The crystal structure of lithium niobate, space group R3c and lattice parameters 0.5418 and 1.3863 nm (H. E. Megaw, Acta Cryst. A24 [1968] 583). The chemical formula is LiNbO3.
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
Download movie Download Crystalmaker file Coordinates Structure |
![]() |
|
![]() |