701 274.2 1200 0.01702 274.3 1199 0.01702 274.4 1200 0.01701 274.5 1200 0.01699 274.6 1200 0.01699 274.7 1200 0.01698 274.9 1200 0.01697 275 1199 0.01696 275.1 1199 0.01697 275.2 1199 0.01697 275.3 1200 0.01698 275.4 1200 0.01701 275.5 1200 0.01702 275.6 1200 0.01702 275.7 1200 0.01703 275.8 1200 0.01702 275.9 1199 0.01702 276 1199 0.01702 276.1 1199 0.01702 276.2 1200 0.01702 276.3 1200 0.01702 276.4 1200 0.01703 276.6 1200 0.01703 276.7 1199 0.01702 276.8 1200 0.01702 276.9 1200 0.01702 277 1200 0.01702 277.1 1200 0.01702 277.2 1199 0.01702 277.3 1199 0.01702 277.4 1199 0.01703 277.5 1199 0.01704 277.6 1199 0.01704 277.7 1200 0.01703 277.8 1200 0.01702 277.9 1200 0.01702 278 1199 0.01704 278.1 1200 0.01704 278.2 1200 0.01704 278.4 1200 0.01704 278.5 1199 0.01704 278.6 1199 0.01704 278.7 1199 0.01706 278.8 1199 0.01704 278.9 1199 0.01703 279 1200 0.01703 279.1 1199 0.01702 279.2 1200 0.01703 279.3 1200 0.01703 279.4 1200 0.01704 279.5 1199 0.01704 279.6 1199 0.01704 279.7 1200 0.01706 279.8 1200 0.01706 279.9 1199 0.01704 280 1200 0.01703 280.2 1199 0.01702 280.3 1199 0.01702 280.4 1199 0.01701 280.5 1200 0.01699 280.6 1200 0.01701 280.7 1200 0.01701 280.8 1199 0.01701 280.9 1199 0.01701 281 1199 0.01701 281.1 1199 0.01701 281.2 1199 0.01701 281.3 1200 0.01702 281.4 1199 0.01702 281.5 1200 0.01702 281.6 1199 0.01703 281.7 1200 0.01704 281.8 1200 0.01704 282 1200 0.01704 282.1 1200 0.01704 282.2 1199 0.01706 282.3 1200 0.01704 282.4 1199 0.01706 282.5 1199 0.01706 282.6 1199 0.01706 282.7 1200 0.01706 282.8 1199 0.01707 282.9 1200 0.01707 283 1199 0.01706 283.1 1200 0.01704 283.2 1199 0.01704 283.3 1200 0.01703 283.4 1199 0.01702 283.5 1199 0.01702 283.6 1199 0.01702 283.8 1199 0.01702 283.9 1199 0.01702 284 1199 0.01702 284.1 1199 0.01702 284.2 1200 0.01701 284.3 1199 0.01699 284.4 1199 0.01699 284.5 1199 0.01699 284.6 1199 0.01697 284.7 1200 0.01697 284.8 1200 0.01697 284.9 1199 0.01694 285 1199 0.01696 285.1 1200 0.01694 285.2 1200 0.01694 285.3 1200 0.01693 285.5 1200 0.01692 285.6 1199 0.01694 285.7 1200 0.01694 285.8 1200 0.01694 285.9 1200 0.01694 286 1200 0.01696 286.1 1199 0.01697 286.2 1199 0.01698 286.3 1200 0.01699 286.4 1200 0.01701 286.5 1199 0.01702 286.6 1199 0.01706 286.7 1200 0.01707 286.8 1200 0.01709 286.9 1199 0.01709 287 1200 0.01707 287.1 1199 0.01707 287.3 1199 0.01706 287.4 1199 0.01706 287.5 1199 0.01707 287.6 1199 0.01707 287.7 1200 0.01708 287.8 1199 0.01707 287.9 1200 0.01707 288 1200 0.01707 288.1 1200 0.01707 288.2 1200 0.01707 288.3 1199 0.01707 288.4 1200 0.01706 288.5 1200 0.01704 288.6 1200 0.01704 288.7 1199 0.01706 288.8 1200 0.01707 288.9 1200 0.01707 289.1 1200 0.01707 289.2 1200 0.01707 289.3 1200 0.01707 289.4 1200 0.01707 289.5 1200 0.01707 289.6 1199 0.01707 289.7 1199 0.01707 289.8 1199 0.01707 289.9 1200 0.01706 290 1200 0.01707 290.1 1199 0.01706 290.2 1200 0.01707 290.3 1200 0.01706 290.4 1199 0.01707 290.5 1199 0.01706 290.6 1200 0.01706 290.7 1199 0.01707 290.9 1200 0.01707 291 1200 0.01706 291.1 1199 0.01706 291.2 1200 0.01707 291.3 1199 0.01708 291.4 1200 0.01707 291.5 1200 0.01706 291.6 1200 0.01704 291.7 1199 0.01704 291.8 1200 0.01703 291.9 1200 0.01704 292 1200 0.01704 292.1 1199 0.01706 292.2 1200 0.01707 292.3 1200 0.01709 292.4 1200 0.01712 292.6 1199 0.01713 292.7 1200 0.01712 292.8 1199 0.01712 292.9 1199 0.01712 293 1200 0.01712 293.1 1200 0.01712 293.2 1200 0.01712 293.3 1200 0.01712 293.4 1200 0.01712 293.5 1200 0.01712 293.6 1199 0.01709 293.7 1200 0.01709 293.8 1200 0.01708 293.9 1199 0.01707 294 1200 0.01707 294.1 1199 0.01709 294.2 1199 0.01709 294.4 1200 0.01709 294.5 1200 0.01709 294.6 1200 0.01709 294.7 1200 0.01708 294.8 1200 0.01707 294.9 1200 0.01707 295 1200 0.01707 295.1 1200 0.01711 295.2 1200 0.01711 295.3 1200 0.01711 295.4 1199 0.01711 295.5 1199 0.01712 295.6 1199 0.01711 295.7 1200 0.01711 295.8 1200 0.01709 295.9 1200 0.01708 296 1200 0.01708 296.2 1200 0.01708 296.3 1200 0.01707 296.4 1199 0.01704 296.5 1200 0.01704 296.6 1199 0.01706 296.7 1200 0.01707 296.8 1199 0.01707 296.9 1199 0.01709 297 1199 0.01712 297.1 1200 0.01712 297.2 1200 0.01712 297.3 1200 0.01712 297.4 1200 0.01712 297.5 1200 0.01712 297.6 1200 0.01712 297.7 1200 0.01712 297.8 1199 0.01713 298 1200 0.01713 298.1 1200 0.01712 298.2 1200 0.01713 298.3 1200 0.01712 298.4 1200 0.01712 298.5 1200 0.01712 298.6 1199 0.01712 298.7 1200 0.01712 298.8 1200 0.01712 298.9 1199 0.01711 299 1199 0.01712 299.1 1200 0.01712 299.2 1200 0.01712 299.3 1200 0.01712 299.4 1200 0.01712 299.5 1200 0.01713 299.6 1200 0.01713 299.8 1200 0.01714 299.9 1200 0.01714 300 1200 0.01714 300.1 1200 0.01712 300.2 1199 0.01712 300.3 1200 0.01712 300.4 1200 0.01712 300.5 1200 0.01712 300.6 1200 0.01712 300.7 1200 0.01712 300.8 1200 0.01714 300.9 1200 0.01714 301 1200 0.01714 301.1 1200 0.01717 301.2 1200 0.01717 301.3 1200 0.01717 301.5 1199 0.01717 301.6 1200 0.01717 301.7 1200 0.01717 301.8 1200 0.01717 301.9 1200 0.01717 302 1200 0.01717 302.1 1199 0.01715 302.2 1199 0.01714 302.3 1200 0.01714 302.4 1200 0.01713 302.5 1199 0.01712 302.6 1199 0.01713 302.7 1199 0.01714 302.8 1200 0.01714 302.9 1200 0.01714 303 1199 0.01714 303.1 1200 0.01714 303.3 1200 0.01713 303.4 1199 0.01714 303.5 1200 0.01714 303.6 1199 0.01714 303.7 1200 0.01715 303.8 1199 0.01714 303.9 1200 0.01714 304 1199 0.01713 304.1 1200 0.01714 304.2 1199 0.01715 304.3 1199 0.01714 304.4 1199 0.01715 304.5 1199 0.01717 304.6 1200 0.01717 304.7 1200 0.01718 304.8 1200 0.01719 304.9 1200 0.01719 305.1 1199 0.01717 305.2 1199 0.01717 305.3 1200 0.01715 305.4 1199 0.01714 305.5 1199 0.01712 305.6 1199 0.01711 305.7 1199 0.01707 305.8 1199 0.01707 305.9 1199 0.01707 306 1200 0.01708 306.1 1199 0.01711 306.2 1200 0.01712 306.3 1200 0.01712 306.4 1200 0.01714 306.5 1200 0.01714 306.6 1199 0.01717 306.7 1199 0.01717 306.9 1199 0.01717 307 1200 0.01717 307.1 1199 0.01717 307.2 1199 0.01717 307.3 1200 0.01714 307.4 1200 0.01714 307.5 1200 0.01714 307.6 1200 0.01715 307.7 1200 0.01714 307.8 1200 0.01713 307.9 1200 0.01714 308 1199 0.01714 308.1 1200 0.01714 308.2 1199 0.01714 308.3 1199 0.01712 308.4 1200 0.01713 308.5 1200 0.01714 308.7 1200 0.01714 308.8 1199 0.01715 308.9 1200 0.01715 309 1200 0.01718 309.1 1200 0.0172 309.2 1200 0.01719 309.3 1200 0.01718 309.4 1200 0.01718 309.5 1200 0.01717 309.6 1200 0.01717 309.7 1200 0.01717 309.8 1200 0.01714 309.9 1199 0.01714 310 1200 0.01712 310.1 1200 0.01714 310.2 1200 0.01717 310.4 1200 0.01717 310.5 1200 0.01717 310.6 1199 0.01717 310.7 1200 0.01717 310.8 1200 0.01715 310.9 1200 0.01717 311 1200 0.01717 311.1 1199 0.01715 311.2 1199 0.01717 311.3 1200 0.01717 311.4 1199 0.01717 311.5 1200 0.01719 311.6 1199 0.01718 311.7 1200 0.01717 311.8 1200 0.01718 311.9 1200 0.01718 312 1199 0.01719 312.2 1200 0.0172 312.3 1200 0.01722 312.4 1199 0.01723 312.5 1199 0.01724 312.6 1200 0.01722 312.7 1199 0.01722 312.8 1199 0.01718 312.9 1199 0.01714 313 1200 0.01712 313.1 1200 0.01711 313.2 1199 0.01709 313.3 1200 0.01712 313.4 1199 0.01714 313.5 1200 0.01717 313.6 1200 0.01715 313.7 1199 0.01717 313.8 1200 0.01718 314 1199 0.01719 314.1 1199 0.01718 314.2 1200 0.01717 314.3 1199 0.01717 314.4 1200 0.01717 314.5 1199 0.01717 314.6 1200 0.01718 314.7 1200 0.01718 314.8 1200 0.01718 314.9 1199 0.01718 315 1200 0.01717 315.1 1200 0.01717 315.2 1199 0.01717 315.3 1200 0.01717 315.4 1199 0.01717 315.5 1199 0.01717 315.6 1199 0.01717 315.8 1200 0.01717 315.9 1200 0.01718 316 1200 0.01717 316.1 1200 0.01718 316.2 1200 0.01717 316.3 1199 0.01717 316.4 1200 0.01717 316.5 1200 0.01715 316.6 1199 0.01719 316.7 1199 0.01718 316.8 1199 0.01718 316.9 1200 0.01717 317 1200 0.01717 317.1 1199 0.01717 317.2 1199 0.01717 317.3 1200 0.01717 317.5 1200 0.01717 317.6 1200 0.01717 317.7 1200 0.01718 317.8 1199 0.01719 317.9 1200 0.01719 318 1200 0.01719 318.1 1199 0.01722 318.2 1199 0.01722 318.3 1200 0.01723 318.4 1200 0.01723 318.5 1200 0.01722 318.6 1200 0.01722 318.7 1200 0.01722 318.8 1200 0.01722 318.9 1200 0.0172 319 1200 0.0172 319.1 1199 0.01719 319.3 1199 0.01719 319.4 1200 0.0172 319.5 1200 0.0172 319.6 1200 0.0172 319.7 1199 0.0172 319.8 1200 0.0172 319.9 1200 0.01722 320 1199 0.01719 320.1 1200 0.01719 320.2 1199 0.01719 320.3 1200 0.0172 320.4 1200 0.0172 320.5 1200 0.0172 320.6 1200 0.0172 320.7 1199 0.0172 320.8 1199 0.01722 320.9 1199 0.01722 321.1 1200 0.01722 321.2 1200 0.01722 321.3 1199 0.01722 321.4 1199 0.0172 321.5 1200 0.01719 321.6 1200 0.01719 321.7 1200 0.01719 321.8 1200 0.0172 321.9 1200 0.0172 322 1199 0.0172 322.1 1200 0.01722 322.2 1199 0.01723 322.3 1200 0.01723 322.4 1199 0.01722 322.5 1199 0.01723 322.6 1200 0.01722 322.7 1199 0.01722 322.9 1200 0.0172 323 1200 0.01719 323.1 1200 0.01719 323.2 1199 0.01718 323.3 1200 0.01718 323.4 1199 0.01717 323.5 1199 0.01717 323.6 1200 0.01717 323.7 1199 0.01717 323.8 1200 0.01718 323.9 1200 0.0172 324 1200 0.01722 324.1 1200 0.01723 324.2 1200 0.01723 324.3 1199 0.01723 324.4 1200 0.01722 324.5 1199 0.01722 324.7 1199 0.0172 324.8 1199 0.0172 324.9 1199 0.0172 325 1200 0.01719 325.1 1200 0.01719 325.2 1200 0.01718 325.3 1200 0.01719 325.4 1199 0.01719 325.5 1200 0.0172 325.6 1199 0.0172 325.7 1200 0.0172 325.8 1200 0.0172 325.9 1200 0.0172 326 1200 0.01719 326.1 1200 0.01719 326.2 1199 0.01718 326.4 1200 0.01718 326.5 1199 0.01717 326.6 1200 0.01719 326.7 1200 0.01718 326.8 1199 0.01718 326.9 1200 0.01718 327 1199 0.01717 327.1 1199 0.01717 327.2 1200 0.01717 327.3 1200 0.01718 327.4 1199 0.01719 327.5 1199 0.01718 327.6 1199 0.01717 327.7 1199 0.01717 327.8 1200 0.01717 327.9 1199 0.01718 328 1200 0.01719 328.2 1200 0.01718 328.3 1200 0.01719 328.4 1200 0.0172 328.5 1199 0.01719 328.6 1200 0.01718 328.7 1200 0.01717 328.8 1199 0.01717 328.9 1200 0.01717 329 1200 0.01717 329.1 1199 0.01717 329.2 1200 0.01714 329.3 1200 0.01714 329.4 1200 0.01714 329.5 1200 0.01714 329.6 1200 0.01717 329.7 1200 0.01714 329.8 1199 0.01714 330 1200 0.01714 330.1 1199 0.01714 330.2 1200 0.01713 330.3 1200 0.01712 330.4 1199 0.01712 330.5 1199 0.01712 330.6 1199 0.01712 330.7 1199 0.01712 330.8 1199 0.01712 330.9 1200 0.01712 331 1200 0.01714 331.1 1200 0.01714 331.2 1200 0.01717 331.3 1200 0.01718 331.4 1200 0.01718 331.5 1200 0.01719 331.6 1200 0.01719 331.8 1200 0.0172 331.9 1200 0.01719 332 1199 0.01718 332.1 1200 0.01718 332.2 1199 0.01717 332.3 1200 0.01718 332.4 1200 0.01718 332.5 1200 0.01719 332.6 1200 0.01719 332.7 1199 0.01719 332.8 1200 0.01719 332.9 1199 0.01719 333 1200 0.01718 333.1 1199 0.01719 333.2 1200 0.0172 333.3 1200 0.0172 333.4 1200 0.0172 333.6 1200 0.01719 333.7 1200 0.01718 333.8 1200 0.01718 333.9 1199 0.01717 334 1199 0.01717 334.1 1200 0.01717 334.2 1200 0.01717 334.3 1200 0.01717 334.4 1200 0.01717 334.5 1200 0.01717 334.6 1200 0.01718 334.7 1199 0.01719 334.8 1200 0.01719 334.9 1200 0.0172 335 1199 0.0172 335.1 1200 0.0172 335.3 1200 0.01722 335.4 1199 0.01722 335.5 1200 0.01722 335.6 1199 0.01722 335.7 1199 0.01719 335.8 1200 0.01717 335.9 1200 0.01713 336 1199 0.01712 336.1 1199 0.01711 336.2 1199 0.01712 336.3 1199 0.01712 336.4 1200 0.01713 336.5 1199 0.01714 336.6 1200 0.01717 336.7 1200 0.01717 336.8 1199 0.01715 336.9 1198 0.01714 337.1 1197 0.01713 337.2 1197 0.01711 337.3 1197 0.01709 337.4 1197 0.01706 337.5 1194 0.01704 337.6 1194 0.01701 337.7 1186 0.01697 337.8 1173 0.01694 337.9 1172 0.01689 338 1172 0.01687 338.1 1172 0.01683 338.2 1169 0.01682 338.3 1168 0.01677 338.4 1165 0.01672 338.5 1164 0.01667 338.6 1159 0.0166 338.7 1152 0.01652 338.9 1147 0.01645 339 1139 0.01637 339.1 1131 0.01631 339.2 1125 0.01628 339.3 1120 0.01623 339.4 1115 0.01618 339.5 1112 0.01613 339.6 1109 0.01607 339.7 1104 0.01602 339.8 1100 0.01593 339.9 1097 0.01587 340 1093 0.01581 340.1 1090 0.01572 340.2 1085 0.01564 340.3 1081 0.01551 340.4 1078 0.01542 340.5 1073 0.01532 340.7 1069 0.01524 340.8 1065 0.01516 340.9 1062 0.01511 341 1058 0.01503 341.1 1054 0.01494 341.2 1051 0.01486 341.3 1047 0.01477 341.4 1043 0.01469 341.5 1040 0.0146 341.6 1036 0.01452 341.7 1033 0.01444 341.8 1030 0.01437 341.9 1026 0.01429 342 1024 0.0142 342.1 1021 0.01412 342.2 1018 0.01401 342.4 1014 0.01394 342.5 1011 0.01382 342.6 1008 0.01373 342.7 1004 0.01363 342.8 1001 0.01354 342.9 998 0.01345 343 994 0.01337 343.1 991 0.01329 343.2 987 0.01321 343.3 984 0.01311 343.4 981 0.01303 343.5 977 0.01295 343.6 975 0.01287 343.7 969 0.01277 343.8 967 0.01271 343.9 964 0.01267 344 959 0.01257 344.2 956 0.01247 344.3 953 0.0124 344.4 950 0.01233 344.5 946 0.01221 344.6 942 0.01215 344.7 939 0.01207 344.8 936 0.01199 344.9 932 0.01191 345 929 0.01182 345.1 925 0.01174 345.2 922 0.01165 345.3 918 0.01157 345.4 914 0.01147 345.5 911 0.0114 345.6 907 0.01131 345.7 904 0.01122 345.8 901 0.01113 346 897 0.01103 346.1 893 0.01095 346.2 890 0.01083 346.3 887 0.01075 346.4 883 0.01067 346.5 881 0.01059 346.6 875 0.01053 346.7 873 0.01043 346.8 869 0.01038 346.9 866 0.01032 347 862 0.01028 347.1 859 0.01018 347.2 856 0.0101 347.3 852 0.009998 347.4 850 0.009887 347.5 844 0.009813 347.6 843 0.009714 347.8 837 0.009639 347.9 836 0.009553 348 832 0.009491 348.1 828 0.009392 348.2 825 0.009305 348.3 821 0.009218 348.4 818 0.009119 348.5 815 0.009045 348.6 811 0.008946 348.7 807 0.008872 348.8 804 0.008785 348.9 801 0.008698 349 801 0.008612 349.1 799 0.008525 349.2 795 0.008451 349.3 791 0.008364 349.4 789 0.008302 349.6 784 0.008203 349.7 781 0.008129 349.8 778 0.008042 349.9 775 0.007943 350 771 0.007856 350.1 767 0.007757 350.2 764 0.007671 350.3 760 0.007571 350.4 757 0.007485 350.5 753 0.007398 350.6 750 0.007299 350.7 746 0.007225 350.8 743 0.007138 350.9 739 0.007064 351 736 0.006977 351.1 732 0.006903 351.3 728 0.006816 351.4 725 0.006742 351.5 721 0.006668 351.6 718 0.006581 351.7 714 0.006507 351.8 711 0.00642 351.9 707 0.006358 352 704 0.006296 352.1 700 0.006234 352.2 696 0.00616 352.3 693 0.006073 352.4 690 0.005974 352.5 686 0.00585 352.6 683 0.005739 352.7 679 0.005677 352.8 676 0.005603 352.9 672 0.005516 353.1 670 0.005429 353.2 666 0.005368 353.3 662 0.005281 353.4 659 0.005207 353.5 656 0.005107 353.6 653 0.005021 353.7 649 0.004934 353.8 646 0.00486 353.9 643 0.004786 354 639 0.004724 354.1 635 0.004649 354.2 632 0.00455 354.3 628 0.004476 354.4 625 0.004377 354.5 621 0.004303 354.6 617 0.004228 354.7 614 0.004154 354.9 610 0.004092 355 607 0.003968 355.1 604 0.003882 355.2 601 0.003783 355.3 598 0.003708 355.4 593 0.003622 355.5 591 0.003547 355.6 587 0.003473 355.7 584 0.003374 355.8 581 0.003312 355.9 577 0.003225 356 574 0.003176 356.1 570 0.003089 356.2 567 0.003027 356.3 564 0.002941 356.4 560 0.002829 356.5 556 0.002743 356.7 553 0.002644 356.8 549 0.002582 356.9 546 0.002532 357 542 0.002483 357.1 539 0.002433 357.2 535 0.002371 357.3 532 0.002309 357.4 529 0.00221 357.5 526 0.002123 357.6 521 0.002049 357.7 518 0.001987 357.8 515 0.001913 357.9 512 0.001839 358 508 0.001764 358.1 504 0.001665 358.2 501 0.001603 358.3 498 0.001517 358.5 494 0.001467 358.6 491 0.001381 358.7 487 0.001343 358.8 484 0.001282 358.9 481 0.001207 359 478 0.001133 359.1 474 0.001046 359.2 471 0.000972 359.3 467 0.0008977 359.4 464 0.0008234 359.5 460 0.0007491 359.6 457 0.00065 359.7 454 0.0005634 359.8 450 0.0004519 359.9 448 0.0003776 360 444 0.000291 360.2 440 0.0002167 360.3 437 0.0001424 360.4 434 6.81e-05 360.5 431 6.191e-06 360.6 428 6.191e-06 360.7 424 -6.81e-05 360.8 420 -0.0001795 360.9 417 -0.0002662 361 413 -0.0003529 361.1 410 -0.0004148 361.2 406 -0.0004891 361.3 403 -0.0005758 361.4 401 -0.00065 361.5 397 -0.0007367 361.6 394 -0.000811 361.7 390 -0.0009101 361.8 387 -0.0009967 362 384 -0.001083 362.1 381 -0.00117 362.2 377 -0.001244 362.3 373 -0.001331 362.4 369 -0.001405 362.5 367 -0.001492 362.6 363 -0.001554 362.7 360 -0.001616 362.8 356 -0.001678 362.9 353 -0.001727 363 350 -0.001802 363.1 348 -0.001851 363.2 345 -0.001913 363.3 342 -0.00195 363.4 340 -0.001975 363.5 337 -0.002 363.6 335 -0.002 363.8 333 -0.002012 363.9 331 -0.002012 364 329 -0.002 364.1 328 -0.001975 364.2 324 -0.001938 364.3 323 -0.001901 364.4 321 -0.001851 364.5 319 -0.001802 364.6 317 -0.00174 364.7 315 -0.001653 364.8 313 -0.001591 364.9 312 -0.001504 365 310 -0.001455 365.1 309 -0.001381 365.2 308 -0.001306 365.3 306 -0.00122 365.4 306 -0.001121 365.6 302 -0.001046 365.7 302 -0.0009348 365.8 300 -0.0008482 365.9 299 -0.0007491 366 298 -0.0006624 366.1 296 -0.0005758 366.2 295 -0.0004643 366.3 293 -0.00039 366.4 292 -0.000291 366.5 291 -0.0002167 366.6 289 -0.0001176 366.7 287 -3.095e-05 366.8 286 6.191e-06 366.9 284 3.095e-05 367 282 0.0003034 367.1 281 0.001418 367.3 279 0.002309 367.4 277 0.002086 367.5 276 0.001752 367.6 274 0.001504 367.7 273 0.001319 367.8 271 0.001195 367.9 269 0.001096 368 267 0.001034 368.1 266 0.0009967 368.2 264 0.000972 368.3 262 0.0009596 368.4 260 0.0009472 368.5 258 0.0009472 368.6 256 0.0009596 368.7 254 0.0009596 368.8 252 0.000972 368.9 249 0.0009844 369.1 248 0.0009967 369.2 246 0.0009967 369.3 244 0.0009967 369.4 242 0.001009 369.5 239 0.001021 369.6 237 0.001034 369.7 234 0.001046 369.8 232 0.001071 369.9 231 0.001096 370 229 0.001121 370.1 226 0.001133 370.2 224 0.001133 370.3 221 0.001108 370.4 220 0.001083 370.5 217 0.001071 370.6 215 0.001046 370.7 213 0.001034 370.9 211 0.001034 371 209 0.001046 371.1 206 0.001034 371.2 203 0.001034 371.3 201 0.001021 371.4 201 0.001009 371.5 198 0.0009967 371.6 196 0.000972 371.7 193 0.0009596 371.8 191 0.0009348 371.9 189 0.0009224 372 187 0.0008977 372.1 184 0.0008729 372.2 181 0.0008729 372.3 180 0.0008605 372.4 177 0.0008358 372.5 174 0.0007986 372.7 173 0.0007615 372.8 171 0.0007243 372.9 168 0.0006748 373 166 0.0006377 373.1 165 0.0006005 373.2 162 0.0005758 373.3 159 0.0005634 373.4 157 0.000551 373.5 156 0.0005634 373.6 154 0.0005634 373.7 151 0.0005634 373.8 149 0.0005634 373.9 148 0.0005634 374 146 0.0005634 374.1 143 0.000551 374.2 141 0.0005262 374.3 140 0.0004767 374.5 138 0.0004519 374.6 136 0.0004272 374.7 134 0.0004024 374.8 133 0.0003776 374.9 131 0.0003529 375 130 0.0003281 375.1 127 0.0003157 375.2 126 0.000291 375.3 124 0.0002786 375.4 123 0.0002662 375.5 121 0.0002538 375.6 120 0.0002414 375.7 118 0.0002291 375.8 116 0.0002167 375.9 116 0.0001919 376 115 0.0001795 376.2 113 0.0001672 376.3 112 0.0001548 376.4 110 0.00013 376.5 109 0.0001176 376.6 109 9.286e-05 376.7 107 6.81e-05 376.8 106 5.572e-05 376.9 105 3.095e-05 377 103 1.857e-05 377.1 102 6.191e-06 377.2 101 6.191e-06 377.3 99 6.191e-06 377.4 98 6.191e-06 377.5 98 6.191e-06 377.6 96 6.191e-06 377.7 96 6.191e-06 377.8 95 6.191e-06 378 93 6.191e-06 378.1 93 6.191e-06 378.2 92 -6.191e-06 378.3 91 -6.191e-06 378.4 91 -1.857e-05 378.5 90 -1.857e-05 378.6 88 -4.334e-05 378.7 87 -5.572e-05 378.8 87 -6.81e-05 378.9 86 -8.048e-05 379 84 -0.0001176 379.1 84 -0.0001424 379.2 84 -0.0001672 379.3 83 -0.0001672 379.4 81 -0.0001919 379.5 81 -0.0002043 379.6 81 -0.0002167 379.8 81 -0.0002167 379.9 80 -0.0002167 380 79 -0.0002167 380.1 77 -0.0002291 380.2 77 -0.0002291 380.3 76 -0.0002414 380.4 76 -0.0002414 380.5 75 -0.0002538 380.6 74 -0.0002662 380.7 74 -0.000291 380.8 73 -0.0003034 380.9 73 -0.0003157 381 72 -0.0003157 381.1 71 -0.0003157 381.2 71 -0.0003157 381.3 70 -0.0003157 381.4 70 -0.0003157 381.6 69 -0.0003157 381.7 68 -0.0003157 381.8 68 -0.0003405 381.9 68 -0.0003653 382 68 -0.0003653 382.1 66 -0.0003653 382.2 66 -0.0003653 382.3 65 -0.0003776 382.4 65 -0.0003776 382.5 65 -0.00039 382.6 64 -0.00039 382.7 63 -0.0004024 382.8 63 -0.0004024 382.9 63 -0.0004024 383 62 -0.0004148 383.1 62 -0.0004148 383.3 62 -0.0004148 383.4 61 -0.0004148 383.5 61 -0.0004272 383.6 60 -0.0004396 383.7 59 -0.0004272 383.8 59 -0.0004272 383.9 59 -0.0004272 384 59 -0.0004272 384.1 59 -0.0004519 384.2 59 -0.0004643 384.3 58 -0.0004643 384.4 57 -0.0004643 384.5 57 -0.0004643 384.6 56 -0.0004643 384.7 55 -0.0004643 384.8 55 -0.0004643 384.9 55 -0.0004643 385.1 55 -0.0004891 385.2 55 -0.0005015 385.3 55 -0.0005015 385.4 54 -0.0005262 385.5 54 -0.0005386 385.6 54 -0.0005634 385.7 54 -0.0005881 385.8 54 -0.0006129 385.9 52 -0.0006005 386 52 -0.0006005 386.1 52 -0.0005758 386.2 52 -0.0005634 386.3 52 -0.0005634 386.4 52 -0.0005386 386.5 51 -0.0005386 386.6 51 -0.0005386 386.7 50 -0.0005262 386.9 50 -0.0005386 387 50 -0.0005386 387.1 49 -0.0005634 387.2 49 -0.0005634 387.3 49 -0.0005634 387.4 49 -0.0005758 387.5 48 -0.0005881 387.6 48 -0.0006129 387.7 48 -0.0006377 387.8 48 -0.0006624 387.9 48 -0.0006872 388 46 -0.0006872 388.1 47 -0.0006748 388.2 46 -0.0006748 388.3 46 -0.0006624 388.4 46 -0.0006624 388.5 46 -0.00065 388.7 46 -0.00065 388.8 46 -0.00065 388.9 46 -0.0006377 389 45 -0.0006377 389.1 45 -0.00065 389.2 45 -0.00065 389.3 44 -0.0006624 389.4 44 -0.0006624 389.5 44 -0.0006624 389.6 44 -0.0006872 389.7 43 -0.0006996 389.8 43 -0.000712 389.9 43 -0.0007367 390 43 -0.0007367 390.1 43 -0.0007243 390.2 43 -0.000712 390.3 43 -0.000712 390.5 42 -0.0006996 390.6 42 -0.0006996 390.7 42 -0.0006872 390.8 42 -0.000712 390.9 41 -0.000712 391 41 -0.000712 391.1 41 -0.000712 391.2 41 -0.0007243 391.3 41 -0.0007367 391.4 41 -0.0007491 391.5 41 -0.0007491 391.6 40 -0.0007615 391.7 40 -0.0007615 391.8 40 -0.0007615 391.9 40 -0.0007615 392 40 -0.0007739 392.2 40 -0.0007615 392.3 40 -0.0007739 392.4 39 -0.0007739 392.5 39 -0.0007739 392.6 38 -0.0007739 392.7 38 -0.0007739 392.8 38 -0.0007862 392.9 38 -0.0007862 393 38 -0.0007986 393.1 38 -0.0007986 393.2 38 -0.0007986 393.3 38 -0.0007986 393.4 38 -0.0007862 393.5 37 -0.0007862 393.6 38 -0.0007862 393.7 37 -0.0007862 393.8 37 -0.0007862 394 37 -0.0007986 394.1 37 -0.000811 394.2 37 -0.0007986 394.3 37 -0.0007986 394.4 37 -0.0007862 394.5 37 -0.0007862 394.6 37 -0.0007986 394.7 36 -0.0007986 394.8 36 -0.000811 394.9 36 -0.000811 395 36 -0.000811 395.1 35 -0.0008234 395.2 35 -0.0008234 395.3 35 -0.0008234 395.4 34 -0.000811 395.5 35 -0.000811 395.6 34 -0.000811 395.8 35 -0.000811 395.9 34 -0.0008234 396 34 -0.000811 396.1 34 -0.0008234 396.2 34 -0.0008234 396.3 34 -0.0008234 396.4 34 -0.000811 396.5 34 -0.0008234 396.6 34 -0.0008358 396.7 34 -0.0008482 396.8 34 -0.0008605 396.9 34 -0.0008605 397 34 -0.0008605 397.1 34 -0.0008605 397.2 34 -0.0008729 397.3 33 -0.0008605 397.4 33 -0.0008605 397.6 32 -0.0008605 397.7 33 -0.0008605 397.8 32 -0.0008605 397.9 32 -0.0008605 398 32 -0.0008482 398.1 32 -0.0008605 398.2 32 -0.0008605 398.3 32 -0.0008729 398.4 32 -0.0008853 398.5 31 -0.0009101 398.6 31 -0.0009224 398.7 31 -0.0009348 398.8 31 -0.0009224 398.9 31 -0.0009348 399 31 -0.0009224 399.1 31 -0.0009101 399.2 30 -0.0009101 399.4 30 -0.0009101 399.5 30 -0.0008977 399.6 30 -0.0008977 399.7 30 -0.0008853 399.8 30 -0.0008977 399.9 30 -0.0009101 400 30 -0.0009101 400.1 30 -0.0009101 400.2 30 -0.0008853 400.3 30 -0.0008729 400.4 30 -0.0008605 400.5 30 -0.0008605 400.6 30 -0.0008605 400.7 30 -0.0008605 400.8 30 -0.0008605 400.9 30 -0.0008729 401.1 30 -0.0008853 401.2 29 -0.0008977 401.3 29 -0.0009101 401.4 29 -0.0009101 401.5 29 -0.0009101 401.6 29 -0.0008977 401.7 29 -0.0008977 401.8 29 -0.0008977 401.9 29 -0.0008853 402 29 -0.0008853 402.1 29 -0.0008853 402.2 29 -0.0008853 402.3 29 -0.0008853 402.4 28 -0.0008853 402.5 28 -0.0008853 402.6 28 -0.0008977 402.7 28 -0.0008977 402.9 29 -0.0009101 403 27 -0.0009101 403.1 27 -0.0009101 403.2 27 -0.0009224 403.3 27 -0.0009348 403.4 27 -0.0009472 403.5 27 -0.0009596 403.6 27 -0.0009596 403.7 27 -0.000972 403.8 27 -0.0009596 403.9 27 -0.0009472 404 27 -0.0009224 404.1 27 -0.0009224 404.2 27 -0.0009101 404.3 27 -0.0009101 404.4 27 -0.0009224 404.5 27 -0.0009224 404.7 27 -0.0009224 404.8 27 -0.0009224 404.9 27 -0.0009348 405 26 -0.0009472 405.1 27 -0.0009596 405.2 26 -0.0009348 405.3 26 -0.0009348 405.4 26 -0.0009596 405.5 26 -0.0009596 405.6 26 -0.0009596 405.7 26 -0.0009472 405.8 26 -0.0009348 405.9 26 -0.0009348 406 26 -0.0009348 406.1 26 -0.0009348 406.2 26 -0.0009348 406.3 26 -0.0009348 406.5 26 -0.0009348 406.6 26 -0.0009348 406.7 25 -0.0009348 406.8 25 -0.0009348 406.9 25 -0.0009224 407 25 -0.0009348 407.1 25 -0.0009348 407.2 25 -0.0009348 407.3 24 -0.0009348 407.4 24 -0.0009224 407.5 24 -0.0009348 407.6 24 -0.0009224 407.7 24 -0.0009348 407.8 24 -0.0009348 407.9 24 -0.0009348 408 24 -0.0009348 408.2 24 -0.0009348 408.3 24 -0.0009348 408.4 24 -0.0009348 408.5 24 -0.0009348 408.6 24 -0.0009348 408.7 24 -0.0009348 408.8 24 -0.0009348 408.9 24 -0.0009348 409 24 -0.0009348 409.1 23 -0.0009348 409.2 23 -0.0009348 409.3 23 -0.0009348 409.4 24 -0.0009224 409.5 23 -0.0009348 409.6 23 -0.0009348 409.7 23 -0.0009348 409.8 23 -0.0009472 410 23 -0.0009596 410.1 23 -0.0009596 410.2 23 -0.000972 410.3 23 -0.000972 410.4 23 -0.000972 410.5 23 -0.0009844 410.6 23 -0.0009967 410.7 23 -0.001009 410.8 23 -0.001009 410.9 23 -0.001009 411 23 -0.001009 411.1 23 -0.0009967 411.2 23 -0.0009967 411.3 23 -0.0009967 411.4 23 -0.0009967 411.5 23 -0.0009967 411.6 23 -0.0009967 411.8 23 -0.0009967 411.9 23 -0.0009844 412 22 -0.0009844 412.1 22 -0.0009844 412.2 22 -0.0009844 412.3 22 -0.0009967 412.4 22 -0.0009967 412.5 22 -0.0009967 412.6 22 -0.001009 412.7 22 -0.001009 412.8 21 -0.0009967 412.9 21 -0.0009844 413 21 -0.000972 413.1 21 -0.000972 413.2 21 -0.000972 413.3 21 -0.0009844 413.4 21 -0.001021 413.6 21 -0.001059 413.7 21 -0.001059 413.8 21 -0.001083 413.9 21 -0.001071 414 21 -0.001071 414.1 21 -0.001059 414.2 21 -0.001046 414.3 21 -0.001021 414.4 21 -0.001021 414.5 21 -0.001009 414.6 21 -0.001009 414.7 21 -0.0009967 414.8 21 -0.0009967 414.9 21 -0.0009967 415 21 -0.0009967 415.1 21 -0.0009967 415.2 21 -0.0009967 415.4 21 -0.0009967 415.5 20 -0.0009844 415.6 21 -0.0009844 415.7 21 -0.0009967 415.8 21 -0.0009844 415.9 20 -0.001009 416 21 -0.001009 416.1 20 -0.001009 416.2 20 -0.0009967 416.3 20 -0.001009 416.4 20 -0.001009 416.5 20 -0.001009 416.6 20 -0.001021 416.7 20 -0.001021 416.8 20 -0.001021 416.9 20 -0.001021 417.1 20 -0.001034 417.2 20 -0.001059 417.3 20 -0.001059 417.4 20 -0.001046 417.5 20 -0.001046 417.6 20 -0.001046 417.7 20 -0.001046 417.8 20 -0.001034 417.9 20 -0.001034 418 20 -0.001034 418.1 20 -0.001034 418.2 20 -0.001046 418.3 20 -0.001046 418.4 20 -0.001059 418.5 20 -0.001059 418.6 19 -0.001059 418.7 19 -0.001071 418.9 19 -0.001059 419 19 -0.001059 419.1 20 -0.001071 419.2 19 -0.001071 419.3 19 -0.001059 419.4 19 -0.001059 419.5 18 -0.001059 419.6 19 -0.001046 419.7 19 -0.001059 419.8 19 -0.001059 419.9 19 -0.001059 420 18 -0.001071 420.1 18 -0.001083 420.2 19 -0.001059 420.3 18 -0.001059 420.4 19 -0.001059 420.5 18 -0.001046 420.7 18 -0.001059 420.8 18 -0.001059 420.9 18 -0.001059 421 18 -0.001059 421.1 18 -0.001071 421.2 18 -0.001071 421.3 18 -0.001083 421.4 18 -0.001083 421.5 18 -0.001083 421.6 18 -0.001083 421.7 18 -0.001083 421.8 18 -0.001083 421.9 18 -0.001096 422 18 -0.001083 422.1 18 -0.001083 422.2 18 -0.001071 422.3 18 -0.001059 422.5 18 -0.001071 422.6 18 -0.001071 422.7 18 -0.001096 422.8 18 -0.001108 422.9 18 -0.001108 423 18 -0.001108 423.1 18 -0.001121 423.2 18 -0.001121 423.3 18 -0.001108 423.4 18 -0.001121 423.5 18 -0.001121 423.6 18 -0.001133 423.7 18 -0.001133 423.8 18 -0.001133 423.9 18 -0.001121 424 18 -0.001108 424.1 18 -0.001096 424.3 18 -0.001083 424.4 18 -0.001059 424.5 18 -0.001046 424.6 17 -0.001034 424.7 18 -0.001021 424.8 17 -0.001021 424.9 17 -0.001034 425 17 -0.001046 425.1 18 -0.001059 425.2 17 -0.001059 425.3 17 -0.001071 425.4 17 -0.001071 425.5 17 -0.001083 425.6 17 -0.001108 425.7 16 -0.001108 425.8 16 -0.001108 426 17 -0.001096 426.1 17 -0.001096 426.2 17 -0.001071 426.3 16 -0.001071 426.4 16 -0.001096 426.5 16 -0.001108 426.6 16 -0.001121 426.7 16 -0.001133 426.8 16 -0.001133 426.9 16 -0.001145 427 16 -0.001133 427.1 17 -0.001121 427.2 16 -0.001121 427.3 16 -0.001096 427.4 16 -0.001083 427.5 16 -0.001071 427.6 16 -0.001071 427.8 16 -0.001059 427.9 16 -0.001071 428 16 -0.001071 428.1 16 -0.001071 428.2 16 -0.001071 428.3 16 -0.001083 428.4 16 -0.001083 428.5 16 -0.001083 428.6 16 -0.001083 428.7 16 -0.001083 428.8 16 -0.001071 428.9 16 -0.001071 429 16 -0.001083 429.1 16 -0.001096 429.2 16 -0.001096 429.3 16 -0.001096 429.4 16 -0.001096 429.6 16 -0.001083 429.7 16 -0.001096 429.8 16 -0.001108 429.9 16 -0.001108 430 16 -0.001108 430.1 16 -0.001108 430.2 16 -0.001108 430.3 16 -0.001108 430.4 16 -0.001121 430.5 16 -0.001133 430.6 16 -0.001145 430.7 16 -0.001158 430.8 16 -0.00117 430.9 16 -0.001158 431 16 -0.001158 431.1 16 -0.001158 431.2 16 -0.001158 431.4 16 -0.001158 431.5 16 -0.001158 431.6 15 -0.001145 431.7 15 -0.001145 431.8 15 -0.001158 431.9 16 -0.001158 432 15 -0.001158 432.1 15 -0.001158 432.2 15 -0.001158 432.3 15 -0.001158 432.4 15 -0.001121 432.5 16 -0.001096 432.6 15 -0.001071 432.7 16 -0.001059 432.8 16 -0.001059 432.9 15 -0.001059 433.1 15 -0.001059 433.2 15 -0.001059 433.3 15 -0.001059 433.4 15 -0.001083 433.5 16 -0.001108 433.6 15 -0.001121 433.7