EM10Ti (9Cr 1Mo 0.1C 0.17Ti)
Concentration profiles (obtained with a micro probe analyser)
of Cr, Mo, Si and Ti within the matrix of the steel normalised at 1150°C/ 30 min.
Ti is in solid solution.