#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  S_W[ 7]  S_W[ 8]  S_W[ 9]  S_W[10]  S_W[11]  S_W[12]  S_W[13]  S_W[14]  S_W[15]  S_W[16]  S_W[17]  S_W[18]  S_W[19]  S_W[20]  S_W[21]  S_W[22]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 WX2/k7 WX2/k8 WX2/k9 WX2/k10 WX2/k11 WX2/k12 WX2/k13 WX2/k14 WX2/k15 WX2/k16 WX2/k17 WX2/k18 WX2/k19 WX2/k20 WX2/k21 WX2/k22 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
16 20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       0.3      0.8293  18.43 2044 0.135  0.12   0.04862 0.02643 0.04074 0.1257 0.218  0.1229 0.07944 0.07872 0.03371 0.1166 0.07919 0.05637 0.01307 0.1595 0.1647 0.06626 0.3517 0.1653 0.07742 0.05936 290.9  596.6   -1382   -1102330752 0  0.82932  448.91   18.43  2044 0.82932  448.91   18.43  2044 Inf     Inf     Inf     Inf     0.013214 1127.1  
16 2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    0.3      0.8292  18.43 2044 7.367  6.552  2.654  1.443  2.224  6.86   11.9   6.711  4.337  4.298  1.84   6.366  4.323  3.077  0.7134 8.708  8.991  3.617  19.2   9.025  4.226  3.241  171.2  358.8   -675.9  1    0  0.82921  496.91   18.43  2044 0.82921  496.91   18.43  2044 -70.952 -120.68 -124.79 287.84  0.0079441 670.95  
16 1.002    1.009    0.5273   0.6094   0.8425   0.9164   1.522    0.9586   0.7626   0.89     0.8476   1.085    0.7467   0.6759   0.3663   1.278    1.151    0.6612   1.507    1.156    0.918    0.5224   0.029758 0.5368  1212  2044 77.74  42.23  43.02  54.59  29.11  25.19  60.46  27.88  95.41  42.01  10.42  31.27  58.93  56.51  28.67  68.19  31.12  95.04  71.28  50.44  71.41  351.8  290.8  309.4   -269.8  1    0  0.53684  4652.9   1212   2044 0.53684  4652.9   1212   2044 4355.8  4299.9  4295.9  4665.2  0.00038864 2320.9  
16 0.9108   0.6816   0.3574   0.5856   0.5787   0.4712   1.236    0.5193   0.7978   0.6391   0.4871   0.6503   0.6014   0.5534   0.2439   1.117    0.6607   0.6798   1.292    0.8483   0.9313   1.174    0.024747 0.4829  1577  2044 87.43  44.15  42.81  80.52  49.91  55.06  105.5  67.4   60.42  38.69  13.63  60.86  42.09  52.55  37.11  52.17  73.83  86.42  61.68  79.49  124.6  314.9  304.1  309.4   -186.5  1    0  0.48292  4862.9   1577   2044 0.48292  4862.9   1577   2044 4617.2  4560.8  4556.7  4926.5  0.00032739 2736.3  
16 0.8668   0.4677   0.239    0.5969   0.4972   0.3601   1.307    0.4421   0.6348   0.4373   0.3498   0.5468   0.3994   0.4239   0.1788   0.8308   0.5861   0.6483   1.023    0.7761   1.128    2.372    0.023561 0.4576  1649  2044 77.54  34.85  59.44  79.27  52.68  64.88  103.2  47.87  106.3  39.14  15.67  55.63  38.5   89.67  53.67  60.83  120.9  79.48  105    93.59  129.7  232.3  309    309.4   -134    1    0  0.45763  4927.5   1649   2044 0.45763  4927.5   1649   2044 4725.9  4669.4  4665.3  5035.3  0.00030782 2826.6  
16 0.7732   0.2841   0.189    0.5769   0.4237   0.2979   1.355    0.3146   0.6726   0.3048   0.2762   0.4367   0.2547   0.4234   0.1554   0.6655   0.6653   0.5887   1.058    0.7676   1.334    3.996    0.022968 0.4543  1722  2044 109.9  47.97  61.2   78.78  70.83  63.3   85.32  34.75  68.58  69.92  18.56  60.57  75.44  91.38  56.16  82.62  49.54  70.02  67.12  96.77  77.74  161.4  309.7  309.4   -96.62  1    0  0.45428  4947.1   1722   2044 0.45428  4947.1   1722   2044 4790.4  4733.9  4729.8  5099.8  0.00030217 2902.5  
16 0.8218   0.2067   0.1515   0.5509   0.4228   0.2436   1.273    0.1918   0.5658   0.284    0.2456   0.3632   0.2306   0.4237   0.1383   0.6245   0.4752   0.501    0.8726   0.7725   1.2      5.537    0.022888 0.4543  1734  2044 97.31  90.67  95.21  86.39  71.12  94.67  96.63  93.54  96.92  80.59  23.47  87.55  91.98  91.27  70.81  93.84  97.12  96.7   98.62  95.54  96.13  84.1   305.7  309.4   -55.78  1    0  0.45428  4949.3   1734   2044 0.45428  4949.3   1734   2044 4806.1  4749.8  4745.7  5115.5  0.00030059 2899.4  
16 0.8203   0.2136   0.1532   0.553    0.4219   0.2463   1.275    0.2005   0.5687   0.2863   0.251    0.3692   0.2321   0.423    0.1411   0.6259   0.481    0.5036   0.8751   0.7717   1.203    5.315    0.022862 0.4543  1738  2044 97.67  84.91  93.08  85.76  71.43  92.58  96.37  85.54  95.92  79.28  22.48  84.74  90.85  91.56  68.11  93.41  94.77  95.69  98.06  95.74  95.62  91.27  306.1  309.4   -58.29  1    0  0.45428  4949.8   1738   2044 0.45428  4949.8   1738   2044 4806    4749.6  4745.5  5115.4  0.00030053 2905    
16 0.8203   0.2126   0.1531   0.5527   0.4221   0.2462   1.275    0.1994   0.5687   0.2859   0.2498   0.3686   0.2319   0.4231   0.1405   0.6259   0.4807   0.5035   0.875    0.7718   1.203    5.335    0.022865 0.4543  1738  2044 97.66  85.64  93.21  85.84  71.37  92.71  96.37  86.52  95.95  79.47  22.71  85.03  90.93  91.53  68.63  93.42  94.88  95.73  98.07  95.73  95.61  90.59  306.1  309.4   -57.97  1    0  0.45428  4949.8   1738   2044 0.45428  4949.8   1738   2044 4806    4749.7  4745.6  5115.4  0.00030053 2904.4  