#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  S_W[ 7]  S_W[ 8]  S_W[ 9]  S_W[10]  S_W[11]  S_W[12]  S_W[13]  S_W[14]  S_W[15]  S_W[16]  S_W[17]  S_W[18]  S_W[19]  S_W[20]  S_W[21]  S_W[22]  S_W[23]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 WX2/k7 WX2/k8 WX2/k9 WX2/k10 WX2/k11 WX2/k12 WX2/k13 WX2/k14 WX2/k15 WX2/k16 WX2/k17 WX2/k18 WX2/k19 WX2/k20 WX2/k21 WX2/k22 WX2/k23 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
11 20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       20       0.3      0.52    11.56 920 0.1549 0.07252 0.2672 0.0732 0.05423 0.07709 0.03082 0.09405 0.03149 0.08064 0.04761 0.0754 0.03779 0.1311 0.04672 0.04869 0.355  0.07506 0.3897 0.1504 1.173  0.2027 0.01323 178.2  517.9   -994.3  11.6 0  0.52002  177.54   11.56  920 0.52002  177.54   11.56  920 -724.58 -776.88 -780.53 -206.66 0.017994 619.47  
11 2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    2.707    0.3      0.52    11.56 920 8.455  3.96   14.59  3.996  2.961  4.209  1.683  5.135  1.719  4.403  2.6    4.117  2.063  7.16   2.551  2.658  19.38  4.098  21.27  8.213  64.02  11.07  0.7223 104.4  294.9   -486.3  1    0  0.52     208.2    11.56  920 0.52     208.2    11.56  920 -215.81 -261.54 -265.24 79.135  0.010783 367.95  
11 1.309    0.8123   1.828    0.8142   0.6737   0.9542   0.5578   0.9582   0.7347   0.7956   0.8503   0.7636   0.6148   1.315    0.9364   0.6754   2.152    1.102    1.943    1.256    2.741    1.389    0.3663   0.03571  0.2742  430   920 36.48  105.6  12.64  47.93  36.53  13.65  7.533  12.43  2.803  24.72  10.53  15.62  22.4   24.2   7.709  15.18  19.43  10.57  53.74  53.85  36.6   44.45  273.5  201.9  218.4   -230.6  1    0  0.27416  1951.8   430    920 0.27416  1951.8   430    920 1749.6  1695.8  1692.2  1968    0.00057783 1118.8  
11 0.837    0.9239   0.6658   0.6038   0.445    0.3942   0.1812   0.3586   0.1929   0.4149   0.3787   0.3196   0.3326   0.7245   0.374    0.2963   0.9736   0.4618   1.481    0.9784   1.67     0.9918   0.7132   0.027632 0.2715  711.2 920 56.69  56.08  36.61  30.8   35.3   29.6   15.07  44.09  3.145  43.93  18.82  27.36  19.12  46.78  19.34  45.04  54.48  22.95  67.79  80.11  64.44  74     278.7  197.2  218.4   -77.27  1    0  0.27152  2071.1   711.2  920 0.27152  2071.1   711.2  920 1982.7  1929.5  1925.8  2201.1  0.00045881 1384.1  
11 0.658    0.713    0.422    0.348    0.2798   0.2542   0.09576  0.2662   0.0636   0.2886   0.2357   0.1821   0.1634   0.5512   0.2669   0.235    0.751    0.2987   1.252    0.9169   1.353    0.8845   1.368    0.02741  0.2707  720.5 920 48.91  37.72  57.3   48.38  37.06  24.5   25.48  40.49  1.767  30.8   32.33  50.48  33.88  46.91  27.2   43.92  31.57  17.96  43.43  80.1   57.51  76.89  281    194.9  218.4   10.19   1    0  0.27067  2075.6   720.5  920 0.27067  2075.6   720.5  920 2072.7  2019.7  2016    2291.1  0.00045339 1385.6  
11 0.4767   0.4489   0.3385   0.2559   0.1808   0.151    0.07074  0.1877   0.01853  0.1675   0.1995   0.1454   0.1124   0.4117   0.2072   0.1822   0.4354   0.1788   0.8423   0.848    1.035    0.7956   2.655    0.027324 0.2717  727.8 920 50.39  68.73  48.53  61.67  53.66  32.77  21.23  29.96  3.057  35.65  30.06  53.47  49.1   44.77  9.516  33.74  46.34  7.604  49.76  59.02  64.17  76.86  273.3  194.8  218.4   92.13   1    0  0.27168  2074.7   727.8  920 0.27168  2074.7   727.8  920 2152.4  2099.5  2095.9  2370.8  0.00045337 1392.4  
11 0.3513   0.385    0.2478   0.2119   0.1424   0.1079   0.04602  0.1126   0.008943 0.1062   0.1541   0.1166   0.09369  0.2991   0.09326  0.1214   0.308    0.07195  0.6081   0.667    0.8359   0.7101   5.101    0.027372 0.2717  725.2 920 92.77  93.45  90.58  90     86.54  64.22  50.16  83.28  13.12  88.64  50.36  83.14  70.63  84.78  46.98  76.07  92.57  46.98  95.49  95.38  98.3   96.51  74.03  184.2  218.4   172.2   1    0  0.27168  2075.9   725.2  920 0.27168  2075.9   725.2  920 2202.3  2150.5  2146.9  2420.7  0.00044534 1353.9  
11 0.3567   0.3868   0.2537   0.2138   0.1452   0.1139   0.05145  0.1216   0.01085  0.1115   0.155    0.1186   0.09588  0.3078   0.1181   0.1296   0.3153   0.08942  0.6153   0.6715   0.839    0.708    4.555    0.027175 0.2717  735.8 920 89.98  92.61  86.43  88.35  83.18  57.63  40.14  71.45  8.909  80.47  49.76  80.37  67.45  80.06  29.3   66.71  88.35  30.42  93.26  94.12  97.56  97.08  92.83  186.1  218.4   160.5   1    0  0.27168  2077.7   735.8  920 0.27168  2077.7   735.8  920 2197.2  2145.1  2141.5  2415.6  0.00044471 1370.8  
11 0.3568   0.387    0.2533   0.2139   0.145    0.1128   0.04963  0.1198   0.01018  0.1108   0.1573   0.1185   0.09551  0.3074   0.1086   0.1279   0.3148   0.08414  0.6154   0.6718   0.839    0.7087   4.603    0.02721  0.2717  733.9 920 89.94  92.52  86.7   88.31  83.43  58.78  43.13  73.54  10.12  81.47  48.36  80.48  67.98  80.28  34.64  68.47  88.61  34.35  93.23  94.02  97.56  96.88  90.93  185.7  218.4   163.4   1    0  0.27168  2077.4   733.9  920 0.27168  2077.4   733.9  920 2199    2147    2143.4  2417.4  0.00044475 1367.5  

