[MAP Logo]

Materials Algorithms Project
Data Library



Data Library MAP_WELD_INCLUSIONS

  1. Provenance of code.
  2. Purpose of code.
  3. Description of subroutine's operation.
  4. References.
  5. Any additional information.
  6. Download source code.
  7. Links.

Provenance of Source Code

Kazutoshi Ichikawa,
Nippon Steel Corporation,
Welding and Joining Research Center,
20-1 Shintomi, Futsu, Chiba 293-8511,
Japan

Top | Next

Purpose

Provides chemical and geometrical data on oxide inclusions in low-alloy, ferritic steel welds.

Top | Next | Prev

Description

The file which is downloaded contains the following information:

Table 1 lists chemical compositions of welds / wt.%. Only deoxidising compositions (Si, Mn, Al, Ti), nitrogen and oxygen concentrations are listed.

Table 2 lists geometrical characteristics of inclusions in the welds. The first column is the identification mark, the second the mean three--dimensional particle diameter in micrometres, the third the inclusion volume fraction multiplied by 1000, the fourth the number of particles per cubic millimetre, the fifth the mean centre-to-centre interparticle spacing in micrometres, the sixth the mean surface-to-surface interparticle spacing in micrometres. The last column gives the reference number.

Table 3 lists the chemical compositions of inclusions / wt.%.

Top | Next | Prev

References

  1. A. O. Kluken and O. Grong, Metallurgical. Transactions, 20A (1989) 1335-1349.
  2. A. G. Fox, M. W. Eakes and G. L. Franke, Welding Journal, Oct. (1996) 330s-342s.
  3. G. Thewlis, Joining & Materials, 2 (1998) 25-32.
  4. G. Thewlis, Materials Science and Technology, 10 (1994) 110-125.
  5. J. M. Dowling, J. M. Corbett and H. W. Kerr, Metallurgical Transactions, 17A (1986) 1611-1623.
  6. G. M. Evans, Welding Journal, Oct. (1995) 249s-261s.
  7. K. Ichikawa, T. Koseki and M. Fuji, Science and Technology of Welding and Joining, 2 (1997) 231-235.

Top | Next | Prev

Further Comments

None.

Top | Next | Prev

Download data

Download data library

Top | Prev