H.K.D.H. Bhadeshia,
Phase Transformations Group,
Department of Materials Science and Metallurgy,
University of Cambridge,
Cambridge, U.K.
Estimate the derivative of MAP_STEEL_GMART. It is used by MAP_STEEL_MART in estimating the volume fraction of martensite.
| Language: | FORTRAN |
| Product form: | Source code |
MAP_STEEL_GMDASH estimates the derivative of MAP_STEEL_GMART:
MAP_STEEL_GMDASH = 1/VMART(1 - VMART) + log(1 - VMART)/(VMART2)
None supplied.
None.
No information supplied.
None.
DOUBLE PRECISION VMART,MAP_STEEL_GMDASH,XGMD
READ (5,*) VMART
XGMD = MAP_STEEL_GMDASH(VMART)
WRITE (6,*) XGMD
STOP
END
9.089D-02
0.5674566
None.
martensite
MAP originated from a joint project of the National Physical Laboratory and the University of Cambridge.