C. S. Downs,
Phase Transformations Group,
Department of Materials Science and Metallurgy,
University of Cambridge,
Cambridge CB2 3QZ, U.K.
Added to MAP: September 2001.
Provides dilatometric data on the transformation from austenite of 10Cr steel during continuous cooling at different cooling rates.
The data are split into the separate cooling rates, 1, 2, 4, 8, 16, 32 C/s.
Chemical data are also supplied.
Format of data in file 35Ni-b.txt
Column 1: is the sample ID.
Column 2: is Carbon concentration / weight %.
Column 3: is Silicon concentration / weight %.
Column 4: is Manganese concentration / weight %.
Column 5: is Sulphur concentration / weight %.
Column 6: is Phosporus concentration / weight %.
Column 7: is Nickel concentration / weight %.
Column 8: is Chromium concentration / weight %.
Column 9: is Molybdenum concentration / weight %.
Column 10: is Vanadium concentration / weight %.
Column 11: is Cobalt concentration / weight %.
Column 12: is Tungsten concentration / weight %.
Column 13: is Niobium concentration / weight %.
Column 14: is Nitrogen concentration / weight %.
Column 15: is Oxygen concentration / weight %.
Column 16: is Temperature / C.
Column 17: is Dilatation Delta L/L /dimensionless.
Column 18: is Time.
None.
materials, data, dilatation, dilatometric data, austenite, transformation, steel, cooling, cooling rate.
MAP originated from a joint project of the National Physical Laboratory and the University of Cambridge.
MAP Website administration / map@msm.cam.ac.uk