Yan Pei and Harry are at the Linepipe workshop organised in Moscow by CBMM of Brazil. Harry took the opportunity for discussions and experiments at MiSIS (Moscow Institute for Iron and Steel).

Russian currency |

|

|

Abrasive wear test sample |

|

|

|

|

Tim O'Connor, Olga Ushkanova and Sergey Kaloshkin, at MiSIS, Moscow |

Tim is a humanities Professor, and now a metallurgist, handling an important sample of steel |

Here Tim, who is the Vice Rector of MiSIS, kindly helps to clear our lunch utensils |

Abrasive wear test. The pin has a 52100 ball at the end, and the disc is the test sample |

|

|

The equipment for the abrasion test, at MiSIS in Moscow |

The disc in position |

|

The abrasion after the test |

Moscow in early April, like the U.K., had significant snow |

|

|

|

|

Vodka |

|

The workshop |

|

|

There was simultaneous translation available |

|

|

|

Yan Pei on the podium, waiting for her turn to give the lecture |

Yan Pei in action |

This is the russian translation of her TTT diagram |

Phil Kirkwood indulging in lunch |

Pipe laying ship |

|

|