#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
21    0.938     1.16    1.002    0.839   0.1799    2.911   0.1302  0.3411 40.24  60  15.74  16.87  15.99  14.67  11.47  18.48  19.63   59.09  -102.3 21.4 15  0.34106   42.064  40.24  60  0.34106   42.064  40.24  60 -64.926 -76.006 -78.202 -5.8393 0.011229  80.414 