0.8 kJ/mm heat input. Montage with weld metal on the right and heat-affected zone on the left. The photograph was taken at position 1 of the weld metal, along a horizontal traverse which covers the 'recrystallised' region where weld-beads overlap, as illustrated in the schematic drawing.