This program produces the input lines required for the MAP_STEEL_DILAT program (commonly known as len3.for) [1] from converted (tsm.out) thermec data and the knowledge of the minimum diliataion time.
| Language: | FORTRAN |
| Product form: | Source code and sample data files; |
| Compiled program for Solaris 2.5, 2.5.1 and 2.6 O.S. on a Sun Sparc computer. |
This program uses the information in a thermec data file to calculate the change in dilatation value, with respect to the initial dilatation, at any specified times after the specified start time (This should correspond to the start time of the transformation.). An average over 3 data points is used for the dilatation values to compensate for fluctuations in the readings. The name of the thermec data file must be supplied as input data to the program. The times (in seconds), after the start time, at which the calculations are to be made, are read by the program from a separate file, called timestep.
None.
No information supplied.
None.
N/A - complete program
THERM = thermec.dat (thermec file, too big to put here) ST = 398.0
file in.len: dilatation temp C time s 0.0000384 385.0 2.0 0.0013275 359.0 4.0 0.0034885 332.0 6.1 0.0043111 312.0 8.0 0.0043605 293.0 10.0 0.0042948 274.0 12.1 0.0041688 255.0 14.0 0.0038398 234.0 16.0 0.0035268 213.0 18.1 0.0032418 195.0 20.0 0.0030001 174.0 22.0 0.0026168 154.0 24.0 0.0023368 135.0 26.0 0.0020405 115.0 28.0 0.0018378 98.0 30.0 0.0016075 88.0 32.1 0.0015305 80.0 34.0 0.0013548 73.0 36.0 0.0013655 68.0 38.1 0.0013218 63.0 40.0
None.
dilatation, thermec, len3
Download source code
Download compiled program
MAP originated from a joint project of the National Physical Laboratory and the University of Cambridge.
MAP Website administration / map@msm.cam.ac.uk