History:
  12/04/1999   L.Sree Harsha, This file contains the steps to run 
     Ultimate Tensile Strength Model.
*******************************************************************


a) Create data file containg input elements as (in order)

Column	Variable	
1	C
2	Si
3	Mn
4	S	
5	P       
6	Ni	
7	Cr	
8	Mo	
9	V	
10	Cu	
11	Co	
12	W
13	O(p)	
14	Ti(p)	
15	B(p)	
16	Nb(p)	
17	HI	
18	IT	
19	pwhtT	
20	pwhtt	

p - PPM wt.

HI - Heat Input in kJ/mm
IT- Interpass Temperature in deg.C
pwhtT - post weld heat treatment in deg. C [For as-welded condition, Temp. = 20.0, time= 0.0]
pwhtt - post weld heat treatment time in hr.

b) change the input file name as "test.dat".

c) type "csh harsha_uts.gen" at command prompt in directory
   
d) Finally, the results (UTS (MPa)) are written in "Uresult.dat".