  831.0802962   78.7279374  752.3523588  909.8083218
  823.8030906   70.5974850  753.2056056  894.4005756
  816.8469330   63.1664586  753.6804744  880.0134798
  810.2276112   56.4504696  753.7771416  866.6779926
  803.9583552   50.4642474  753.4941078  854.4226908
  798.0503664   45.2201400  752.8303146  843.2705064
  792.5118474   40.7231748  751.7886726  833.2349340
  787.3478256   36.9664722  750.3812652  824.3142978
  782.5605942   33.9259536  748.6346406  816.4865478
  703.4957328   72.3222360  631.1734968  775.8179688
  703.0628472   64.2238884  638.8389588  767.2867356
  702.4211922   57.0088638  645.4122402  759.4300560
  701.5847034   50.6289168  650.9557866  752.2135320
  700.5684630   45.0331560  655.5352188  745.6016190
  699.3887880   40.1705136  659.2182744  739.5593016
  698.0631420   35.9908038  662.0723382  734.0539458
  696.6094296   32.4463986  664.1630310  729.0558282
  695.0465256   29.4939918  665.5525338  724.5405174