XSIZE  5
YSIZE  5
ZSIZE  5
DIMENSIONS 3
GEOMETRY PERIODIC
SPLAY 10.0d0
TWIST 0.1d0
BEND  1.0d0
K_24 0.0d0
FIELD 0.00d0
DELTA 0.00d0
CYCLES 20
ITERATIONS 1000
NANNEAL 1
BETAINIT 30d0
BETAFACTOR 10d0
ANGLEFACTOR 0.10d0
DIRECTORY