To calculate the non-uniform elongation and the volume fraction of inclusions in the primary microstructure of low alloy steel weld deposits.
| Language: | FORTRAN |
| Product form: | Source code |
The plastic strain of steel weld deposits can be factorised into a uniform and a non-uniform component. It is possible to express the non-uniform component in terms of the inclusion content of the weld deposits [1]. MAP_STEEL_ELONG calculates the percentage non-uniform elongation in the primary microstructure, and the volume fraction of inclusions from the following equations:
None.
No information supplied.
None.
DOUBLE PRECISION NELONG,OXYPPM,RATIO,SUL,VINC
C
WRITE (*,*) 'Input oxygen ppm, sulphur wt%, ratio yield to ',
& 'tensile strength:'
READ (*,*) OXYPPM,SUL,RATIO
CALL MAP_STEEL_ELONG(NELONG,SUL,OXYPPM,VINC,RATIO)
WRITE (*,1) NELONG, VINC
STOP
1 FORMAT ('Non-uniform elongation = ',F8.2,' %'/
& 'Volume fraction of inclusions = ',F8.4 )
END
Input oxygen ppm, sulphur wt%, ratio yield to tensile strength: 316 0.008 0.177
Non-uniform elongation = 15.36 % Volume fraction of inclusions = 0.0022
None.
elongation, inclusions, steel, weld