#Elongation Error Tensile-Strength Error Yield-Strength Error
19.7443588 0.8451192 651.6881685 12.8751093 513.7879006 14.1456038
15.7764507 0.8241384 586.0013602 11.5741264 478.8818877 8.3451225
20.4713015 0.9160064 482.9921171 10.6549241 406.3279484 11.0935873
37.6986917 1.2281998 210.9894576 18.1918375 134.8113933 11.5572053