 0.071304       0.0207101          0.050594        0.092014       
 0.069032       0.0198868          0.049145        0.088919       
 0.066714       0.0190767          0.047637        0.085791       
 0.064349       0.0182811          0.046068        0.082630       
 0.061937       0.0175017          0.044435        0.079439       
 0.059477       0.0167404          0.042736        0.076217       
 0.056968       0.0159996          0.040969        0.072968       
 0.054411       0.015282          0.039129        0.069693       
 0.051804       0.0145909          0.037213        0.066394       
 0.049146       0.0139302          0.035216        0.063077       
 0.046439       0.0133043          0.033135        0.059743       
 0.043680       0.0127186          0.030961        0.056399       
 0.040870       0.012179          0.028691        0.053049       
 0.038007       0.0116923          0.026314        0.049699       
 0.035091       0.0112659          0.023825        0.046357       
 0.032122       0.0109074          0.021215        0.043030       
 0.029100       0.0106246          0.018475        0.039724       
 0.026022       0.0104246          0.015598        0.036447       
 0.022890       0.0103135          0.012576        0.033203       
 0.019702       0.0102956          0.009406        0.029997       
 0.016457       0.0103728          0.006084        0.026830       
 0.013156       0.010545          0.002611        0.023701       
 0.009797       0.0108095         -0.001013        0.020606       
 0.006380       0.0111617         -0.004782        0.017541       
 0.002904       0.0115961         -0.008692        0.014500       
-0.000631       0.012106         -0.012737        0.011475       
-0.004226       0.0126848         -0.016911        0.008458       
-0.007882       0.0133262         -0.021208        0.005444       
-0.011599       0.0140241         -0.025623        0.002425       
-0.015378       0.0147733         -0.030151       -0.000605       
-0.019220       0.0155692         -0.034789       -0.003650       
-0.023124       0.0164079         -0.039532       -0.006716       
-0.027093       0.0172861         -0.044379       -0.009807       
-0.031126       0.0182011         -0.049327       -0.012925       
-0.035224       0.0191506         -0.054375       -0.016074       
-0.039389       0.0201328         -0.059521       -0.019256       
-0.043619       0.0211465         -0.064766       -0.022473       
-0.047918       0.0221903         -0.070108       -0.025727       
-0.052284       0.0232637         -0.075547       -0.029020       
-0.056719       0.0243659         -0.081084       -0.032353       