#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
 6 0.0004985      3.4 0.0005002    1.348   0.5107   0.2642  0.14872  0.6136 55.48  60 8.697e-06   15.1 7.307e-05   14.3  14.02  27.33   4.52  -69.69   61.44  120  5  0.61359   30.745  55.48  60  0.61359   30.745  55.48  60  88.343  94.257  91.903  18.652 0.011893  64.735 