Drs Subrata Mukherjee and Sourabh Chatterjee (PT Group member) win the Tata Innovista Award for work on bake-hardening high-strength, low-alloy steel. The new material is suited to automotive applications, competing against the transformation-induced plasticity and dual phase steels.
![]() |
![]() |
|