H. Fujii, H.K.D.H. Bhadeshia,
Phase Transformations Group,
Department of Materials Science and Metallurgy,
University of Cambridge,
Cambridge, U.K.
Provides data on the fatigue crack growth rate in nickel base superalloys.
The tar file contains data on the fatigue crack growth rate in nickel base superalloys as a function of 51 variables. File Fatigue.nickel.superalloy.data has the actual data, while Fatigue.nickel.superalloy.info contains an ASCII text version of this explanation.
The data are arranged in columns as follows :-
| Column | Data | |
|---|---|---|
| 1 | da/dN, the crack growth distance (micrometers) per fatigue cycle. | |
| 2 | Logarithm to base 10 of da/dN. | |
| 3 | Stress intensity range in MPa/(sqrt. m). | |
| 4 | Logarithm to base 10 of the stress intensity range. | |
| 5 | Temperature in Kelvin. | |
| 6, 7 | Minimum and Maximum grain size in micrometers. | |
| 8 | Difference in grain size between major and minor phase. | |
| 9, 10, 11 | First heat treatment temperature (K), time (hours) and cooling rate (K/s). | |
| 12, 13, 14 | Second heat treatment temperature (K), time (hours) and cooling rate (K/s). | |
| 15, 16, 17 | Third heat treatment temperature (K), time (hours) and cooling rate (K/s). | |
| 18 | Frequency in Hertz. | |
| 19 | Loading time in seconds. | |
| 20 | Unloading time in seconds. | |
| 21 | Load shape. | |
| 22 | Test atmosphere pressure. | |
| 23 | "R-ratio", a fatigue parameter. | |
| 24 | Short or long crack growth (0 or 1). | |
| 25 | Sample thickness in mm. | |
| 26 | Yield strength in MPa. | |
| 27-53 | give concentrations of elements in the nickel, weight percent :- | |
|
Nickel Chromium Cobalt Molybdenum Aluminium Titanium Iron Carbon Boron Zirconium Silicon Niobium Manganese Copper Phosphorus Calcium Magnesium Sulphur Tin Lead Bismuth Silver Tungsten Tantalum Hafmium Rhenium Yttrium Oxide (Y2O3) |
||
None.
materials, data, fatigue, crack, growth, growth rate, nickel, superalloy