![[MAP Logo]](../../maplogo1.gif) 
*TC is now with the Materials Engineering Department, Parsons Power Generation Systems Ltd, Heaton Works, Shields Road, Newcastle Upon Tyne, NE6 2YL
Provides dilatometric data on the martensite transformation of wrought steels and weld deposits on rapid cooling.
The tar file msdb.tar contains three files. File msdb.data contains the chemical composition of the steels studied followed by three measured martensite start temperatures. Files msdb.info and msdb.tex contain, respectively, text and plain TeX versions of this documentation.
Column 1 is Sample ID.
Column 2 is Carbon concentration (weight%)
Column 3 is Silicon concentration (weight%)
Column 4 is Manganese concentration (weight%)
Column 5 is Sulphur concentration (weight%)
Column 6 is Phosphorus concentration (weight%)
Column 7 is Nickel concentration (weight%)
Column 8 is Chromium concentration (weight%)
Column 9 is Molybdenum concentration (weight%)
Column 10 is Vanadium concentration (weight%)
Column 11 is Cobalt concentration (weight%)
Column 12 is Tungsten concentration (weight%)
Column 13 is Niobium concentration (weight%)
Column 14 is Nitrogen concentration (weight%) (N if not available)
Column 15 is Oxygen concentration (weight%) (N if not available)
Column 16 is Measured MS
Column 17 is Measured MS
Column 18 is Measured MS
None.
materials, data, dilatation, dilatometric data, martensite, transformation, wrought, steel, weld deposit, weld, cooling
MAP originated from a joint project of the National Physical Laboratory and the University of Cambridge.
MAP Website administration / map@msm.cam.ac.uk