#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
14   0.9309   0.7388   0.9001   0.7934   0.5246    3.477  0.13035  0.3531 41.56  60  22.38  20.34  20.94  21.95  19.52  24.82  18.41   34.62  -77.82 10.5  2   0.3531    41.65  41.56  60   0.3531    41.65  41.56  60 -18.338 -29.259  -31.47  16.282 0.011099  79.254 