 0.013956       0.0318743         -0.017919        0.045830       
 0.019766       0.0296931         -0.009927        0.049459       
 0.024929       0.0276157         -0.002687        0.052545       
 0.029442       0.0256367          0.003805        0.055078       
 0.033300       0.023751          0.009549        0.057051       
 0.036499       0.0219537          0.014545        0.058453       
 0.039035       0.0202404          0.018795        0.059275       
 0.040902       0.0186077          0.022295        0.059510       
 0.042095       0.0170535          0.025042        0.059149       
 0.042608       0.0155784          0.027029        0.058186       
 0.042433       0.0141863          0.028247        0.056619       
 0.041564       0.0128865          0.028677        0.054450       
 0.039992       0.0116966          0.028296        0.051689       
 0.037711       0.0106453          0.027065        0.048356       
 0.034710       0.0097762          0.024934        0.044486       
 0.030982       0.00914879          0.021834        0.040131       
 0.026518       0.00883149          0.017687        0.035350       
 0.021308       0.00888412          0.012424        0.030192       
 0.015344       0.00933538          0.006009        0.024680       
 0.008617       0.0101738         -0.001557        0.018790       
 0.001117       0.0113601         -0.010243        0.012477       
-0.007163       0.0128473         -0.020010        0.005685       
-0.016230       0.0145946         -0.030825       -0.001635       
-0.026092       0.0165718         -0.042664       -0.009520       
-0.036754       0.0187586         -0.055513       -0.017996       
-0.048221       0.021142         -0.069363       -0.027079       
-0.060496       0.023714         -0.084210       -0.036782       
-0.073581       0.0264699         -0.100051       -0.047111       
-0.087474       0.0294066         -0.116881       -0.058068       
-0.102174       0.0325222         -0.134697       -0.069652       
-0.117676       0.0358147         -0.153491       -0.081861       
-0.133971       0.0392818         -0.173253       -0.094689       
-0.151050       0.0429206         -0.193971       -0.108129       
-0.168899       0.0467272         -0.215626       -0.122172       
-0.187501       0.0506965         -0.238198       -0.136805       
-0.206836       0.0548223         -0.261659       -0.152014       
-0.226881       0.059097         -0.285978       -0.167784       
-0.247607       0.0635116         -0.311118       -0.184095       
-0.268983       0.0680557         -0.337039       -0.200927       
-0.290974       0.0727176         -0.363691       -0.218256       