P. E. J. Rivera Díaz del Castillo
Phase Transformations and Complex Properties Group,
Department of Materials Science and Metallurgy,
University of Cambridge,
Cambridge, U.K.
The program solves the mass balance equation for spherical precipitates, when capillarity is taken into account, as supersaturation is varied, and for given values of dimensionless radius (particle radius over critical radius for nucleation).