|  | Materials Algorithms ProjectMaterials Data Library
 | ![[A logo showing the University of Cambridge Crest]](https://www.phase-trans.msm.cam.ac.uk/Univ.jpg)
 | 
    
    
    This library contains a selection of data files, intended to act as input for many of the programs contained elsewhere on the site.
    Format of documentation within this library.
    
    Datasets available
    
    
        
        
        - MAP_DATA_ADI_RETAINED-AUSTENITE
- The dataset contains 1910 X-ray diffraction measurements of retained austenite in austempered ductile cast iron (ADI) for a large number of cast iron compositions and heat treatments.
 
- MAP_DATA_AUSTENITIC_STMECH
- The yield and ultimate tensile strength data on austenitic stainless steels as a function of test temperature, chemical composition and heat treatment temperatures.
 
- MAP_DATA_CREEP_RUPTURE
- Provides 2066 creep rupture test results of steels (mainly of two kinds of steels: 2.25Cr and 9-12 wt% Cr ferritic steels).
 
- MAP_DATA_FAT_NI_MAT
- Provides data on the fatigue crack growth rate in nickel base superalloys.
 
- MAP_DATA_SURFACE_TENSION
- This code calculates the variation of surface tension and temperature dependence of surface tension (surface tension coefficient) with temperature for the following cases: (a) pure iron and (b) Fe-S binary alloy system, with a given sulphur content.
 
- MAP_DATA_THERMAL
- Thermal conductivity data for steel.
 
- MAP_DATA_THERMAL10
- Thermal conductivity data for steel.
 
    
    
        
        
        - MAP_DATA_HARDFACE
- Provides composition and microstructure data for hard facing alloys produced by several methods.
 
- MAP_DATA_WELD
- Provides chemical composition and mechanical property data for a collection of all weld metal deposits.
 
- MAP_DATA_WELD_HOT_MAT
- Contains data on the solidification hot cracking of welds in impure low-alloy steels.
 
- MAP_DATA_WELD_INCLUSIONS
- Provides chemical and geometrical data on oxide inclusions in low-alloy, ferritic steel welds.
 
- MAP_DATA_WELD_MAT
- Contains weld metal chemical analysis data (wt% and ppm by wt) and Charpy toughness values (in Joules).
 
    
    
        
        
        - MAP_DATA_AC
- Provides dilatometric data on the austenite transformation of wrought steels and weld deposits on heating at differing rates.
 
- MAP_DATA_AC_MS
- Provides dilatometric data on the austenite transformation (on heating; three different rates) and the martensite transformation (on rapid cooling) of wrought steels and weld deposits.
 
- MAP_DATA_ADI_KINETIC
- Provides dilatometric data on the kinetics of bainite formation in nodular iron for different austenitising temperatures and times, and austempering temperatures.
 
- MAP_DATA_AUSTENMAT
- Provides data on formation of austenite in steels.
 
- MAP_DATA_BAINITE_ISO
- Provides kinetics of isothermal bainite transformation at 375, 416 and 450¡C for a steel of composition: Fe-0.11C-1.50Si-1.53Mn-0.008P-0.006S-0.043Sol.Al-0.035 wt.%.
 
- MAP_DATA_BAINITE_NORM
- Provides normalised kinetics of isothermal bainite transformation at 416¡C for a steel of composition: Fe-0.11C-1.50Si-1.53Mn-0.008P-0.006S-0.043Sol.Al-0.035 wt.% after intercritically annealing at 750¡C for 1 min, 4 mins or 1 hour.
 
- MAP_DATA_BAIN_MECH_MAT
- Provides dilatometric data on the mechanical stabilisation of the bainite transformation when it occurs in plastically deformed austenite and on the martensite start temperature of the austenite which is left untransformed after completion of bainite transformation at 475 degrees centigrade.
 
- MAP_DATA_CONTINUOUS_COOLING
- Provides dilatometric data on the bainite transformation in bainitic steels continuously cooled at 0.1¡C/s between 50¡C above the predicted bainite start, and the predicted martensite start temperature.
 
- MAP_DATA_DILATATION_1CrSTEEL
- Provides dilatometric data on the transformation from austenite of 1Cr steel during continuous cooling at different cooling rates.
 
- MAP_DATA_DILATATION_2CrSTEEL
- Provides dilatometric data on the transformation from austenite of 2Cr steel during continuous cooling at different cooling rates.
 
- MAP_DATA_DILATATION_10CrSTEEL
- Provides dilatometric data on the transformation from austenite of 10Cr steel during continuous cooling at different cooling rates.
 
- MAP_DATA_DILATATION_35NiSTEEL
- Provides dilatometric data on the transformation from austenite of 35Ni steel during continuous cooling at different cooling rates.
 
- MAP_DATA_DILATATION_FSTEEL
- Provides dilatometric data on the transformation from austenite of 'F' steel during continuous cooling at different cooling rates.
 
- MAP_DATA_FORGING_ISO
- Provides dilatometric data on the isothermal decomposition of austenite at 973 K, 913 K and 873 K in a medium carbon microalloyed forging steel of composition: 0.37C - 1.45Mn - 0.56Si - 0.04Cr - 0.025Mo - 0.11V - 0.14Cu - 0.015Ti. Data for two different prior austenite grain sizes are supplied.
 
- MAP_DATA_HCM2S
- Provides dilatometric data on the transformation of austenite during continuous cooling at different (constant) cooling rates, for a power plant steel known commercially as HCM2S. The steel is manufactured by Sumitomo Metals in Japan and is used for making boilers in power plant.
 
- MAP_DATA_MS
- Provides dilatometric data on the martensite transformation of wrought steels and weld deposits on rapid cooling.
 
- MAP_DATA_MS_2004
- A database for the Ms temperature of steels as a function of chemical composition.
 
- MAP_DATA_SEGREGATE
- Provides dilatometric data on the transformation of austenite during continuous cooling at different (constant) cooling rates, for a chemically segregated steel and its homogenised equivalent. The homogenised steel was heat treated at 1200 oC for 48 hours in order to minimise concentration gradients.
 
- MAP_DATA_THERMEC_DILAT
- Provides dilatometric data on the martensitic transformation when it occurs in elastically or plastically deformed austenite.
 
    
    
        
        
        - MAP_DATA_LATTMISFIT
- Provides data necessary to create a neural network model to predict lattice mismatch in nickel-based superalloys.
 
- MAP_DATA_NEURAL_MS
- Provides a database giving Ms data for steels of various composition, and a trained neural network model (provided as a spreadsheet) for calculating Ms temperatures for steels of arbitrary composition.
 
- MAP_DATA_WELDHOT
- Complete dataset of weights for neural network analysis of solidification cracking of welds.
 
- MAP_DATA_WELDNEURAL
- Complete datasets for neural network analysis of weld toughness.
 
[Back to top]
    
    
    
        
        
        - MAP_DATA_MTDATA_CAPILLARITY
- To allow calculation of capillarity corrected equilibrium with thermodynamic calculation software such as MT-DATA.
- Language: FORTRAN
 
 
[Back to top]