Materials Algorithms Project
|
Subhankar Das Bakshi
Phase Transformations Group,
Department of Materials Science and Metallurgy,
University of Cambridge,
Cambridge CB3 0FS, U.K.
E-mail: sd444@cam.ac.uk or subhankar.dasbakshi@gmail.com
Added to MAP: April 2014.
To calculate the distribution of forces and stresses during rolling contact of to rigid, parallel and flat cylinders assuming Hertzian contact between the mating surfaces under various conditions of slip. To estimate the magnitude and distribution of normal and tangential forces acting over the Hertzian contact half-width and subsequently calculates the tangential, normal and shear stresses under plane strain condition. A range of stress distribution from perfect rolling to perfect sliding between mating cylinders can be calculated.
| Language: | C source code |
| Product form: | Source code |