High-Strength Steels
H. K. D. H. Bhadeshia
Abstract
Systematic alloy design combined with innovative technology has led to the successful exploitation of new ultra-high strength steels. The physical metallurgy of some of the latest of these strong steels is summarised, with a view to reflecting the exciting state of both the basic research and the commercial enterprise behind the developments.
Future Aspects of Metals and Ceramics,
Institute of Materials,
eds. J. A. Charles, G. W. Greenwood and G. C. Smith, 1992, pp. 25-74.
Download PDF file of paper.
Related Papers
-
"Hard Bainite"
ISIJ International, Vol. 43 (2003) 1238-1243.
C. Garcia Mateo, F. G. Caballero and H.K.D.H. Bhadeshia
-
"Effect of Plastic Deformation on the Formation of Acicular Ferrite"
Materials Science and Engineering A, Vol. 360A, 2003, 249-257.
C. H. Lee, H. K. D. H. Bhadeshia and H.-C. Lee
-
"Acceleration of Low-Temperature Bainite"
ISIJ International, Vol. 43 (2003) 1821-1825..
C. Garcia Mateo, F. G. Caballero and H.K.D.H. Bhadeshia
-
"Three-Dimensional Atom Probe Analysis of Carbon Distribution in Low-Temperature Bainite"
Scripta Materialia, Vol. 50, 2004, 1277-1281.
M. Peet, S. S. Babu, M. K. Miller and H. K. D. H. Bhadeshia
-
"Developments in Martensitic and Bainitic Steels: Role of The Shape Deformation"
Materials Science and Engineering A, Vol. 378A, 2004, pp. 34-39.
H. K. D. H. Bhadeshia
-
"Nucleation Theory for High-Carbon Bainite"
Materials Science and Engineering A, Vol. 378A, 2004, pp. 289-292.
C. Garcia-Mateo and H. K. D. H. Bhadeshia
-
"Tempering of a Hard Mixture of Bainitic Ferrite and Austenite"
Materials Science and Technology, Vol. 20, 2004, 814-818.
C. Garcia-Mateo, M. Peet, F. G. Caballero and H. K. D. H. Bhadeshia
-
"Large Chunks of Very Strong Steel"
Millenium Steel, Vol. 5, 2004, 25-28.
Also published in Spanish; Metalurgia e Materiais, 61 (2005) 106-109. Translated by Professor Fernando Rizzo.
H. K. D. H. Bhadeshia
-
"Kinetics of the Bainite Transformation"
Proceedings of the Royal Society of London, Vol. A460, 2004, 1710-1722.
H. Matsuda and H. K. D. H. Bhadeshia
-
"Bainite formation influenced by large stress"
Materials Science and Technology, Vol. 20, 2004, 1499-1505.
K. Hase, C. Garcia-Mateo and H. K. D. H. Bhadeshia
-
"Effect of 30 Tesla Magnetic Field on Transformations in a Novel Bainitic Steel"
Scripta Materialia, Vol. 52, 2004, pp. 461-466.
R. A. Jaramillo, S. S. Babu, G. M. Ludtka, R. A. Kisner, J. B. Wilgen, G.
Mackiewicz-Ludtka, D. M. Nicholson, S. M. Kelly, M. Murugananth and H.
K. D. H. Bhadeshia
-
"Very Strong Bainite"
Current Opinion in Solid State and Materials Science, Vol. 8, 2005, pp. 251-257.
F. G. Caballero and H. K. D. H. Bhadeshia
 |
 |