The results of Moorthy et al. related peak position to average grain size
They suggested that this was due to reduction in grain boundary energy on tempering
It is often observed that other magnetic properties depend on grain size
But this may be because of changes in grain boundary structure rather than grain size itself
This is a subject of investigation at the moment [6]