-1.65748 0.107511 0.749067 0.0523577 0.0637436 -0.00612257 0.0686926 0.23548 0.126483 0.0100912 0.421588 -0.000609133 -0.1499 0.369227 0.0363676 0.0719546 -0.0684635 -0.0197121 0.0978236 0.524402 -0.528797 0.616845 -0.952088 -0.000657194 -0.870791 -0.0306615 0.0652944 0.0901386 -0.162448 0.451131 0.015217 -0.00805634 0.0942386 -0.000169394 0.294585 -2.66515 -0.119409 -0.0196647 0.0902961 -3.63733 -0.0139859 -0.613461 -0.457472 0.518548 1.61202 -0.377861 -0.0208773 0.155683 0.0293404 0.178827 0.215992 0.170365 0.0608126 0.00440318 0.157728 -0.00225296 0.20699 -0.256707 -0.0951478 -0.0885351 -0.0865714 0.0426023 0.00242237 -0.344744 -0.0176683 -5.46536 0.474949 -0.16854 0.895872 0.00355623 0.0476687 -0.146747 0.0372881 -0.221018 -0.0423992 -0.015878 0.0557372 6.48447e-05 -0.388109 2.33577 -0.0569915 -0.0770315 -0.0419464 3.34966 0.00248245 0.423451 0.131172 -0.574184 -3.49325 -0.332804 0.378164 0.00204744 -0.0608929 -0.622605 0.655599 -0.346101 -0.379976 0.0014759 -0.112553 -0.00258219 -0.742958 -1.19714 -0.338464 -0.00936975 0.106077 3.6509 0.059044 -2.84268 -0.00677237 -0.0343535 -3.9496 -2.53504 3.33923 -0.525314 3.47855 -2.14515 