|   A brittle crack forming some 14 h after manual metal arc welding of a Jumbo H-beam. Photograph courtesy of Professor Nobutaka Yurioka.
 |   The failure of a beam (in a building) during the Hanshin earthquake. Photograph courtesy of Professor Nobutaka Yurioka.
 | 
   
    |   The failure of a column beam connection during the Hanshin earthquake. Photograph courtesy of Professor Nobutaka Yurioka.
 |   Column to column joining using the manual metal arc welding process. Photograph courtesy of Professor Nobutaka Yurioka.
 | 
   
    |   A cylinder column, welded, for the Yokohama Minato Mirai 21 building, which is 79 stories above ground and the tallest skyscraper in Japan (971 feet). Photograph courtesy of Professor Nobutaka Yurioka.
 |   Yokohama Minato Mirai 21 building,  during the construction stage. Photograph courtesy of Professor Nobutaka Yurioka.
 | 
   
    |   Yokohama Minato Mirai 21 building,  during the construction stage. Photograph courtesy of Professor Nobutaka Yurioka.
 |   The completed Yokohama Minato Mirai 21 building. Photograph courtesy of Professor Nobutaka Yurioka.
 |