Date and time of run 15-JAN-2007 21:39:49 > 20070115213804 MTDATA 4.74 2004-11-18 12:00, LOG D:\MTDATA\Work\mt51.log > 20070115213804 user2 on DVF-400-* using D:\MTDATA\DVF\mtdata.exe > 20070115213948 MODULE 3 creates MPI file D:\MTDATA\Work\def.mpi > 20070115213949 MODULE 3 reads MPI file D:\MTDATA\Work\def.mpi > 20070115213949 MODULE 3 creates MPR file D:\MTDATA\Work\def.mpr $(Number of lines of title) 8 * DATAFILE = D:\MTDATA\Work\def.mpi - CREATED 21:39:48 15-JAN-2007 * SYSTEM = C,Mn,Ni,Fe, * NUMBER OF PHASES = 23 * NUMBER OF SPECIES = 81 * DATA FILE = D:\MTDATA\Work\def.mpi *** PROBLEM settings *** SYSTEM ELEMENTS : CFeMnNi NUMBER COMPONENT STATUS AMOUNT DELTA REF.P 1 C NORMAL 10.9316 2 Mn #PARA! 41.4103 3 Ni #PARA! 68.7170 4 Fe #PARA! 1675.30 NUMBER PHASE STATUS MODEL 1 DIAMOND_A4 absent PURE SUBSTANCE 2 GRAPHITE absent PURE SUBSTANCE 3 LIQUID absent REDLICH-KISTER 4 BCC_A2 NORMAL SUBLATTICE 5 CBCC_A12 absent SUBLATTICE 6 CEMENTITE absent SUBLATTICE 7 CUB_A13 absent SUBLATTICE 8 FCC_A1 1 M-G SUBLATTICE 9 FE4N absent SUBLATTICE 10 FECN_CHI absent PURE SUBSTANCE 11 HCP_A3 absent SUBLATTICE 12 KSI_CARBIDE absent PURE SUBSTANCE 13 M3C2 absent SUBLATTICE 14 M5C2 absent SUBLATTICE 15 M7C3 absent SUBLATTICE 16 V3C2 absent SUBLATTICE 17 M23C6 absent SUBLATTICE 18 AL5FE4 absent REDLICH-KISTER 19 ORTHORHOMBIC_A20 absent PURE SUBSTANCE 20 TETRAGONAL_U absent PURE SUBSTANCE 21 LAVES_C14 absent SUBLATTICE 22 LAVES_C15 absent SUBLATTICE 23 BCC_B2 absent CHEMICAL ORDERING(C) NUMBER SUBSTANCE STATUS/CONSTRAINT 1 C NORMAL 2 C NORMAL 3 C NORMAL 4 Fe NORMAL 5 Mn NORMAL 6 Ni NORMAL 7 Fe:1 NORMAL 8 Mn:1 NORMAL 9 Ni:1 NORMAL 10 C:2 NORMAL 11 Va:2 NORMAL 12 Fe:1 NORMAL 13 Mn:1 NORMAL 14 Ni:1 NORMAL 15 C:2 NORMAL 16 Va:2 NORMAL 17 Fe:1 NORMAL 18 Mn:1 NORMAL 19 Ni:1 NORMAL 20 C:2 NORMAL 21 Fe:1 NORMAL 22 Mn:1 NORMAL 23 Ni:1 NORMAL 24 C:2 NORMAL 25 Va:2 NORMAL 26 Fe:1 NORMAL 27 Mn:1 NORMAL 28 Ni:1 NORMAL 29 C:2 NORMAL 30 Va:2 NORMAL 31 Fe:1 NORMAL 32 Mn:1 NORMAL 33 Ni:1 NORMAL 34 C:2 NORMAL 35 Va:2 NORMAL 36 Fe5C2 NORMAL 37 Fe:1 NORMAL 38 Mn:1 NORMAL 39 Ni:1 NORMAL 40 C:2 NORMAL 41 Va:2 NORMAL 42 Fe3C NORMAL 43 Fe:1 NORMAL 44 Mn:1 NORMAL 45 C:2 NORMAL 46 Fe:1 NORMAL 47 Mn:1 NORMAL 48 C:2 NORMAL 49 Fe:1 NORMAL 50 Mn:1 NORMAL 51 Ni:1 NORMAL 52 C:2 NORMAL 53 Fe:1 NORMAL 54 Mn:1 NORMAL 55 C:2 NORMAL 56 Fe:1 NORMAL 57 Mn:1 NORMAL 58 Ni:1 NORMAL 59 Fe:2 NORMAL 60 Mn:2 NORMAL 61 Ni:2 NORMAL 62 C:3 NORMAL 63 Fe NORMAL 64 Mn NORMAL 65 Fe NORMAL 66 Fe NORMAL 67 Fe:1 NORMAL 68 Mn:1 NORMAL 69 Ni:1 NORMAL 70 Fe:2 NORMAL 71 Mn:2 NORMAL 72 Ni:2 NORMAL 73 Fe:1 NORMAL 74 Ni:1 NORMAL 75 Fe:2 NORMAL 76 Ni:2 NORMAL 77 Fe:1 NORMAL 78 Ni:1 NORMAL 79 Fe:2 NORMAL 80 Ni:2 NORMAL 81 Va:3 NORMAL UNARY SOURCE Tmin/K Tmax/K C mtsol 298.15 6000.00 C mtsol 298.15 6000.00 C mtsol 298.15 6000.00 Fe mtsol 298.15 6000.00 Mn mtsol 298.15 2000.00 Ni mtsol 298.15 3000.00 Fe:C mtsol 298.15 6000.00 Fe:Va mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Mn:Va mtsol 298.15 2000.00 Ni:C mtsol 298.15 3000.00 Ni:Va mtsol 298.15 3000.00 Fe:C mtsol 298.15 6000.00 Fe:Va mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Mn:Va mtsol 298.15 2000.00 Ni:C NODATA 298.15 298.00 Ni:Va mtsol 298.15 3000.00 Fe:C mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Ni:C mtsol 298.15 3000.00 Fe:C mtsol 298.15 6000.00 Fe:Va mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Mn:Va mtsol 298.15 2000.00 Ni:C NODATA 298.15 298.00 Ni:Va mtsol 298.15 3000.00 Fe:C mtsol 298.15 6000.00 Fe:Va mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Mn:Va mtsol 298.15 2000.00 Ni:C mtsol 298.15 3000.00 Ni:Va mtsol 298.15 3000.00 Fe:C mtsol 298.15 6000.00 Fe:Va mtsol 298.15 6000.00 Mn:C NODATA 298.15 298.00 Mn:Va mtsol 298.15 2000.00 Ni:C NODATA 298.15 298.00 Ni:Va mtsol 298.15 3000.00 Fe5C2 mtsol 298.15 6000.00 Fe:C mtsol 298.15 6000.00 Fe:Va mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Mn:Va mtsol 298.15 2000.00 Ni:C mtsol 298.15 3000.00 Ni:Va mtsol 298.15 3000.00 Fe3C mtsol 298.15 6000.00 Fe:C mtsol 298.15 6000.00 Mn:C mtsol 298.15 6000.00 Fe:C mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Fe:C mtsol 298.15 6000.00 Mn:C mtsol 298.15 2000.00 Ni:C mtsol 298.15 3000.00 Fe:C mtsol 298.15 6000.00 Mn:C mtsol 298.15 6000.00 Fe:Fe:C mtsol 298.15 6000.00 Fe:Mn:C mtsol 298.15 2000.00 Fe:Ni:C mtsol 298.15 3000.00 Mn:Fe:C mtsol 298.15 2000.00 Mn:Mn:C mtsol 298.15 2000.00 Mn:Ni:C NODATA 298.15 298.00 Ni:Fe:C mtsol 298.15 3000.00 Ni:Mn:C NODATA 298.15 298.00 Ni:Ni:C mtsol 298.15 3000.00 Fe mtsol 298.15 6000.00 Mn mtsol 298.15 6000.00 Fe mtsol 298.15 6000.00 Fe mtsol 298.15 6000.00 Fe:Fe mtsol 298.15 6000.00 Fe:Mn NODATA 298.15 298.00 Fe:Ni NODATA 298.15 298.00 Mn:Fe NODATA 298.15 298.00 Mn:Mn mtsol 298.15 2000.00 Mn:Ni NODATA 298.15 298.00 Ni:Fe NODATA 298.15 298.00 Ni:Mn NODATA 298.15 298.00 Ni:Ni mtsol 298.15 3000.00 Fe:Fe mtsol 298.15 6000.00 Fe:Ni NODATA 298.15 298.00 Ni:Fe NODATA 298.15 298.00 Ni:Ni mtsol 298.15 3000.00 Fe:Fe:Va mtsol 298.15 6000.00 Fe:Ni:Va NODATA 298.15 298.00 Ni:Fe:Va NODATA 298.15 298.00 Ni:Ni:Va mtsol 298.15 3000.00 TEMPERATURE : 993.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 Stage 1* only requested *** MULTIPHASE - Stage 1* Results *** Temperature = 993.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7964E+03 FCC_A1 0.0060854 0.0230523 0.0382534 Fe 1.7964E+03 FCC_A1 0.9326089 Gibbs Energy = -7.9269959518E+07 J System Enthalpy = 4.9920639315E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 973.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 973.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7964E+03 FCC_A1 0.0060854 0.0230523 0.0382534 Fe 1.7964E+03 FCC_A1 0.9326089 Gibbs Energy = -7.6680077253E+07 J System Enthalpy = 4.8762489240E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 953.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 953.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7964E+03 FCC_A1 0.0060854 0.0230523 0.0382534 Fe 1.7964E+03 FCC_A1 0.9326089 Gibbs Energy = -7.4113934353E+07 J System Enthalpy = 4.7610563983E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 933.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 933.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7964E+03 FCC_A1 0.0060854 0.0230523 0.0382534 Fe 1.7964E+03 FCC_A1 0.9326089 Gibbs Energy = -7.1571898312E+07 J System Enthalpy = 4.6464870292E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 913.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 913.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 8.2002E+02 BCC_A2 0.0001185 0.0231907 0.0384831 9.7634E+02 FCC_A1 0.0110970 0.0229361 0.0380605 Fe 8.2002E+02 BCC_A2 0.9382077 9.7634E+02 FCC_A1 0.9279064 Gibbs Energy = -6.9074937273E+07 J System Enthalpy = 4.2414155253E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 893.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 893.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.2711E+03 BCC_A2 0.0002005 0.0231888 0.0384799 5.2522E+02 FCC_A1 0.0203281 0.0227220 0.0377052 Fe 1.2711E+03 BCC_A2 0.9381308 5.2522E+02 FCC_A1 0.9192447 Gibbs Energy = -6.6670926335E+07 J System Enthalpy = 3.9266715806E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 873.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 873.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.4416E+03 BCC_A2 0.0002705 0.0231872 0.0384772 3.5473E+02 FCC_A1 0.0297176 0.0225042 0.0373439 Fe 1.4416E+03 BCC_A2 0.9380651 3.5473E+02 FCC_A1 0.9104344 Gibbs Energy = -6.4324499626E+07 J System Enthalpy = 3.7055922962E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 853.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 853.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.5300E+03 BCC_A2 0.0003284 0.0231858 0.0384750 2.6637E+02 FCC_A1 0.0391525 0.0222854 0.0369807 Fe 1.5300E+03 BCC_A2 0.9380108 2.6637E+02 FCC_A1 0.9015814 Gibbs Energy = -6.2024606552E+07 J System Enthalpy = 3.5159759939E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 833.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 833.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.5834E+03 BCC_A2 0.0003742 0.0231848 0.0384732 2.1295E+02 FCC_A1 0.0485527 0.0220673 0.0366189 Fe 1.5834E+03 BCC_A2 0.9379678 2.1295E+02 FCC_A1 0.8927610 Gibbs Energy = -5.9767089516E+07 J System Enthalpy = 3.3425589042E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 813.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 813.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.6189E+03 BCC_A2 0.0004082 0.0231840 0.0384719 1.7750E+02 FCC_A1 0.0578623 0.0218514 0.0362606 Fe 1.6189E+03 BCC_A2 0.9379359 1.7750E+02 FCC_A1 0.8840256 Gibbs Energy = -5.7549869830E+07 J System Enthalpy = 3.1795604452E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 793.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 793.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.6439E+03 BCC_A2 0.0004309 0.0231835 0.0384710 1.5249E+02 FCC_A1 0.0670428 0.0216385 0.0359073 Fe 1.6439E+03 BCC_A2 0.9379146 1.5249E+02 FCC_A1 0.8754114 Gibbs Energy = -5.5371757146E+07 J System Enthalpy = 3.0241957354E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 773.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 773.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.6623E+03 BCC_A2 0.0004430 0.0231832 0.0384706 1.3403E+02 FCC_A1 0.0760683 0.0214292 0.0355599 Fe 1.6623E+03 BCC_A2 0.9379032 1.3403E+02 FCC_A1 0.8669426 Gibbs Energy = -5.3232028899E+07 J System Enthalpy = 2.8748937428E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 753.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 753.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.6764E+03 BCC_A2 0.0004454 0.0231831 0.0384705 1.1993E+02 FCC_A1 0.0849220 0.0212238 0.0352192 Fe 1.6764E+03 BCC_A2 0.9379010 1.1993E+02 FCC_A1 0.8586350 Gibbs Energy = -5.1130247656E+07 J System Enthalpy = 2.7306637927E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 733.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 733.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.6875E+03 BCC_A2 0.0004390 0.0231833 0.0384707 1.0888E+02 FCC_A1 0.0935934 0.0210227 0.0348854 Fe 1.6875E+03 BCC_A2 0.9379070 1.0888E+02 FCC_A1 0.8504985 Gibbs Energy = -4.9066170096E+07 J System Enthalpy = 2.5908281121E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 713.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 713.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.6963E+03 BCC_A2 0.0004249 0.0231836 0.0384713 1.0003E+02 FCC_A1 0.1020767 0.0208259 0.0345589 Fe 1.6963E+03 BCC_A2 0.9379202 1.0003E+02 FCC_A1 0.8425384 Gibbs Energy = -4.7039697104E+07 J System Enthalpy = 2.4548937862E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 693.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 693.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7036E+03 BCC_A2 0.0004043 0.0231841 0.0384721 9.2806E+01 FCC_A1 0.1103695 0.0206336 0.0342398 Fe 1.7036E+03 BCC_A2 0.9379396 9.2806E+01 FCC_A1 0.8347572 Gibbs Energy = -4.5050844527E+07 J System Enthalpy = 2.3224851962E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 673.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 673.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7095E+03 BCC_A2 0.0003782 0.0231847 0.0384731 8.6815E+01 FCC_A1 0.1184715 0.0204457 0.0339279 Fe 1.7095E+03 BCC_A2 0.9379640 8.6815E+01 FCC_A1 0.8271549 Gibbs Energy = -4.3099725370E+07 J System Enthalpy = 2.1933055606E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 653.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 653.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7146E+03 BCC_A2 0.0003480 0.0231854 0.0384742 8.1774E+01 FCC_A1 0.1263843 0.0202622 0.0336234 Fe 1.7146E+03 BCC_A2 0.9379924 8.1774E+01 FCC_A1 0.8197301 Gibbs Energy = -4.1186538796E+07 J System Enthalpy = 2.0671135127E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 633.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 633.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7189E+03 BCC_A2 0.0003149 0.0231861 0.0384755 7.7476E+01 FCC_A1 0.1341106 0.0200830 0.0333260 Fe 1.7189E+03 BCC_A2 0.9380234 7.7476E+01 FCC_A1 0.8124804 Gibbs Energy = -3.9311563544E+07 J System Enthalpy = 1.9437082161E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 613.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 613.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7226E+03 BCC_A2 0.0002801 0.0231870 0.0384768 7.3765E+01 FCC_A1 0.1416539 0.0199080 0.0330357 Fe 1.7226E+03 BCC_A2 0.9380561 7.3765E+01 FCC_A1 0.8054024 Gibbs Energy = -3.7475154356E+07 J System Enthalpy = 1.8229193039E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 593.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 593.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7258E+03 BCC_A2 0.0002447 0.0231878 0.0384782 7.0524E+01 FCC_A1 0.1490180 0.0197372 0.0327523 Fe 1.7258E+03 BCC_A2 0.9380893 7.0524E+01 FCC_A1 0.7984925 Gibbs Energy = -3.5677740662E+07 J System Enthalpy = 1.7046001331E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 573.1500 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 10.93165 41.41032 68.71699 1675.304 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 0.1313000 2.275000 4.033000 93.56070 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 993.150 to 573.150 by -20.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 573.1500 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg C undef undef 1.093165E+01 1.313000E-01 Mn undef undef 4.141032E+01 2.275000E+00 Ni undef undef 6.871699E+01 4.033000E+00 Fe undef undef 1.675304E+03 9.356070E+01 Total 1.796363E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles C Mn Ni 1.7287E+03 BCC_A2 0.0002097 0.0231886 0.0384795 6.7660E+01 FCC_A1 0.1562075 0.0195705 0.0324756 Fe 1.7287E+03 BCC_A2 0.9381221 6.7660E+01 FCC_A1 0.7917465 Gibbs Energy = -3.3919827036E+07 J System Enthalpy = 1.5886227859E+07 J