 0.115448       0.0212871          0.094161        0.136735       
 0.108407       0.0197474          0.088660        0.128154       
 0.101629       0.0183067          0.083322        0.119936       
 0.095110       0.0169617          0.078148        0.112071       
 0.088844       0.015709          0.073135        0.104553       
 0.082826       0.0145452          0.068281        0.097371       
 0.077052       0.0134673          0.063584        0.090519       
 0.071515       0.0124722          0.059043        0.083988       
 0.066212       0.0115575          0.054655        0.077770       
 0.061136       0.0107211          0.050415        0.071857       
 0.056282       0.00996186          0.046320        0.066244       
 0.051645       0.0092793          0.042366        0.060925       
 0.047220       0.00867396          0.038546        0.055894       
 0.043000       0.00814737          0.034852        0.051147       
 0.038980       0.00770192          0.031278        0.046682       
 0.035156       0.00734059          0.027816        0.042497       
 0.031521       0.00706647          0.024455        0.038588       
 0.028071       0.00688204          0.021189        0.034953       
 0.024800       0.00678841          0.018011        0.031588       
 0.021702       0.0067847          0.014918        0.028487       
 0.018773       0.00686779          0.011905        0.025641       
 0.016007       0.00703238          0.008975        0.023040       
 0.013399       0.00727156          0.006128        0.020671       
 0.010945       0.00757752          0.003367        0.018522       
 0.008638       0.00794216          0.000696        0.016580       
 0.006475       0.00835767         -0.001883        0.014833       
 0.004450       0.00881685         -0.004367        0.013267       
 0.002559       0.00931322         -0.006754        0.011872       
 0.000797       0.00984106         -0.009044        0.010638       
-0.000841       0.0103954         -0.011237        0.009554       
-0.002359       0.0109719         -0.013331        0.008613       
-0.003762       0.0115667         -0.015328        0.007805       
-0.005053       0.0121765         -0.017229        0.007124       
-0.006237       0.0127983         -0.019035        0.006561       
-0.007318       0.0134295         -0.020748        0.006111       
-0.008301       0.0140678         -0.022368        0.005767       
-0.009188       0.0147108         -0.023899        0.005523       
-0.009984       0.0153568         -0.025341        0.005373       
-0.010693       0.0160039         -0.026697        0.005311       
-0.011318       0.0166503         -0.027968        0.005333       