The phenomenological theory of martensite crystallography has been used in conjunction with the Patel and Cohen model to estimate the transformation texture that develops when martensite or bainite grow under the influence of an external stress, but also to calculate the orientations of the habit planes of the selected variants of martensite.
Tata Search, Vol. 2 (2009) 226-232

| ε-carbide | Mathematical Models | 3d | Cyclic | Bain | 
| Residual stress | TRIP | Thermal stability | Hot-strength | Strain partitioining | 
| Uphill diffusion | Tiny | Mechanicallly Alloyed | Topology | Retained Austenite | 
| PT Group Home | Materials Algorithms |