Effect of Alloy Composition and
Casting Conditions on Intermetallics
Their composition and crystallographic structure depends upon the alloy composition and casting velocity of the ingot and cooling rate of the melt.
- The type of intermetallics can change during processing
 
Their size depends on casting velocity
- Increasing the casting velocity decreases particle size. 
 - Size of particles affects final product performance (recrystallisation, can scoring).
 