      Column   Minimum     Maximum       Mean           Std. Dev
         1        0.3200        1.1900        0.6360        0.1948
         2        0.5400        0.7900        0.6907        0.0609
         3        0.0040        0.0180        0.0092        0.0034
         4        0.9000        1.2700        1.1023        0.0947
         5       70.0000      300.0000      108.6667       38.8395
         6        0.9000       22.0000        5.2100        3.7385
         7        0.0000      130.0000       59.7667       27.7249
         8        6.7800      136.9560       60.4324       29.1824