Jack Christian's contributions to the theory of transformations in metals and alloys are distinguished by their lasting value and standard of scholarship. This paper is a short celebration of his far-reaching influence on the theory of martensitic phase transformations.
Journal de Physique IV, Vol. 112 (2003) 17-25.
![]() |
|
![]() |