An experiment designed to produce a range of plastic strains in a single specimen that is forged from a well-defined shape into a flat disc. These images and the movie have kindly been provided by Martin Kearney (Sheffield Forgemasters) and Dan Cogswell (Rolls-Royce Marine).
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |