#H S_W[ 1]  S_W[ 2]  S_W[ 3]  S_W[ 4]  S_W[ 5]  S_W[ 6]  S_W[ 7]  S_W[ 8]  S_W[ 9]  S_W[10]  S_W[11]  S_W[12]  S_W[13]  S_W[14]  S_W[15]  S_W[16]  S_W[17]  S_W[18]  S_W[19]  S_W[20]  S_W[21]  S_W[22]  S_W[23]  S_W[24]  S_W[25]  S_W[26]  S_W[27]  S_W[28]  S_W[29]  S_W[30]  S_W[31]  S_W[32]  S_W[33]  S_W[34]  S_W[35]  S_W[36]  S_W[37]  S_W[38]  S_W[39]  S_W[40]  S_W[41]  S_W[42]  S_W[43]  S_W[44]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 WX2/k4 WX2/k5 WX2/k6 WX2/k7 WX2/k8 WX2/k9 WX2/k10 WX2/k11 WX2/k12 WX2/k13 WX2/k14 WX2/k15 WX2/k16 WX2/k17 WX2/k18 WX2/k19 WX2/k20 WX2/k21 WX2/k22 WX2/k23 WX2/k24 WX2/k25 WX2/k26 WX2/k27 WX2/k28 WX2/k29 WX2/k30 WX2/k31 WX2/k32 WX2/k33 WX2/k34 WX2/k35 WX2/k36 WX2/k37 WX2/k38 WX2/k39 WX2/k40 WX2/k41 WX2/k42 WX2/k43 WX2/k44 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
2  42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       42       0.3      4.721   104.9 1976 0.1757 0.3024 0.2228 0.02038 0.08741 0.0128 0.0005501 0.009188 0.01121 0.0129 0.002206 0.04588 0.003271 0.03837 0.2009 0.006284 0.000638 0.004511 0.01595 0.006206 0.006703 0.005534 0.03139 0.01806 0.009067 0.02713 0.02652 0.02297 0.02031 0.001309 0.02471 0.007586 0.02594 0.02218 0.02089 0.0158 0.03498 0.02168 0.04298 0.008557 0.02211 0.09262 0.1664 0.05503 77.49  187.1   -414.4  2    0  4.7215   477.92   104.9  1976 4.7215   477.92   104.9  1976 97.694  30.072  25.951  284.76  0.005919 398.96  
2  5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    5.684    0.3      4.721   104.9 1976 9.595  16.51  12.17  1.113  4.772  0.6989 0.03004 0.5017 0.6119 0.7042 0.1204 2.505  0.1786 2.095  10.97  0.3431 0.03484 0.2462 0.8707 0.3388 0.3659 0.3022 1.714  0.9859 0.495  1.481  1.448  1.254  1.109  0.07147 1.349  0.4142 1.416  1.211  1.14   0.8627 1.909  1.184  2.347  0.4672 1.207  5.056  9.084  3.005  50.27  140.4   -236.4  1    0  4.7213   489.23   104.9  1976 4.7213   489.23   104.9  1976 275.35  218.35  214.22  415.77  0.0046789 295.66  
2  2.407    3.136    3.285    0.871    1.904    0.7693   0.7693   0.7693   0.7693   0.7693   0.7693   1.157    0.7693   2.023    2.646    0.7693   0.7693   0.7693   1.224    0.7693   0.7693   0.7693   0.9349   0.7693   0.7693   0.8068   0.7963   0.7693   0.7693   0.7693   1.054    0.7693   0.9483   0.8386   0.9941   0.7693   1.101    0.8915   1.926    0.7693   0.841    1.488    2.981    1.202    0.070024 2.051   836.5 1976 30.41  52.69  124.7  228.5  126    13.72  177.9  65.81  32.94  57.67  46.71  0.645  361.2  0.2171 1.545  296.6  32.28  1.536  23.7   31.91  3.618  3.791  131.3  29.14  5.504  11.91  0.7007 31.4   117.7  17.16  67.07  297.3  217.6  566.1  6.296  3.554  26.21  24.26  4.581  4.597  67.9   529.4  415.8  123.3  68.97  -81.07  -85.33  1    0  2.0507   3012.9   836.5  1976 2.0507   3012.9   836.5  1976 2892    2827.6  2823.5  2810.9  0.001209 1098.2  
2  1.332    2.366    4.086    1.463    2.198    0.341    1.51     0.6904   0.5063   0.62     0.5898   0.1566   1.675    0.2738   0.3581   1.62     0.4423   0.1041   0.7312   0.4571   0.2548   0.2609   1.131    0.4565   0.1878   0.2827   0.1078   0.438    0.8574   0.4232   1.083    1.363    1.45     2.213    0.3432   0.1932   0.608    0.5529   0.6979   0.1755   1.464    3.511    6.691    1.533    0.046376 2.051   1907  1976 99.37  92.54  80.6   80.96  94.6   69.79  46.2   81.71  76.05  88.78  79.44  35.21  76.15  11.85  84.34  66.84  97.65  83.85  66.44  90.35  32.97  32.97  89.69  82.77  92.33  97.01  38.24  96.87  94.73  56.71  63.5   94.64  93.03  81.26  52.81  56.34  85.96  63.06  34.89  88.32  22.4   95.14  82.55  75.75  67.87  -123    -48     1    0  2.0507   3326.4   1907   1976 2.0507   3326.4   1907   1976 3220.5  3157.2  3153.1  3097.6  0.0011117 2164.5  
2  1.334    2.359    3.81     1.345    2.158    0.3747   1.135    0.6648   0.5038   0.6289   0.5592   0.1186   1.49     0.131    0.3443   1.37     0.444    0.1445   0.7456   0.461    0.3127   0.3127   1.089    0.4594   0.2166   0.2867   0.07744  0.4401   0.8419   0.4328   1.007    1.332    1.409    2.01     0.3733   0.3046   0.6228   0.56     1.032    0.2162   0.8778   3.434    6.13     1.468    0.046362 1.997   1858  1976 129.4  65.58  118.9  223.3  102.1  39.93  116.4  97.01  94.47  144.8  118.3  54.86  216.8  6.956  108.1  129.9  116.7  47.84  138.4  97.28  23.18  23.12  204.7  120.2  35.83  74.16  40.45  107.1  145.3  35.98  149.6  144.2  156.1  159.3  12.88  25.55  98.47  30.14  2.967  43.41  128.5  123.5  120.8  47.14  66.72  -119.3  -46.06  1    0  1.9972   3346.1   1858   1976 1.9972   3346.1   1858   1976 3237.4  3174.6  3170.5  3118.2  0.0010833 2111.5  
2  1.525    1.981    4.351    2.078    2.203    0.304    1.45     0.7002   0.5591   0.815    0.6589   0.1186   2.303    0.05056  0.377    1.648    0.4877   0.1373   1.103    0.4826   0.3204   0.32     1.587    0.5698   0.1536   0.2534   0.06204  0.4667   1.025    0.357    1.621    1.609    1.775    2.656    0.1901   0.2565   0.6759   0.3756   0.5366   0.1809   1.696    3.829    6.827    1.047    0.045739 1.987   1899  1976 104.5  92.47  94.2   91.92  71.56  55.78  75.86  96.75  109.1  102    102.2  56.58  114.1  24.07  117.2  110.3  104.6  42.56  117.3  126.7  22.7   22.65  139.6  118.9  70.55  80.61  54.42  72.9   121.6  32.67  92.39  117.9  119.9  103.1  10.19  41.59  100.5  41.62  0.06126 45.82  56.89  105.8  103.7  70.55  66.61  -122.2  -47.98  1    0  1.9867   3354.2   1899   1976 1.9867   3354.2   1899   1976 3248.3  3186.6  3182.4  3126.1  0.001076 2152    
2  1.565    2.005    4.381    2.018    1.878    0.3046   1.442    0.7314   0.6533   0.8748   0.7037   0.1203   2.518    0.04386  0.4264   1.803    0.5061   0.1242   1.376    0.5822   0.3173   0.3169   1.89     0.6705   0.1641   0.2343   0.06091  0.4078   1.139    0.284    2.109    1.754    1.954    2.8      0.09551  0.31     0.7295   0.3218   0.1048   0.1627   1.707    3.95     7.043    0.915    0.045618 1.987   1909  1976 99.21  90.24  92.95  97.47  98.41  55.55  76.65  88.68  79.89  88.5   89.61  54.94  95.42  31.95  91.64  92.19  97.18  51.96  75.41  87.06  23.15  23.1   98.39  85.85  61.82  94.33  56.47  95.44  98.48  51.61  54.58  99.2   98.95  92.81  40.34  28.47  86.3   56.68  1.606  56.62  56.18  99.4   97.47  92.31  66.62  -126.5  -45.56  1    0  1.9867   3354.8   1909   1976 1.9867   3354.8   1909   1976 3253.5  3193.6  3189.4  3127    0.0010756 2162.2  
2  1.564    2.003    4.379    2.019    1.882    0.3042   1.446    0.7279   0.6383   0.8684   0.7018   0.12     2.509    0.04635  0.4226   1.792    0.5056   0.1275   1.322    0.5714   0.3222   0.3218   1.885    0.6583   0.1599   0.2352   0.06096  0.411    1.138    0.2879   2.056    1.753    1.952    2.79     0.1244   0.276    0.7212   0.336    0.529    0.1683   1.701    3.949    7.044    0.9242   0.045618 1.987   1909  1976 99.26  90.43  93.04  97.41  98.06  55.69  76.23  89.53  83.68  89.79  90.11  55.24  96.14  28.61  93.31  93.34  97.37  49.35  81.61  90.38  22.45  22.4   98.89  89.08  65.09  93.58  56.36  93.97  98.78  50.22  57.43  99.35  99.15  93.47  23.78  35.9   88.3   51.99  0.06298 52.96  56.57  99.45  97.43  90.48  66.72  -122.9  -49.13  1    0  1.9867   3354.8   1909   1976 1.9867   3354.8   1909   1976 3249.9  3188.3  3184.2  3127    0.0010757 2162.5  
2  1.564    2.003    4.379    2.019    1.882    0.3043   1.445    0.7283   0.6404   0.8691   0.7004   0.1201   2.509    0.04529  0.4228   1.792    0.5056   0.1266   1.331    0.5723   0.3176   0.3173   1.886    0.6595   0.1617   0.2352   0.061    0.4108   1.138    0.2876   2.062    1.753    1.952    2.791    0.1096   0.2965   0.7226   0.3319   0.1062   0.1664   1.703    3.949    7.047    0.9234   0.045619 1.987   1909  1976 99.26  90.44  93.04  97.38  97.97  55.65  76.33  89.44  83.15  89.65  90.45  55.2   96.11  29.95  93.2   93.29  97.37  50     80.61  90.08  23.11  23.05  98.87  88.74  63.64  93.61  56.3   94.09  98.77  50.31  57.11  99.34  99.14  93.43  30.63  31.11  87.96  53.28  1.561  54.15  56.43  99.45  97.34  90.63  66.65  -126.3  -45.7   1    0  1.9867   3354.8   1909   1976 1.9867   3354.8   1909   1976 3253.3  3193.3  3189.2  3127    0.0010756 2162.2  

