Minature Tensile Tests
H. K. D. H. Bhadeshia
These photographs were taken at the National Institute for Materials Science in Tsukuba, Japan.
Minature tensile test (or creep test) specimen
This is a small, home made, thermomechanical simulator for the minature tensile tests. The strain is measured using a laser.
The minature samples are spark eroded from a solid block