Steel covered in snow.
|
Steel covered in snow.
|
Steel covered in snow.
|
|
The hot-rolling mill.
|
Hot-rolling mill.
|
|
Hot coils.
|
Bars of steel.
|
The bar straightening device with eccentric rolls.
|
|
The river Emma, crystal clear water. Hans Roelofs.
|
|
All of the steel is produced from recycled scarp.
|
A ladle for about 12 tonnes of steel.
|
The ladle is heated up before pouring in molten steel in order to avoid exposing the ceramic lining to thermal shock.
|
The ceramic lining inside the ladle - the bricks towards the top are different, designed to resist any aggressive slag.
|
The electric arc furnace with carbon electrodes.
|
Oxygen being blown into the molten steel.
|
In the metallography laboratory.
|
Continuously cast billets used to make long products.
|
Stainless steel inside the double-decker train from Luzern to Zurich airport.
|
The Macintosh in Switzerland.
|
|