#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  S_W[ 7]  S_W[ 8]  S_W[ 9]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 WX2/k7 WX2/k8 WX2/k9 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
13   0.1766   0.5461    1.501    0.161  0.03873  0.01969  0.00295   0.1022    2.982 0.098013 0.09965 20.75  30  8.305  11.83  12.59  8.634  4.348  1.448 0.006798   4.95  15.23  8.927  -146.1   123.9   20  0 0.099647   29.971  20.75  30 0.099647   29.971  20.75  30  162.72  154.08  152.21  16.606 0.0061803  35.928 