-4.18972e-06 1.25599e-07 0.0505464 -0.0278567 3.16035e-06 0.000171634 0.00843538 -0.0244392 0.0253233 -2.1623e-05 3.6147e-07 0.174036 -0.0889165 1.092e-05 0.000588863 0.0289355 -0.0777447 0.0892368 -4.54797e-06 8.17921e-08 0.0499231 -0.0282073 3.20175e-06 0.000173859 0.00853816 -0.02471 0.0256394 1.58793e-06 3.18172e-08 0.0172217 -0.00942249 1.06618e-06 5.75525e-05 0.00284112 -0.00819924 0.00847361 -3.90913e-06 7.86551e-08 0.0303671 -0.0172489 1.95461e-06 0.000105645 0.0052041 -0.0150797 0.0155601 5.44868e-06 -7.7881e-08 -0.0415937 0.023137 -2.61819e-06 -0.000142242 -0.00699351 0.0202956 -0.0209512 8.944e-06 -1.7064e-07 -0.104756 0.0574433 -6.66841e-06 -0.000362594 -0.0177355 0.0500157 -0.0542995 -2.19764e-08 -9.00427e-08 -0.0593793 0.0324723 -3.68819e-06 -0.000200555 -0.00985354 0.028513 -0.0296548 -9.67858e-06 1.71394e-07 0.0911708 -0.0504434 5.81271e-06 0.000315702 0.0154733 -0.0439725 0.0471239 1.55482e-05 -2.76706e-07 -0.145818 0.0773396 -9.24132e-06 -0.000498972 -0.0245447 0.0670781 -0.0759467 1.2151e-06 3.11559e-08 0.00729196 -0.00472116 5.30006e-07 2.91493e-05 0.00141878 -0.00422335 0.00424152 0.170037 -0.538627 -1.83724 -0.545334 -0.181439 -0.332462 0.44665 1.13097 0.629054 -0.987232 1.56166 -0.0907781 