Estimation of the Fracture Toughness of Tempered Nanostructured Bainite

A. Al Hamdany, D. Al Fattal, T. A. Jabbar and H. K. D. H. Bhadeshia

Abstract

Fine structures consisting of a mixture of extremely thin bainite plates embedded in a matrix of austenite, are now a commercial proposition. Whereas the phase transformation theory for such structures is fairly well established, the understanding of their mechanical properties is not. The present work is an attempt to express the fracture toughness of such steels using a neural network method exploiting data available for martensitic and ordinary bainitic steels. It is demonstrated that in spite of uncertainties, the model captures reasonable trends and is able to estimate unseen experimental results on the nanostructured bainite.

Materials Science and Technology, 28 (2012) 685-689

Download paper

Download related papers

Dowload data

fracture toughness of superbainite






Envelope Coefficients Filling welds Hot Delta
Satoh Fields Piping European welds Poles
Mixed Creep Extraordinary ductility Problems Mechanical stabilisation

PT Group Home Materials Algorithms