#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
 1 0.002259    4.036 0.001396    1.626   0.6228   0.2439  0.14761  0.6036 55.41  60 0.001107  91.62 0.000262  87.84  86.85  96.39  4.591  -16.14   7.648    1  0  0.60364   31.231  55.41  60  0.60364   31.231  55.41  60  37.996  41.647  39.293  21.856 0.011728  64.807 