#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  S_W[ 7]  S_W[ 8]  S_W[ 9]  S_W[10]  S_W[11]  S_W[12]  S_W[13]  S_W[14]  S_W[15]  S_W[16]  S_W[17]  S_W[18]  S_W[19]  S_W[20]  S_W[21]  S_W[22]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 WX2/k7 WX2/k8 WX2/k9 WX2/k10 WX2/k11 WX2/k12 WX2/k13 WX2/k14 WX2/k15 WX2/k16 WX2/k17 WX2/k18 WX2/k19 WX2/k20 WX2/k21 WX2/k22 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
14 20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       0.3      1.099   24.43 2044 0.08832 0.03683 0.0527 0.02741 0.01652 0.1233 0.255  0.2036 0.06138 0.03316 0.03659 0.06493 0.05806 0.01985 0.01518 0.1495 0.08054 0.05611 0.4745 0.07306 0.06097 0.04716 240.6  568.3   -1210   -662538496 0  1.0991   466.38   24.43  2044 1.0991   466.38   24.43  2044 Inf     Inf     Inf     Inf     0.011131 941.34  
14 2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    0.3      1.099   24.43 2044 4.822  2.011  2.877  1.497  0.9018 6.731  13.92  11.12  3.351  1.811  1.998  3.545  3.17   1.084  0.8288 8.164  4.397  3.064  25.9   3.989  3.329  2.575  140.9  338.7   -591.6  1    0  1.0991   507.16   24.43  2044 1.0991   507.16   24.43  2044 5.8689  -41.658 -45.78  344.55  0.0067434 561.59  
14 0.8322   0.569    0.5684   0.6574   0.5611   0.9662   1.723    1.338    0.6718   0.5907   0.955    0.8126   0.6468   0.4103   0.3786   1.235    0.8225   0.6394   1.771    0.7664   0.8641   0.4781   0.033987 1.099   1903  2044 51.02  45.51  65.24  25.37  20.98  52.82  34.34  45.47  54.39  38.01  16.05  39.33  55.51  47.17  42.35  39.23  47.62  54.9   60.54  49.76  32.66  82.52  189.3  269     -199.3  1    0  1.0991   4122.7   1903   2044 1.0991   4122.7   1903   2044 3847.7  3796.7  3792.6  4116.6  0.00064473 2624.7  
14 0.6911   0.5061   0.5336   0.5345   0.4963   0.8111   1.15     1.023    0.6075   0.522    0.7296   0.6815   0.58     0.4105   0.3826   0.9132   0.6835   0.5713   1.469    0.6568   0.7155   0.4939   0.034427 0.5724  965.8 2044 148.6  68.18  17.23  56.22  20.73  50     37.1   42.78  77.57  62.01  23.44  76.68  98.16  100.9  45.61  106.7  53.74  100.5  74.9   170.5  62.67  546.7  243.7  269     -151.6  1    0  0.57238  4472.4   965.8  2044 0.57238  4472.4   965.8  2044 4262.5  4208.5  4204.5  4531.4  0.00042133 1894.6  
14 0.8912   0.4589   0.227    0.5218   0.3291   0.588    0.7285   0.687    0.5631   0.4882   0.5999   0.6758   0.6174   0.4702   0.3143   1.015    0.534    0.6042   1.289    0.939    0.6973   1.445    0.025216 0.5068  1594  2044 138.8  65.21  36.85  72.09  89.67  60.26  47.23  72.42  111.5  76.01  12.47  49.27  102.2  56.42  40.52  85.17  62.97  92.44  95.27  107.4  61.45  297.7  266.4  269     -132.2  1    0  0.50682  4822.4   1594   2044 0.50682  4822.4   1594   2044 4620    4565    4560.9  4889    0.00033082 2609.3  
14 1.07     0.3869   0.1438   0.5075   0.4356   0.4643   0.5169   0.5979   0.6112   0.4703   0.3523   0.4946   0.6424   0.3707   0.226    0.9604   0.4423   0.5933   1.271    0.9905   0.6174   2.791    0.023879 0.4897  1718  2044 90.78  38.52  77.12  68.78  97.6   73.55  84.17  58.33  69.99  61.82  7.123  33.89  60.43  52.88  44.33  115.9  84.76  45.12  52.35  85.46  66.23  242.2  273.4  269     -105.9  1    0  0.48969  4874.2   1718   2044 0.48969  4874.2   1718   2044 4711.7  4656.5  4652.4  4980.7  0.00031583 2759.4  
14 1.029    0.2478   0.133    0.4633   0.5146   0.4045   0.4909   0.4635   0.5188   0.3948   0.171    0.3009   0.5067   0.2804   0.1709   1.054    0.4232   0.4031   0.9235   0.925    0.5487   4.761    0.023519 0.4897  1771  2044 98.22  93.87  90.2   82.56  69.94  96.92  93.35  97.06  97.15  87.74  30.22  91.56  97.11  92.43  77.46  96.24  92.57  97.73  99.19  97.98  83.86  83.25  269.2  269     -56.09  1    0  0.48969  4882     1771   2044 0.48969  4882     1771   2044 4743.4  4688.5  4684.4  5012.4  0.00031243 2796.7  
14 1.029    0.2558   0.1337   0.4689   0.4941   0.4063   0.4917   0.4674   0.5209   0.4005   0.2106   0.3152   0.5107   0.2859   0.1782   1.05     0.4242   0.4082   0.9265   0.9262   0.5458   4.49     0.023491 0.4897  1775  2044 98.11  88.08  89.24  80.57  75.87  96.04  93.04  95.44  96.35  85.24  19.94  83.48  95.62  88.87  71.31  97     92.14  95.33  98.53  97.74  84.73  93.61  269.8  269     -60.47  1    0  0.48969  4882.5   1775   2044 0.48969  4882.5   1775   2044 4741.4  4686.4  4682.3  5010.4  0.0003124 2803    
14 1.029    0.2551   0.1336   0.4679   0.498    0.4062   0.4917   0.4672   0.5209   0.3999   0.1975   0.3134   0.5105   0.2854   0.1769   1.05     0.4241   0.4079   0.9265   0.9261   0.5483   4.508    0.023495 0.4897  1774  2044 98.11  88.63  89.34  80.94  74.67  96.09  93.06  95.51  96.37  85.5   22.67  84.43  95.68  89.18  72.35  96.98  92.18  95.44  98.54  97.75  83.99  92.87  269.7  269     -59.47  1    0  0.48969  4882.4   1774   2044 0.48969  4882.4   1774   2044 4742.1  4687.1  4683.1  5011.1  0.0003124 2802    