Provenance of Data

C. S. Downs,
Phase Transformations Group,
Department of Materials Science and Metallurgy,
University of Cambridge,
Cambridge CB2 3QZ, U.K.

Added to MAP: September 2001.

Top | Next

Purpose

Provides dilatometric data on the transformation from austenite of 3.5Ni steel during continuous cooling at different cooling rates.

Top | Next | Prev

Description

The data are split into the separate cooling rates, 1, 2, 4, 8, 16, 32 C/s.

Chemical data are also supplied.

Format of data in file 35Ni-b.txt

Column 1: is the sample ID.

Column 2: is Carbon concentration / weight %.

Column 3: is Silicon concentration / weight %.

Column 4: is Manganese concentration / weight %.

Column 5: is Sulphur concentration / weight %.

Column 6: is Phosporus concentration / weight %.

Column 7: is Nickel concentration / weight %.

Column 8: is Chromium concentration / weight %.

Column 9: is Molybdenum concentration / weight %.

Column 10: is Vanadium concentration / weight %.

Column 11: is Cobalt concentration / weight %.

Column 12: is Tungsten concentration / weight %.

Column 13: is Niobium concentration / weight %.

Column 14: is Nitrogen concentration / weight %.

Column 15: is Oxygen concentration / weight %.

Column 16: is Temperature / C.

Column 17: is Dilatation Delta L/L /dimensionless.

Column 18: is Time.

Top | Next | Prev

References

Top | Next | Prev

Further Comments

None.

Top | Next | Prev

Keywords

materials, data, dilatation, dilatometric data, austenite, transformation, steel, cooling, cooling rate.

Top | Next | Prev

Download

Download data

Top | Prev


MAP originated from a joint project of the National Physical Laboratory and the University of Cambridge.

MAP Website administration / map@msm.cam.ac.uk

Top | Data Library Index | MAP Homepage Valid HTML 3.2!