#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  S_W[ 7]  S_W[ 8]  S_W[ 9]  S_W[10]  S_W[11]  S_W[12]  S_W[13]  S_W[14]  S_W[15]  S_W[16]  S_W[17]  S_W[18]  S_W[19]  S_W[20]  S_W[21]  S_W[22]  S_W[23]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 WX2/k7 WX2/k8 WX2/k9 WX2/k10 WX2/k11 WX2/k12 WX2/k13 WX2/k14 WX2/k15 WX2/k16 WX2/k17 WX2/k18 WX2/k19 WX2/k20 WX2/k21 WX2/k22 WX2/k23 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
6  20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       0.3      0.5792  12.87 920 0.09201 0.09924 0.2267 0.0508 0.05542 0.1217 0.0392 0.1768 0.1224 0.2678 0.01566 0.07941 0.08442 0.04837 0.04044 0.01638 0.7566 0.1848 0.5589 0.1018 1.229  0.547  0.1056 128.9  126.2   -544.1  24   0  0.57923  197.36   12.87  920 0.57923  197.36   12.87  920 -280.94 -329.76 -333.44 -154.78 0.013244 452.86  
6  2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    0.3      0.5792  12.87 920 5.024  5.418  12.38  2.774  3.026  6.647  2.14   9.653  6.683  14.62  0.8549 4.335  4.609  2.641  2.208  0.8946 41.31  10.09  30.52  5.556  67.11  29.87  5.764  93.42  75.86   -266.1  1    0  0.57921  212.6    12.87  920 0.57921  212.6    12.87  920 -7.8582 -52.803 -56.509 68      0.0097683 331.63  
6  0.7395   0.7275   1.187    0.5105   0.5218   0.8752   0.4696   0.9902   1.062    1.237    0.3663   0.6323   0.7562   0.5657   0.6121   0.3663   2.198    1.198    1.741    0.731    2.513    1.858    0.6996   0.037436 0.4436  633.1 920 76.04  67.9   11.86  19.69  59.47  25.2   60.95  11.32  4.184  22.27  16.94  23.39  12.02  66.6   18.44  14.27  54.93  103.4  42.78  18.46  139.4  91.53  305.5  117.8  112.7   -104.5  1    0  0.4436   1839.4   633.1  920 0.4436   1839.4   633.1  920 1727.1  1679.4  1675.7  1839.8  0.00066159 1034.9  
6  0.6836   0.6256   0.4164   0.2383   0.4309   0.4637   0.4129   0.339    0.2739   0.5931   0.2251   0.3148   0.2723   0.5263   0.351    0.1543   1.656    1.371    1.164    0.3234   2.986    1.815    1.501    0.033256 0.4255  769.4 920 59.66  17.57  22.95  63.85  17.22  34.6   39.54  44.62  2.894  33.94  10.6   46.17  29.39  123.1  29.74  43.42  133.7  124.8  61.35  150.8  107.8  115.7  228.2  114.7  112.7   -43.41  1    0  0.42548  1889     769.4  920 0.42548  1889     769.4  920 1821    1773.8  1770.1  1933.8  0.0006003 1160.7  
6  0.5481   0.27     0.2116   0.2066   0.1862   0.2981   0.2787   0.2424   0.07366  0.3523   0.1085   0.2244   0.1644   0.6329   0.2537   0.1248   1.953    1.641    0.9452   0.4313   3.113    1.973    2.735    0.032506 0.4102  776.5 920 61.19  28.83  28.85  61.1   71.25  50.41  37.97  105.3  4.548  47.34  31.39  13.64  27.29  39.38  15.75  70.19  63.71  153    109.1  107.7  97.09  82.15  268.8  111.6  112.7   -5.018  1    0  0.41022  1907.5   776.5  920 0.41022  1907.5   776.5  920 1875.7  1829    1825.3  1988.4  0.00057411 1157.4  
6  0.4461   0.1559   0.127    0.1729   0.1755   0.2382   0.1868   0.2822   0.03311  0.2481   0.1007   0.08744  0.09894  0.4095   0.1241   0.1304   1.573    2.142    1.042    0.4672   3.078    1.8      5.358    0.031858 0.4125  812.8 920 62.89  35.21  45.82  42.94  63.17  83.59  45.8   52.58  2.065  58.92  26.18  11.03  26.69  60.78  7.025  69.55  73.31  102.9  80.02  77.28  102.2  95.5   185.7  108.9  112.7   24.08   1    0  0.41249  1909.5   812.8  920 0.41249  1909.5   812.8  920 1910.5  1864.1  1860.4  2023.2  0.00056849 1184.4  
6  0.3704   0.105    0.1017   0.1215   0.1527   0.249    0.1428   0.2217   0.011    0.1964   0.07824  0.0337   0.06203  0.3341   0.04704  0.1323   1.366    2.252    0.9754   0.4233   3.124    1.772    8.571    0.031892 0.4125  811.1 920 91.22  77.56  71.43  87     83.5   76.51  78.39  85.21  18.7   93.97  43.33  74.25  67.88  91.33  48.89  67.49  97.29  93.08  91.3   94.15  99.28  98.51  72.57  103.9  112.7   57.89   1    0  0.41249  1910     811.1  920 0.41249  1910     811.1  920 1933    1887.5  1883.8  2045.7  0.00056326 1165.7  
6  0.3735   0.1128   0.1052   0.1262   0.1541   0.2437   0.1492   0.2282   0.01214  0.1984   0.07898  0.04233  0.06823  0.3368   0.06543  0.1302   1.37     2.238    0.9783   0.4245   3.123    1.771    7.778    0.031795 0.4125  816.1 920 89.72  67.28  66.69  80.56  81.97  79.85  71.79  80.42  15.35  92.06  42.52  47.06  56.12  89.87  25.27  69.67  96.64  94.22  90.75  93.61  99.32  98.68  88.12  104.9  112.7   52.7    1    0  0.41249  1910.4   816.1  920 0.41249  1910.4   816.1  920 1930.6  1884.9  1881.2  2043.3  0.00056358 1173.9  
6  0.3739   0.1112   0.1047   0.1256   0.1542   0.2451   0.148    0.2274   0.01202  0.1984   0.08041  0.03942  0.06676  0.3371   0.05768  0.131    1.37     2.24     0.9785   0.4246   3.123    1.771    7.893    0.031813 0.4125  815.1 920 89.54  69.23  67.45  81.32  81.87  78.95  72.94  80.97  15.65  92.06  41.02  54.27  58.61  89.71  32.51  68.88  96.64  94.06  90.71  93.58  99.32  98.64  85.56  104.6  112.7   53.99   1    0  0.41249  1910.3   815.1  920 0.41249  1910.3   815.1  920 1931.4  1885.7  1882    2044.1  0.00056345 1172.1  