PPT Slide
TiN
TiN
Ti(N,C)
Ti(N,C)
Ti(Mo)C
TiN
TiC
ferrite
a)
b)
Globular particles
Ti(Mo)C
EM10Ti (9Cr 1Mo 0.1C 0.17Ti)
Steel normalised at 1200 °C/30min and quenched