#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  S_W[ 7]  S_W[ 8]  S_W[ 9]  S_W[10]  S_W[11]  S_W[12]  S_W[13]  S_W[14]  S_W[15]  S_W[16]  S_W[17]  S_W[18]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 WX2/k7 WX2/k8 WX2/k9 WX2/k10 WX2/k11 WX2/k12 WX2/k13 WX2/k14 WX2/k15 WX2/k16 WX2/k17 WX2/k18 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
13   0.6069   0.2165   0.4052   0.4862   0.1935   0.6381    0.468   0.2883   0.1981   0.1577   0.2457   0.4886   0.7562   0.1778   0.7012     1.24   0.6443    3.689 0.025688  0.2957 896.1 1107  94.03   86.3  85.02  96.08  90.34  94.01   91.6  89.05  82.68  84.69  76.91   84.6  91.03  81.72   97.1  98.91  97.84   93.2  210.9     201  -27.25    1  0  0.29567   2558.1  896.1 1107  0.29567   2558.1  896.1 1107  2487.1  2442.2  2438.5    2688 0.00039281  1635.3 